• Title/Summary/Keyword: Selective laser melting(SLM)

Search Result 46, Processing Time 0.026 seconds

Influence of Hot Isostatic Press on Quasi-static and Dynamic Mechanical Properties of SLM-printed Ti-6Al-4V Alloy (SLM 방식으로 적층 제조된 Ti-6Al-4V 합금의 HIP 처리에 따른 준정적 및 동적 기계적 특성 변화)

  • Jang, Ji-Hoon;Choi, Young-Sin;Kim, Hyeoung-Kyun;Lee, Dong-Geun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.33 no.3
    • /
    • pp.99-106
    • /
    • 2020
  • Selective laser melting (SLM) is an additive manufacturing process by melting metallic powders and stacking into layers, and can product complex shapes or near-net-shape (NNS) that are difficult to product by conventional processes. Also, SLM process is able to raise the efficiency of production by creating a streamlined manufacturing process. For manufacturing in SLM process using Ti-6Al-4V powder, analysis of microstructural evolution and evaluation of mechanical properties are essential because of rapid melting and solidification process of powders according to high laser power and rapid scan speed. In addition, it requires a post-processing because the soundness and mechanical properties are degraded by defects such as pore, un-melted powder, lack-of-fusion, etc. In this study, hot isostatic press (HIP) was conducted as a post-processing on SLM-printed Ti-6Al-4V alloy. Microstructure of post-processed Ti-6Al-4V alloy was compared to as-built Ti-6Al-4V, and the evolution of quasi-static (Vickers hardness, room temperature tensile characteristic) and dynamic (high-cycle fatigue characteristic) mechanical properties were analyzed.

Analysis of the microstructure of melting-pool in aluminum specimens fabricated by SLM technique (SLM 기법으로 제작한 알루미늄 시편 내부 멜팅풀 미세조직 분석)

  • Kim, Moo-Sun
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.12
    • /
    • pp.115-119
    • /
    • 2020
  • Selective Laser Melting (SLM) technology is state-of-the-art additive manufacturing process technology that produces a three-dimensional structure by irradiating a laser on a fine metal powder to perform the fusion of a specific area and repeat this process. Owing to the characteristics of the additive manufacturing process, the melting phenomenon of the metal material by the laser has directionality depending on the process conditions, such as the irradiation direction of the laser and the build-up direction. For this reason, the composition of the metal material in the structure exhibits non-uniform characteristics. In this study, aluminum (AlSi10Mg) specimens were manufactured by applying SLM technology, and the material composition characteristics of the specimen were analyzed. The specimens were manufactured as cylinders by the build-up orientation of 0°, 45°, and 90°. The surface morphology of the specimen plane was analyzed optically. TEM analysis was performed on the core and the interface of the melting-pool inside the specimen generated by laser irradiation. The analysis results confirmed that there was a difference between the nano cell structure of the core and the interface of the melting-pool, and that the composition ratio of Si appeared higher at the interface than at the core of the cell.

A Finite Element Model of Melt Pool for the Evaluation of Selective Laser Melting Process Parameters (선택적 레이저 용융 공정의 공정변수 평가를 위한 용융풀 유한요소 모델)

  • Lee, Kanghyun;Yun, Gun Jin
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.23 no.3
    • /
    • pp.195-203
    • /
    • 2020
  • Selective laser melting(SLM) is one of the powder bed fusion(PBF) processes, which enables quicker production of nearly fully dense metal parts with a complex geometry at a moderate cost. However, the process still lacks knowledge and the experimental evaluation of possible process parameter sets is costly. Thus, this study presents a finite element analysis model of the SLM process to predict the melt pool characteristics. The physical phenomena including the phase transformation and the degree of consolidation are considered in the model with the effective method to model the volume shrinkage and the evaporated material removal. The proposed model is used to predict the melt pool dimensions and validated with the experimental results from single track scanning process of Ti-6Al-4V. The analysis result agrees with the measured data with a reasonable accuracy and the result is then used to evaluated each of the process parameter set.

Microstructure-Properties Relationships of Ti-6Al-4V Parts Fabricated by Selective Laser Melting

