• 제목/요약/키워드: NbC

검색결과 1,380건 처리시간 0.029초

$MnO_2$ 첨가에 따른 $0.95(K_{0.5}Na_{0.5})NbO_3$-0.05Li$(Sb_{0.8}Nb_{0.2})O_3$ 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristics of $0.95(K_{0.5}Na_{0.5})NbO_3$-0.05Li$(Sb_{0.8}Nb_{0.2})O_3$ Ceramics with the amount of $MnO_2$ addition)

  • 김도형;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.172-173
    • /
    • 2008
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_3$-0.05Li$(Sb_{0.8}Nb_{0.2})O_3$ + $Ag_2O$ + x wt% $MnO_2$ were investigated as a function of the amount of $MnO_2$ addition in order to improve dielectric and piezoelectric properties of Lead-free piezoelectric ceramics. With increasing the amount of $MnO_2$ addition, density and electromechanical coupling factor $(k_p)$ increased up to 0.3wt.% $MnO_2$ and decreased above 0.3wt.% $MnO_2$. At the sintering temperature of 1020 $^{\circ}C$, Electromechanical coupling factor $(k_p)$, density, dielectric constant $({\varepsilon}r)$ and mechanical quality factor $(Q_m)$ of composition ceramics with 0.4wt% $Ag_2O$ addition showed the optimal value of 0.431, 4.33 g/$cm^3$, 820 and 119, respectively.

  • PDF

고온선박엔진용 MoSi$_2$금속간화합물의 경도와 방전가공특성 (Hardness and EDM Processing of MoSi$_2$Intermetallics for High Temperature Ship Engine)

  • 윤한기;이상필
    • 한국해양공학회지
    • /
    • 제16권6호
    • /
    • pp.60-64
    • /
    • 2002
  • This paper describes the machining characteristics of the MoSi$_2$--based composites through the process of electric discharge drilling with various tubular electrodes. In addition to hardness characteristics, microstructures of Nb/MoSi$_2$laminate composites were evaluated from the variation of fabricating conditions, such as preparation temperature, applied pressure, and pressure holding time. MoSi$_2$-based composites have been developed in new materials for jet engines of supersonic-speed airplanes and gas turbines for high-temperature generators. These high performance engines may require new hard materials with high strength and high temperature-resistance. Also, with the exception of grinding, traditional machining methods are not applicable to these new materials. Electric discharge machining (EDM) is a thermal process that utilizes a spark discharge to melt a conductive material. The tool electrode is almost -unloaded, because there is n direct contact between the tool electrode and the work piece. By combining a non-conducting ceramic with more conducting ceramic, it was possible to raise the electrical conductivity. From experimental results, it was found that the lamination from Nb sheet and MoSi$_2$ powder was an excellent strategy to improve hardness characteristics of monolithic MoSi$_2$. However, interfacial reaction products, like (Nb, Mo)SiO$_2$and Nb$_2$Si$_3$formed at the interface of Nb/MoSi$_2$, and increased with fabricating temperature. MoSi$_2$composites, with which a hole drilling was not possible through the conventional machining process, enhanced the capacity of ED-drilling by adding MbSi$_2$, relative to that of SiC or ZrO$_2$reinforcements.

Ti-Nb계 합금의 상변화가 기계적 성질에 미치는 영향 (Effects of phase changes on mechanical properties of Ti-Nb alloys)

