• 제목/요약/키워드: Low melting temperature

검색결과 450건 처리시간 0.028초

직류 전력케이블용 반도전 복합체의 열적 특성 (Thermal Properties of Semiconductive Composites for DC Power Cable)

  • 이기정;서범식;양종석;성백룡;박대희
    • 한국전기전자재료학회논문지
    • /
    • 제26권1호
    • /
    • pp.49-55
    • /
    • 2013
  • In this paper, semiconducting shield specimens for a DC cable os fabricated and characterized by measurement of volume resistance, tensile strength, and the coefficient of expansion to show the electrical and mechanical characteristics of the semiconducting shield. Due to the PTC phenomenon, the volume resistance at $25^{\circ}C$ increases rapidly in comparison to the volume resistance at $90^{\circ}C$. Since the compounding ration of carbon black is low, the tensile strength and density become lower and the coefficient of expansion is increased. As the general specification of the tensile strength and density is $0.8kgf/mm^2$ and 150%, respectively, the fabricated specimen in this paper has excellent mechanical characteristic.

고체 추진기관 선진국 기술 동향에 관한 연구 (A Study on the Advanced Technology of Solid Rocket Propulsion)

  • 김형원;박종승
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2010년도 제35회 추계학술대회논문집
    • /
    • pp.221-224
    • /
    • 2010
  • 최근에 인공위성을 궤도에 올리는데 막대한 비용이 들어가므로, 소형이면서 좀 더 신뢰도가 높은 인공위성이 요구되어 왔다. 추진제의 새로운 바인더(HTPB, GAP)와 산화재(CL20, ADN)의 발명은 로켓의 추력을 다양하게 하는데 많은 기여를 했다. 제조 공정을 획기적으로 변화시키는 낮은 온도에서 녹는 열가소성 추진제는 비용을 상당히 절감시켰다. 인공위성을 궤도에 정확하게 안착시키는데 어려움이 있었던 고체 연료 로켓은 액체추진제를 사용하는 PBS를 상단에 추가 설치함으로 정확도를 증진시켰다. 이 논문에서 또한 선진화된 노즐재료와 연소관에 대해서도 방향을 제시한다.

  • PDF

Control of Mechanical Properties of Polyurethane Elastomers Synthesized with Aliphatic Diisocyanate Bearing a Symmetric Structure

  • Kojio, Ken;Nozaki, Shuhei;Takahara, Atsushi;Yamasaki, Satoshi
    • Elastomers and Composites
    • /
    • 제54권4호
    • /
    • pp.271-278
    • /
    • 2019
  • Polyurethane elastomers (PUEs) were synthesized using trans-1,4-bis(isocyanatomethyl) cyclohexane (1,4-H6XDI), poly(oxytetramethylene) glycol, 1,4-butanediol (BD), and 1,1,1-trimethylol propane (TMP). To control the molecular aggregation state and mechanical properties of these PUEs, hard segment contents of 20 and 30 wt% and BD/TMP ratios of 10/0 and 8/2 were chosen. Differential scanning calorimetry and small-angle X-ray scattering measurements revealed that the degree of microphase separation increased with an increase in both hard segment content and BD ratio. The Young's modulus and strain at break of the 1,4-H6XDI-based PUE were 6-20 MPa and 5-15, respectively. Incorporation of 20% TMP as a cross-linking agent into BD increased the melting temperature of the hard segment chains, that is, heat resistance, and decreased the Young's modulus. This could be due to the low density of the physical cross-linking network and the dispersion of hard segment chains in the soft segment matrix in the PUE in the presence of 20% TMP.

Optimization of Material and Process for Fine Pitch LVSoP Technology

  • Eom, Yong-Sung;Son, Ji-Hye;Bae, Hyun-Cheol;Choi, Kwang-Seong;Choi, Heung-Soap
    • ETRI Journal
    • /
    • 제35권4호
    • /
    • pp.625-631
    • /
    • 2013
  • For the formation of solder bumps with a fine pitch of 130 ${\mu}m$ on a printed circuit board substrate, low-volume solder on pad (LVSoP) technology using a maskless method is developed for SAC305 solder with a high melting temperature of $220^{\circ}C$. The solder bump maker (SBM) paste and its process are quantitatively optimized to obtain a uniform solder bump height, which is almost equal to the height of the solder resist. For an understanding of chemorheological phenomena of SBM paste, differential scanning calorimetry, viscosity measurement, and physical flowing of SBM paste are precisely characterized and observed during LVSoP processing. The average height of the solder bumps and their maximum and minimum values are 14.7 ${\mu}m$, 18.3 ${\mu}m$, and 12.0 ${\mu}m$, respectively. It is expected that maskless LVSoP technology can be effectively used for a fine-pitch interconnection of a Cu pillar in the semiconductor packaging field.

