레이저를 이용한 결정질 실리콘 태양전지의 Double Texturing 제조 및 특성 (Characteristics of Double Texturization by Laser and Reactive Ion Etching for Crystalline Silicon Solar Cell)

  • 권준영;한규민;최성진;송희은;유진수;유권종;김남수
    • 한국재료학회지
    • /
    • 제20권12호
    • /
    • pp.649-653
    • /
    • 2010
  • In this paper, double texturization of multi crystalline silicon solar cells was studied with laser and reactive ion etching (RIE). In the case of multi crystalline silicon wafers, chemical etching has problems in producing a uniform surface texture. Thus various etching methods such as laser and dry texturization have been studied for multi crystalline silicon wafers. In this study, laser texturization with an Nd:$YVO_4$ green laser was performed first to get the proper hole spacing and $300{\mu}m$ was found to be the most proper value. Laser texturization on crystalline silicon wafers was followed by damage removal in acid solution and RIE to achieve double texturization. This study showed that double texturization on multi crystalline silicon wafers with laser firing and RIE resulted in lower reflectance, higher quantum yield and better efficiency than that process without RIE. However, RIE formed sharp structures on the silicon wafer surfaces, which resulted in 0.8% decrease of fill factor at solar cell characterization. While chemical etching makes it difficult to obtain a uniform surface texture for multi crystalline silicon solar cells, the process of double texturization with laser and RIE yields a uniform surface structure, diminished reflectance, and improved efficiency. This finding lays the foundation for the study of low-cost, high efficiency multi crystalline silicon solar cells.

Characterization of Band Gaps of Silicon Quantum Dots Synthesized by Etching Silicon Nanopowder with Aqueous Hydrofluoric Acid and Nitric Acid

  • Le, Thu-Huong;Jeong, Hyun-Dam
    • Bulletin of the Korean Chemical Society
    • /
    • 제35권5호
    • /
    • pp.1523-1528
    • /
    • 2014
  • Silicon quantum dots (Si QDs) were synthesized by etching silicon nanopowder with aqueous hydrofluoric acid (HF) and nitric acid ($HNO_3$). Then, the hydride-terminated Si QDs (H-Si QDs) were functionalized by 1- octadecene (ODE). By only controlling the etching time, the maximum luminescence peak of octadecylterminated Si QDs (ODE-Si QDs) was tuned from 404 nm to 507 nm. The average optical gap was increased from 2.60 eV (ODE-Si QDs-5 min) for 5 min of etching to 3.20 eV (ODE-Si QDs-15 min) for 15 min of etching, and to 3.40 eV (ODE-Si QDs-30 min) for 30 min of etching. The electron affinities (EA), ionization potentials (IP), and quasi-particle gap (${\varepsilon}^{qp}_{gap}$) of the Si QDs were determined by cyclic voltammetry (CV). The quasi-particle gaps obtained from the CV were in good agreement with the average optical gap values from UV-vis absorption. In the case of the ODE-Si QDs-30 min sample, the difference between the quasi-particle gap and the average optical gap gives the electron-hole Coulombic interaction energy. The additional electronic levels of the ODE-Si QDs-30 min and ODE-Si QDs-15 min samples determined by the CV results are interpreted to have originated from the Si=O bond terminating Si QD.

Dependence of cation ratio in Oxynitride Glasses on the plasma etching rate

  • Lee, Jung-Ki;Hwang, Seong-Jin;Lee, Sung-Min;Kim, Hyung-Sun
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 추계학술발표대회
    • /
    • pp.44.2-44.2
    • /
    • 2009
  • Polycrystalline materials suchas yttria and alumina have been applied as a plasma resisting material for the plasma processing chamber. However, polycrystal line material may easily generate particles and the particles are sources of contamination during the plasma enhanced process. Amorphous material can be suitable to prevent particle generation due to absence of grain-boundaries. We manufactured nitrogen-containing $SiO_2-Al_2O_3-Y_2O_3$ based glasses with various contents of silicon and fixed nitrogen content. The thermal properties, mechanical properties and plasma etching rate were evaluated and compared for the different composition samples. The plasma etching behavior was estimated using XPS with depth profiling. From the result, the plasma etching rate highly depends on the silicon content and it may results from very low volatile temperature of SiF4 generated during plasma etching. The silicon concentration at the plasma etched surface was very low besides the concentration of yttrium and aluminum was relatively high than that of silicon due to high volatile temperature of fluorine compounds which consisted with aluminum and yttrium. Therefore, we conclude that the samples having low silicon content should be considered to obtain low plasma etching rate for the plasma resisting material.

