COMPARISON OF THE PHYSICAL PROPERTIES OF FOUR KINDS OF ACRYLIC RESIN DENTURE TEETH
4종 아크릴릭 레진 인공치의 물리적 성질에 관한 비교
- Hwang, Jong-Woo (Dept. of Prosthodontics School of Dentistry, Chosun University) ;
- Chung, Chae-Heon (Dept. of Prosthodontics School of Dentistry, Chosun University) ;
- Ko, Yeong-Mu (Dept. of Dental Materials, Chosun University)
- Published : 1995.04.01
Abstract
To compare the wear resistance of four kinds of commercial acrylic resin teeth [SR-Orthosit PosterioresR(Ivoclar Co., Liechtenstein), Endura PosteriorR(Shofu Inc. Japan), trubyte IPN teethR(Dentsply International Inc., York,), Trubyte BiotoneR(dentsply Inermational Inc. Brazil) by means of the toothbrush abrasion method, the artificial resin teeth were embedded in epoxy resin with the occlusal surfaces aligned in one plane for a total of 40 blocks. There after, each lock was mounted in the arm of the toothbrush abrasion machine(K 236, Japan). Wear measurements were made on the three preconditioned states. Those were as follows : no treatment specimens, thermocycled specimens, and thermocycled specimens which were immeresed applied load of 400g during the buring the brushing cycle. At the end of the 30,000-stroke cycle, each specimen was removed, and weighed. The microhardness of four kinds of commercial resin teeth were determined by means of microhardness tester. Microhardness tests were performed on te no treatment specimens, thermocycled specimens, and thermocycled specimens with immersion in the denture cleansing solution. Finally, the comparison of thermal properties were perfomed using differential scanning calorimeter(DSC-1500). The following results were obtained : 1. In the case of no treatment teeth, the wear amount of endura Posterior(EN) was the greatest among the others(p<0.01), and the wear amount of three kinds of artificial resin teeth was increased in the order of Trubyte IPN teeth(IN), Trubyte Biotone(BN), SR-Orthosit Posteriores(SN) but there was no statistic significance(p>0.01). 2. The wear amount of Trubyte IPN teeth(IT) and Trubyte Biotone(BT), was increased due to thermocycling effect, but that of Endura Posteriores(ET) was decreased conversely(p<0.01). 3. Except for the SR-Orthosit Posteriores(STC), the wear amount of three kinds of artificial resing teeth(that is, ETC, ITC, BTC) was increased due to denture cleansing solution