Magnetic Properties of FeZrBAg Soft Magnetic Thin Films with High Permeability and High Magnetization (고투자율, 고포화자화 FeZrBAg 연자성 박막의 자기적 특성)

  • 민복기;김현식;송재성
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.6
    • /
    • pp.285-290
    • /
    • 1999
  • The magnetic properties of sputtered amorphous $Fe_{86.7}Zr_{3.3}B_4Ag_6$ thin films, which contains an additional insoluble element Ag, have been investigated as a function of uniaxal field annealing temperature. The amorphous $Fe_{86.7}Zr_{3.3}B_4Ag_6$ thin films produced by relatively low temperature annealing at 40$0^{\circ}C$ for 1 hour was found to have very high permeability of 7800 at 50 MHz, 0.2 mOe, high magnetization of 1.7 T, low coercivity of 1.0 Oe and very low core loss of 1.4 W/cc at 1 MHz, 0.1 T, respectively. It is notable that the permeability and core loss values for various kinds of the soft magnetic thin films reported up to now. The reason for the appearance for the good soft magnetic properties is presumably due to the homogeneous formation of very fine bcc $\alpha$-Fe clusters with the size in the amorphous $Fe_{86.7}Zr_{3.3}B_4Ag_6$ thin films matrix, which can be deduced from the XRD results.

  • PDF

Effect of α-Fe Content on the Magnetic Properties of MnBi/α-Fe Nanocomposite Permanent Magnets by Micro-magnetic Calculation

  • Li, Y.Q.;Yue, M.;Zuo, J.H.;Zhang, D.T.;Liu, W.Q.;Zhang, J.X.;Guo, Z.H.;Li, W.
    • Journal of Magnetics
    • /
    • v.18 no.3
    • /
    • pp.245-249
    • /
    • 2013
  • A finite element model was built for MnBi/${\alpha}$-Fe nanocomposite permanent magnets, and the demagnetization curves of the magnets were simulated by micro-magnetic calculation. The microstructure of the cubic model is composed of 64 irregular grains with an average grain size of 20 nm. With the volume fraction of soft magnetic phase (t vol. %) ranged from 5 to 20 vol. %, both isotropic and anisotropic nanocomposite magnets show typical single-phase permanent magnets behavior in their demagnetization curves, illustrating good intergranular exchange coupling effect between soft and hard magnetic phases. With the increase of volume fraction of soft magnetic phase in both isotropic and anisotropic magnets, the coercive force of the magnets decreases monotonically, while the remanence rises at first to a peak value, then decreases. The optimal values of maximum energy products of isotropic and anisotropic magnets are 84 and $200kJ/m^3$, respectively. Our simulation shows that the MnBi/${\alpha}$-Fe nanocomposite permanent magnets own excellent magnetic properties and therefore good potential for practical applications.

Characteristics of Silica Coated ${\gamma}-Fe_{2}O_{3}$ with Heat-treatment (열처리에 따른 실리카 피착 ${\gamma}-Fe_{2}O_{3}$의 특성)

  • Lee, J.Y.;Byeon, T.B.;Kim, D.Y.;Lee, H.;Han, K.H.;Sohn, J.G.
    • Journal of the Korean Magnetics Society
    • /
    • v.3 no.2
    • /
    • pp.108-114
    • /
    • 1993
  • This paper presents a study on the effects of silica coating in the production of ${\gamma}-Fe_{2}O_{3}$ powders suitable for magnetic recording media. Emphasis has been put on investigating the relationship between the powder characteristics and the effects of silica coating in the heat-treatment stage of ${\gamma}-Fe_{2}O_{3}$ production. After we prepared non-coated ${\gamma}-Fe_{2}O_{3}$ and silica coated ${\gamma}-Fe_{2}O_{3}$ with coating water glass on the surface of goethite and heattreatment process, we compared and investigated powder characteristics. As silica coated layer played a role of preventing the powders from overreduction to metal iron and rapid oxidation, silica coated ${\gamma}-Fe_{2}O_{3}$ showed superior magnetization value due to inhibiting t!1e adulteration of ${\alpha}-Fe_{2}O_{3}$ into the final product. When silica coated layer acted as a sintering restrainer, silica coated ${\gamma}-Fe_{2}O_{3}$ showed high coercivity and specific sur-face area due to good acicularity.

