• 제목/요약/키워드: Synthesized powder materials

검색결과 786건 처리시간 0.027초

습식 직접 합성법에 의한 세라믹(PZT) 분말의 합성 (Synthesis of Pizoceramic (PZT) Powder by Wet-direct Process)

  • 이수호;김한근;최헌일;설수덕;사공건
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1990년도 하계학술대회 논문집
    • /
    • pp.265-268
    • /
    • 1990
  • In this study, PZT powder prepared by the wet direct process was synthesized. As starting materials, $TiCl_4$. $ZrOCl_2{\cdot}8H_2O$ and PbO were used. Uniformly shape and fine-grained PZT powder was obtained by the wet-direct process and PZT powder was characterized by XRD, DTA analysis. The X-ray diffraotion peaks from the PZT powder were observed at 700($^{\circ}C$) or over.

  • PDF

전기폭발법으로 제조된 니켈기 초내열합금 나노분말의 용가재로의 응용가능성에 관한 평가 (Evaluation on the Applicability as Filler materials of Ni-Based Super Alloying Nano Size Powder by Pulsed Wire Evaporation(PWE) Method)

  • 김경호;이민구;김광호;이창규;김흥희
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.168-170
    • /
    • 2005
  • Nickel base brazes containing boron and silicon as melting point depressants are used extensively in the joining and repair of hot-section components in next generation nuclear reactor and aero-engine. Therefore, the present study has investigated the preliminary applicability of nickel based alloying nano powders. Nano Ni-based alloying powders synthesized by Pulsed Wire Evaporation (PWE) method. It's powder morphology and phase transformation temperature were analyzed by scanning electron microscopy, transmission electron microscopy, and differential scanning calorimeter(DSC). The powder particle size was approximately 10${\sim}$100nm and exhibits a quite even equiaxed shape. The results of DSC measurement show that both the nano Inconel 625 nano powder and Inconel 718 nano powder presents similar liquidus temperatures approximately $1373^{\circ}C$ and $1380^{\circ}C$ respectively.

  • PDF

Synthesis and Characterization of Y2O3 Powders by a Modified Solvothermal Process

  • Jeong, Kwang-Jin;Bae, Dong-Sik
    • 한국재료학회지
    • /
    • 제22권2호
    • /
    • pp.78-81
    • /
    • 2012
  • $Y_2O_3$ nanomaterials have been widely used in transparent ceramics and luminescent devices. Recently, many studies have focused on controlling the size and morphology of $Y_2O_3$ in order to obtain better material performance. $Y_2O_3$ powders were prepared under a modified solvothermal condition involving precipitation from metal nitrates with aqueous ammonium hydroxide. The powders were obtained at temperatures at $250^{\circ}C$ after a 6h process. The properties of the $Y_2O_3$ powders were studied as a function of the solvent ratio. The synthesis of $Y_2O_3$ crystalline particles is possible under a modified solvothermal condition in a water/ethylene glycol solution. Solvothermal processing condition parameters including the pH, reaction temperature and solvent ratio, have significant effects on the formation, phase component, morphology and particle size of yttria powders. Ethylene glycol is a versatile, widely used, inexpensive, and safe capping organic molecule for uniform nanoparticles besides as a solvent. The characterization of the synthesized Y2O3 powders were studied by XRD, SEM (FE-SEM) and TG/DSC. An X-ray diffraction analysis of the synthesized powders indicated the formation of the $Y_2O_3$ cubic structure upon calcination. The average crystalline sizes and distribution of the synthesized $Y_2O_3$ powders was less than 2 um and broad, respectively. The synthesized particles were spherical and hexagonal in shape. The morphology of the synthesized powders changed with the water and ethylene glycol ratio. The average size and shape of the synthesized particles could be controlled by adjusting the solvent ratio.

역-마이셀 공정에 의한 NiAl2O4 무기안료 나노 분말의 합성 및 특성 (Synthesis and Characterization of NiAl2O4 Inorganic Pigment Nanoparticles by a Reverse Micelle Processing)

