Ti 합금의 기계가공 방법에 따른 경도 변화에 관한 연구 (Hardness of Ti alloys by mechanical processing methods)

  • 반재삼;김규하;정상원;기강호;조규종
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.792-795
    • /
    • 2002
  • In previous researches, it is reported that Ti-10Ta-10Nb is robuster than Ti-6A1-4V which is used as a biomaterial in a experiment of cytotoxicity. Ti-10Ta-10Nb has enough hardness to be required as a biomaterial because the change of its hardness can be controlled more than 100% according to heat treatment condition and manufacturing condition. There are many hardness changing condition including Cast Homogenization, Solution treatment. Forging, Rolling in this research. The changing form and amount of new Ti-10Ta-10Nb to be developed in this researches, are measured as quantitative. Specially, the changing hardness amount of the specimen that is manufactured in single phase temperature, i.e. 80$0^{\circ}C$, are measured in case of high temperature rolling and high temperature cast condition.

  • PDF

Simulation of impact toughness with the effect of temperature and irradiation in steels

  • Wang, Chenchong;Wang, Jinliang;Li, Yuhao;Zhang, Chi;Xu, Wei
    • Nuclear Engineering and Technology
    • /
    • 제51권1호
    • /
    • pp.221-227
    • /
    • 2019
  • One of the important requirements for the application of reduced activation ferritic/martensitic steel is to retain proper mechanical properties in irradiation and high temperature conditions. In order to simulate the impact toughness with the effect of temperature and irradiation, a simulation model based on energy balance method consisted of crack initiation, plastic propagation and cleavage propagation stages was established. The effect of temperature on impact toughness was analyzed by the model and the trend of the simulation results was basicly consistent with the previous experimental results of CLAM steels. The load-displacement curve was simulated to express the low temperature ductile-brittle transition. The effect of grain size and inclusion was analyzed by the model, which was consistent with classical experiment results. The transgranular-intergranular transformation in brittle materials was also simulated.

이속압연된 Cu-3.0Ni-0.7Si 합금의 어닐링에 따른 두께방향으로의 미세조직 및 기계적 특성 변화 (Change in Microstructure and Mechanical Properties through Thickness with Annealing of a Cu-3.0Ni-0.7Si Alloy Deformed by Differential Speed Rolling)

  • 이성희
    • 한국재료학회지
    • /
    • 제28권5호
    • /
    • pp.295-300
    • /
    • 2018
  • Effects of annealing temperature on the microstructure and mechanical properties through thickness of a Cu-3.0Ni-0.7Si alloy processed by differential speed rolling are investigated in detail. The copper alloy with a thickness of 3 mm is rolled to a 50 % reduction at ambient temperature without lubricant and subsequently annealed for 0.5 h at $200-900^{\circ}C$. The microstructure of the copper alloy after annealing is different in the thickness direction depending on the amount of the shear and compressive strain introduced by the rolling; the recrystallization occurs first in the upper roll side and center regions which are largely shear-deformed. The complete recrystallization occurs at an annealing temperature of $800^{\circ}C$. The grain size after the complete recrystallization is finer than that of the conventional rolling. The hardness distribution of the specimens annealed at $500-700^{\circ}C$ is not uniform in the thickness direction due to partial recrystallization. This ununiformity of hardness corresponds well to the amount of shear strain in the thickness direction. The average hardness and ultimate tensile strength has the maximum values of 250 Hv and 450 Mpa, respectively, in the specimen annealed at $400^{\circ}C$. It is considered that the complex mode of strain introduced by rolling directly affects the microstructure and the mechanical properties of the annealed specimens.

Lead Screw 공정 설계를 위한 전조 해석 (Thread Rolling Analysis for Lead Screw Process Design)

  • 신명수;차성훈;김종봉;김종호;나승우
    • Elastomers and Composites
    • /
    • 제44권4호
    • /
    • pp.391-396
    • /
    • 2009
  • 본 연구에서는 전조공정의 수치해석을 수행하였다. 해석을 이용한 공정 인자 설계에 앞서서, 효율적이고 신뢰성 있는 해석을 위한 해석 조건에 대하여 연구를 수행하였다. 치형의 개수와 요소의 수에 대한 해석 결과를 바탕으로 해석의 정도를 보장하고 효율적으로 해석을 수행할 수 있는 조건을 설정하였다. 그리고, 프랭크 각도와 치형의 끝단부 라운드 등의 금형의 형상과 성형 온도가 유효 응력, 유효 변형율, 전조력, 그리고 크랙 발생에 미치는 영향을 알아보았다. 해석은 DEFORM-3D를 이용하여 수행하였다. 프랭크 각도와 치형의 끝단 부 라운드는 전조력에 영향을 미치는 것을 확인할 수 있었으며, 성형 온도 조건에 따라서 유효 변형률과 전조력, 그리고 크랙을 예상 할 수 있었다.

