Microstructure and Mechanical Properties of CoCrFeMnNi-type High-entropy Alloy Fabricated by Selective Laser Melting: A Review (선택적 레이저 용융법으로 제조된 CoCrFeMnNi계 고엔트로피합금의 미세조직 및 기계적 물성 연구 동향)

  • Park, Jeong Min
    • Journal of Powder Materials
    • /
    • v.29 no.2
    • /
    • pp.132-151
    • /
    • 2022
  • The CoCrFeMnNi high-entropy alloy (HEA), which is the most widely known HEA with a single face-centered cubic structure, has attracted significant academic attention over the past decade owing to its outstanding multifunctional performance. Recent studies have suggested that CoCrFeMnNi-type HEAs exhibit excellent printability for selective laser melting (SLM) under a wide range of process conditions. Moreover, it has been suggested that SLM can not only provide great topological freedom of design but also exhibit excellent mechanical properties by overcoming the strength-ductility trade-off via producing a hierarchical heterogeneous microstructure. In this regard, the SLM-processed CoCrFeMnNi HEA has been extensively studied to comprehensively understand the mechanisms of microstructural evolution and resulting changes in mechanical properties. In this review, recent studies on CoCrFeMnNi-type HEAs produced using SLM are discussed with respect to process-induced microstructural evolution and the relationship between hierarchical heterogeneous microstructure and mechanical properties.

Characteristics of Ni-based Alloy Bond in Diamond Tool Using Vacuum Brazing Method

  • An, Sang-Jae;Song, Min-Seok;Jee, Won-Ho
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1130-1131
    • /
    • 2006
  • We found that the """interface reaction between Ni-based alloy bond, diamond, and steel core is very critical in bond strength of diamond tool. None element from metal bond diffuses into the steel core but the Fe element of steel core was easily diffused into the bond. This diffusion depth of Fe has a great effect on the bonding strength. The Cr in steel core accelerated the Fe diffusion and improved the bond strength, on the other hand, carbon decreased the strength. Ni-based alloy bond including Cr was chemically bonded with diamond by forming Cr carbide. However, the Cr and Fe in STS304 were largely interdiffused, the strength was very low. The Cr passivity layer formed at surface of STS304 made worse strength at commissure in brazing process.

  • PDF

Giant Magnetoresistance Behavior and the Effect of Ferromagnetic Layer on the Co-Ag Nano-granular Alloy Films (Co - Ag 합금박막의 거대자기저항 및 강자성 상하지층의 효과)

  • 김용혁;이성래
    • Journal of the Korean Magnetics Society
    • /
    • v.7 no.1
    • /
    • pp.31-37
    • /
    • 1997
  • The magnetoresistance and the saturation field behavior of the Co-Ag nano granular films as a function of the composition and the ferromagnetic underlayer and overlayermaterials were investigated. The maximum magnetoresistance of 23% and the saturation field of 2.3 kOe at room temperature were obtained in the as-deposited 3000$\AA$ $Co_{30}Ag_{70}$ single alloy films. The magnetoresistance and the saturation field of 100$\AA$ $Co_{30}Ag-{70}$ alloy film were 3.65 % and 3.0 kOe respectively. Those of the sandwiched films with 200$\AA$ Fe were 3.3 % and 1.23 kOe respectively. The saturation field of the sandwiched alloy films could be reduced by the exchange coupling between the ferromagnetic layers and the alloy layer. The effective depth of the exchange coupling was approximately 150$\AA$ in each Fe layer. Among the Fe, Co, and FeNi, the most effective materials to reduce the saturation field of the sandwiched alloy films was Fe.

  • PDF

Thermal Stability Improvement of Ni-Silicide using Ni-Co alloy for Nano-scale CMOSFET (나노급 CMOSFET을 위한 니켈-코발트 합금을 이용한 니켈-실리사이드의 열안정성 개선)

  • Park, Kee-Young;Jung, Soon-Yen;Han, In-Shik;Zhang, Ying-Ying;Zhong, Zhun;Li, Shi-Guang;Lee, Ga-Won;Wang, Jin-Suk;Lee, Hi-Deok
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.1
    • /
    • pp.18-22
    • /
    • 2008
  • In this paper, the Ni-Co alloy was used for thermal stability estimation comparison with Ni structure. The proposed Ni/Ni-Co structure exhibited wider range of rapid thermal process windows, lower sheet resistance in spite of high temperature annealing up to $700^{\circ}C$ for 30 min, more uniform interface via FE-SEM analysis, NiSi phase peak. Therefore, The proposed Ni/Ni-Co structure is highly promising for highly thermal immune Ni-silicide for nano-scale MOSFET technology.

The Effect of Composition and Current Condition on Magnetic Properties of Co-Fe-Ni Soft Magnetic Alloy (합금 조성과 전류조건이 CoFeNi 3원계 합금의 자기특성에 미치는 영향)

  • Jeung, Won-Young;Kim, Hyun-Kyung;Lee, Jeong-Oh
    • Journal of the Korean Magnetics Society
    • /
    • v.15 no.4
    • /
    • pp.241-245
    • /
    • 2005
  • CoFeNi alloys are some of the most studied soft magnetic materials because of their applications as write-head core materials in HDD and MEMS. Ternary CoFeNi films with high saturation magnetic flux density, Bs and low coercivity, He were successfully grown by electrodeposition. The optimal composition was $Co_{30}\;Fe_{34}\;Ni_{36}(at\%)$, and Bs and Hc were 1.9 T and 0.16 A/m, respectively. The XRD and TEM results show that the low Hc of the CoFeNi films was due to very fine crystal particles and mixed fcc and bcc phases.

