PZT powders were prepared by the molten salt synthesis method. The porous PZT ceramics were made from a mixture of PZT and polyvinylalcohol(PVA) by BURPS(Bumout Plastic Sphere) technique. The 3-3 type composites were fabricated by impregnating an sintered porous PZT ceramics with various polymer matrices. The relative permittivity of 3-3 type composite specimens was shown 860-1,100 smaller than that of solid PZT ceramics(2,100), and the dissipation factors of composite specimens were about 0.02 to 0.03. The piezoelectric coefficient d$_{33}$ of composite specimens(285-328*10$^{12}$ C/N) was comparable with that of single phase PZT specimens(364*10$^{-12}$ C/N). The thickness mode coupling factor k$_{t}$(O.5-0.6) of composite specimens was comparable with that of single phase PZT specimens(k$_{t}$-0.7), and the mechanical quality factor of composite specimens was smaller than 10, and thus these 3-3 type composite specimens would be believed as a good candidates for broad band transducer applications.ons.
Nowadays, the increasing demands upon mobile devices such as wireless sensor networks and the recent advent of low power electrical devices such as MEMS make such renewable power sources attractive. A vibration-driven MEMS lead zirconate titanate $Pb(Zr,Ti)O_3$ (PZT) cantilever device is developed for energy harvesting application. This paper presents a piezoelectric based energy harvester which is suitable for power generating from conventional vibration and has in providing energy for low power electron ic devices. The PZT cantilever is used d33 mode to get the electrical power. The PZT cantilever based energy harvester with the dimension of 7 mm${\times}$3 mm${\times}$0.03 mm is fabricated using micromachining technologies. This PZT cantilever has the mechanical resonance frequency with a 900 Hz. With these conditions, we get experimentally the 37 uW output power from this device with the application of 1g acceleration using the 900 Hz vibration. From this study, we show the feasibility of one of energy harvesting candidates using PZT based structure. This PZT energy harvester could be used for various applications such a batteryless micro sensors and micro power generators.
대한전기학회 2008년도 Techno-Fair 및 합동춘계학술대회 논문집 전기물성,응용부문
/
pp.169-170
/
2008
The heterolayered PZT/PT thick films were fabricated by two different methods - thick films of the PZT by screen printing method on alumina substrates electrodes with Pt, thin films of $PbTiO_3$ by the spin coating method on the PZT thick films and once more thick films of the PZT by the screen printing method on the $BaTiO_3$ layer The structural and the dielectric properties were investigated for effect of various stacking sequence of sol-gel prepared $PbTiO_3$ coating solution at interface of the PZT thick films. The insertion of $PbTiO_3$ interlayer yielded the PZT thick films with homogeneous and dense grain structure with the number of $PbTiO_3$ layers. The leakage current density of the PZT/$PbTiO_3-1$ film is less that $4.41{\times}10^{-9}\;A/cm^2$ at 5 V.
Transactions on Electrical and Electronic Materials
/
제6권4호
/
pp.177-185
/
2005
Fatigue characteristics of lead zirconate titanate (PZT) films deposited by electron cyclotron resonance plasma enhanced chemical vapor deposition (ECR-PECVD) were investigated. The fatigue characteristics were investigated with respect to PZT film thickness, domain structure, fatigue pulse height, temperature, electrode materials and electrode configurations. The used top and bottom electrode materials were Pt and $RuO_2$. In the fatigue characteristics with fatigue pulse height and PZT film thickness, the fatigue rates are independent of the applied fatigue pulse height at the electric field regions to saturate the P-E hysteresis and polarization $(P^*,\;P^A)$ characteristics. The unipolar and bipolar fatigue characteristics of PZT capacitors with four different electrode configurations $(Pt//Pt,\;Pt//RuO_2,\;RuO_2//Pt,\;and\;RuO_2//RuO_2)$ were also investigated. The polarization-shifts during the unipolar fatigue and the temperature dependence of fatigue rate suggest that the migration of charged defects should not be expected in our CVD-PZT films. It seems that the polarization degradations are attributed to the formation of charged defects only at the Pt/PZT interface during the domain switching. The charged defects pin the domain wall at the vicinity of Pt/PZT interface. When the top and bottom electrode configurations are of asymmetric $(Pt//RuO_2,\;RuO_2//Pt)$, the internal fields can be generated by the difference of charged defect densities between top and bottom interfaces.
