• 제목/요약/키워드: Sn-3.5Ag Pb-free solder

검색결과 100건 처리시간 0.028초

Pb Free Sn-2%Ag-x%Bi계 Solder의 특성에 관한 연구 (A study on the characteristics of Pb free Sn-2%Ag-x%Bi solder alloys)

  • 흥순국;박일경;강정윤
    • Journal of Welding and Joining
    • /
    • 제16권3호
    • /
    • pp.148-156
    • /
    • 1998
  • The purpose of this study is to investigate the characteristics of Pb-Free Sn-2%Ag-Bi solder alloys. The solder alloys used in this study is Sn-2%Ag-(3,5,7,9%) Bi It is examined that their properties such as melting range, wettability, microstructure, microhardness, and tensile property. The addition of Bi(3,5,7,9%) lowered the melting point of the solder and the melting range was 196~203$^{\circ}C$. The wettability of the solder as equal to that of Sn-37% Pb solder. The morphology of structure did not change largely by addition of Bi. But the structure of cellular dendrite of linear type displayed. The tensile strength of the solder was superior to that of Sn-37%Pb solder. But the elongation was inferior to that of Sn-37%Pb solder. The hardness of Sn-2%Ag solder was tow times and that of Sn-2%Ag-Bi solder was three times of that in Sn-37%Pb solder. But the effect of increment of Bi content did not change largely.

  • PDF

Sn-Ag-X계 무연솔더 접합부의 미세조직 및 전단강도에 관한 연구 (A Study on the Characteristics of Sn-Ag-X Solder Joint)

  • 김문일;문준권;정재필
    • Journal of Welding and Joining
    • /
    • 제20권2호
    • /
    • pp.77-81
    • /
    • 2002
  • Many kinds of Pb-free solder have been investigated because of the environmental concerns. Sn-Ag-Cu system is well blown as most competitive Pb-free solder. However, since Sn-Ag-Cu system has relatively high melting point compared to Sn-Pb eutectic, it may a limitation, the some application. In this study, Bi and In contained solder of $Sn_3Ag_8Bi_5In$ which has relatively lower melting point, $188~204^{\circ}C$, was investigated. $Sn_3Ag_8Bi_5In$ solder ball of $500\mu\textrm{m}$ diameter was set on the Ni/Cu/Cr-UBM and reflow soldered in the range of $220~240^{\circ}C$ for 5~15s. The maximum shear strength of the solder ball was around 170mN by reflowing at $240^{\circ}C$ for 10s. Intermetallic compound formed on the UBM of Si-wafer was analysed by SEM(scanning electron microscope) and XRD(X-ray diffractometer).

무연 솔더 볼의 전단강도와 공정조건 최적화에 관한 연구 (A Study on the Process Condition Optimization and Shear Strength of Lead Free Solder Ball)

  • 김경섭;선용빈;장호정;유정희;김남훈;장의구
    • 마이크로전자및패키징학회지
    • /
    • 제9권2호
    • /
    • pp.39-43
    • /
    • 2002
  • 48 $\mu$BGA 패키지에 Sn-37Pb 공정 솔더와 Sn-0.7Cu, Sn-3.5 Ag, Sn-2.0Ag-0.75Cu, Sn-2.0Ag-0.7Cu-3.0Bi 4종류의 무연 솔더를 적용하여, 미세 솔더 볼의 경도와 조성에 따른 솔더 접합부의 전단강도에 대해서 연구하였다. 실험 결과, 솔더 볼의 짖눌림은 Sn-2.0Ag-0.7Cu-3.0Bi에서 0.043mm로 큰 경도값을 얻었다. 또한 전단 강도 값은 무연 솔더가 Sn-37Pb 솔더보다 높았으며, Sn-2.0Ag-0.7Cu-3.0 Bi에서 최대 52% 높은 값을 나타내었다.

  • PDF

Immersion Ag가 도금된 Cu기판을 가진 Pb-free solder 접합부의 신뢰성 평가 (Reliability evaluation of Pb-free solder joint with immersion Ag-plated Cu substrate)

  • 윤정원;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년도 춘계 학술대회 개요집
    • /
    • pp.30-32
    • /
    • 2006
  • The interfacial reaction and reliability of eutectic Sn-Pb and Pb-free eutectic Sn-Ag ball-grid-array (BGA) solders with an immersion Ag-plated Cu substrate were evaluated following isothermal aging at $150^{\circ}C$. During reflowing, the topmost Ag layer was dissolved completely into the molten solder, leaving the Cu layer exposed to the molten solder for both solder systems. A typical scallop-type Cu-Sn intermetallic compound (IMC) layer was formed at both of the solder/Cu interfaces during reflowing. The thickness of the Cu-Sn IMCs for both solders was found to increase linearly with the square root of isothermal aging time. The growth of the $Cu_3Sn$ layer for the Sn-37Pb solder was faster than that for the Sn-3.5Ag solder, In the case of the Sn-37Pb solder, the formation of the Pb-rich layer on the Cu-Sn IMC layer retarded the growth of the $Cu_6Sn_5$ IMC layer, and thereby increased the growth rate of the $Cu_3Sn$ IMC layer. In the ball shear test conducted on the Sn-37Pb/Ag-plated Cu joint after aging for 500h, fracturing occurred at the solder/$Cu_6Sn_5$ interface. The shear failure was significantly related to the interfacial adhesion strength between the Pb-rich and $Cu_6Sn_5$ IMC layers. On the other hand, all fracturing occurred in the bulk solder for the Sn-3.5Ag/Ag-plated Cu joint, which confirmed its desirable joint reliability.