  • 손정훈;배동식
    • 한국재료학회지
    • /
    • 제25권2호
    • /
    • pp.95-99
    • /
    • 2015
  • $NiAl_2O_4$ nanoparticle was synthesized by a reverse micelle processing for inorganic pigment. $Ni(NO_3)_2{\cdot}6H_2O$ and $Al(NO_3)_3{\cdot}9H_2O$ were used for the precursor in order to synthesize $NiAl_2O_4$ nanoparticles. The aqueous solution, which consisted of a mixing molar ratio of Ni/Al, was 1:2 and heat treated at $800{\sim}1100^{\circ}C$ for 2h. The average size and distribution of synthesized $NiAl_2O_4$ powders are in the range of 10-20 nm and narrow, respectively. The average size of the synthesized $NiAl_2O_4$ powders increased with an increasing water-to-surfactant molar ratio and heating temperature. The crystallinity of synthesized $NiAl_2O_4$ powder increased with an increasing heating temperature. The synthesized $NiAl_2O_4$ powders were characterized by X-ray diffraction analysis(XRD), a field emission scanning electron microscopy(FE-SEM), and a color spectrophotometer. The properties of synthesized powders were affected as a function such as a molar ratio and heating temperature. Results indicate that synthesis using a reverse miclle processing is a favorable process to obtain $NiAl_2O_4$ spinels at low temperatures. The procedure performed suggests that this new synthesis route for producing these oxides has the advantage of being fast and simple. Colorimetric coordinates indicate that the pigments obtained exhibit blue colors.

Synthesis of Metal and Ceramic Magnetic Nanoparticles by Levitational Gas Condensation (LGC)

  • Uhm, Y.R.;Lee, H.M.;Lee, G.J.;Rhee, C.K.
    • Journal of Magnetics
    • /
    • 제14권2호
    • /
    • pp.75-79
    • /
    • 2009
  • Nickel (Ni) and ferrite ($Fe_3O_4$, $NiFe_2O_4$) nanoparticles were synthesized by LGC using both wire feeding (WF) and micron powder feeding (MPF) systems. Phase evolution and magnetic properties were then investigated. The Ni nanopowder included magnetic-ordered phases. The LGC synthesis yielded spherical particles with large coercivity while the abnormal initial magnetization curve for Ni indicated a non-collinear magnetic structure between the core and surface layer of the particles. Since the XRD pattern cannot actually distinguish between magnetite ($Fe_3O_4$) and maghemite (${\gamma}-Fe_2O_3$) as they have a spinel type structure, the phase of the iron oxide in the samples was unveiled by $M{\ddot{o}}ssbauer$ spectroscopy. The synthesized Ni-ferrite consisted of single domain particles, including an unusual ionic state. The synthesized nanopowder bore an active surface due to the defects that affected abnormal magnetic properties.

Morphological Variation and Luminescence Properties of ZnO Micro/Nanocrystals Synthesized by Thermal Evaporation Method

  • Lee, Won-Jae;Lee, Geun-Hyoung
    • 한국재료학회지
    • /
    • 제27권10호
    • /
    • pp.530-533
    • /
    • 2017
  • ZnO micro/nanocrystals with different morphologies were synthesized by thermal evaporation of various zinc source materials in an air atmosphere. Zinc acetate, zinc carbonate and zinc iodide were used as the source materials. No catalysts or substrates were used in the synthesis of the ZnO crystals. The scanning electron microscope(SEM) image showed that the morphology of ZnO crystals was strongly dependent on the source materials, which suggests that source material is one of the key factors in controlling the morphology of the obtained ZnO crystals. Tetrapods, nanogranular shaped crystals, spherical particles and crayon-shaped crystals were obtained using different source materials. The X-ray diffraction(XRD) pattern revealed that the all the ZnO crystals had hexagonal wurtzite crystalline structures. An ultraviolet emission was observed in the cathodoluminescence spectrum of the ZnO crystals prepared via thermal evaporation of Zn powder. However, a strong green emission centered at around 500 nm was observed in the cathodoluminescence spectra of the ZnO crystals prepared using zinc salts as the source materials.

나노 실리카와 카본블랙이용 탄화열 반응으로 나노 SiC 합성 및 특성 (Synthesis of SiC Nanoparticles by a Sol-Gel Process)

  • 정광진;배동식
    • 한국재료학회지
    • /
    • 제23권4호
    • /
    • pp.246-249
    • /
    • 2013
  • Nano-sized ${\beta}$-SiC nanoparticles were synthesized combined with a sol-gel process and a carbothermal process. TEOS and carbon black were used as starting materials for the silicon source and carbon source, respectively. $SiO_2$ nanoparticles were synthesized using a sol-gel technique (Stober process) combined with hydrolysis and condensation. The size of the particles could be controlled by manipulating the relative rates of the hydrolysis and condensation reactions of tetraethyl orthosilicate (TEOS) within the micro-emulsion. The average particle size and morphology of synthesized silicon dioxide was about 100nm and spherical, respectively. The average particles size and morphology of the used carbon black powders was about 20nm and spherical, respectively. The molar ratio of silicon dioxide and carbon black was fixed to 1:3 in the preparation of each combination. $SiO_2$ and carbon black powders were mixed in ethanol and ball-milled for 12 h. After mixing, the slurries were dried at $80^{\circ}C$ in an oven. The dried powder mixtures were placed in alumina crucibles and synthesized in a tube furnace at $1400{\sim}1500^{\circ}C$ for 4 h with a heating rate of $10^{\circ}C$/min under flowing Ar gas (160 cc/min) and furnace cooling down to room temperature. SiC nanoparticles were characterized by XRD, TEM, and SAED. The XRD results showed that high purity beta silicon carbide with excellent crystallinity was synthesized. TEM revealed that the powders are spherical shape nanoparticles with diameters ranging from 15 to 30 nm with a narrow distribution.