Ti-6Al-4V 합금의 형상 링 압연공정 설계 및 제조기술 (Design and Manufacturing processes of Ti-6Al-4V profiled ring-products)

  • 김국주;김남용;이진모;염종택
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.72-75
    • /
    • 2009
  • Design and Manufacturing processes of Ti-6Al-4V profiled ring-products were investigated with three-dimensional FEM simulation and experimental analyses. FEM simulation for the ring-rolling process was used to calculate the state variables such as strain, strain rate and temperature. In the simulation results of strain and temperature distributions for a plane ring rolling process, the strain level at the surface area is higher than that at the mid-plane, but the temperature level at the surface area is lower than that at mid-plane due to heat transfer between the workpiece and the work roll. These distributions showed a great influence on the evolution of microstructure in different positions. In order to induce the uniform deformation of the profile ring and reduce the applied load, the final blank was prepared by two-step processes. The mechanical properties of Ti-6Al-4V alloy ring products made in this work were investigated with tensile and impact tests and analyzed with the evolution of microstructures during the ring rolling process.

  • PDF

고탄소강의 구상화속도에 미치는 초기 미세조직, 냉간압연 및 온도의 영향 (Effect of Initial Microstructure, Cold Rolling and Temperature on the Spheroidization Rate of Cementite in High Carbon Steel)

  • 김준호;하태권
    • 소성∙가공
    • /
    • 제22권3호
    • /
    • pp.158-164
    • /
    • 2013
  • The spheroidization behavior of cementite in a SK85 high carbon steel was investigated in this study. Fine and coarse pearlite microstructures were obtained by appropriate heat treatments according to the TTT diagram of SK85 high carbon steel. Hot rolled plates of SK85 steel were austenitized at $800^{\circ}C$ for 2 hrs and then put directly into a salt bath at either $570^{\circ}C$ or $670^{\circ}C$ to obtain a fine pearlite (FP) structure and a coarse pearlite (CP) structure, respectively. Cold rolling was subsequently conducted on those specimens with reduction ratios from 0.2 to 0.4. Spheroidization heat treatments were conducted at the subcritical temperatures of 600 and $720^{\circ}C$ for 1 to 32 hrs to elucidate the effect of initial microstructures, heat treatment temperature, and cold reduction ratios on the cementite spheroidization rate. Spheroidization proceeded with fragmentation of cementite plates, spheroidization of the cementite platelets, and coarsening consecutively. Mechanical fragmentation of cementite by cold rolling expedited the rate of spheroidization. The spheroidization rate of FP was much more rapid than that of CP and the spheriodization rate increased with increases in the cold reduction ratio.

2.25% Cr-1%Mo 합금계 열연강판 제조기술 (Manufacturing 2.25Cr-1Mo Steel In Hot Rolling Strip Mill)

  • 노태훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.390-398
    • /
    • 1999
  • The thermomechanical control process(in hot rolling strip mill) was employed to produce 2.25Cr-1Mo steel, which is to be construction material for the steam generator for power plant. Although the Conventional processes has been the primary means of producing the 2.25Cr-1Mo steel, an alternative method was used to meet the specification of ASTM heat treatment for A387-22-Classl using autotempering after coiling in hot rolling strip mill. The microstructures, tensile properties at various temperatures, and creep-rupture properties have been investigated to compare the properties with those of materials produced by the conventional process and to certify the application of the thermomechanical control process to an actual process of manufacturing 2.25-Cr-1Mo steel, this in turn, will reduce the cost of the process. About 14 to 34% glanular bainite (remainder proetectoid ferrite) formed in a coil, and this variety of volume fraction stems from the different cooling rates, which varies with position of the coil after coiling. Tensile testing from room temperature to 700$^{\circ}C$ indicated that strength increases with test temperature showing peaks at around 600$^{\circ}C$. Creep-rupture properties have been being investigated at the temperature of 500$^{\circ}C$ with 27.5, 32kg/$\textrm{mm}^2$ loads and have showed no rupture for over 1000 hours.

