경질양극산화된 5083-H321 알루미늄 합금의 해수 내 액적충격침식부식 손상 연구 (Investigation of Liquid Droplet Impingement Erosion Corrosion based on the Flow Rate of Anodized 5083-H321 Al Alloy in Seawater)

  • 신동호;김성종
    • Corrosion Science and Technology
    • /
    • 제19권6호
    • /
    • pp.310-317
    • /
    • 2020
  • This study investigated the damage to the specimen due to liquid droplet impingement erosion corrosion, which improved the corrosion resistance and durability via hard anodization of 5083-H321 aluminum alloy, which is widely used for small ships and marine structures. The experiment combined liquid droplet impingement erosion and electrochemical equipment with the flow rates in natural seawater solution. Subsequently, Tafel extrapolation of polarization curves was performed to evaluate damage due to the liquid droplet impingement erosion corrosion. The damaged surface was observed using a 3D microscope and a scanning electron microscope. The degree of pitting damage was measured using the Image J program, and the surface hardness was measured using the micro-Vickers hardness tester. The corrosion current density, area, depth, and ratio of the damaged areas increased with the increase in flow rate. The grain size of the damaged area at a flow rate of 20 m s-1 showed fewer and minor differences in height, and a smooth curved shape. The hardness of the damaged surface tended to decrease with increase in flow rate.

배관 재질 손상에 미치는 액적충돌침식의 영향에 대한 연구 (A Study for the Effect of Liquid Droplet Impingement Erosion on the Loss of Pipe Flow Materials)

  • 김경훈;조연수;김형준
    • 한국분무공학회지
    • /
    • 제18권1호
    • /
    • pp.9-15
    • /
    • 2013
  • Wall thinning of pipeline in power plants occurs mainly by flow acceleration corrosion (FAC), cavitation erosion (C/E), liquid droplet impingement erosion (LDIE). Wall thinning by FAC and C/E has been well investigated; however, LDIE in plant industries has rarely been studied due to the experimental difficulty of setting up a long injection of highly-pressurized air. In this study, we designed a long-term experimental system for LDIE and investigate the behavior of LDIE for three kinds of materials (A106B, SS400, A6061). The main control parameter was the air-water ratio (${\alpha}$), which was defined as the volumetric ratio of water to air (0.79, 1.00, 1.72). In order to clearly understand LDIE, the spraying velocity (${\nu}$) of liquid droplets was controled larger then 160 m/s and the experiments were performed for 15 days. Therefore, this research focuses relation between erosion rate and air-water ratio on the various pipe-flow materials. NPP(nuclear power plant)'s LDIE prediction theory and management technique were drawn from the obtained data.

배관 침부식 손상 연속모사 장비 개발 및 실증 (Development and demonstration of an erosion-corrosion damage simulation apparatus)

  • 남원창;류경하;김재형
    • Corrosion Science and Technology
    • /
    • 제12권4호
    • /
    • pp.179-184
    • /
    • 2013
  • Pipe wall thinning caused by erosion and corrosion can adversely affect the operation of aged nuclear power plants. Some injured workers owing to pipe rupture has been reported and power reduction caused by unexpected pipe damage has been occurred consistently. Therefore, it is important to develop erosion-corrosion damage prediction model and investigate its mechanisms. Especially, liquid droplet impingement erosion(LDIE) is regarded as the main issue of pipe wall thinning management. To investigate LDIE mechanism with corrosion environment, we developed erosion-corrosion damage simulation apparatus and its capability has been verified through the preliminary damage experiment of 6061-Al alloy. The apparatus design has been based on ASTM standard test method, G73-10, that use high-speed rotator and enable to simulate water hammering and droplet impingement. The preliminary test results showed mass loss of 3.2% in conditions of peripheral speed of 110m/s, droplet size of 1mm-diameter, and accumulated time of 3 hours. In this study, the apparatus design revealed feasibility of LDIE damage simulation and provided possibility of accelerated erosion-corrosion damage test by controlling water chemistry.