  • PDF

Sn-37mass%Pb 솔더 및 Sn-3.5mass%Ag 무연솔더를 이용한 ${\mu}BGA$ 솔더접합부의 열피로수명 예측 (Thermal Fatigue Life Prediction of ${\mu}BGA$ Solder Joint Using Sn-37mass%Pb Solder and Sn-3.5mass%Ag Lead-free Solder)

  • 신영의;이준환;하범용;정승부;정재필
    • Journal of Welding and Joining
    • /
    • 제19권4호
    • /
    • pp.406-412
    • /
    • 2001
  • This study is focussed on the numerical prediction of the thermal fatigue life of a ${\mu}BGA$(Micro Ball Grid Array) solder joint. Numerical method is used to perform three-dimensional finite element analysis for Sn-37mass%Pb. Sn-3.5mass%Ag solder alloys during the given thermal cycling. Strain values, along with the result of mechanical fatigue tests for solder alloys were then used to predict the solder joint fatigue life using the Coffin-Manson equation. In this study, a practical correlation for the prediction of the thermal fatigue life is suggested by using the dimensionless variable $\gamma$. As a result. it could be found that Sn-3.5mass%Ag has longer fatigue life than Sn-37mass%Pb in low cycle fatigue. In addition. the result with ${\gamm}ashow$a good agreement with the FEA results.

  • PDF

무연 Sn-Ag-Bi-Ga계 솔더의 특성에 관한 연구 (A Study on the Characteristic of Pb-free Sn-Ag-Bi-Ga Solder Alloys)

  • 노보인;이보영
    • Journal of Welding and Joining
    • /
    • 제18권6호
    • /
    • pp.42-47
    • /
    • 2000
  • The object of this study is to estimate Sn-Ag-Bi-Ga solder alloy as a substitute for Sn-37Pb alloy. For Sn-Ag-Bi-Ga alloys, Ag, Bi and Ga contents are varied. (Ag : 1~5%, Ga : 3%, Bi : 3~6%) Comparing to Sn-37Pb alloy Sn-Ag-Bi-Ga alloys have wider melting temperature range up to max. $18.7^{\circ}C$. With increasing Ag, Bi contents, the wettability of the alloys increased up to max. 6.6 mN. The vickers hardness of the alloys was max. 46.4 Hv. The ultimate tensile stress of the alloys was max. 60.3 MPa and the elongation was max. 1.2%. The joint strength between circuit board and solder was max. 55.5 N and the joint strength between connector and solder was max. 176.1 N. There were no cracks in this alloys after thermal shock test.

  • PDF

Sn-Ag-X계 무연솔더부의 특성 연구 -기판 도금층에 따른 Sn-Ag-Bi-In 솔더의 젖음특성- (A Study on the Characteristics of Sn-Ag-X Solder Joint -The Wettability of Sn-Ag-Bi-In Solder to Plated Substrates-)

  • 김문일;문준권;정재필
    • 한국표면공학회지
    • /
    • 제35권1호
    • /
    • pp.11-16
    • /
    • 2002
  • As environmental concerns increasing, the electronics industry is focusing more attention on lead free solder alternatives. In this research, we have researched wettability of intermediate solder of Sn3Ag9Bi5In, which include In and Bi and has similar melting temperature to Sn37Pb eutectic solder. We investigated the wetting property of Sn3Ag9Bi5In. To estimate wettability of Sn3Ag9Bi5In solder on various substrates, the wettability of Sn3Ag9Bi5In solder on high-pure Cu-coupon was measured. Cu-coupon that plated Sn, Ni and Au/Ni and Si-wafer adsorbed Ni/Cu under bump metallurgy on one side. As a result, the wetting property of Sn3Ag9Bi5In solder is a little better than that of Sn37Pb and Sn3.5Ag.