  • PDF

후판 압연시 선단부 두께편차 보상을 위한 롤갭 설정에 관한 연구 (A Study on the Roll Gap Set-up to Compensate Thickness Variation at Top-end in Plate Rolling)

  • 임홍섭;주병돈;이건엽;서재형;문영훈
    • 소성∙가공
    • /
    • 제18권4호
    • /
    • pp.290-295
    • /
    • 2009
  • The roll gap set-up in the finishing mill is one of the most important technologies in the hot plate rolling process. As the target thickness can be obtained by the correct set-up of the roll gap, improving the roll gap set-up technology is very critical for plate thickness accuracy. The main cause of thickness variation in hot plate mills is the non-uniform temperature distribution along the length of the slab. The objective of this study is to adjust the roll gap set-up for the thickness accuracy of plate in hot rolling process considering top-end temperature drop. Therefore this study has concentrated on determining the correct amounts of thickness variation according to top-end temperature drop and roll gap to compensate thickness variation. The control method of roll gap set-up which can improve the thickness accuracy was proposed. The off-line simulation of compensated roll gap significantly decreases top-end thickness variation.

Ag-CdO계 전기접점재료의 미세조직에 미치는 열처리 조건과 산화 공정의 영향 (The Effect of The Heat Treatment Condition and the Oxidation Process on the Microstructure of Ag-CdO Contact Materials)

  • 권기봉;남태운
    • 한국주조공학회지
    • /
    • 제25권6호
    • /
    • pp.226-232
    • /
    • 2005
  • Contact material is widely used in the field of electrical parts. Ag-CdO material has a good wear resistance and stable contact resistance. In order to establish optimizing heat treatment condition, rolling temperature and oxidation process, we studied the microstructure of Ag-CdO material with various conditions. The experimental procedure were melting using high frequency induction, heat treatment, rolling and internal oxidation. And we experimented on difference process, Post-oxidaion. In this study, we obtained the optimizing heat treatment condition was $700^{\circ}C$ for 15 min. and the optimizing rolling temperature was $730^{\circ}C$. In investigation of the microstructure of oxidized material, coarse oxide and depleted oxidation layer existed. The hardness was average Hv 70. When we used Post-oxidation, oxides were finer than prior process and depleted oxidation layer did not exist. The hardness of Post-oxidation material was average Hv 80. And the optimizing rolling temperature was $800^{\circ}C$.

해양플랜트용 후판강의 미세조직과 기계적 특성에 미치는 압연 조건의 영향 (Effect of Rolling Conditions on Microstructure and Mechanical Properties of Thick Steel Plates for Offshore Platforms)

  • 김종철;서용찬;황성두;신상용
    • 한국재료학회지
    • /
    • 제28권8호
    • /
    • pp.478-488
    • /
    • 2018
  • In this study, three kinds of steels are manufactured by varying the rolling conditions, and their microstructures are analyzed. Tensile and Charpy impact tests are performed at room temperature to investigate the correlation between microstructure and mechanical properties. In addition, heat affected zone(HAZ) specimens are fabricated through the simulation of the welding process, and the HAZ microstructure is analyzed. The Charpy impact test of the HAZ specimens is performed at $-40^{\circ}C$ to investigate the low temperature HAZ toughness. The main microstructures of steels are quasi-polygonal ferrite and pearlite with fine grains. Because coarse granular bainite forms with an increasing finish rolling temperature, the strength decreases and elongation increases. In the steel with the lowest reduction ratio, coarse granular bainite forms. In the HAZ specimens, fine acicular ferrites are the main features of the microstructure. The volume fraction of coarse bainitic ferrite and granular bainite increases with an increasing finish rolling temperature. The Charpy impact energy at $-40^{\circ}C$ decreases with an increasing volume fraction of bainitic ferrite and granular bainite. In the HAZ specimen with the lowest reduction ratio, coarse bainitic ferrite and granular bainite forms and the Charpy impact energy at $-40^{\circ}C$ is the lowest.