• 제목/요약/키워드: PECVD $SiO_x$

검색결과 64건 처리시간 0.023초

Characteristic and moisture permeability of SiOxCy thin film synthesized by Atmospheric pressure-plasma enhanced chemical vapor deposition

  • Oh, Seung-Chun;Kim, Sang-Sik;Shin, Jung-Uk
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2011년도 춘계학술대회 및 Fine pattern PCB 표면 처리 기술 워크샵
    • /
    • pp.171-171
    • /
    • 2011
  • Atmospheric pressure- plasma enhanced chemical vapor deposition(AP-PECVD)Processes are recognized as promising and cost effective methods for wide-area coating on sheets of steel, glass, polymeric web, etc. In this study, $SiO_xC_y$ thin films were deposited by using AP-PECVD with a dielectric barrier discharge(DBD). The characteristic of $SiO_xC_y$ thin films were investigated as afunction of the HMDSO/O2/He flow rate. And the moisture permeability of $SiO_xC_y$ thin films was studied. The $SiO_xC_y$ thin films were characterized by the Fourier-transformed Infrared(FT-IR) spectroscopy and also investigated by X-ray photo electron spectroscopy(XPS), Auger Electron Spectroscopy(AES). The moisture permeability of $SiO_xC_y$ thin films was investigated by $H_2O$ permeability tester Detailed experimental results will be demonstrated through th present work.

  • PDF

결정질 실리콘 태양전지 응용을 위한 SiNx 및 SiO2 박막의 패시베이션 특성 연구 (Passivation properties of SiNx and SiO2 thin films for the application of crystalline Si solar cells)

  • 정명일;최철종
    • 한국결정성장학회지
    • /
    • 제24권1호
    • /
    • pp.41-45
    • /
    • 2014
  • 다양한 공정 조건으로 $SiN_x$$SiO_2$ 박막을 형성하고 이에 대한 패시베이션 특성에 대한 연구를 수행하였다. Plasma enhanced chemical vapor deposition(PECVD)을 이용하여 증착된 $SiN_x$ 박막의 경우, 증착 두께가 증가함에 따라 페시베이션 특성이 향상되는 것을 관찰하였다. 이는 PECVD 증착 공정 중 유입되는 수소 원자들이 실리콘 표면에 존재하는 Dangling bond와 결합하여 소수 캐리어의 재결합 현상을 효과적으로 감소시켰기 때문이다. 건식 산화법으로 형성된 $SiO_2$ 박막은 습식 산화법으로 형성된 것 보다 치밀한 계면 구조를 가짐으로 인하여 약 20배 이상 우수한 패시베이션 특성을 나타내었다. 건식 산화 공정 온도가 증가함에 따라 패시베이션 특성이 열화되는 현상이 발생하였고, Capacitance-voltage(C-V) 및 Conductance-voltage(G-V) 분석을 통하여 $SiO_2$/실리콘 계면에 존재하는 계면 결함 밀도 증가에 의해 나타나는 현상임을 알 수 있었다.

Enhanced Anti-reflective Effect of SiNx/SiOx/InSnO Multi-layers using Plasma Enhanced Chemical Vapor Deposition System with Hybrid Plasma Source

  • Choi, Min-Jun;Kwon, O Dae;Choi, Sang Dae;Baek, Ju-Yeoul;An, Kyoung-Joon;Chung, Kwun-Bum
    • Applied Science and Convergence Technology
    • /
    • 제25권4호
    • /
    • pp.73-76
    • /
    • 2016
  • Multi-layer films of $SiN_x/SiO_x$/InSnO with anti-reflective effect were grown by new-concept plasma enhanced chemical vapor deposition system (PECVD) with hybrid plasma source (HPS). Anti-reflective effect of $SiN_x/SiO_x$/InSnO was investigated as a function of ratio of $SiN_x$ and $SiO_x$ thickness. Multi-layers deposited by PECVD with HPS represents the enhancement of anti-reflective effect with high transmittance, comparing to the layers by conventional radio frequency (RF) sputtering system. This change is strongly related to the optical and physical properties of each layer, such as refractive index, composition, film density, and surface roughness depending on the deposition system.

