Synthesis and Photoluminescence Properties of Red-Emitting (Y,Al)VO4:Eu3+ Nanophosphors (적색 발광 (Y,Al)VO4:Eu3+ 형광체 나노입자의 합성과 발광 특성)

  • Seo, Jung-Hyun;Choi, Sung-Ho;Nahm, Sahn;Jung, Ha-Kyun
    • Korean Journal of Materials Research
    • /
    • v.22 no.2
    • /
    • pp.103-109
    • /
    • 2012
  • Red-emitting $Eu^{3+}$-activated $(Y_{0.95-x}Al_x)VO_4$ (0 < x $\leq$ 0.12) nanophosphors with the particle size of ~30 nm and the high crystallinity have been successfully synthesized by a hydrothermal reaction. In the synthetic process, deionized water as a solvent and ethylene glycol as a capping agent were used. The crystalline phase, particle morphology, and the photoluminescence properties of the excitation spectrum, emission intensity, color coordinates and decay time, of the prepared $(Y_{0.95-x}Al_x)VO_4:Eu^{3+}$ nanophosphors were compared with those of the $YVO_4:Eu^{3+}$. Under 147 nm excitation, $(Y_{0.95-x}Al_x)VO_4$ nanophosphors showed strong red luminescence due to the $^5D_0-^7F_2$ transition of $Eu^{3+}$ at 619 nm. The luminescence intensity of $YVO_4:Eu^{3+}$ enhanced with partial substitution of $Al^{3+}$ for $Y^{3+}$ and the maximum emission intensity was accomplished at the $Al^{3+}$ content of 10 mol%. By the addition of $Al^{3+}$, decay time of the $(Y,Al)VO_4:Eu^{3+}$ nanophosphor was decreased in comparison with that of the $YVO_4:Eu^{3+}$ nanophosphor. Also, the substitution of $Al^{3+}$ for $Y^{3+}$ invited the improvement of color coordinates due to the increase of R/O ratio in emission intensity. For the formation of transparent layer, the red nanophosphors were fabricated to the paste with ethyl celluloses, anhydrous terpineol, ethanol and deionized water. By screen printing method, a transparent red phosphor layer was formed onto a glass substrate from the paste. The transparent red phosphor layer exhibited the red emission at 619 nm under 147 nm excitation and the transmittance of ~80% at 600 nm.

Synthesis of Dodecanethiol-Capped Nanoparticles Using Ionic Liquids (이온성 액체를 이용한 dodecanethiol로 안정화된 금속 나노입자 합성)

  • Lee, Young-Eun;Lee, Seong-Yun;You, Seong-Sik
    • Korean Chemical Engineering Research
    • /
    • v.50 no.5
    • /
    • pp.795-801
    • /
    • 2012
  • Nanoparticles have received significant attention because of their unusual characteristics including high surface area to volume ratios. Thiol ligand have been used as stabilizers of metal nanoparticles since Brust et al. They reported the preparation method of ligand capped metal nanoparticles by protecting the nanoparticles with a self-assembled monolayer of dodecanethiolate. In this method, volatile organic compounds (VOCs) were used as sovents. This study was carried out to replace these VOCs with room temperature ionic liquids (RTILs). We used two type of ILs to prepare metal nanoparticles. One is a hydrophobic IL, [BMIM][[$PF_6$] (1-Butyl-3-methylimidazolium hexafluorophosphate) purchased from IL maker, C-Tri from Korea and the other one is a hydrophilic one, [BMIM][Cl] (1-Buthy-3-methylimdazolium chloride) sinthesized by us. In the case of preparing Ag and Au nanoparticles using [BMIM][Cl], we didn't use phase transition reagents and ethanol because it has hydrophilic property and preparing Au, Ag nanoparticles using [BMIM][[$PF_6$] the method is as same as Brust et al.'s except using [BMIM][[$PF_6$] instead of organic solvent because it has hydrophobic property. FT-IR and UV-vis, TEM, TGA analysis have been used in an attempt to determine the particle size and verify functional groups. The particle size obtained from TEM was very similar to those obtained by Brust et al. This is a clear example of ligand capped metal nanoparticles prepared using ionic liquids. And the experimental result demonstrated ionic liquids can act as a highly effective medium for the preparation and stabilization of gold and silver metal nanoparticles.

