• Title/Summary/Keyword: SiC particle

Search Result 519, Processing Time 0.027 seconds

The Kinetics of $Si_3N_4$ Formation from Korean Rice Hulls (국산 왕겨로부터 질화규소 형성에 관한 속도론적 연구)

  • 강상원;천성순
    • Journal of the Korean Ceramic Society
    • /
    • v.16 no.2
    • /
    • pp.99-105
    • /
    • 1979
  • Themogravimetric analysis was used to investigate the kinetics of the $Si_3N_4$ formation from Korean rice hulls in the temperature range from $1990^{\circ}C$ to $1370^{\circ}C$. The experimental results indicated that the reaction rate controlling step in the overall process is the diffusion of CO gas from the surface of carbon particle to main body of $N_2$ gas fluid through the stagnant gas film around the carbon particle. The kinetics followed a nearly linear rate law at the initil reaction stage. The activiation energy for the formation of $Si_3N_4$ from Korean rice hulls was 43.5Kcal/mole.

  • PDF

Fabrication of Porous SiC Ceramics by Partial Sintering and their Properties (부분소결공정에 의한 다공질 탄화규소 세라믹스의 제조 및 특성)

  • 김신한;김영욱;윤중열;김해두
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.7
    • /
    • pp.541-547
    • /
    • 2004
  • Addition of large particles restrains densification by small particles in mixed particle systems. In the present study, large SiC whiskers or particles were introduced into small particles for restraining densification and the mixtures were sintered using yttrium aluminum garnet (Y$_3$A1$\sub$5/O$\sub$12/, YAG) as a sintering additive. By controlling the content of large SiC whiskers or particles and the applied pressure during sintering, porous SiC ceramics, with a porosity ranging from 0.3% to 39%, were fabricated. Porosity increased with increasing the content of restraining materials. SiC whiskers were more effective than large SiC partcles for restraining densification. Permeability of the porous SiC ceramics increased with increasing the porosity. Flexural strength decreased with increasing porosity. A noticeable increase in strain to failure was observed in the porous ceramics with a porosity ranging from 18% to 39%.

Microstructure and Formability of Semi-solid A390 Alloys made by uniform heating (균일가열법으로 제조한 반용융 A390합금의 미세조직 및 성형성)

  • 엄정필;장동훈;김득규;윤병은;임수근
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1997.06a
    • /
    • pp.160-173
    • /
    • 1997
  • Microstructure of hypereutectic Al-17wt.% Si alloy, fabricated by mechanical stirring and by reheating at semi-solid state, was investigated by optical microscope. Flow behavior semi-solid metal also was investigated at diffentent mould temperatures 280$^{\circ}C$, 290$^{\circ}C$ and 300$^{\circ}C$. Size of silicon particles were increased over 100$\mu\textrm{m}$ during solidification as a result of stirring. It is considered as microstructural coarsening by bonding between neighbouring primary silion particles during stirring of slurry. In case of reheating at semi-solid state, however, primary silicon particle was not increased at size of 40$\mu\textrm{m}$ and nearly spherical aluminum solde particle also could be obtained uniformly in distribution. The fludity of Al-17wt.% Si alloys at semi-solid state was improved when solid fraction was 0.7 at mould temperature of 300$^{\circ}C$ than other conditions.

  • PDF

The Effect of SiC Nanopaticles on Interface of Micro-bump manufactured by electroplating (나노입자가 전해도금으로 형성된 미세범프의 계면에 미치는 영향)

  • Sin, Ui-Seon;Lee, Se-Hyeong;Lee, Chang-U;Jeong, Seung-Bu;Kim, Jeong-Han
    • Proceedings of the KWS Conference
    • /
    • 2007.11a
    • /
    • pp.245-247
    • /
    • 2007
  • Sn-base solder bump is mainly used in micro-joining for flip chip package. The quantity of intermetallic compounds that was formed between Cu pad and solder interface importantly affects reliability. In this research, micro-bump was fabricated by two binary electroplating and the intermetallic compounds(IMCs) was estimated quantitatively. When the micro Sn-Ag solder bump was made by electroplating, SiC powder was added in the plating solution for protecting of intermetallic growth. Then, the intermetallic compounds growth was decrease with increase of amount of SiC power. However, if the mount of SiC particle exceeds 4 g/L, the effect of the growth restraint decrease rapidly.