  • 박효병
    • 대한치과기공학회지
    • /
    • 제27권1호
    • /
    • pp.9-17
    • /
    • 2005
  • The use of titanium alloys as biomaterials is increasing due to their superior biocompatibility and enhanced corrosion resistance compared to conventional stainless steels and cobalt-based alloys. Ti-6Al-4V ($\alpha+\beta$type) alloy instead of pure titanium ($\alpha$type) is being widely used as biomaterials has some characteristics such as high fatigue strength, tensile strength and corrosion resistance. But it has been reported recently that the vanadium element expresses cytotoxicity and the aluminium element is related with dementia of Alzheimer type and neurotoxicity. In order to overcome their detrimental effects, $\beta$-phase stabilizer Nb was chosen in the present study. This paper was described the influence of phase changes of Ti-Nb alloys on mechanical properties. Ti-3wt.%Nb($\alpha$type),Ti-20wt.%Nb($\alpha+\beta$type) and Ti-40wt.%Nb($\beta$type) alloys were melted by vacuum arc furnace. The specimens were homogenized at 1050$^{\circ}C$ for 24hr and were then hot rolled to 50% reduction. Each alloys were solution heat treated at $\beta$ zone and $\alpha+\beta$ zone after homogenization and then were aged. The mechanical properties of Ti alloys were analysed by hardness test, tensile test, elongation test and SEM test. The results can be summarized as follows: 1) The higher hardness value of $\alpha+\beta$type alloy was obtained compared to the, $\alpha,\beta$type alloys. 2) The aged treated showed better hardness compared to the solution heat treated, homogenized. 3) In the case of solution and aging treatment at $\beta$region, the $\alpha+\beta$type alloy showed the most highest tensile strength and $\beta$type alloy showed the best elongation.

  • PDF

Zr-2.5Nb 압력관에서 Striation Spacing과 DHCV의 관계 (A Correlation of Striation Spacing and DHC Velocity in Zr-2.5Nb Tubes)

  • 최승준;안상복;박순삼;김영석
    • 대한기계학회논문집A
    • /
    • 제28권8호
    • /
    • pp.1109-1115
    • /
    • 2004
  • The objective of this study is to elucidate what governs delayed hydride cracking (DHC) in Zr-2.5Nb tubes by correlating the striation spacings with DHCV(DHC Velocity). To this end, DHC tests were conducted on the compact tension specimens taken from the Zr-2.5Nb tubes at different temperatures ranging from 100 to $300^{\circ}C$ with a 3 to 6 data set at each test conditions. The compact tension specimens were electrolytically charged with 27 to 87 ppm H before DHC tests. After DHC tests, the striation spacings and DHCV were determined with the increasing the test temperature and yield strength. The striation spacing and DHCV increased as a function of yield $strength^2$ and the temperature. Since the plastic zone size ahead of the crack tip can be represented by ${\sim}(K_{IH}/{\sigma}_{Y})^2$, we conclude that the striation spacing is governed by the plastic zone size which in turn determines a gradient of hydrogen concentration at the crack tip. The relationship between the plastic zone size and the striation spacing was validated through a complimentary experiment using double cantilever beam specimens. Two main factors to govern DHCV of Zr-2.5Nb tubes are concluded to be hydrogen diffusion and a hydrogen concentration gradient at the crack tip that are controlled by temperature and yield strength, respectively. The activation energy of DHCV in the Zr-2.5Nb tubes is discussed on the basis of temperature dependency of hydrogen diffusion and the striation spacing.

생체의학 임플란트재료로서 Ti-Nb계 합금의 조직과 기계적 성질에 미치는 HEMM의 영향 (The Effect of HEMM on Microstructure and Mechanical Properties of Ti-Nb Alloy for Implant Biomedical Materials)

  • 우기도;최갑송;이현범;김인용
    • 한국재료학회지
    • /
    • 제17권11호
    • /
    • pp.587-592
    • /
    • 2007
  • Al-42wt%Nb powder was prepared by high-energy mechanical milling(HEMM). The particle size, phase transformation and microstructure of the as-milled powder were investigated by particle size distribution (PSD) analyzer, scanning electron microscopy (SEM), X-ray diffractometery (XRD), transmission electron microscopy (TEM)and differential thermal analysis (DTA). The milled powders were heated to a sintering temperature at 1000C with under vaccum with vaccum tube furnace. Microstructural examination of sintered Ti-42wt%Nb alloy using 4h-milled powder showed Ti-rich phases (${\alpha}$-Ti) which are fine and homogeneously distributed in the matrix (Nb-rich phase: ${\beta}$-Ti). The sintered Ti-42wt%Nb alloy with milled powder showed higher hardness. The microstructure of the as quenched specimens fabricated by sintering using mixed and milled powder almost are same, but the hardness of as quenched specimen fabricated by using mixed powder increased due to solution hardening of Nb in Ti matrix. The aging effect of these specimens on microstructural change and hardening is not prominent.