Synthesis of TiO2 Fine Powder by Sol-Gel Process and Reaction Mechanism(II) : Hydrolysis of Titanium n-Propoxide (졸-겔법에 의한 TiO2미분말 합성과 반응메카니즘(II): Titanium n-propoxide의 가수분해)

  • Myung, Jung-Jae;Park, Jin-koo;Chung, Yong-Sun;Kyong, Jin-Bum;Kim, Ho-Kun
    • Applied Chemistry for Engineering
    • /
    • v.8 no.5
    • /
    • pp.777-783
    • /
    • 1997
  • $TiO_2$ powders were synthesized via hydrolysis reaction of titanium n-propoxide in n-propanol solvent and the reaction rates were studied by use of UV-vis spectroscopic method. Concentration of water, reaction temperature, reaction time and acid-base effects of the solution were investigated to determine the optimum conditions for $TiO_2$ powder synthesis. The reaction were controlled to proceed to pseudo-first orders reaction in the presence of excess water in n-propanol solvent. The rate constants which varied with temperature and concentration of water were calculated by Guggenheim method. Reaction using $D_2O$ was also carried out to determine the catalytic character of water. $TiO_2$ powders were synthesized only in the neutral and basic solution and those were almost spheric forms having average particle size of $0.4-0.7{\mu}m$ diameter. Particle size decreased with increasing concentration of water and reaction temperature, however, increased with increasing reaction time. Associative $S_N2$ mechanism for the hydrolysis was proposed from the data of n-value in the transition state and thermodynamic parameter. $D_2O$ solvent isotope effect showed that $H_2O$ molecules reacted as nucleophilic catalysis.

  • PDF

Simulation of Mixing Behavior for Dredging Plume using Puff Model (퍼프모형을 이용한 준설플륨의 혼합거동 모의)

  • Kim, Young-Do;Park, Jae-Hyeon;Lee, Man-Soo
    • Journal of Korea Water Resources Association
    • /
    • v.42 no.10
    • /
    • pp.891-896
    • /
    • 2009
  • The puff models have been developed to simulate the advection-diffusion processes of dredging suspended solids, either alone or in combination with Eulerian models. Computational efficiency and accuracy are of prime importance in designing these hybrid approaches to simulate a pollutant discharge, and we characterize two relatively simple Lagrangian techniques in this regard: forward Gaussian puff tracking (FGPT), and backward Gaussian puff tracking (BGPT). FGPT and BGPT offer dramatic savings in computational expense, but their applicability is limited by accuracy concerns in the presence of spatially variable flow or diffusivity fields or complex no-flux or open boundary conditions. For long simulations, particle and/or puff methods can transition to an Eulerian model if appropriate, since the relative computational expense of Lagrangian methods increases with time for continuous sources. Although we focus on simple Lagrangian models that are not suitable to all environmental applications, many of the implementation and computational efficiency concerns outlined herein would also be relevant to using higher order particle and puff methods to extend the near field.

Preparation of Styrene-Ethyl acylate Core-shell Structured Detection Materials for aMeasurement of the Wall Contamination by Emulsion Polymerization