  • PDF

Mechanical Properties of Chemical Vapor Deposited SiC Coating Layer (화학증착법에 의하여 제조된 탄화규소 코팅층의 기계적 특성)

  • Lee, Hyeon-Keun;Kim, Jong-Ho;Kim, Do-Kyung
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.8 s.291
    • /
    • pp.492-497
    • /
    • 2006
  • SiC coating has been introduced as protective layer in TRISO nuclear fuel particle of High Temperature Gas cooled Reactor (HTGR) due to excellent mechanical stability at high temperature. In order to inhibit the failure of the TRISO particles, it is important to evaluate the fracture strength of the SiC coating layer. ]n present work, thin silicon carbide coating was fabricated using chemical vapor deposition process with different microstructures and thicknesses. Processing condition and surface status of substrate.affect on the microstructure of SiC coating layer. Sphere indentation method on trilayer configuration was conducted to measure the fracture strength of the SiC film. The fracture strength of SiC film with different microstructure and thickness were characterized by trilayer strength measurement method nanoindentation technique was also used to characterize the elastic modulus and th ε hardness of the SiC film. Relationships between microstructure and mechanical properties of CVD SiC thin film were discussed.

Development of Micro Tensile Test of CVD-SiC coating Layer for TRISO Nuclear Fuel Particles at elevated temperature

  • Lee, Hyun-Min;Park, Kwi-Il;Kim, Do-Kyung
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2012.05a
    • /
    • pp.95.1-95.1
    • /
    • 2012
  • Very High Temperature gas cooler Reactor (VHTR) has been considered as one of the most promising nuclear reactor because of many advantages including high inherent safety to avoid environmental pollution, high thermal efficiency and the role of secondary energy source. The TRISO coated fuel particles used in VHTR are composed of 4 layers as OPyC, SiC, IPyC and buffer PyC. The significance of CVD-SiC coatings used in tri-isotropic(TRISO) nuclear coated fuel particles is to maintain the strength of the whole particle. Various methods have been proposed to evaluate the mechanical properties of CVD-SiC film at room temperature. However, few works have been attempted to characterize properties of CVD-SiC film at high temperature. In this study, micro tensile system was newly developed for mechanical characterization of SiC thin film at elevated temperature. Two kinds of CVD-SiC films were prepared for micro tensile test. SiC-A had [111]-preferred orientation, while SiC-B had [220]-preferred orientation. The free silicon was co-deposited in SiC-B coating layer. The fracture strength of two different CVD-SiC films was characterized up to $1000^{\circ}C$.The strength of SiC-B film decreased with temperature. This result can be explained by free silicon, observed in SiC-B along the columnar boundaries by TEM. The presence of free silicon causes strength degradation. Also, larger Weibull-modulus was measured. The new method can be used for thin film material at high temperature.

  • PDF

Wear Characteristics of SiC by Sintered Temperature and SiO2 Contents (소결온도 및 SiO2 첨가량에 따른 탄화규소의 마모 특성)

  • Park, Sung-Ho;Park, Won-Jo;Yoon, Han-Ki
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.32 no.11
    • /
    • pp.1003-1009
    • /
    • 2008
  • In this study, liquid phase sintered SiC (LPS-SiC) materials were made by hot pressing method. The particle size of nano-SiC powder was 30nm. Alumina ($Al_2O_3$), yttria ($Y_2O_3$) and silica ($SiO_2$) were used for sintering additives. To investigate effects of $SiO_2$, ratios of $SiO_2$ contents were changed by five kinds. Materials have been sintered for 1 hour at $1760^{\circ}C$, $1780^{\circ}C$ and $1800^{\circ}C$ under the pressure of 20MPa. The system of sintering additives which affects a property of sintering as well as the influence depending on compositions of sintering additives were investigated by measurement of density, mechanical properties such as flexural strength, vickers hardness and sliding wear resistance were investigated to make sure of the optimum condition which is about matrix of $SiC_f$/SiC composites. The abrasion test condition apply to load of 20N at 100RPM for 20min. Sintered density, flexural strength of fabricated LPS-SiC increased with increasing the sintering temperature. And in case of LPS-SiC with low $SiO_2$, sliding wear resistance has very excellent. Monolithic SiC $1800^{\circ}C$ sintering temperatures and 3wt% have excellent wear resistance.

