• 제목/요약/키워드: Precipitation of $Ti_2Cu$

검색결과 14건 처리시간 0.021초

치과용 Ti-Xwt%Cu 합금의 연삭성 (Grindability of Ti-Xwt%Cu Alloys for Dental Applications)

  • 안재석
    • 대한치과기공학회지
    • /
    • 제31권4호
    • /
    • pp.31-36
    • /
    • 2009
  • This study evaluated the grindability of series of Ti-Cu alloys in order to develop a Ti alloy with better grindability than commercially pure titanium(CP Ti). Experimental Ti-Xwt%Cu alloys(X=2, 5, 10) were made in an argon-arc melting furnace. Slabs of experimental alloys were ground using a SiC abrasive wheel on an electric handpiece at circumferential speed(15000, 30000rpm) by applying a force(250, 300gr). Grindability was evaluated by measuring the amount of metal volume removed after grinding for 2 minutes. Data were compared to those for CP Ti and Ti-6wt%Al-4wt%V alloy. From results, It was observed that the grindability of Ti-Cu alloys increased with an increase in the Cu concentration compared to CP Ti, particularly the 10wt%Cu alloy exhibited the highest grindability at all speeds. By alloying with Cu, the Ti exhibited better grindability at high speed. The continuous precipitation of $Ti_2Cu$ among the ${\alpha}$-matrix grains made this material less ductile and facilitated more effective grinding because small segments more readily formed. The Ti-10wt%Cu alloy has a great potential for use as a dental machining alloy.

  • PDF

Al-Si-Mg-Cu 합금의 자동차 엔진 사용 온도에서 열처리 조건에 따른 열확산도 변화 (Change in Thermal Diffusivity of Al-Si-Mg-Cu Alloy According to Heat Treatment Conditions at Automotive Engine Operating Temperature)

  • 최세원
    • 한국재료학회지
    • /
    • 제31권11호
    • /
    • pp.642-648
    • /
    • 2021
  • The precipitation effect of Al-6%Si-0.4%Mg-0.9%Cu-(Ti) alloy (in wt.%) after various heat treatments was studied using a laser flash device (LFA) and differential scanning calorimetry (DSC). Solid solution treatment was performed at 535 ℃ for 6 h, followed by water cooling, and samples were artificially aged in air at 180 ℃ and 220 ℃ for 5 h. The titanium-free alloy Al-6%Si-0.4%Mg-0.9%Cu showed higher thermal diffusivity than did the Al-6%Si-0.4%Mg-0.9%Cu-0.2%Ti alloy over the entire temperature range. In the temperature ranges below 200 ℃ and above 300 ℃, the value of thermal diffusivity decreased with increasing temperature. As the sample temperature increased between 200 ℃ and 400 ℃, phase precipitation occurred. From the results of DSC analysis, the temperature dependence of the change in thermal diffusivity in the temperature range between 200 ℃ and 400 ℃ was strongly influenced by the precipitation of θ'-Al2Cu, β'-Mg2Si, and Si phases. The most important factor in the temperature dependence of thermal diffusivity was Si precipitation.

공침법으로 제초한 SrTiO$_3$바리스터의 전기적 특성 (The Electric Properties of SrTiO$_3$Varistor Prepared by Co-precipitation Process)

  • 이종필;신현창;최정철;최승철
    • 마이크로전자및패키징학회지
    • /
    • 제7권3호
    • /
    • pp.7-11
    • /
    • 2000
  • 공침법을 이용하여 제조한 $SrTiO_3$분말에 $CuO-SiO_2$첨가물을 혼합하여 저전압구동형 SrTiO$_3$세라믹 바리스터 소자를 제조하였다. $CuO-SiO_2$첨가물을 이용한 $SrTiO_3$세라믹 바리스터제조 공정은 복잡한 공정을 단순화시킬 수 있을 뿐만 아니라, 일반적인 소결온도보다 100~$150^{\circ}C$ 낮은 온도에서도 소결이 되었다. 이 바리스터의 비직선계수($\alpha$) 값은 첨가물 5 wt% 혼합하여 $1350^{\circ}C$에서 하소한 시편에서 8.47의 최고값을 나타냈으며, 이때의 구동전압은 7 V 이하로 낮은 구동전압을 가진 바리스터를 제조할 수 있었다.