High Performance p-type SnO thin-film Transistor with SiOx Gate Insulator Deposited by Low-Temperature PECVD Method

  • U, Myeonghun;Han, Young-Joon;Song, Sang-Hun;Cho, In-Tak;Lee, Jong-Ho;Kwon, Hyuck-In
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • 제14권5호
    • /
    • pp.666-672
    • /
    • 2014
  • We have investigated the gate insulator effects on the electrical performance of p-type tin monoxide (SnO) thin-film transistors (TFTs). Various SnO TFTs are fabricated with different gate insulators of a thermal $SiO_2$, a plasma-enhanced chemical vapor deposition (PECVD) $SiO_x$, a $150^{\circ}C$-deposited PEVCD $SiO_x$, and a $300^{\circ}C$-deposited PECVD $SiO_x$. Among the devices, the one with the $150^{\circ}C$-deposited PEVCD $SiO_x$ exhibits the best electrical performance including a high field-effect mobility ($=4.86cm^2/Vs$), a small subthreshold swing (=0.7 V/decade), and a turn-on voltage around 0 (V). Based on the X-ray diffraction data and the localized-trap-states model, the reduced carrier concentration and the increased carrier mobility due to the small grain size of the SnO thin-film are considered as possible mechanisms, resulting in its high electrical performance.

무기 및 유기 박막을 포함하는 웨이퍼 적층 구조의 본딩 결합력 (Bond Strength of Wafer Stack Including Inorganic and Organic Thin Films)

  • 권용재;석종원
    • Korean Chemical Engineering Research
    • /
    • 제46권3호
    • /
    • pp.619-625
    • /
    • 2008
  • 패시베이션 및 절연 목적으로 이용하는 플라즈마 화학기상증착(PECVD)법에 의해 증착된 무기막과 웨이퍼 간 본딩 접착제로 이용하는 유기 박막 적층면의, 열 순환에 의한 잔류 응력 및 본딩 결합력의 효과를 4점 굽힙 시험법과 웨이퍼 곡률 측정법에 의해 평가하였다. 무기막으로는 산화 규소막($SiO_2$)과 산화 질화막($SiN_x$)이, 유기 박막으로는 BCB(Benzocyclobutene)가 이용되었다. 이를 통해, 열 순환 동안 무기막과 유기막 사이에서의 잔류 응력과 본딩 결합력의 상관관계에 대한 모델식을 개발하였다. 최대 온도 350 및 $400^{\circ}C$에서 수행한 열 순환 공정에서, PECVD 산화 질화막과 BCB로 구성된 다층막에서, 본딩 결합력은 첫 번째 순환 공정 동안 감소한다. 이는 산화질화막 내 잔류인장응력의 증가가 다층막의 잔류응력에 의해 변형되는 에너지 및 본딩 결합력의 감소를 유도한다는 모델식의 예측과 일치하며, PECVD 산화 규소막내 잔류 압축 응력의 감소가 다층막의 잔류응력에 의해 변형되는 에너지 및 본딩 결합력 상승을 이끄는 산화 규소막과 BCB 구조의 본딩 결합력 결과와 비교된다. 이러한 산화 규소막과 산화 질화막을 포함한 다층막의 상반된 본딩 결합력은 증착 공정 후 막 내에 형성된 수소 결합이 고온 순환 공정 동안 축합 반응을 통해 더 밀집되어 인장응력을 형성하기 때문임을 알 수 있었다.