Lamp ZMR에 의한 SOI에서 비대칭 선형가열의 효과 (Effect of Asymmetric Line Heating in SOI Lamp ZMR)

  • 반효동;이시우;임인곤;주승기
    • 한국결정성장학회지
    • /
    • 제2권2호
    • /
    • pp.53-62
    • /
    • 1992
  • SOI구조 형성을 위항 대용융 재결정(ZMR) 공정에서 타원형의 반사경을 기울여 빔강도분포를 인위적으로 변화시켜 실리콘 박막을 재결정시켰다. 비대칭 선형가열 효과를 해석하기 위하여 전산모사를 행하여 응고계면 근처에서의 온도분포와 열구배 변화를 조사하였다. 상부집속열원의 경사각이 증가할수록 액상의 과냉도와 실리콘 박막내의 결함열 간격은 증가하였다. 주된 결함은 연속적인 아결정립계였고 결함밀도가 낮은 경우는 isolated threading dislocations만이 관찰되었다. 단면 TEM과 박막 XRD 분석결과 실리콘 박막은 (100) 집합조직을 갖는 단결정 박막으로 재결정되었음을 확인할 수 있었다.

  • PDF

Development of a Porous Scaffold-Manufacturing Method by Blending Silk Fibroin and Agarose Polymer Solutions

  • Park, Seung-Won;Kweon, Hae-Yong;Goo, Tae-Won;Kim, Seong-Ryul;Jo, You-Young;Choi, Gwang-Ho
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • 제25권1호
    • /
    • pp.75-79
    • /
    • 2012
  • Low-melting-temperature agarose gel solution, as a novel porogen was combined with a silk fibroin solution to generate interconnected porous networks. The porosity of the resultant silk fibroin-agarose scaffolds was greater than that of the scaffolds generated with agarose and deionized water. The porosities of silk fibroin scaffolds containing agarose gel at 0.5%, 1.0%, 1.5%, 2.0% [w/v] were 110.9%, 111.7%, 120.9%, and 123.0%, respectively. Lastly, the internal space generated in scaffolds after dissolution of the agarose gel provides a good environment for cell growth and movement within the scaffold.

V2O5 도핑된 NiCuZn 페라이트로 제조된 칩인덕터에서의 Ag/cu 석출 (Ag and Cu Precipitation in Multi-Layer Chip Inductors Prepared with V2O5 Doped NiCuZn Ferrites)

  • 제해준;김병국
    • 한국재료학회지
    • /
    • 제13권8호
    • /
    • pp.503-508
    • /
    • 2003
  • The purpose of this study is to investigate the effect of $V_2$$O_{5}$ addition on the Ag and Cu precipitation in the NiCuZn ferrite layers of 7.7${\times}$4.5${\times}$1.0 mm sized multi-layer chip inductors prepared by the screen printing method using 0∼0.5 wt% $V_2$$O_{5}$ -doped ferrite pastes. With increasing the $V_2$$O_{5}$ content and sintering temperature, Ag and Cu oxide coprecipitated more and more at the polished surface of ferrite layers during re-annealing at $840^{\circ}C$. It was thought that during the sintering process, V dissolved in the NiCuZn ferrite lattice and the Ag-Cu liquid phase of low melting point was formed in the ferrite layers due to the Cu segregation from the ferrite lattice and Ag diffusion from the internal electrode. During re-annealing at $840^{\circ}C$, the Ag-Cu liquid phase came out the polished surface of ferrite layers, and was decomposed into the isolated Ag particles and the Cu oxide phase during the cooling process.