고잔류자화 $\alpha$-Fe기 Nd-Fe-B 초미세결정립 합금의 자기특성 (Magnetic Properties of $\alpha$-Fe Based Nd-Fe-B Nanocrystalline with High Remanence)

  • 조용수;김윤배;박우식;김창석;김택기
    • 한국자기학회지
    • /
    • 제5권1호
    • /
    • pp.38-41
    • /
    • 1995
  • $\alpha$-Fe를 주상으로 하는 새로운 Nd-Fe-B계 합금을 개발하기 위하여 Nd 함유량을 4at.%로 고정시킨 Nd-Fe-B 초미세결정립합금의 제조 및 자기특성이 조사되었다. 급속응고법으로 제조된 $Nd_{4}Fe_{85.5}B_{10.5}$ 비정질합금은 결정화하여 $\alpha$-Fe 기지상에 $Nd_{2}Fe_{14}B$이 형성되나 자기특성${_{i}H_{c}=95.5kA/m(1.2kOe),\;Br=1.2T}$은 열화된다. Nb 및 Cu를 첨가한 $Nd_{4}Fe_{82}B_{10}Nb_{3}Cu_{1}$ 합금은 $\alpha$-Fe 결정립미세화(<30nm)로 보자력이 207kA/m(2.6 kOe)로 증가하나 잔류자화는 개선되지 않았다. 이 합금조성에 8at.% Co 첨가는 결정립을 더욱 미세화시키며 자기특성을 개선 시킨다. 최적열처리조건에서 $Nd_{4}Fe_{74}Co_{8}B_{10}Nb_{3}Cu_{1}$ 합금의 잔류자화, 보자력 및 최대에너지적이 각각 1.34 T, 219 kA/m (2.75kOe) 및 $95.5kJ/m^{3}$(12MGOe) 이다.

  • PDF

Microstructure and Biocompatibility of Ti-Nb-Si-HA Composites Fabricated by Rapid Sintering Using HEMM Powders

  • Woo, Kee-Do;Kim, Sang-Hyuk;Kang, Dong-Soo;Kim, Dong-Gun
    • 한국재료학회지
    • /
    • 제23권7호
    • /
    • pp.353-358
    • /
    • 2013
  • To improve coating ability and the life of the coating, Ti based composite materials with hydroxyapatite(HA) should be developed. The raw materials of Ti-26wt%, Nb-1wt%, and Si with 10wt% HA were mixed for 24 h by a mixing machine and milled for 1 h to 6 h by planetary mechanical ball milling. Ti-26%Nb-1%Si-(10%HA) composites, composed of nontoxic elements, were fabricated successfully by spark plasma sintering(SPS) at $1000^{\circ}C$ under 70MPa. The relative density of the sintered Ti-Nb-Si-HA composites using the 24 h mixed powder, and the 6 h milled powder, was 91% and 97 %, respectively. The effects of HA contents and milling time on microstructure and mechanical properties were investigated by SEM and hardness tester, respectively. The Vickers hardness of the composites increased with increasing milling time and higher HA content. The Young's modulus of the sintered Ti-26%Nb-1%Si-10%HA composite using the 6 h-milled powder was 55.6 GPa, as obtained by compression test. Corrosion resistance of the Ti-26wt%Nb-1wt%Si composite was increased by milling and by the addition of 10wt%HA. Wear resistance was improved with increasing milling time. Biocompatibility of the Ti-Nb-Si alloys was improved by the addition of HA.

DNA Dynamics: a Fluorescence Resonance Energy Transfer Study Using a Long-Lifetime Metal-Ligand Complex