  • PDF

Cl2/HBr/CF4 반응성 이온 실리콘 식각 후 감광막 마스크 제거 (Removal of Photoresist Mask after the Cl2/HBr/CF4 Reactive Ion Silicon Etching)

  • 하태경;우종창;김관하;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제23권5호
    • /
    • pp.353-357
    • /
    • 2010
  • Recently, silicon etching have received much attention for display industry, nano imprint technology, silicon photonics, and MEMS application. After the etching process, removing of etch mask and residue of sidewall is very important. The investigation of the etched mask removing was carried out by using the ashing, HF dipping and acid cleaning process. Experiment shows that oxygen component of reactive gas and photoresist react with silicon and converting them into the mask fence. It is very difficult to remove by using ashing or acid cleaning process because mask fence consisted of Si and O compounds. However, dilute HF dipping is very effective process for SiOx layer removing. Finally, we found optimized condition for etched mask removing.

기계화학적 극미세 가공기술을 이용한 PDMS 복제몰딩 공정용 서브마이크로 몰드 제작에 관한 연구 (A Study on the Fabrication of Sub-Micro Mold for PDMS Replica Molding Process by Using Hyperfine Mechanochemical Machining Technique)

  • 윤성원;강충길
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2004년도 추계학술대회 논문집
    • /
    • pp.351-354
    • /
    • 2004
  • This work presents a simple and cost-effective approach for maskless fabrication of positive-tone silicon master for the replica molding of hyperfine elastomeric channel. Positive-tone silicon masters were fabricated by a maskless fabrication technique using the combination of nanoscratch by Nanoindenter ⓡ XP and XOH wet etching. Grooves were machined on a silicon surface coated with native oxide by ductile-regime nanoscratch, and they were etched in a 20 wt% KOH solution. After the KOH etching process, positive-tone structures resulted because of the etch-mask effect of the amorphous oxide layer generated by nanoscratch. The size and shape of the positive-tone structures were controlled by varying the etching time (5, 15, 18, 20, 25, 30 min) and the normal loads (1, 5 mN) during nanoscratch. Moreover, the effects of the Berkovich tip alignment (0, 45$^{\circ}$) on the deformation behavior and etching characteristic of silicon material were investigated.

  • PDF

The study of silicon etching using the high density hollow cathode plasma system

  • Yoo, Jin-Soo;Lee, Jun-Hoi;Gangopadhyay, U.;Kim, Kyung-Hae;Yi, Jun-Sin
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2003년도 International Meeting on Information Display
    • /
    • pp.1038-1041
    • /
    • 2003
  • In the paper, we investigated silicon surface microstructures formed by reactive ion etching in hollow cathode system. Wet anisotropic chemical etching technique use to form random pyramidal structure on <100> silicon wafers usually is not effective in texturing of low-cost multicrystalline silicon wafers because of random orientation nature, but High density hollow cathode plasma system illustrates high deposition rate, better film crystal structure, improved etching characteristics. The etched silicon surface is covered by columnar microstructures with diameters form 50 to 100nm and depth of about 500nm. We used $SF_{6}$ and $O_{2}$ gases in HCP dry etch process. This paper demonstrates very high plasma density of $2{\times}10^{12}$ $cm^{-3}$ at a discharge current of 20 mA. Silicon etch rate of 1.3 ${\mu}s/min$. was achieved with $SF_{6}/O_{2}$ plasma conditions of total gas pressure=50 mTorr, gas flow rate=40 sccm, and rf power=200 W. Our experimental results can be used in various display systems such as thin film growth and etching for TFT-LCDs, emitter tip formations for FEDs, and bright plasma discharge for PDP applications. In this paper we directed our study to the silicon etching properties such as high etching rate, large area uniformity, low power with the high density plasma.

