• 제목/요약/키워드: Powder Deposition Density

검색결과 55건 처리시간 0.024초

플라즈마에 의한 고밀도침적물 제조시 변수들의 영향 (Effect of Parameters for Dense Bleposit by Plasma)

  • 정인하
    • 한국분말재료학회지
    • /
    • 제5권2호
    • /
    • pp.111-121
    • /
    • 1998
  • Thick and dense deposit of higher than 97% of theoretical density was formed by induction plasma spraying. To investigate the effects of powder morphology on the density of deposit, two different kinds of Yttria-Stabilized-Zirconia powder, METCO202NS (atomized & agglomerated) and AMDRY146 (fused & crushed), were used and compared. After plasma treatment, porous METCO202NS powder was all the more densely deposited and its density was increased. In addition to the effect of powder morphology, the process parameters such as, sheath gas composition, probe position, particle size and spraying distance, and so on, were evaluated. The result of experiment with AMDRY146 powder, particle size and spraying distance affected highly on the density of the deposit. The optimum process condition for the deposition of -75 ${\mu}m$ of 20%-Yttria-Stabilized-Zirconia powder was 120/201/min of Ar/$H_2$ gas rate, 80 kW of plasma plate power, 8 cm of probe position and 150 Torr of spraying chamber pressure, at which its density showed 97.91% of theoretical density and its deposition rate was 20 mm/min. All the results were assessed by statistical approach what is called ANOVA.

  • PDF

에너지 밀도 및 분말 증착 밀도를 고려한 직접 에너지 증착법 기반 Ti-6Al-4V 합금의 적층공정 최적화 (Additive Manufacturing Optimization of Directed Energy Deposition-Processed Ti-6Al-4V Alloy using Energy Density and Powder Deposition Density)

  • 이유경;김은성;천세호;설재복;성효경;오정석;김형섭;이태경;남태현;김정기
    • 한국분말재료학회지
    • /
    • 제28권6호
    • /
    • pp.491-496
    • /
    • 2021
  • The process optimization of directed energy deposition (DED) has become imperative in the manufacture of reliable products. However, an energy-density-based approach without a sufficient powder feed rate hinders the attainment of an appropriate processing window for DED-processed materials. Optimizing the processing of DED-processed Ti-6Al- 4V alloys using energy per unit area (Eeff) and powder deposition density (PDDeff) as parameters helps overcome this problem in the present work. The experimental results show a lack of fusion, complete melting, and overmelting regions, which can be differentiated using energy per unit mass as a measure. Moreover, the optimized processing window (Eeff = 44~47 J/mm2 and PDDeff = 0.002~0.0025 g/mm2) is located within the complete melting region. This result shows that the Eeff and PDDeff-based processing optimization methodology is effective for estimating the properties of DED-processed materials.

플라스틱 봉투 표면에서 지문을 현출하기 위한 Vacuum Metal Deposition (VMD)과 분말법의 비교 (Comparison of vacuum metal deposition (VMD) and powder method for developing latent fingerprint on plastic envelope surface)

  • 김채원;이나래;김태원;유제설
    • 분석과학
    • /
    • 제33권3호
    • /
    • pp.159-166
    • /
    • 2020
  • 진공금속증착법(vacuum metal deposition, 이하 VMD)는 비다공성과 반다공성 표면의 잠재지문을 현출하는데 효과적이다. VMD는 일반적인 기법으로 현출할 수 없거나 어려운 표면에 유류된 지문을 현출하는 경우에서 활용할 수 있다. VMD 기법이 권장되는 표면은 비닐, 폴리머 지폐, 마그네틱 코팅 처리가 된 티켓 등이 있다. 본 연구에서는 택배 봉투로 주로 사용되는 분홍색 고밀도 폴리에틸렌 봉투(HDPE)와 저밀도 폴리에틸렌 봉투(LDPE)에 지문을 유류한 뒤 최소 12시간부터 최대 28일이 경과한 지문을 현출하기 위한 금의 최소 투입량을 탐색하였다. 그리고 그 결과를 흑색분말, 형광분말의 효과와 비교하였다. 또한, 실제로 배송에 사용된 택배 봉투를 수거한 다음 HDPE와 LDPE로 분류하고 pseudo-operation test를 시행하였다. 그 결과, VMD는 HDPE와 LDPE 표면에서 비교적 일관된 지문 현출 결과를 보여주었다.