  • PDF

Synthesis and Characterization of TiO2/CuS Nanocomposite Fibers as a Visible Light-Driven Photocatalyst

  • An, HyeLan;Kang, Leeseung;Ahn, Hyo-Jin;Choa, Yong-Ho;Lee, Chan Gi
    • 한국세라믹학회지
    • /
    • 제55권3호
    • /
    • pp.267-274
    • /
    • 2018
  • $TiO_2/CuS$ nanocomposites were fabricated by precipitation of nanosized CuS via sonochemical method on electrospun $TiO_2$ nanofibers, and their structure, chemical bonding states, optical properties, and photocatalytic activity were investigated. In the $TiO_2/CuS$ nanocomposite, the position of the conduction band for CuS was at a more negative than that of TiO; meanwhile, the position of the valence band for CuS was more positive than those for TiO, indicating a heterojunction structure belonging to type-II band alignment. Photocatalytic activity, measured by decomposition of methylene blue under visible-light irradiation (${\lambda}$ > 400 nm) for the $TiO_2/CuS$ nanocomposite, showed a value of 85.94% at 653 nm, which represented an improvement of 52% compared to that for single $TiO_2$ nanofiber (44.97% at 653 nm). Consequently, the photocatalyst with $TiO_2/CuS$ nanocomposite had excellent photocatalytic activity for methylene blue under visible-light irradiation, which could be explained by the formation of a heterojunction structure and improvement of the surface reaction by increase in surface area.

Ti가 첨가된 Mn-Cu 혼합산화물을 이용한 저온 SCR 반응 특성 (Characterization of Low Temperature Selective Catalytic Reduction over Ti Added Mn-Cu Metal Oxides)

  • 이현희;박광희;차왕석
    • 공업화학
    • /
    • 제24권6호
    • /
    • pp.599-604
    • /
    • 2013
  • 본 연구는 공침법으로 Ti가 첨가된 Mn-Cu 혼합산화물을 이용하여 $200^{\circ}C$ 이하의 저온 영역에서의 $NH_3$-SCR 반응특성에 관한 것이다. 제조된 촉매들은 BET, XRD, XPS, TPD를 이용하여 각각의 물리/화학적 특성을 분석하였다. Mn-Cu 혼합산화물은 매우 큰 비표면적과 저온에서의 높은 SCR 효율을 나타내었으며, Ti가 첨가된 경우 상대적으로 높은 SCR 효율과 $N_2$ 선택도를 나타내었다. 이러한 결과는 Ti가 첨가됨에 따라 화학 흡착된 산소종($Me-O_{ads}$)이 증가하여 NO가 $NO_2$로의 산화가 촉진되고, $Mn^{3+}$와 같은 $NH_3$의 흡착점의 수가 증가되었기 때문이다.

구리함량과 어닐링 온도가 NiTi 합금의 형상기억효과에 미치는 영향 (Effect of Cu Content and Annealing Temperature on the Shape Memory Effect of NiTi-based Alloy)

  • 양혁진;문형주;조예슬;박준홍;윤현준;최인철;오명훈
    • 열처리공학회지
    • /
    • 제37권2호
    • /
    • pp.79-85
    • /
    • 2024
  • The effects of annealing heat treatment and the addition of Cu element on the shape memory effect of the NiTi-based alloy were investigated by analyzing differential scanning calorimeter results and characterizing recovery rate through 3D scanning after Vickers hardness test. Through 3D scanning of impressions after Vickers hardness test, the strain recovery rates for specimens without annealing treatment and annealed specimens at 400, 450, and 500℃ were measured as 45.96%, 46.76%, 52.37%, and 43.57%, respectively. This is because as the annealing temperature increases, both B19' and NiTi2 phases, which can impede martensitic transformation, are incorporated within the NiTi matrix. Particularly, additional phase transformation from R-phase to B19' observed in specimens annealed at 400 and 450℃ significantly contributes to the improvement in strain recovery rates. Additionally, the results regarding the Cu element content indicate that when the total content of Ni and Cu is below 49.6 at.%, the precipitation of fine B19' and NiTi2 phases within the matrix can greatly influence the transformation enthalpy and temperature range, resulting in relatively lower strain recovery rates in NiTi alloys with a small amount of Cu element produced in this study.

Photocatalytic Degradation of Oxytetracycline Using Co-precipitation Method Prepared Fe2O3/TiO2 Nanocomposite

  • Jia, Yuefa;Liu, Chunli;Li, Rong
    • Journal of Magnetics
    • /
    • 제21권1호
    • /
    • pp.46-50
    • /
    • 2016
  • $Fe_2O_3/TiO_2$ nanocomposite were successfully synthesized by co-precipitation method using $Fe(NO_3)_3{\cdot}9H_2O$ and $Ti(SO_4)_2$ as raw materials. Structural and textural features of the mixed oxide samples were characterized by X-ray diffractometer, field emission scanning electron microscopy and energy-dispersive X-ray. The effects of initial concentration of oxytetracycline (OTC), different competitive ions and organics on the photocatalytic degradation rate of OTC by the $Fe_2O_3/TiO_2$ nanocomposite were analyzed under UV and visible light irradiation. The results indicate that the optimized initial concentration of OTC was 50 mg/L to achieve the best photocatalytic efficiency. $Cu^{2+}$, $NH_4{^+}$, $C_3H_8O$ and EDTA in the aqueous suspension were found to suppress the degradation rate of OTC, whereas the effect of $NO_3{^-}$ and $H_2C_2O_4$ can be ignored.