BTMSM/O2 고유량으로 증착된 SiOCH 박막의 2차원 상관관계 분석을 통한 유전특성 연구 (Dielectric Characteristics through 2D-correlation Analysis of SiOCH Thin Film deposited by BTMSM/O2 High Flow Rates)

  • 김민석;황창수;김홍배
    • 한국전기전자재료학회논문지
    • /
    • 제21권6호
    • /
    • pp.544-551
    • /
    • 2008
  • We have studied the dielectric characteristics of low-k interlayer dielectric materials fabricated by PECVD for various precursor's flow rates. BTMSM precursor was introduced with the flow rates from 42 sccm to 60 sccm by 2 sccm step in the constant flow rate of 60 sccm $O_2$. The absorption intensities of Si-O-$CH_x$ bonding group and Si-$CH_x$ bonding group changed synchronously for the variation of precursor flow rate, but the intensity of Si-O-Si(C) responded asynchronously with the $CH_x$ combined bonds. The heat treatment reduced the FTIR absorption intensity of Si-O-$CH_x$ bonding group and Si-$CH_x$ bonding group but increased the intensity of Si-O-Si(C). The nanopore and free space formed by the increasement of caged link mode and cross link mode of Si-O-Si(C) group implied the origin of low-k SiOCH films.

BTMSM/$O_2$ 고유량으로 증착된 low-k SiOCH 박막의 전기적인 특성 (Electrical characteristics of low-k SiOCH thin film deposited by BTMSM/$O_2$ high flow rates)

  • 김민석;황창수;김홍배
    • 반도체디스플레이기술학회지
    • /
    • 제7권1호
    • /
    • pp.41-45
    • /
    • 2008
  • We studied the electrical characteristics of low-k SiOCR interlayer dielectric(ILD) films fabricated by plasma enhanced chemical vapor deposition (PECVD). The precursor bis-trimethylsilylmethane (BTMSM) was introduced into the reaction chamber with the various flow rates. The absorption intensities of Si-O-$CH_x$, bonding group and Si-$CH_x$, bonding group changed synchronously for the variation of precursor flow rate, but the intensity of Si-O-Si(C) responded asynchronously with the $CH_x$, combined bonds. The SiOCH films revealed ultra low dielectric constant around 2.1(1) and reduced further below 2.0 by heat treatments.

  • PDF

Remote PECVD SiO$_{2}$ 를 이용한 InSb MIS 소자의 특성 (Characteristics of InSb MIS device prepared by remote PECVD SiO$_{2}$)

  • 이재곤;최시영
    • 전자공학회논문지A
    • /
    • 제33A권12호
    • /
    • pp.59-64
    • /
    • 1996
  • InSb MIS devices prepared by remote PECVD SiO$_{2}$ were fabricated. The SiO$_{2}$ films on InSb were deposited at atemperature range of 67~190$^{\circ}$C. The effects of deposition temperature on the structural characteristics of the SiO$_{2}$ films evaluated Auger electron spectroscopy showed that atomic raito of silicon to oxygen was 0.5 and composition toms were distributed uniformaly throuout the oxide film. The transition region is about 100$\AA$ for SiO$_{2}$/InSb interface. The leakage current density at 1MV/cm and the breakdownelectric field of the MiS device using SiO$_{2}$ film deposited at 105$^{\circ}$C were about 22 nA/cm$^{2}$ and 3.5MV/cm, respectively. The interface-state density at mid-bandgap extracted from 1 MHz high frequency C-V measurement was about 2X10$^{11}$ cm$^{-2}$eV$^{-1}$.

  • PDF

HMDSO와 산소를 이용한 PECVD 증착 $SiO_xC_y$필름의 특성연구 (Characterization of $SiO_xC_y$ films deposited by PECVD using BMDSO and Oxygen)