초미립 MnxZn1-xFe2O4(x = 0.69~0.74)분말의 제조 및 자기적 성질 (Synthesis of Ultra Eine MnxZn1-xFe2O4(x = 0.69~0.74) Powder and Its Magnetic Properties)

  • 곽재은;이완재
    • 한국분말재료학회지
    • /
    • 제9권6호
    • /
    • pp.449-454
    • /
    • 2002
  • $MnxZn_{1-x}Fe_2O_4$ (x=0.69~0.74) powders synthesized by the thermal decomposition of organic acid salts. The obtained powders were uniform in composition and ultra-fine particle with about 400 nm. The amount of spinel phase of these powders was about 50% in X-ray diffraction patterns. The calcination of powder was carried out at $900^{\circ}C$ for 2 hours in air. After the powders were calcined. the mean size of powder was about 500 nm and the amount of spinel phase was increased over about 65%. The maximum amount of spinel phase was about 75% in the specimen of X=0.72. The magnetic properties of calcined $Mn_{0.72}Zn_{0.28}Fe_2O_4$ powders were the best among the different among the different compositions.

글리신-질산염 연소법으로 합성된 SrAl2O4:Eu2+,Dy3+ 형광체의 발광 및 장잔광 특성 (Photoluminescence and Long-phosphorescent Characteristics of SrAl2O4:Eu2+,Dy3+ Phosphor by Glycine-nitrate Combustion Method)

  • 이영기;김정열;이유기
    • 한국재료학회지
    • /
    • 제20권7호
    • /
    • pp.364-369
    • /
    • 2010
  • A $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor powder with stuffed tridymite structure was synthesized by glycine-nitrate combustion method. The luminescence, formation process and microstructure of the phosphor powder were investigated by means of X-ray diffraction (XRD), scanning electron microscopy (SEM) and photoluminescence spectroscopy (PL). The XRD patterns show that the as-synthesized $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor was an amorphous phase. However, a crystalline $SrAl_2O_4 $ phase was formed by calcining at $1200^{\circ}C$ for 4h. From the SEM analysis, also, it was found that the as-synthesized $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor was in irregular porous particles of about 50 ${\mu}m$, while the calcined phosphor was aggregated in spherical particles with radius of about 0.5 ${\mu}m$. The emission spectrum of as-synthesized $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor did not appear, due to the amorphous phase. However, the emission spectrum of the calcined phosphor was observed at 520 nm (2.384eV); it showed green emission peaking, in the range of 450~650 nm. The excitation spectrum of the $SrAl_2O_4:Eu^{2+},Dy^{3+}$ phosphor exhibits a maximum peak intensity at 360 nm (3.44eV) in the range of 250~480 nm. After the removal of the pulse Xe-lamp excitation (360 nm), also, the decay time for the emission spectrum was very slow, which shows the excellent longphosphorescent property of the phosphor, although the decay time decreased exponentially.

In-situ Synthesis of Cu-TiB2 Nanocomposite by MA/SPS

  • Kwon, Young-Soon;Kim, Ji-Soon;Kim, Hwan-Tae;Moon, Jin-Soo;D.V Dudina;O.I. Lomovsky
    • 한국분말재료학회지
    • /
    • 제10권6호
    • /
    • pp.443-447
    • /
    • 2003
  • Nano-sized $TiB_2$ was in situ synthesized in copper matrix through self-propagating high temperature synthesis (SHS) with high-energy ball milled Ti-B-Cu elemental mixtures as powder precursors. The size of $TiB_2$ particles in the product of SHS reaction decreases with time of preliminary mechanical treatment ranging from 1 in untreated mixture to 0.1 in mixtures milled for 3 min. Subsequent mechanical treatment of the product of SHS reaction allowed the $TiB_2$ particles to be reduced down to 30-50 nm. Microstructural change of $TiB_2$-Cu nanocomposite during spark plasma sintering (SPS) was also investigated. Under simultaneous action of pressure, temperature and electric current, titanium diboride nanoparticles distributed in copper matrix move, agglomerate and form a interpenetrating phase composite with a fine-grained skeleton.