  • PDF

The Effects of $O_2$ Partial Prewwure on Soft Magnetic Properties of Fe-Hf-O Thin Films (Fe-Hf-O계 박막에서 산소 분압 변화가 박막특성에 미치는 영향)

  • 박진영;김종열;김광윤;한석희;김희중
    • Journal of the Korean Magnetics Society
    • /
    • v.7 no.5
    • /
    • pp.243-248
    • /
    • 1997
  • The effect of $O_2$ partial pressure on microstructure and soft magnetic properties of as-deposited Fe-Hf-O thin film alloys, which are produced by rf magnetron sputtering method in $Ar+O_2$ mixed gas atmosphere, are investigated. Saturation magnetization ($4{\pi}M_s$) of Fe-Hf-O film were decreased with increasing $O_2$ partial pressure, the best soft magnetic properties exhibit at $O_2$ partial pressure of 10%. With further increase of $O_2$ partial pressure, soft magnetic properties decreased continuously. The $Fe_{82}Hf_{3.4}O_{14.6}$ film with $P_{O2}=10%$ exhibits good soft magnetic properties with $4{\pi}M_s=17.7kG$, $H_c=0.7Oe$ and ${\mu}_ {eff}$ (1~100 MHz)=2,500, respectively. The addition of O is effective in grain refinement. In case of $P_{O2}=15%$, it is observed that $Fe_3O_4$ compound is formed and high frequency soft magnetic properties are decrease. The electrical resistvity($\rho$) of Fe-Hf-O film is increased with increasing $O_2$ partial pressure. Electrical resistivity of $Fe_{82}Hf_{3.4}O_{14.6}$ film was 5 times higher than that of the film without oxygen. Thus, it is considered that the good magnetic properties of $Fe_{82}Hf_{3.4}O_{14.6}$ film results from decreasing the $\alpha$-Fe grain size by precipitates (Hf and O), high electrical resistivity.

  • PDF

Enhanced magnetic properties of FeCo alloys by engineering crystallinity and composition (FeCo의 결정성 및 조성 제어를 통한 자기 특성 향상)

  • Kim, Dan-Bi;Kim, Ji-Won;Eom, Nu-Si-A;Park, Seong-Heum;Im, Jae-Hong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2018.06a
    • /
    • pp.32.1-32.1
    • /
    • 2018
  • Novel soft magnetic materials can be achieved by altering material properties such as morphology, composition, crystallinity, and grain size of soft magnetic alloys. Especially, magnetic properties (i.e., saturation magnetization, coarcivity) of soft magnetics are significantly affected by grain boundaries which act as a control of magnetic domain wall movement. Thus, we herein develop a two-step electroless plating method to control morphology and grain size of FeCo films for excellent magnetic properties. Accordingly, the chemical composition to control the degree of polarization of FeCo alloys was altered by electroless deposition parameters; for example, electrolyte concentration and temperature. The grain size and crystallinity of FeCo alloys was dramatically affected by the reaction temperature because the grain growth mechanism dominantly occurs at $90^{\circ}C$ where as the neucleation only happens at $50^{\circ}C$. By simply controlling the temperature, the micron-sized FeCo grains embedded FeCo film was synthesized where the large grains allow high magnetization originated from larger magnetic domain with low corecivity and the nano-sized grains allow excellent soft magnetic properties due to the magnetic correlation length.

  • PDF

Soft Magnetoresistive Properties of Conetic Thin Film Depending on Ta Buffer Layer (버퍼층 Ta에 의존하는 코네틱 박막의 연자성 자기저항 특성)

  • Choi, Jong-Gu;Hwang, Do-Guwn;Lee, Sang-Suk;Choi, Jin-Hyub;Lee, Ky-Am;Rhee, Jang-Rho
    • Journal of the Korean Magnetics Society
    • /
    • v.19 no.6
    • /
    • pp.197-202
    • /
    • 2009
  • The property of soft magnetism for the Corning glass/non-buffer or buffer Ta/Conetic(NiFeCuMo)/Ta prepared by the ion beam deposition sputtering was studied. The effect of crystal property and post annealing treatment depending on the thickness of Conetic thin films was investigated. The coercivities of Conetic thin films with easy and hard direction along to the applying magnetic field during deposition were compared with each other. The coercivity and magnetic susceptibility of Ta(5 nm)/Conetic(50 nm) thin film were 0.12 Oe and 1.2 ${\times}\;10^4$, respectively. From these results, firstly, the Conetic thin film was more soft magnetism thin film than other one such as permalloy NiFe. Secondly, the usage of soft magnetism Conetic thin film for GMR-SV (giant magneoresistance-spin valve) or MTJ (Megnetic Tunnel Junction) structure in a low magnetic field can be possible.