  • 김성룡;이호영
    • 한국진공학회지
    • /
    • 제10권2호
    • /
    • pp.182-188
    • /
    • 2001
  • 폴리카보네이트 시트의 내마모성을 향상시키기 위하여 HMDSO 모노머와 산소를 사용하여 플라즈마 기상증착시킨 $SiO_xC_y$ 필름의 특성을 분석하였다. RF출력, 산소투입량, 수소투입량을 변화시키면서 각 증착조건에 따른 생성된 필름의 화학결합구조, 원소조성, 표면조도, 헤이즈 특성에 미치는 영향을 FTIR, XPS, AFM, Hazemeter를 이용하여 알아보았다. HMDSO와 산소를 사용한 박막의 증착은 100 nm/min이상의 높은 증착속도를 가졌고,증착실험에서 얻은 증착필름의 원소조성을 XPS를 이용하여 구한 결과, 종전의 다른 유기실리콘계 모노머를 사용했을때보다 박막에 존재하는 탄소잔류물을 효과적으로 감소시키는 것을 확인하였다. 또한, RF출력 200 Watt에서 산소가 100 sccm투입되었을 때 가장 우수한 헤이즈 특성을 보이는 막을 얻을 수 있었다. 본 연구로부터 HMDSO/$O_2$시스템이 탄소함량이 낮은 박막을 형성시키고 내마모도가 좋은 박막을 증착시키는데 효과적인 것을 알 수 있었다.

  • PDF

저온 선형 PECVD를 이용한 OLED용 Encapsulation 특성 연구

  • 윤승진;김성진;최정수;조병성;정석철
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.180-180
    • /
    • 2016
  • 최근 디스플레이 시장의 주요 키워드는 flexible organic light emitting diode (OLED) 이다. OLED 소자의 수명을 결정하는 가장 큰 요인 중의 하나는 공기 중의 O2와 H2O에 의한 유기물의 열화이다. 따라서 공기 중의 O2나 H2O가 유기물에 쉽게 침투하는 것을 막는 것은 소자의 수명 향상을 위하여 필수적이라 할 수 있다[1-3]. SiNx 박막은 경질로 투과성이 우수하며, 화학적 불활성인 특성으로 이러한 Barrier 역할로 연구되어 산업분야에 다양하게 응용되고 있다[4]. SiNx 박막은 일반적으로 plasma enhanced chemical vapor deposition (PECVD) 기술을 이용하여 증착되는데 기존의 PECVD 기술을 이용한 SiNx 박막은 낮은 water vapor transmission rate (WVTR) 등의 문제점들로 인해 한계점이 들어났다. 본 연구에서는, flexible display의 thin film encapsulation (TFE) 공정에서의 적용을 알아보기 위해 $370{\times}470$ size를 증착할 수 있는 In-line 장비를 이용하였으며, 기존의 PECVD 기술의 문제점으로 지적되고 있는 낮은 WVTR을 해결하기 위하여 저온 (<$100^{\circ}C$) 선형 PECVD 기술을 이용하여 WVTR을 개선하고자 하였다. 공정가스로는 SiH4와 NH3를 사용하였으며, SiH4 Carrier 가스로 He을 추가적으로 사용하였다. 또한 공정 압력은 100mTorr를 유지하였다. 증착된 SiNx 박막의 물리적, 화학적 특성 분석을 위해 분광엘립소메타, field emission electron microscopy (FESEM), X-ray diffraction (XRD), Rutherford backscattering spectrometry (RBS) 등을 이용하여 측정하였으며, 박막에 투습되는 수분의 양은 MOCON사의 AQUATRAN 2(W)로 측정하였다. OLED 소자를 구현하기 위해서는 기본적으로 봉지층에 투습되는 양을 $10-6g/m2{\cdot}day$ 이하로 막아줘야 한다고 알려져 있으나, 기존의 PECVD 기술을 이용하여 제작된 SiNx 박막의 WVTR은 $10-2{\sim}10-3g/m2{\cdot}day$ 레벨의 WVTR 결과를 보이고 있다. 본 연구에서 사용된 저온 선형 PECVD 기술을 이용하여 제작된 SiNx 박막의 WVTR은 $5.0{\times}10-5g/m2{\cdot}day$ 이하의 개선된 결과를 확인 할 수 있었다. 또한 flexible display에 적용하기 위해 SiNx 박막의 두께를 최소화한 100nm의 두께에서도 WVTR은 $5.0{\times}10-5g/m2{\cdot}day$ 이하의 결과가 유지됨을 알 수 있었다.

  • PDF