Sn-Bi도금 $Sn-3.5\%Ag$ 솔더를 이용한 Capacitor의 저온 솔더링 (Lower Temperature Soldering of Capacitor Using Sn-Bi Coated $Sn-3.5\%Ag$ Solder)

  • 김미진;조선연;김숙환;정재필
    • Journal of Welding and Joining
    • /
    • 제23권3호
    • /
    • pp.61-67
    • /
    • 2005
  • Since lead (Pb)-free solders for electronics have higher melting points than that of eutectic Sn-Pb solder, they need higher soldering temperatures. In order to decrease the soldering temperature we tried to coat Sn-Bi layer on $Sn-3.5\%Ag$ solder by electroplating, which applies the mechanism of transient liquid phase bonding to soldering. During heating Bi will diffuse into the $Sn-3.5\%Ag$ solder and this results in decreasing soldering temperature. As bonding samples, the 1608 capacitor electroplated with Sn, and PCB, its surface was finished with electroless-plated Ni/Au, were selected. The $Sn-95.7\%Bi$ coated Sn-3.5Ag was supplied as a solder between the capacitor and PCB land. The samples were reflowed at $220^{\circ}C$, which was lower than that of normal reflow temperature, $240\~250^{\circ}C$, for the Pb-free. As experimental result, the joint of $Sn-95.7\%Bi$ coated Sn-3.5Ag showed high shear strength. In the as-reflowed state, the shear strength of the coated solder showed 58.8N, whereas those of commercial ones were 37.2N (Sn-37Pb), 31.4N (Sn-3Ag-0.5Cu), and 40.2N (Sn-8Zn-3Bi). After thermal shock of 1000 cycles between $-40^{\circ}C$ and $+125^{\circ}C$, shear strength of the coated solder showed 56.8N, whereas the previous commercial solders were in the range of 32.3N and 45.1N. As the microstructures, in the solder $Ag_3Sn$ intermetallic compound (IMC), and along the bonded interface $Ni_3Sn_4$ IMC were observed.

전단펀치-크리프 시험에 의한 리플로우 시간별 Pb-free 솔더 합금 접합부에 대한 고온 크리프 물성 평가 (Material Property Evaluation of High Temperature Creep on Pb-free Solder Alloy Joint to Reflow Time by Shear Punch-creep Test)

  • 함영필;허우진;유효선;양성모
    • 한국자동차공학회논문집
    • /
    • 제21권1호
    • /
    • pp.145-153
    • /
    • 2013
  • In this study, shear punch-creep (SP-Creep) at Sn-4Ag/Cu pad the joint was tested by using environment-friendly Pb-free solder alloy Sn-4Ag of electronic components. Pb eutectic alloy (Sn-37Pb) joints limited to environmental issues with reflow time (10sec, 30sec, 100sec, 300sec) according to two types of solder alloy joints are compared and evaluated by creep strain rate, rupture time and IMC (Intermetallic Compound) behavior. As the results, reflow time increases with increasing thickness of IMC can be seen at overall 100sec later in case of two solder joints on the IMC thickness of Sn-4Ag solder joints thicker than Sn-37Pb solder joints. In addition, when considering creep evaluation factors, lead-free solder alloy Sn-4Ag has excellent creep resistance more than Pb eutectic alloy. For this reason, the two solder joints, such as in the IMC (Cu6Sn5) was formed. However, the creep resistance of Sn-4Ag solder joints was largely increased in the precipitation strengthening effect of dispersed Ag3Sn with interface more than Sn-37Pb solder joints.

리플로우 솔더링 공정 조건에 따른 Sn-Bi-Ag와 Sn-Ag-Cu 복합 무연 솔더 접합부 특성 연구 (A Study on Properties of Pb-free Solder Joints Combined Sn-Bi-Ag with Sn-Ag-Cu by Conditions of Reflow Soldering Processes)

  • 김자현;천경영;김동진;박영배;고용호
    • 마이크로전자및패키징학회지
    • /
    • 제29권3호
    • /
    • pp.55-61
    • /
    • 2022
  • 본 연구에서는 용융온도가 중온계 무연 솔더인 Sn-3.0Ag-0.5Cu(SAC305)와 저온계 무연 솔더인 Sn-57Bi-1Ag를 사용하여 형성된 복합 무연 솔더 접합부의 특성에 대하여 보고 하였다. SAC305 솔더볼이 형성된 ball grid array(BGA) 패키지와 Sn-57Bi-1Ag 솔더 페이스트가 도포된 flame retardant-4(FR-4) 인쇄회로기판(printed circuit board, PCB)을 리플로우 솔더링 공정을 이용하여 복합 무연 솔더 접합부를 형성 하였다. 공정 온도 프로파일을 두 가지 형태로 달리하여 리플로우 솔더링 공정을 진행하였으며 리플로우 솔더링 공정 조건에 따른 계면 반응, 금속간화합물(intermetallic compound, IMC)의 형성, Bi의 확산 거동 등 복합 무연 솔더 접합부 계면 특성을 비교 분석 하였다. 또한, 열 충격 시험을 통하여 리플로우 솔더링 공정에 따른 복합 무연 솔더 접합부의 신뢰성 특성을 비교하고 열 충격 시험 전후 전단 시험을 진행하여 접합부의 기계적 특성 변화를 분석하였다.