Browse > Article
http://dx.doi.org/10.4191/KCERS.2009.46.5.447

Fabrication of SiCf/SiC Composites using an Electrophoretic Deposition  

Lee, Jong-Hyun (School of Materials Science and Engineering, Yeungnam University)
Gil, Gun-Young (School of Materials Science and Engineering, Yeungnam University)
Yoon, Dang-Hyok (School of Materials Science and Engineering, Yeungnam University)
Publication Information
Abstract
Continuous SiC fiber-reinforced SiC composites ($SiC_f$/SiC) were fabricated by electrophoretic deposition (EPD). Nine types of slurries with different powder contents, binder resin amounts and slurry pH were deposited on Tyranno$^{TM}$-SA fabrics by EPD at 135 V for ten minutes to determine the optimal conditions. Further EPD using the optimum slurry conditions was performed on fabrics with four different pyrolitic carbon (PyC) thicknesses. The density of the hot-pressed composites decreased with increasing PyC thickness due to the difficulty of infiltrating the slurry into the narrow gaps between the fibers. On the other hand, the mechanical strength increased with increasing PyC thickness despite the decrease in density, which was explained by the enhanced crack deflection with increasing PyC thickness. The $SiC_f$/SiC composites showed the highest density and flexural strength of 94% and 342 MPa, respectively, showing EPD as a feasible method for dense $SiC_f$/SiC fabrication.
Keywords
Slurry; Zeta potential; Electrophoretic deposition; $SiC_f$/SiC composite; Hot pressing;
Citations & Related Records

Times Cited By SCOPUS : 2
연도 인용수 순위
1 S.J. Dapkunas, “Ceramic Heat Exchangers,” Am. Ceram. Soc. Bull., 67 388-91 (1988)   ScienceOn
2 Y. Takeda, “Development of High-Thermal-Conductive SiC Ceramics,” Am. Ceram. Soc. Bull., 67 1961-63 (1988)
3 R.J. Kerans and T.A. Parthasarathy, “Crack Deflection in Ceramic Composites and Fiber Coating Design Criteria,” Compos. Part A, 30 521-24 (1999)   DOI   ScienceOn
4 B. Riccardi, P. Fenici, A.F. Rebelo, L. Giancarli, G.L. Marois, and E. Philippe, “Status of the European R&D Activities on $SiC_f/SiC$ Composites for Fusion Reactors,” Fusion Eng. Des., 51-52 11-22 (2000)   DOI   ScienceOn
5 B. Riccardi, L. Giancarli, A. Hasegawa, Y. Katoh, A. Kohyama, R.H. Jones, and L.L. Snead, “Issues and Advances in $SiC_f/SiC$ Composites Development for Fusion Reactors,” J. Nucl. Mater., 329-333 56-65 (2004)   DOI   ScienceOn
6 R. Yamada, T. Taguvhi, and N. Igawa, “Mechanical and Thermal Properties of 2D and 3D SiC/SiC Composites,” J. Nucl. Mater., 283-287 574-78 (2000)   DOI   ScienceOn
7 Y. Katoh, S.M. Dong, and A. Kohyama, “Thermo-mechanical Properties and Microstructure of Silicon Carbide Composites Fabricated by Nano-infiltrated Transient Eutectoid Process,” Fusion Eng. Des., 61-62 723-31 (2002)   DOI   ScienceOn
8 S. Dong, Y. Katoh, and A. Kohyama, “Preparation of SiC/ SiC Composites by Hot Pressing, Using Tyranno-SA Fibers as Reinforcement,” J. Am. Ceram. Soc., 86 [1] 26-32 (2003)   DOI   ScienceOn
9 T. Ishikawa, Y. Kohtoku, K. Kumagawa, T. Yamamura, and T. Nagasawa, “High-Strength Alkai-Resistant Sintered SiC Fibre Stable to $2,200^{\circ}C$,” Nature, 391 773-75 (1998)   DOI   ScienceOn
10 L. Besra, and M. Liu, “A Review on Fundamentals and Applications of Electrophoretic Deposition (EPD),” Prog. Mater. Sci., 52 1-61 (2007)   DOI   ScienceOn
11 K. Yoshida, K. Matsukawa, M. Imai, and T. Yano, “Formation of Carbon Coating on SiC Fiber for Two-Dimensional $SiC_f/SiC$ Composites by Electrophoretic Deposition,” Mat. Sci. Eng. B, 161 188-92 (2009)   DOI   ScienceOn
12 S. Novak, K. Rade, K. König, and A.R. Boccaccini, “Electrophoretic Deposition in the Production of SiC/SiC Composites for Fusion Reactor Applications,” J. Eur. Ceram. Soc., 28 2801-07 (2008)   DOI   ScienceOn
13 K. Yoshida, K. Matsukawa, and T. Yano, “Microstructure and Mechanical Properties of Silicon Carbide Fiber-Reinforced Silicon Carbide Composite Fabricated by Electrophoretic Deposition and Hot-Pressing,” J. Nucl. Mater., 386-388 643-46 (2009)   DOI   ScienceOn
14 J.H. Lee, P. Yonathan, D.H. Yoon, W.J. Kim, and J.Y. Park, “Dispersion Stability and Its Effect on Tape Casting of Solvent-Based SiC Slurries,” J. Ceram. Proc. Res., 10 301-07 (2009)
15 A. Ortona, A. Donato, G. Filacchioni, U.D. Angelis, A.L. Barbera, C.A. Nannetti, B. Riccardi, and J. Yeatman, “ $SiC-SiC_f$ CMC Manufacturing by Hybrid CVI-PIP Techniques: Process Optimasation,” Fusion Eng. Des., 51-52 159-63 (2000)   DOI   ScienceOn
16 K. Shimoda, J.S. Park, T. Hinoki, and A. Kohyama, “Influence of Pyrolytic Carbon Interface Thickness on Microstructure and Mechanical Properties of SiC/SiC Composites by NITE Process,” Ceram. Sci. Technol., 68 98-105 (2008)   DOI   ScienceOn