다기능 금속산화물의 하수처리 적용-흡착 및 살균 (The application of multifunctional metal oxide for wastewater treatment: Adsorption and disinfection)

  • 김희곤;박덕신;안병렬
    • 상하수도학회지
    • /
    • 제33권4호
    • /
    • pp.251-258
    • /
    • 2019
  • The physical treatment such as chemical precipitation or adsorption was usually added after biological treatment in wastewater treatment process since it was enforced to reduce the concentration of phosphate for wastewater effluent to 0.2 mg/L as P which was well known as one of main nutrient causing eutrophication in waterbody. Therefore, the new material functioned for both adsorption and disinfection was prepared with Fe and Cu, and $TiO_2$, respectively, by changing the ratio of concentration referred to tri-metal (TM). According to SEM-EDS, $TiO_2$ was 30~40% composition for any TM regardless of any synthesis condition. However, the ratio of composition for Fe and Cu was dependent on the initial Fe and Cu concentration, respectively. The removal efficiency of phosphate was obtained to 15% at low initial concentration and the maximum uptake (Q) was calculated to ~11 mg/g through Langmuir isotherm model using TM1 which was synthesized at 1000 mg/L, 1000 mg/L, and 2 g (10 g/L) for $Fe(NO_3)_3$, $Cu(NO_3)_2$, $TiO_2$, respectively. In disinfection test, the efficiency of virus removal using TM was increased with increase of dosage of TM and can be reached 98% at 0.2 g.

침상구조의 루틸상 TiO2 초미분체를 이용한 광촉매 반응에 대한 연구 (Study on Photocatalytic Reaction Using Acicular TiO2 Rutile Powder)

  • 황두선;구숙경;김광수;민형섭;이은구;김선재
    • 한국재료학회지
    • /
    • 제12권8호
    • /
    • pp.641-649
    • /
    • 2002
  • The redox properties of a homogeneously-precipitated $TiO_2$ rutile powder with a BET surface area of ~$200 m^2$/g, consisting of an acicular primary particle, were characterized using photocatalytic reaction in aqueous 4-chlorophenol, Cu-EDTA and Pb-EDTA solutions under ultraviolet irradiation, compared to those of commercial P-25 X$200 m_2$ powder with a spherical primary particle as well as home-made anatase $TiO_2$ powder with ~$200 m^2$/g BET surface area. Here, the anatase powder also includes mainly the primary particles very similar to the acicular shapes of the rutile $TiO_2$ powder. The rutile powder showed the fastest decomposition rate and the largest amount in the photoredor, compared with the anatase or P-25 powder, while the anatase powder unexpectedly showed the slowest rate and the smallest amount in the same experiments regardless of almost the same surface area. From results, the excellent photoredox abilities of this rutile powder appears to be due to specific powder preparation method, like a homogeneous precipitation leading to direct crystallization from the solution, regardless of their crystalline structures even when having the similar particle shape and surface area.

중금속폐수에서 구리의 전기화학적 침전처리 (Electrochemical Precipitation Treatment of Copper from an Heavymetal Wastewater)

  • 김재우;이재동;이우식;지은상
    • 한국환경보건학회지
    • /
    • 제23권3호
    • /
    • pp.1-6
    • /
    • 1997
  • This research was conducted in the laboratory to investigate an alternative of Copper(Cu) removal from an heavymetal wastewater using the electrochemical precipitation(ECP) process. The ECP unit consisted of an electrolytic cell made of Titanium plate and Steel plate representing anode and cathode. The DC power source applied to the ECP unit had electrical potential(E) of 50$\pm$ 1V, respectively. The synthetic wastewater used in the experiments contained Cu in the 10 mg/l concentration and the electrode separation were 2, 3, 4 cm and the initial pH were 3, 6, 9, 12, and electrolytic concentration were 0.005, 0.0125, 0.025, 0.0375 mole, and the real heavymetal wastewater used in the experiments. From the experiment for removal efficiency according to pH variation, the low pH area doesn't give the coagulation effect by Ti(OH)$_4$ because process interfere with the coagulation and oxidation reaction, therefore the optimum pH was 4-7. The removal rate was 97.75% after the lapse of 30 minutes when copper concentration and electrolytic concentration were respectively 10 mg/l and 0.025 mole. The removal rate was 96.41% after the lapse of 30minutes when the real heavymetal wastewater used. The optimum consumption of power showed 27KWh/m$^3$ when copper concentration, electrolyte concentration and cell potential were respectively 10 mg/l, 0.025 mole and 50$\pm$ 1 Volt.

  • PDF