Synthesis of Silicon Carbide Nano-Powder from a Silicon-Organic Precursor by RF Inductive Thermal Plasma (RF 유도 열플라즈마를 이용한 유기 용매로 부터의 탄화규소 나노 분말 합성)

  • Ko, Sang-Min;Koo, Sang-Man;Kim, Jin-Ho;Cho, Woo-Seok;Hwang, Kwang-Taek
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.523-527
    • /
    • 2012
  • Silicon carbide (SiC) has recently drawn an enormous amount of industrial interest due to its useful mechanical properties, such as its thermal resistance, abrasion resistance and thermal conductivity at high temperatures. In this study, RF thermal plasma (PL-35 Induction Plasma, Tekna CO., Canada) was utilized for the synthesis of high-purity SiC powder from an organic precursor (hexamethyldisilazane, vinyltrimethoxysilane). It was found that the SiC powders obtained by the RF thermal plasma treatment included free carbon and amorphous silica ($SiO_2$). The SiC powders were further purified by a thermal treatment and a HF treatment, resulting in high-purity SiC nano-powder. The particle diameter of the synthesized SiC powder was less than 30 nm. Detailed properties of the microstructure, phase composition, and free carbon content were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), a thermogravimetric (TG) analysis, according to the and Brunauer-Emmett-Teller (BET) specific surface area from N2 isotherms at 77 K.

Effect of Ceramic Fibers and SiC Opacifiers on Thermal Conductivities of Fumed Silica-Based Thermal Insulation Media (탄화규소 불투명화재와 세라믹섬유가 Fumed 실리카 단열재의 열전도도에 미치는 영향)

  • Kwon, Young-Pil;Kwon, Hyuk-Chon;Park, Sung;Lee, Jae-Chun
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.12
    • /
    • pp.747-750
    • /
    • 2007
  • The thermal conductivities of nano-sized fumed silica-based insulation media were investigated by varying a mean particle size of the silicon carbide opacifiers and ceramic fiber content. Opacifying effect of ceramic fiber and silicon carbide powders was discussed in terms of their content and the mean particle size of them. As the fiber contents increased from 10 wt% to 30 wt% in a material, its thermal conductivity at temperatures of about $620^{\circ}C$ decreased from 0.171 $Wm^{-1}K^{-1}$ to 0.121 $Wm^{-1}K^{-1}$. Meanwhile, the thermal conductivity at temperatures of about $625^{\circ}C$ decreased from 0.128 $Wm^{-1}K^{-1}$ to 0.092 $Wm^{-l}K^{-1}$ as the mean SiC particle size decreased from $31{\mu}m$ to $10{\mu}m$.

Application of the full factorial design to modelling of Al2O3/SiC particle reinforced al-matrix composites

  • Altinkok, Necat
    • Steel and Composite Structures
    • /
    • v.21 no.6
    • /
    • pp.1327-1345
    • /
    • 2016
  • $Al_2O_3$/SiC particulate reinforced (Metal Matrix Composites) MMCs which were produced by using stir casting process, bending strength and hardening behaviour were obtained using an analysis of variance (ANOVA) technique that uses full factorial design. Factor variables and their ranges were: particle size $2-60{\mu}m$; the stirring speed 450 rpm, 500 rpm and the stirring temperature $620^{\circ}C$, $650^{\circ}C$. An empirical equation was derived from test results to describe the relationship between the test parameters. This model for the tensile strength of the hybrid composite materials with $R^2$ adj = 80% for the bending strength $R^2$ adj = 89% were generated from the data. The regression coefficients of this model quantify the tensile strength and bending strengths of the effects of each of the factors. The interactions of all three factors do not present significant percentage contributions on the tensile strength and bending strengths of hybrid composite materials. Analysis of the residuals versus was predicted the tensile strength and bending strengths show a normalized distribution and thereby confirms the suitability of this model. Particle size was found to have the strongest influence on the tensile strength and bending strength.