  • PDF

Photoelectrochemical Hydrogen Production on Textured Silicon Photocathode

  • Oh, Il-Whan
    • 전기화학회지
    • /
    • 제14권4호
    • /
    • pp.191-195
    • /
    • 2011
  • Wet chemical etching methods were utilized to conduct Si surface texturing, which could enhance photoelectrochemical hydrogen generation rate. Two different etching methods tested, which were anisotropic metal-catalyzed electroless etching and isotropic etching. The Si nano-texture that was fabricated by the anisotropic etching showed ~25% increase in photocurrent for H2 generation. The photocurrent enhancement was attributed to the reduced reflection loss at the nano-textured Si surface, which provided a layer of intermediate density between water and the Si substrate.

KOH 용액을 이용한 단결정 실리콘의 이방성 식각특성에 관한 연구 (A study on anisotropic etching property of single-crystal silicon using KOH solution)

  • 김환영;천인호;김창교;조남인
    • 한국결정성장학회지
    • /
    • 제7권3호
    • /
    • pp.449-455
    • /
    • 1997
  • KOH 용액을 이용한 단결정 실리콘의 이방성 식각 특성을 조사하였다. n형 (100) 단결정 실리콘 웨이퍼를 시료로 사용하였으며, 식각 비율이 월등히 작은 $SiO_2$층을 실리콘 식각의 마스크로 사용하였다. 실리콘의 식각속도와 식각상태는 KOH 용액의 농도와 온도조건 뿐만 아니라 용액의 균일도, 용액의 교반속도와 교반방향 등에 따라 큰 차이가 발생하였다. 실리콘의 식각 속도는 KOH 농도가 낮아질수록 증가하며, 온도는 높아질수록 증가하는 경향을 보였으며, 20 wt%~50 wt%의 농도 범위와 $50^{\circ}C~105^{\circ}C$의 온도 범위에서 식각속도는 $10\mu \textrm{m}/hr~250\mu\textrm{m}/hr$로서 큰 폭으로 변화하였다. 식각된 표면의 거칠기중 hillock의 발생은 (100)면과 (111)면의 식각 속도 비율이 커질수록 증가함을 알 수 있었다.

  • PDF

태양전지 제작을 위한 Hollow Cathode Plasma System의 실리콘 건식식각에 관한 연구 (A study on Silicon dry Etching for Solar Cell Fabrication Using Hollow Cathode Plasma System)

  • 유진수;;이준신
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제53권2호
    • /
    • pp.62-66
    • /
    • 2004
  • This paper investigated the characteristics of a newly developed high density hollow cathode plasma (HCP) system and its application for the etching of silicon wafers. We used SF$_{6}$ and $O_2$ gases in the HCP dry etch process. Silicon etch rate of $0.5\mu\textrm{m}$/min was achieved with $SF_6$$O_2$plasma conditions having a total gas pressure of 50mTorr, and RF power of 100 W. This paper presents surface etching characteristics on a crystalline silicon wafer and large area cast type multicrystlline silicon wafer. The results of this experiment can be used for various display systems such as thin film growth and etching for TFT-LCDs, emitter tip formations for FEDs, and bright plasma discharge for PDP applications.s.

HDP를 이용한 실리콘 단결정 Deep Dry Etching에 관한 특성 (Characterization of Deep Dry Etching of Silicon Single Crystal by HDP)

  • 박우정;김장현;김용탁;백형기;서수정;윤대호
    • 한국세라믹학회지
    • /
    • 제39권6호
    • /
    • pp.570-575
    • /
    • 2002
  • 현재 전기 . 전자 기술의 추세는 소형화를 비롯하여 집적화, 저전력화, 저가격화의 장점을 가진 MEMS(Micro Electro Mechanical Systems) device의 개발에 주력하고 있으며, 이를 위해서는 고종횡비와 높은 식각 속도를 가진 HDP(High Density Plasma) etching 기술 개발이 필수적이라 할 수 있다. 이를 위하여 우리는 Inductively Coupled Plasma(ICP) 장비를 이용하여 각 공정 변수에 의한 실리콘 deep trench식각 반응을 연구하였다. 실험 공정 변수인 platen power, etch/passivation cycle time에서 etching 단계 시간에 따른 변화와 SF$_{6}$:C$_4$F$_{8}$ 가스유량을 변화시켜 연구하였으며 또한 이들의 profile, scallops, 식각 속도, 균일도, 선택비도 관찰하였다.