  • Kang, Jung-Sook;Lakowicz, Joseph-R.;Piszczek, Grzegorz
    • Archives of Pharmacal Research
    • /
    • 제25권2호
    • /
    • pp.143-150
    • /
    • 2002
  • Fluorescent probes bound to DNA typically display nanosecond decay times and reveal only nanosecond motions. We extend the time range of measurable DNA dynamics using $[Ru(pby)_2(dppz)]^{2+}$ (bpy=2.2'-bipyridine, dppz=dipyrido[3,2-a2',3'-c]phenazine) (RuBD) which displays a mean lifetime near 90 ns. To test the usefulness of RuBD as a probe for diffusive processes in calf thymus DNA, we compared the efficiencies of fluorescence resonance energy transfer (FRET) using three donors which display lifetimes near 5 ns for acridine orange (AO), 22 ns for ethidum bromide (EB) and 92 ns for RuBD, with nile blue (NB) as the acceptor. The F rster distances for AO-NB, EB-NB and RuBD-NB donor-acceptor pairs were 42.3, 52.3, and $30.6{\;}{\AA}$, respectively. All three donors showed dramatic decreases in fluorescence intensities and more rapid intensity decays with increasing NB concentrations. The intensity decays of AO and EB in the presence of varying concentrations of NB were satisfactorily described by the one-dimensional FRET model without diffusion (Blumen and Manz, 1979). In the case of the long-lifetime donor RuBD, the experimental phase and modulation somewhat deviated from the recovered values computed from this model. The recovered NB concentrations and FRET efficiencies from the model were slightly larger than the expected values, however, the recovered and expected values did not show a significant difference. Thus, it is suggested that the lifetime of RuBD is too short to measure diffusive processes in calf thymus DNA.

저에너지 양전자 소멸 분광법을 이용한 Nb3Ge 박막 특성 (The Characterization of Nb3Ge by Slow Positron Annihilation Spectroscopy)

  • 이종용;배석환
    • 한국진공학회지
    • /
    • 제19권6호
    • /
    • pp.489-494
    • /
    • 2010
  • 저속 에너지 도플러 넓어짐 양전자 소멸 분광법으로 $Nb_3Ge$ 시료내의 원자 크기 정도 고체 구조 특성에 대하여 조사하였다. A15 화합물 구조로 된 $Nb_3Ge$ 시료를 상온에서 초전도 특성을 갖는 상전이 온도 근처의 S-변수를 측정하였다. 양전자와 전자의 쌍소멸로 발생하는 511 keV 감마선 스펙트럼의 수리적 해석 방법인 S-변수를 사용하여, 상전이 근처 온도에서 박막의 구조 변화를 측정하였다. 양전자의 입사 에너지에 따른 S-변수는 0.598에서 0.594로 온도의 변화에 의하여 감소하였으며 이때 초전도 전이와는 무관함을 나타낸다. 고온으로 갈수록 일반적인 트랩핑 비율은 커지고 양전자 흐름은 공공(voids) 근처에서 소멸하는 것이 보였다. 이 결과로부터 양전자가 초전자와 소멸하기 보다는 상전자와 소멸하는 것으로 판단된다.

액츄에이터 응용을 위한 Pb(Ni1/3Nb2/3)O3-PbTiO3 세라믹스의 압전 특성에 미치는 Fe2O3 첨가 영향 (Effects of Fe2O3 Addition on Piezoelectric Properties of Pb(Ni1/3Nb2/3)O3-PbTiO3 Ceramics for Actuator Applications)

  • 임은경;김창일;이영진;임종인;백종후
    • 한국전기전자재료학회논문지
    • /
    • 제19권10호
    • /
    • pp.935-941
    • /
    • 2006
  • In this paper, the dielectric and piezoelectric properties of $0.4Pb(Ni_{1/3}Nb_{2/3})O_3+0.6Pb(Zr_{405}Ti_{595})O_3+X\;wt%\;Fe_2O_3$ ceramics were investigated with the addition of $Fe_2O_3$ and sintering temperature. Dielectric constant and piezoelectric constant increased with amount of $Fe_2O_3$ to 0.25 wt% and then decreased the further addition of $Fe_2O_3$. It seems that $Fe_2O_3$ acts as a sintering aid at the sintering temperature of $1150^{\circ}C$. By the addition of $Fe_2O_3$., sintering temperature of the system was lowered from $1250^{\circ}C\;to\;1100^{\circ}C$. The piezoelectric properties showed the maximum value of ${\varepsilon}r=4669,\;d_{33}=810(10^{-12}m/V)$, kp = 77 %, Qm = 55, in $0.4Pb(Ni_{1/3}Nb_{2/3})O_3\;-0.6Pb(Zr_{0.405}Ti_{0.595})O_3+0.25wt%\;Fe_2O_3$ ceramics having composition near the morphotropic phase boundary. The composition may be appropriate for actuator materials because of high piezoelectric constant and electromechanical coupling factor.