  • Mezzetta, Justin;Choi, Joon-Phil;Milligan, Jason;Danovitch, Jason;Chekir, Nejib;Bois-Brochu, Alexandre;Zhao, Yaoyao Fiona;Brochu, Mathieu
    • International Journal of Precision Engineering and Manufacturing-Green Technology
    • /
    • v.5 no.5
    • /
    • pp.605-612
    • /
    • 2018
  • This work investigates the relationships between the static mechanical properties of Ti-6Al-4V manufactured through selective laser melting (SLM) and post-process heat treatments, namely stress relieve, annealing and hot isostatic pressing (HIP). In particular, Ti-6Al-4V parts were fabricated in three different build orientations of X, Z, and $45^{\circ}$ to investigate the multi-directional mechanical properties. The results showed that fully densified Ti-6Al-4V parts with densities of up to 99.5% were obtained with optimized SLM parameters. The microstructure of stress relieved and mill annealed samples was dominated by fine ${\alpha}^{\prime}$ martensitic needles. After HIP treatment, the martensite structure was fully transformed into ${\alpha}$ and ${\beta}$ phases (${\alpha}+{\beta}$ lamellar). Within the realm of tensile properties, the yield and ultimate strength values were found statistically similar with respect to the built orientation for a given heat treatment. However, the ductility was found orientation dependent for the HIP samples, where a lower value was observed for samples built in the X direction.

Effect of support thickness on the adaptation of Co-Cr alloy copings fabricated using selective laser melting (출력 지지대 두께가 선택적 레이저 용융법으로 제작된 금속 하부구 조물 적합도에 미치는 영향)

  • Jae-Hong Kim;Se-Yeon Kim
    • Journal of Technologic Dentistry
    • /
    • v.45 no.3
    • /
    • pp.67-73
    • /
    • 2023
  • Purpose: This in vitro study aimed to evaluate the clinical acceptability of precision of fit of the support thickness of Co-Cr alloy copings fabricated using selective laser melting (SLM). Methods: Thirty dental stone models of maxillary left molar abutments were manufactured, images were taken using a scanner, and a computer-aided design program was used to design the form of a conventional metal ceramic crown coping. Overall, 30 single copings were made from Co-Cr alloy using SLM and divided into three support radius groups (0.1, 0.25, and 0.35 mm) of 10 for each. Digitized data were superimposed with three-dimensional inspection software to quantitatively obtain the machinability of a ceramic crown coping, and visual differences were confirmed using a color map. The root mean square values of the ceramic crown coping group were statistically analyzed using one-way analysis of variance (α=0.05). Results: The precision of fit was superior with 0.25 mm compared with 0.1 mm and 0.35 mm, and the results exhibited significant differences (p<0.05). All specimens showed that various support thicknesses did not exceed the clinically permitted value of 120 ㎛, which mean that more than 0.1 mm and 0.35 mm of support radius for SLM was adequate. Conclusion: The support thickness of Co-Cr alloy restoration fabricated using SLM is shown to affect the adaptation.

Microstructures and Characterization of Al-Si-Mg Alloy Processed by Selective Laser Melting with Post-Heat-treatment (선택적 레이저 용융공정으로 제조된 Al-Si-Mg 합금의 열처리에 따른 미세조직 및 특성평가)

  • Lee, Gi Seung;Eom, Yeong Seong;Kim, Kyung Tae;Kim, Byoung Kee;Yu, Ji Hun
    • Journal of Powder Materials
    • /
    • v.26 no.2
    • /
    • pp.138-145
    • /
    • 2019
  • In this study, Al-Si-Mg alloys are additively manufactured using a selective laser melting (SLM) process from AlSi10Mg powders prepared from a gas-atomization process. The processing parameters such as laser scan speed and laser power are investigated for 3D printing of Al-Si-Mg alloys. The laser scan speeds vary from 100 to 2000 mm/s at the laser power of 180 and 270 W, respectively, to achieve optimized densification of the Al-Si-Mg alloy. It is observed that the relative density of the Al-Si-Mg alloy reaches a peak value of 99% at 1600 mm/s for 180 W and at 2000 mm/s for 270W. The surface morphologies of the both Al-Si-Mg alloy samples at these conditions show significantly reduced porosities compared to those of other samples. The increase in hardness of as-built Al-Si-Mg alloy with increasing scan speed and laser power is analyzed due to high relative density. Furthermore, it was found that cooling conditions after the heat-treatment for homogenization results in the change of dispersion status of Si phases in the Al-Si matrix but also affects tensile behaviors of Al-Si-Mg alloys. These results indicate that combination between SLM processing parameters and post-heat treatment should be considered a key factor to achieve optimized Al-Si alloy performance.