RTV 실리콘 고무의 표면열화와 내오손 특성과의 상관관계 (Relation between Surface degradation and Anti-pollution Characteristics in RTV Silicone Rubber)

  • 연복희;이태호;허창수;이상엽
    • 한국전기전자재료학회논문지
    • /
    • 제13권7호
    • /
    • pp.598-606
    • /
    • 2000
  • In this paper we investigated the relation between the surface degradations and anti-pollution characteristics of Room Temperature Vulcanized(RTV) silicone rubber coating that has different roughness through immersing into saline water. We utilized several analytic techniques such as atomic force microscopy(AFM) scaning electron microscopy(SEM) contact angle Salt Deposit Density(SDD) and average leakage current under the condition of salt fog. It is found that the surface roughness of treated RTV silicone rubber increased and the hydrophobicity of sample surface decreased with increasing the duration o immersion into water due to the erosion of base polymer the melting down alumina trihydrate(ATH) and the diffusion of Low Molecular weight(LMW) fluid. Despite the roughness of surface had been increased by water immersion excellant anti-pollution and recovery characteristics were maintained and SDD saturated to 0.1~0.14mg/cm$^2$. The average leakage current under salt fog increased with surface roughness. Measurement of average leakage current will be helpful to investigate surface degradation and lifetime expectation of RTV silicone coating.

  • PDF

Alkaline Sizing of Mechanical Pulp

  • Kim, Bong-Yong;Akira Isogai
    • 펄프종이기술
    • /
    • 제32권5호
    • /
    • pp.1-7
    • /
    • 2000
  • Alkaline Sizing behavior and mechanism of handsheets, which were prepared from thermomechanical pulp (TMP) with alkylketene dimer (AKD), were studied in terms of the conditions of the handsheet-making. AKD content in the TMP handsheets was increased with increasing of AKD addition level and the addition of a polyamideamine-epichlorohydrin resin (PAE) clearly enhanced AKD retention as well as the resultant sizing performance of TMP handsheets. Although drying of the AKD sized TMP webs at $20^{\circ}C$ led to no or quite low sizing level, but TMP handsheets sized with AKD had higher sizing degrees with increasing of the temperature of heat treatment. Scanning electron microscopic observations of the AKD-sized TMP handsheets showed that AKD emulsion particles were present on pulp fiber surfaces independently without coagulation in the TMP handsheets dried at $20^{\circ}C$. Heat treatment of the AKD-sized handsheets resulted in disappearance of the AKD emulsion particles because of their melting and spreading. The addition of calcium carbonate filler to the TMP suspensions did not influence on AKD content in the TMP handsheets. Nevertheless, their sizing degrees clearly increased by the addition of $CaCO_3$filler. Probably, AKD molecules adsorbed on the $CaCO_3$filler particles contribute to the enhancement of sizing performance. Thus, AKD can give sizing features effectively to the TMP handsheets, when they are made under suitable conditions.

  • PDF

제어압연${\cdot}$제어냉각기술을 이용한 고강도 냉간성형용 비조질강의 개발 (Development of High Strength Microalloyed Steel for Cold Forming by Controlled Rolling and Cooling Technology)

  • 김남규;박상덕;김병옥;최회진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.321-324
    • /
    • 2005
  • The main purpose of the present study has been placed on investigating the effects of controlled rolling and cooling on the microstructures and mechanical properties of C-Si-Mn-V steels for cold forming. The steels were manufactured in vacuum induction melting(VIM) furnace and casted to 1.1ton Ingots and the ingots were forged to $\Box150$ billet. The forged billets were reheated in walking beam furnace and rolled to coil, the stocks were rolled by Controlled Rolling and Cooling Technology (CRCT), so rolled at low temperature by water spraying applied in rolling stage and acceleratly cooled before coiling. Rolled coils were cold drawed to the degree of $27\%$ of area reduction without heat treatment. Microstructual observation, tensile test, compression test and charpy impact tests were conducted. The mechanical properties of the steels were changed by area reduction of cold drawing and it is founded that there are optimum level of cold drawing to minimize compression stress for these steels. From the result of this study, it is conformed that mechanical properties and microstructure of C-Si-Mn-V steels for cold forming were enhanced by accelerated cooling and founded optimum level of cold drawing.