Ferroelectric PZT thin films were fabricated on the RuO$_2$/Pt, Pt bottom electrode with a PZT(53/47) metal alkoxide solutions. All PZT thin films showed a uniform grain structure without the presence of rosette structure. The PZT thin films were etched as a function of Cl$_2$/Ar and additive CF$_4$ into Cl$_2$(80%)/Ar(20%). The etch rates of PZT thin films were 1970 ${\AA}$/min at 30 % additive CF$_4$ into Cl$_2$(80%)/Ar(20%). The remanent polarization and leakage current density in PZT thin film on the RuO$_2$/Pt were 64.2 ${\mu}$C/cm$^2$, 1.4${\times}$10$\^$-6/ respectively.
This paper gives characterization of substrate and PZT(53/47) thin film deposited by metalorganic decomposition, which is concerned in deposition process and device fabrication process, to fabricate micro electro mechanical system (MEMS) device with piezoelectric material. The PZT thin films deposited by MOD at 700^{\circ}C$ for 30 minutes had a polycrystallinity, that is, no substrate dependence, while different interface were developed depending on the bottom electrodes. Such a structural variation could influence on not only the properties of the PZT film but also etching process for fabricating MEMS devices. Therefore the electrode structure is a very important factor in the deposition of the PZT film during etching process by HF acid for MEMS device with piezoelectric material. Piezoelectric coefficients of the PZT films on the different substrates were 40 and 80 pm/V at an applied voltage of 4V. Based in these results, it was possible for deposition of the PZT film by MOD to apply MEMS device fabrication process based on piezoelectricity after selection of proper bottom electrode.
PZT(80/0) powder was prepared by a sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The coating and drying procedure was repeated 4 times. And then the PZT(20/80) precusor solution was spin-coated on the PZT thick films. A concentration of a coating solution was 0.5mol/L and the number of coating was varied from 0 to 6. The porosity decreased and the grain size increased with increasing the number of coatings. The thickness of the PZT-6(6: number of coatings) films was about $60{\mu}m$. The relative dielectric constant increased and the dielectric loss decreased with increasing the number of PZT(20/80) sol coatings. The relative dielectric constant and dielectric loss of the PZT-6 thick film were 275 and 3.5%, respectively. The remanent polarization, coercive field and breakdown strength of the PZT-6 film were $19.8{\mu}C/cm^2$, 13.7kV/cm and 130kV/cm, respectively.
The Pb $(Zr_{0.52}Ti_{0.48})O_3/(Ba_{0.6}Sr_{0.4}TiO_3$ [PZT(52/48)/BST(60/40)] heterolayered thin films were fabricated on the Pt/Ti/$SiO_2$/Si by RF sputtering method. The structural properties of the PZT(52/48)/BST(60/40) heterolayered thin films were investigated with Ar/$O_2$ ratio condition. All the PZT(52/48)/BST(60/40) heterolayered thin films had shown the PZT(111), (200) and BST(200) Peaks of the tetragonal structure. Increasing the Ar/$O_2$ ratio, the average roughness was increased. The thickness ratio of the to the PZT and BST thin film was 1:2. In the case of the PZT(52/48)/BST(60/40) heterolayered thin films with Ar/$O_2$ ratio of 80/20, the average roughness was 3.4 [nm].
The effect of excimer laser annealing on the structural and dielectric behaviors of $PbZr_{0.52}Ti_{0.48}O_3$ (PZT) thin films has been investigated. The amorphous PZT thin films were prepared on Pt/Ti/$SiO_2$/Si substrates by a sol-gel method. The PZT precursor was prepared from lead acetate, zirconium acetylacetonate, and titanium isopropoxide. The starting materials were dissolved in n-propanol and 1,3-propanediol. After, the amorphous PZT thin films were laser-annealed (using KrF excimer laser) as a function of the laser energy density and the number of laser pulse. Structural properties of PZT thin films are characterized by using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The dielectric characterization was done on a RT66A test system and a Agilent 4294A impedance analyzer. The PZT thin films show that excimer laser irradiation drastically improved the crystallization and dielectric properties of the PZT thin films, depending on the energy density and the pulse number.
Thick PZT films are required for the cases of micro actuators and sensors with high driving force, high breakdown voltage and high sensitivity, and so on. In this work, thick PZT films were fabricated by Sol-Gel multi-coating method. Total 8 types of samples using thick PZT films with thicknesses, about $1{\mu}m$ and $2{\mu}m$, and Pt top electrodes shapes for measuring transverse piezoelectric coefficient ($e_{31,f}$) were fabricated using MEMS processes. They were characterized by fabricated e31,f measurement system before and after poling. $e_{31,f}$ values of samples after poling were higher than before poling. Those of $2{\mu}m$ thick PZT films were also higher than $1{\mu}m$ thick PZT films. And those with long electrodes as top electrodes were also higher than shorter.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.