INDUCTION PLASMA DEPOSITION TECHNOLOGY FOR NUCLEAR FUEL FABRICATION

  • I. H. Jung;K. K. Bae;Lee, J. W.;Kim, T. K.;M. S. Yang
    • 한국원자력학회:학술대회논문집
    • /
    • 한국원자력학회 1998년도 춘계학술발표회논문집(2)
    • /
    • pp.216-221
    • /
    • 1998
  • A study on induction plasma deposition with ceramic materials, yttria-stabilized-zirconia ZrO$_2$-Y$_2$O$_3$ (m.p 264O $^{\circ}C$), was conducted with a view developing a new method for nuclear fuel fabrication Before making dense pellets more than 96%TD., the spraying condition was optimized through the process parameters, such as chamber pressure, plasma plate power powder spraying distance, sheath gas composition, probe position, particle size and powders different morphology. The results with a 5mm thick deposit on rectangular planar graphite substrates showed a 97.11% theoretical density when the sheath gas flow rate was Ar/H$_2$120/20 l/min, probe position 8cm, particle size -75 ${\mu}{\textrm}{m}$ and spraying distance 22cm by AMDRY146 powder. The degree of influence of the main effects on density were powder morphology. particle size, sheath gas composition, plate power and spraying distance, in that order. Among the two parameter interactions, the sheath gas composition and chamber pressure affects density greatly. By using the multi-pellets mold wheel type, the pellet density did not exceed 94%T.D., owing to the spraying angle.

  • PDF

폴리머를 첨가한 현탁용매에 따른 초전도 후막의 표면특성 (Surface Properties of Superconducting Thick Film with Suspension Solution added with Polymer)

  • 소대화;이영매;임병제;김태완;전용우;코로보바나탈리아
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 추계학술대회 논문집
    • /
    • pp.503-506
    • /
    • 2000
  • YBCO superconducting thick films were prepared on Ag wire by electrophoresis in acetone and ethanol with chemically modified suspension. The addition of organic compounds, such as PEG, EG into suspension solution for improving critical current density was investigated. Surface state, deposition condition, pore distribution and cracks were investigated by using SEM photographs. Controlling preparation conditions were studied for reducing these defects. As a results, in acetone solution, the surface crack of samples was decreased with increasing PEG. On the contrary, the surface crack of sample was increasing with increasing the amount of EG. In ethanol solution without I$_2$, which was generally used for an electrolyte, the deposition time was longer than this of acetone. For that reason the sample deposition in ethanol time was needed with enough stirring time for suspending YBCO powder and deposition time.

  • PDF

유동층 화학기상증착법을 이용하여 제조된 열분해 탄화규소의 특성에 미치는 증착온도의 영향 (Effect of Deposition Temperature on the Property of Pyrolytic SiC Fabricated by the FBCVD Method)

  • 김연구;김원주;여승환;조문성
    • 한국분말재료학회지
    • /
    • 제21권6호
    • /
    • pp.434-440
    • /
    • 2014
  • Silicon carbide(SiC) layer is particularly important tri-isotropic (TRISO) coating layers because it acts as a miniature pressure vessel and a diffusion barrier to gaseous and metallic fission products in the TRISO coated particle. The high temperature deposition of SiC layer normally performed at $1500-1650^{\circ}C$ has a negative effect on the property of IPyC layer by increasing its anisotropy. To investigate the feasibility of lower temperature SiC deposition, the influence of deposition temperature on the property of SiC layer are examined in this study. While the SiC layer coated at $1500^{\circ}C$ obtains nearly stoichiometric composition, the composition of the SiC layer coated at $1300-1400^{\circ}C$ shows discrepancy from stoichiometric ratio(1:1). $3-7{\mu}m$ grain size of SiC layer coated at $1500^{\circ}C$ is decreased to sub-micrometer (< $1{\mu}m$) $-2{\mu}m$ grain size when coated at $1400^{\circ}C$, and further decreased to nano grain size when coated at $1300-1350^{\circ}C$. Moreover, the high density of SiC layer (${\geq}3.19g/cm^3$) which is easily obtained at $1500^{\circ}C$ coating is difficult to achieve at lower temperature owing to nano size pores. the density is remarkably decreased with decreasing SiC deposition temperature.