  • Hwang, Ho-Sang;Seo, Bum-Kyoung;Lee, Dong-Gyu;Lee, Kune-Woo
    • Proceedings of the Korean Radioactive Waste Society Conference
    • /
    • 2009.06a
    • /
    • pp.84-85
    • /
    • 2009
  • New approaches for detecting, preventing and remedying environmental damage are important for protection of the environment. Procedures must be developed and implemented to reduce the amount of waste produced in chemical processes, to detect the presence and/or concentration of contaminants and decontaminate fouled environments. Contamination can be classified into three general types: airborne, surface and structural. The most dangerous type is airborne contamination, because of the opportunity for inhalation and ingestion. The second most dangerous type is surface contamination. Surface contamination can be transferred to workers by casual contact and if disturbed can easily be made airborne. The decontamination of the surface in the nuclear facilities has been widely studied with particular emphasis on small and large surfaces. The amount of wastes being produced during decommissioning of nuclear facilities is much higher than the total wastes cumulated during operation. And, the process of decommissioning has a strong possibility of personal's exposure and emission to environment of the radioactive contaminants, requiring through monitoring and estimation of radiation and radioactivity. So, it is important to monitor the radioactive contamination level of the nuclear facilities for the determination of the decontamination method, the establishment of the decommissioning planning, and the worker's safety. But it is very difficult to measure the surface contamination of the floor and wall in the highly contaminated facilities. In this study, the poly(styrene-ethyl acrylate) [poly(St-EA)] core-shell composite polymer for measurement of the radioactive contamination was synthesized by the method of emulsion polymerization. The morphology of the poly(St-EA) composite emulsion particle was core-shell structure, with polystyrene (PS)as the core and poly(ethyl acrylate) (PEA) as the shell. Core-shell polymers of styrene (St)/ethyl acrylate (EA) pair were prepared by sequential emulsion polymerization in the presence of sodium dodecyl sulfate (SOS) as an emulsifier using ammonium persulfate (APS) as an initiator. The polymer was made by impregnating organic scintillators, 2,5-diphenyloxazole (PPO) and 1,4-bis[5-phenyl-2-oxazol]benzene (POPOP). Related tests and analysis confirmed the success in synthesis of composite polymer. The products are characterized by IT-IR spectroscopy, TGA that were used, respectively, to show the structure, the thermal stability of the prepared polymer. Two-phase particles with a core-shell structure were obtained in experiments where the estimated glass transition temperature and the morphologies of emulsion particles. Radiation pollution level the detection about under using examined the beta rays. The morphology of the poly(St-EA) composite polymer synthesized by the method of emulsion polymerization was a core-shell structure, as shown in Fig. 1. Core-shell materials consist of a core structural domain covered by a shell domain. Clearly, the entire surface of PS core was covered by PEA. The inner region was a PS core and the outer region was a PEA shell. The particle size distribution showed similar in the range 350-360 nm.

  • PDF

Design and Properties of Laminating Waterborne PSA for Eco-friendly Flexible Food Packaging (식품연포장용 라미네이트 수성 감압점착제의 친환경적 적용에 대한 연구)

  • Lee, Jin-Kyoung;Shim, Myoung-Sik;Chin, In-Joo
    • Journal of Adhesion and Interface
    • /
    • v.17 no.2
    • /
    • pp.49-55
    • /
    • 2016
  • In this study, we designed an environment friendly, water-based adhesive using the acrylic emulsion method as a replacement for solvent-based adhesives, which are most commonly used in layered laminates for flexible food packaging. We designed adhesives with different combinations of anionic, non-ionic, and phosphoric ester surfactants, and with different concentrations of chain transfer agent (CTA). We also examined the effect of the degree of cross-linking by synthesizing and comparing 8 test group adhesives with different types of functional monomers. Additionally, we synthesized 2 other test group pressure-sensitive adhesives (PSA) using styrene/alpha-methyl styrene/acrylic acid (SAA) semipolymer dispersing agents (with molecular weights of 13,000 g/mol and 8,600 g/mol, respectively) to replace the conventional surfactants. We evaluated whether the 10 test group pressure-sensitive adhesives met the basic physical property criteria required for flexible food packaging by carrying out a physical analysis of their glass transition temperature (Tg), particle size, adhesion, and molecular weight. In our test, 2 test group adhesives manufactured with the combination of anionic and non-ionic surfactants, CTA concentration of 0.2%, and functional monomers of hydroxyethyl acrylate (HEA) and glycidyl methacrylate (GMA) demonstrated molecular weight and flexibility suitable for flexible packaging, with low adhesiveness and small particle size.

Effect of Stress Level on Strength Parameters of Cemented Sand (응력조건에 따른 고결모래의 강도정수 평가)

  • Lee, Moon-Joo;Choi, Sung-Kun;Choo, Hyun-Wook;Cho, Yong-Soon;Lee, Woo-Jin
    • Journal of the Korean Geotechnical Society
    • /
    • v.23 no.5
    • /
    • pp.143-151
    • /
    • 2007
  • The factors affecting the geotechnical properties of cemented sands are known to be relative density, cementation level, stress level, and particle characteristics such as particle size, shape and surface conditions. It has been widely accepted that the friction angle of cemented sands is not affected by cementation while the cohesion of cemented sands was significantly influenced by cementation. The cementation that is a critical component of the strength of cemented sands will be broken with increasing confining pressure and great caution is required in evaluating the cohesion of cemented specimens due to their fragilities. In this study, a series of drained shear tests were performed with specimens at various cementation levels and confining stresses to evaluate the strength parameters of cemented sands. From the experiments, it was concluded that the cohesion intercept of cemented sand experiences three distinctive zone(cementation control zone, transition zone, and stress control zone), as the cementation level and the confining stress varies. In addition, for accurate evaluation of the strength parameters, the level of confining stress triggering the breakage of cementation bond should be determined. In this study, the relationship between the maximum confining stresses capable of maintaining the cementation bond intact and unconfined compression strength of the cemented sand was established.