Influence of High Temperature Deformation Process Variables on the Microstructure and Thermo-physical Properties of a Ni-Fe-Co Alloy (Fe-Ni-Co 합금의 고온 변형 공정 변수와 미세조직 및 열물리적 특성의 상관 관계)

  • Yoon, D.H.;Jung, J.E.;Chang, Y.W.;Lee, J.H.;Lee, K.S.
    • Transactions of Materials Processing
    • /
    • v.21 no.3
    • /
    • pp.207-214
    • /
    • 2012
  • High temperature deformation behavior of a $Ni_{30}Fe_{53}Co_{17}$ alloy, with its extraordinary low coefficient of thermal expansion less than $10{\times}10^{-6}K^{-1}$ at temperatures ranging from room temperature to 673K, was investigated by conducting a series of compression tests. From an empirical processing map, the appropriate working temperature-strain rate combination for optimum forming was deduced to be in the ~1373K, $10^{-2}s^{-1}$ region. This region has a relatively high power dissipation efficiency, greater than 0.36. Furthermore, open die forging of a 100mm diameter billets was performed to confirm the variation of thermo-physical properties in relation to microstructure. The coefficient of thermal expansion was found to increase considerably with increasing the open die forging temperature and decreasing the cooling rate, which in turn provides a drastic increase in the average grain size.

Cyclic Creep Properties of Nicoseal(Fe-29Ni-17Co) Alloy (Nicoseal(Fe-29Ni-17Co) 합금의 Cyclic 크리프 특성)

  • Park, Yong-Gwon;Choi, Jae-Ha
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.18 no.3
    • /
    • pp.177-182
    • /
    • 2005
  • The steady state cyclic mechanism, and the behaviour of Nicoseal(Fe-29Ni-17Co) have been examined under the condition of square wave stress cyclic tension creep test at the temperature, stress and frequency range of $430{\sim}470^{\circ}C$($0.41{\sim}0.43T_m$), 353~383 MPa, and 3 cpm, respectively. Also, the relationship between cyclic creep and static creep have been examined. The stress exponents(n) for the static creep deformation of this alloy were 11.6, 10.0, 8.4 and 7.9 at the temperature of 430, 445, 460 and $470^{\circ}C$, respectively. The apparent activation energies (Q) for the static creep deformation were 54.2, 51.8, 49.7 and 46.8 kcal/mole for the stress of 353, 363, 373 and 383 MPa, From the above results, it could be considered that the cyclic creep accelaration phenomena was obtained and that the cyclic deformation for Nicoseal seemed to be controlled by dislocation climb over the range of experimental conditions. Nicoseal alloy under the cyclic creep conditions was obtained as P=(T+460)(logt+17). The failure plane observed by SEM showed up transgranular fracture at all range.

Effects of Magnetic Characteristics on Coefficient of Thermal Expansion in Fe-Ni-Co-C Invar Alloy for Transmission Line (송전선 강심용 Fe-Ni-Co-C 합금의 열팽창계수에 미치는 자기적 특석의 영향)

  • Kim, Bong-Seo;Kim, Byung-Geol;Lee, Hee-Woong
    • Proceedings of the KIEE Conference
    • /
    • 2001.07c
    • /
    • pp.1346-1348
    • /
    • 2001
  • Generally, Invar alloy shows very low thermal expansion characteristics, lower than $2{\times}10^{-6}$/K approximately. To apply Fe-Ni-Co-C Invar alloy as a core material for large ampacity transmission line we studied the effects of magnetic properties on coefficient of thermal expansion. The coefficient of thermal expansion(CTE) suddenly decreases with addition of a little carbon(0.08%), increases with the increasing carbon and has a constant value at the composition over than 1.0%C. The trend of Curie temperature change with carbon is similar with that of CTE. Therefore, the CTE has a linear relationship with Curie temperature. However, the CTE linearly decreases with the ratio of saturation magnetization and Curie temperature(${\sigma}_s/T_c$).

  • PDF

Effect of Alloying Elements(Mn, Mo, B) on the High Temperature Deformation Behavior of Low Thermal Expansion Fe-Ni-Co Alloy (Fe-Ni-Co 코바 합금의 고온변형거동에 미치는 합금원소(Mn, Mo, B) 첨가의 영향)

  • Lee, Kee-Ahn;Yun, Ae-Cheon;Park, Jung-Chul;NamKung, Jung;Kim, Mun-Chul
    • Transactions of Materials Processing
    • /
    • v.17 no.4
    • /
    • pp.240-248
    • /
    • 2008
  • The effect of alloying elements(Mn, S, Mo, B) on the high temperature deformation behavior of Fe-29%Ni-17%Co (Kovar) alloy were investigated. And the effect of high temperature oxidation on the hot ductility was also studied. The hot ductility of Kovar alloy was drastically increased with the addition of Mn and lowering of S content. It has been found that the brittle intergranular fracture at high temperature cracking is closely associated with the FeS sulfide along the grain boundary. When Mn was added, the type of sulfide was changed to MnS from FeS and ductile intergranular fracture and transgranular fracture were promoted. The formation of oxide layer was found to have minimized the hot ductility of the Kovar alloy significantly. Grain boundary micro-cracks in the internal oxide region were noted following deformation due to high temperature, one of which acting as a notch that caused the poor hot workability of the oxidized specimen. The addition of Mo to the Kovar alloy could also retard the decrease in the hot ductility of the oxidized specimen through the prevention of notching due to internal oxidation. Hot ductility was remarkably improved by the addition of Boron. The improvement of hot ductility results from the grain boundary migration mainly due to the dynamic recrystallization at lower temperature range ($900{\sim}1000^{\circ}C$).