Comparison of the Marginal Fitness of Ceramic Co-Cr Metal Crown (도재용 코발트-크롬 금속관의 변연적합도 비교)

  • Jeon, Byung-Wook;Kim, Bu-Sob
    • Journal of Technologic Dentistry
    • /
    • v.37 no.2
    • /
    • pp.69-76
    • /
    • 2015
  • Purpose: In this study, the marginal fitness of ceramic Co-Cr metal crown made by precision casting, milling, and selective laser melting method were compared. Methods: The ceramic Co-Cr metal crown manufactured by precision casting used the lost wax(LC specimen) method. The abutment were scanned and then made by milling(CM specimen), selective laser melting(CS specimen) method. The specimen were cut bucco-lingual and mesio-distal, and absolute marginal discrepancy and marginal gap were measured using a digital microscope. The surface roughness of the crown was also observed. Results: On the bucco-lingual axial, absolute marginal discrepancy was the LC specimen $31.72({\pm}4.58){\mu}m$, the CM specimen $78.29({\pm}3.28){\mu}m$ and the CS specimen $143.13({\pm}3.83){\mu}m$, respectively. On the bucco-lingual axial, marginal gap was the LC specimen $22.70({\pm}1.46){\mu}m$, the CM specimen $22.70({\pm}1.49){\mu}m$ and CS specimen $99.60({\pm}1.57){\mu}m$, respectively. Conclusion: For ceramic Co-Cr metal crowns, LC specimen was superior for absolute marginal discrepancy and marginal gap. The surface of metal crowns by selective laser melting were the roughest.

Study on Microstructures and Hardness of STS316L Fabricated by Selective Laser Melting (선택적 레이저 용융공정을 이용한 316L 스테인리스강 분말 3차원 조형체의 미세조직 및 경도 연구)

  • Shin, Gi Hun;Choi, Joon Phil;Kim, Kyung Tae;Kim, Byoung Kee;Yu, Ji Hun
    • Journal of Powder Materials
    • /
    • v.24 no.3
    • /
    • pp.210-215
    • /
    • 2017
  • In this study, STS316L powders prepared by gas atomization are used to manufacture bulk structures with dimensions of $10{\times}10{\times}10mm^3$ using selective laser melting (SLM). The microstructures and hardness of the fabricated 316L stainless steel has been investigated with the laser beam overlap varied from 10% to 70%. The microstructures of the fabricated STS316L samples show a decrease in the balling and satellite of powders introducing defect in the bulk samples and the porosity caused by the gap between the molten metal pools disappearing as the overlap ratio increases, whereas a low overlap ratio results in significant balling and a large amount of isolated powders due to the increased gap between the melt pools. Furthermore, the highest value in Vickers hardness is obtained for the sample fabricated by 30% overlapped laser beams. These results show that the overlap ratio of laser beams in the SLM process should be considered as an important process parameter.

Selective laser melted titanium implants: a new technique for the reconstruction of extensive zygomatic complex defects

  • Rotaru, Horatiu;Schumacher, Ralf;Kim, Seong-Gon;Dinu, Cristian
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • v.37
    • /
    • pp.1.1-1.6
    • /
    • 2015
  • The restoration of extensive zygomatic complex defects is a surgical challenge owing to the difficulty of accurately restoring the normal anatomy, symmetry, proper facial projection and facial width. In the present study, an extensive post-traumatic zygomatic bone defect was reconstructed using a custom-made implant that was made with a selective laser melting (SLM) technique. The computer-designed implant had the proper geometry and fit perfectly into the defect without requiring any intraoperative adjustments. A one-year follow-up revealed a stable outcome with no complications.

A study about sculpture characteristic of SKD61 tool steel fabricated by selective laser melting(SLM) process (SLM 공정으로 제작된 SKD61 공구강의 조형 특성에 관한 연구)

  • Yun, Jaecheol;Choe, Jungho;Kim, Ki-Bong;Yang, Sangsun;Yang, Dong-Yeol;Kim, Yong-Jin;Lee, Chang-Woo;Yu, Ji-Hun
    • Journal of Powder Materials
    • /
    • v.25 no.2
    • /
    • pp.137-143
    • /
    • 2018
  • In this study, two types of SKD61 tool-steel samples are built by a selective laser melting (SLM) process using the different laser scan speeds. The characteristics of two kinds of SKD61 tool-steel powders used in the SLM process are evaluated. Commercial SKD61 tool-steel power has a flowability of 16.68 sec/50 g and its Hausner ratio is calculated to be 1.25 by apparent and tapped density. Also, the fabricated SKD61 tool steel powder fabricated by a gas atomization process has a flowability of 21.3 sec/50 g and its Hausner ratio is calculated to be 1.18. Therefore, we confirmed that the two powders used in this study have excellent flowability. Samples are fabricated to measure mechanical properties. The highest densities of the SKD61 tool-steel samples, fabricated under the same conditions, are $7.734g/cm^3$ (using commercial SKD61 powder) and $7.652g/cm^3$ (using fabricated SKD61 powder), measured with Archimedes method. Hardness is measured by Rockwell hardness testing equipment 5 times and the highest hardnesses of the samples are 54.56 HRC (commercial powder) and 52.62 HRC (fabricated powder). Also, the measured tensile strengths are approximately 1,721 MPa (commercial SKD61 powder) and 1,552 MPa (fabricated SKD61 powder), respectively.