Observation of Molecular Relaxation Behavior of Glucose Powders with Different Structures and Particle Sizes Using Low Field Nuclear Magnetic Resonance (NMR) (NMR을 이용한 구조 및 입도 차이에 따른 분말 포도당의 molecular relaxation behavior의 관찰)

  • Chung, Myung-Soo
    • Korean Journal of Food Science and Technology
    • /
    • v.34 no.6
    • /
    • pp.1140-1144
    • /
    • 2002
  • Molecular relaxation behaviors of crystalline glucose anhydrous, crystalline glucose monohydrate, and amorphous glucose with different particle sizes were observed by measuring spin-spin relaxation time constant $(T_2)$ at the temperature range of $-20\;to\;110^{\circ}C$ using temperature-controlled low field nuclear magnetic resonance spectroscopy. No change in $T_2$ values of crystalline glucose anhydrous was observed throughout the temperature range, whereas $T_2$ values of crystalline glucose monohydrate and amorphous glucose increased from around $45\;and\;65^{\circ}C$, respectively. These results indicate that molecular mobility of crystalline glucose anhydrous does not change even at temperature higher than $100^{\circ}C$ and that the stability of powdered glucose could be improved by increasing the particle size of materials.

Preparation and Properties of Spherical BaMgAl10O17:Eu Phosphor by Multi-step Precipitation Method (다단 침전법에 의한 구형 BaMgAl10O17:Eu 형광체의 제조 및 특성)

  • Park, Jumg-Min;Jung, Ha-Kyun;Park, Hee-Dong;Park, Yoon-Chang
    • Korean Journal of Materials Research
    • /
    • v.12 no.11
    • /
    • pp.840-844
    • /
    • 2002
  • A spherical $BaMgAl_{10}$ $O_{17}$ :Eu phosphor has been synthesized by a multi-step precipitation route. In order to successfully synthesize the phosphor with spherical shape, the hydrated-alumina particles should be controlled for spherical shape. In this process, the hydroxypropyl cellulose (HPC) was used as a dispersing reagent. This reagent plays an important role in that the particles were controlled to have the uniform size of sub-micron. The final product prepared by the multi-step precipitation method maintained spherical shape with uniform size of 0.4$\mu\textrm{m}$. It can be seen in X-ray diffraction patterns, formation of the single phase of $BaMgAl_{10}$ $O_{17}$ :Eu phosphor prepared by the multi-step precipitation method at $1350^{\circ}C$. Also, the emission spectra of spherical $BaMgAl_{O}$ $10_{17}$ :Eu phosphor in the present case was compared with those of commercially-available blue phosphor under VUV (Vacuum Ultra Violet) excitation. The luminescence process of the $BaMgAl_{10}$ $O_{17}$ :Eu phosphor is characterized by the $4f^{6}$$5d^1$longrightarrow4f$^{7}$ transition (blue) of the $Eu^{2+}$ ion acting as an activating center and the maximum luminescence intensity was obtained by reduction treatment at 145$0^{\circ}C$.

Effect of Electrolyte Additive on the Electrochemical Characteristics of Lithium Vanadium Oxide Anode (전해질 첨가제가 리튬 바나듐 옥사이드 전극의 성능에 미치는 영향)

  • Lee, Je-Nam
    • Journal of the Korean Electrochemical Society
    • /
    • v.21 no.3
    • /
    • pp.55-60
    • /
    • 2018
  • The demand for LIBs with higher energy densities has increased continuously because the emergence of wider and more challenging applications including HEV and EV has became imperative. However, in the case of anode material, graphite is insufficient to meet this need. To meet such demand, several type of negative electrode materials like silicon, tin, SiO, and transition metal oxide have been investigated for the advanced lithium secondary batteries. Recently, lithium vanadium oxide, which has a layered structure, is assumed as one of the promising anode material as alternative of graphite. This material shows a high volumetric capacity, which is 1.5 times higher than that of graphite. However, relative low electrical conductivity and particle fracture, which results in the electrolyte decomposition and loss of electric contact between electrode, induce rapid capacity decay. In this report, we investigated the effect of electrolyte additive on the electrochemical characteristics of lithium vanadium oxide.