측면수직보조전계에 의한 전기영동전착 기술 (Electrophoretic Deposition Technique by Vertical Lateral Assisted Field)

  • 소대화;전용우;박정철;번점국
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 기술교육전문연구회
    • /
    • pp.82-85
    • /
    • 2003
  • This dissertation describes an optimization method for fabricating thick films with superconducting YBCO powders by electrophoresis technique. The lateral alternating applied voltage caused to shake the superconducting powder vertically to the deposition field during the process of the oriented deposition so that it was deposited along the c-axis on the silver tape with shaky-aligned EPD. As the result, the optimized thin film fabrication method was obtained to get more dense and uniform surface morphology as well as the improved critical current density. For commercial utilization and efficiency, in this dissertation, alternating voltage of 25-120 V/cm in frequency of 60Hz was proposed to apply it as a subsidiary source for shaky-flow deposition so that the fabricated thin film showed uniform surface morphology with less voids and cracks and $T_{c.zero}$ of 90 K and the critical current density of $3419A/cm^2$.

  • PDF

Fabrication of SiCf/SiC Composites using an Electrophoretic Deposition

  • Lee, Jong-Hyun;Gil, Gun-Young;Yoon, Dang-Hyok
    • 한국세라믹학회지
    • /
    • 제46권5호
    • /
    • pp.447-451
    • /
    • 2009
  • Continuous SiC fiber-reinforced SiC composites ($SiC_f$/SiC) were fabricated by electrophoretic deposition (EPD). Nine types of slurries with different powder contents, binder resin amounts and slurry pH were deposited on Tyranno$^{TM}$-SA fabrics by EPD at 135 V for ten minutes to determine the optimal conditions. Further EPD using the optimum slurry conditions was performed on fabrics with four different pyrolitic carbon (PyC) thicknesses. The density of the hot-pressed composites decreased with increasing PyC thickness due to the difficulty of infiltrating the slurry into the narrow gaps between the fibers. On the other hand, the mechanical strength increased with increasing PyC thickness despite the decrease in density, which was explained by the enhanced crack deflection with increasing PyC thickness. The $SiC_f$/SiC composites showed the highest density and flexural strength of 94% and 342 MPa, respectively, showing EPD as a feasible method for dense $SiC_f$/SiC fabrication.

피복입자핵연료에서 증착조건이 탄화규소층의 특성에 미치는 영향 (Effect of Deposition Parameters on the Property of Silicon Carbide Layer in Coated Particle Nuclear Fuels)

  • 김연구;김원주;여승환;조문성
    • 한국분말재료학회지
    • /
    • 제23권5호
    • /
    • pp.384-390
    • /
    • 2016
  • Tri-isotropic (TRISO) coatings on zirconia surrogate beads are deposited using a fluidized-bed vapor deposition (FB-CVD) method. The silicon carbide layer is particularly important among the coated layers because it acts as a miniature pressure vessel and a diffusion barrier to gaseous and metallic fission products in the TRISO-coated particles. In this study, we obtain a nearly stoichiometric composition in the SiC layer coated at $1400^{\circ}C$, $1500^{\circ}C$, and $1400^{\circ}C$ with 20 vol.% methyltrichlorosilane (MTS), However, the composition of the SiC layer coated at $1300-1350^{\circ}C$ shows a difference from the stoichiometric ratio (1:1). The density decreases remarkably with decreasing SiC deposition temperature because of the nanosized pores. The high density of the SiC layer (${\geq}3.19g/cm^2$) easily obtained at $1500^{\circ}C$ and $1400^{\circ}C$ with 20 vol.% MTS did not change at an annealing temperature of $1900^{\circ}C$, simulating the reactor operating temperature. The evaluation of the mechanical properties is limited because of the inaccurate values of hardness and Young's modulus measured by the nano-indentation method.

High $T_c$, Superconductors for Applications

  • Soh, Deawha;Fan, Zhanguo
    • 한국정보통신학회:학술대회논문집
    • /
    • 한국해양정보통신학회 2003년도 춘계종합학술대회
    • /
    • pp.366-369
    • /
    • 2003
  • High T$_{c}$ superconducting lines will be applied as key materials in the areas of power transmission line; magnetic levitation of vehicle; magnetic separation; magnetic energy storage and marine propulsion. A combination method of electrophoresis deposition and zone-melting for preparation of YBaCuO tape is proposed. The submicron particle powder of YBaCuO made by sol-gel method is used in the electrophoresis process. A 40~50${\mu}{\textrm}{m}$ thickness of YBaCuO film on Ag plate could be deposited in about three minutes. After deposition the film is rolled and heat treated in order to increase the density and the adhesion of the film to the Ag plate. Silver(Ag) and lead oxide(PbO) were added in the YBaCuO powder in order to reduce its melting point. The YBaCuO coating with controlled Ag and PbO contents was preliminarily zone-melted at about 945$^{\circ}C$.>.

  • PDF