Soft Magnetic Properties of CoFeHfO Thin Films (CoFeHfO 박막의 자기적 특성)

  • Lee, K.E.;Tho, L.V.;Kim, S.H.;Kim, C.G.;Kim, C.O.
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.4
    • /
    • pp.197-200
    • /
    • 2006
  • Amorphous alloys of Co-rich magnetic amorphous films are well known as thpical soft magnetic alloys. They are used for many kinds of electric and electronic parts such as magnetic recording heads, transformers and inductors. CoFeHfO thin films were prepared by RF magnetron reactive sputtering. The films were deposited onto Si(100) substrates with a power of 300 W at room temperature. The reactive gas was introduced up to 10% ($O_2$/(Ar + $O_2$)) during deposition, and the $Co_{39}Fe_{34}Hf_{9.5}O_{17.5}$ thin film exhibit excellent soft magnetic properties : saturation magnetization ($4{\pi}M_s$) of 19kG, magnetic coercivity ($H_c$) of 0.37 Oe, anisotropy field ($H_k$) of 48.62 Oe, and an electrical property is also shown to be as high as 300 ${\mu}{\Omega}cm$. It is assumed that the good soft magnetic properties of $Co_{39}Fe_{34}Hf_{9.5}O_{17.5}$ thin film results from high electrical resistivity and large anisotropy field.

Soft x-ray Synchrotron Radiation Spectroscopy Study of Molecule-based Nano Bioparticles Containing Fe (철원소를 함유한 분자기반 생체물질 나노입자들의 연 x선 방사광 분광 연구)

  • Lee, Eun-Sook;Kim, D.H.;Hwang, Ji-Hoon;Lee, Ki-Ho;Kang, J.S.
    • Journal of the Korean Magnetics Society
    • /
    • v.22 no.4
    • /
    • pp.125-129
    • /
    • 2012
  • By employing soft x-ray absorption spectroscopy (XAS) and soft x-ray magnetic circular dichroism (XMCD), the electronic structures of molecule-based nano bioparticles, such as Helicobacter pylori ferritin (H. pylori ferritin), Heme, $NaM[Fe(CN)_6]{\cdot}H_2O$-type Prussian Blue (M=Co, Ni) analogue, have been investigated. The measured Fe 2p XAS spectra reveal that Fe ions are trivalent ($Fe^{3+}$) in H. pylori ferritins, while they are in the $Fe^{2+}-Fe^{3+}$ mixed-valent states in $NaM[Fe(CN)_6]{\cdot}H_2O$ Prussian Blue analogues (M=Co, Ni). According to the Fe 2p XMCD spectrum of high-state H. pylori ferritin, all the $Fe^{3+}$ ions have the same local symmetry and their magnetic moments are aligned in the same direction. It is also found that the Fe 3d orbitals in $NaM[Fe(CN)_6]{\cdot}H_2O$ have a strong covalent bonding to $(CN)^-$ ligands, but with a very weak bonding to the 2p orbitals of O ligands.

Increment of the Exchange Coupling in Fe-Ni Alloy Thin Films Deposited with a Bias Magnetic Field

  • Han, Kyung-Hunn;Kim, Jung-Gi;Cho, Jae-Hun;Lee, Suk-Mock
    • Journal of Magnetics
    • /
    • v.11 no.2
    • /
    • pp.77-82
    • /
    • 2006
  • The structure and magnetic properties of Fe-Ni films, deposited by DC magnetron sputtering on Si(111) wafer, have been studied. The spin wave stiffness constant is determined by Brillouin light scattering (BLS) and compared with the value obtained from magnetization measurements. The range of exchange interaction was determined as 0.4 atomic distances in the film deposited in a bias magnetic field, which is 1/2 that in the film grown in no bias magnetic field. The results show that the dimensions of exchange coupling increased by the sputtering in the magnetic field.

Study on Basic Magnetic Characteristics in New Magnetic Materials(2) - Magnetic Properties of Amorphous $Fe_{80}B_{15}Si_{5}$ alloy Measures with Pulse Method (새 자성재료의 기초자기특성 연구(2) - 펄스측정법에 의한 비정질 $Fe_{80}B_{15}Si_{5}$ 합금의 자기특성)

  • 이용호;신용돌;김인수;이연숙;노태환;강일구
    • Journal of the Korean Magnetics Society
    • /
    • v.1 no.2
    • /
    • pp.42-48
    • /
    • 1991
  • The basic soft magnetic characteristics of a typical Fe based amorphous $Fe_{80}B_{15}Si_{5}$ alloy were measured with pulse metheod. Quantitative relations between magnetostriction, anisotropy energy, reluctivity were investigated. The relative contribution factor of magnetostrictive and uniaxial anisotropy energy to the reluctivity were calculated. The internal stress and induced anisotropy were estimated. A tension applied to the long axis of the sample greatly enhanced induced anisotropy.