Numerical Analysis of Damping Effect of Liquid Film on Material in High Speed Liquid Droplet Impingement

  • Sasaki, Hirotoshi;Ochiai, Naoya;Iga, Yuka
    • International Journal of Fluid Machinery and Systems
    • /
    • 제9권1호
    • /
    • pp.57-65
    • /
    • 2016
  • By high speed Liquid Droplet Impingement (LDI) on material, fluid systems are seriously damaged, therefore, it is important for the solution of the erosion problem of fluid systems to consider the effect of material in LDI. In this study, by using an in-house fluid/material two-way coupled method which considers reflection and transmission of pressure, stress and velocity on the fluid/material interface, high-speed LDI on wet/dry material surface is simulated. As a result, in the case of LDI on wet surface, maximum equivalent stress are less than those of dry surface due to damping effect of liquid film. Empirical formula of the damping effect function is formulated with the fluid factors of LDI, which are impingement velocity, droplet diameter and thickness of liquid film on material surface.

주증기계통 오리피스 후단 소구경 배관의 감육 및 누설 발생 (Cause Analysis for the Wall Thinning and Leakage of a Small Bore Piping Downstream of an Orifice)

  • 황경모
    • Corrosion Science and Technology
    • /
    • 제12권5호
    • /
    • pp.227-232
    • /
    • 2013
  • A number of components installed in the secondary system of nuclear power plants are exposed to aging mechanisms such as FAC (Flow-Accelerated Corrosion), Cavitation, Flashing, and LDIE (Liquid Droplet Impingement Erosion). Those aging mechanisms can lead to thinning of the components. In April 2013, one (1) inch small bore piping branched from the main steam line experienced leakage resulting from wall thinning in a 1,000 MWe Korean PWR nuclear power plant. During the normal operation, extracted steam from the main steam line goes to condenser through the small bore piping. The leak occurred in the downstream of an orifice. A control valve with vertical flow path was placed on in front of the orifice. This paper deals with UT (Ultrasonic Test) thickness data, SEM images, and numerical simulation results in order to analyze the extent of damage and the cause of leakage in the small bore piping. As a result, it is concluded that the main cause of the small bore pipe wall thinning is liquid droplet impingement erosion. Moreover, it is observed that the leak occurred at the reattachment point of the vortex flow in the downstream side of the orifice.

액적충돌침식으로 인한 배관감육 예측체계 구축에 관한 연구 (A Study on the Development of Prediction System for Pipe Wall Thinning Caused by Liquid Droplet Impingement Erosion)

  • 김경훈;조연수;황경모
    • Corrosion Science and Technology
    • /
    • 제12권3호
    • /
    • pp.125-131
    • /
    • 2013
  • The most common pipe wall thinning degradation mechanisms that can occur in the steam and feedwater systems are FAC (Flow Acceleration Corrosion), cavitation, flashing, and LDIE (Liquid Droplet Impingement Erosion). Among those degradation mechanisms, FAC has been investigated by many laboratories and industries. Cavitation and flashing are also protected on the piping design phase. LDIE has mainly investigated in aviation industry and turbine blade manufactures. On the other hand, LDIE has been little studied in NPP (Nuclear Power Plant) industry. This paper presents the development of prediction system for pipe wall thinning caused by LDIE in terms of erosion rate based on air-water ratio and material. Experiment is conducted in 3 cases of air-water ratio 0.79, 1.00, and 1.72 using the three types of the materials of A106B, SS400, and A6061. The main control parameter is the air-water ratio which is defined as the volumetric ratio of water to air (0.79, 1.00, 1.72). The experiments were performed for 15 days, and the surface morphology and hardness of the materials were examined for every 5 days. Since the spraying velocity (v) of liquid droplets and their contact area ($A_c$) on specimens are changed according to the air-water ratio, we analyzed the behavior of LDIE for the materials. Finally, the prediction equations(i.e. erosion rate) for LDIE of the materials were determined in the range of the air-water ratio from 0 to 2%.

예측모델 및 실험을 통한 액적충돌침식 손상 평가 (Evaluation of Liquid Droplet Impingement Erosion through Prediction Model and Experiment)

  • 윤훈;황경모
    • 대한기계학회논문집B
    • /
    • 제35권10호
    • /
    • pp.1105-1110
    • /
    • 2011
  • 유동가속부식(FAC)은 가장 잘 알려진 탄소강 배관 손상 메커니즘으로 현재 국내 전 원전에서는 유동가속부식으로 인한 감육현상을 관리할 수 있는 체계적인 방안이 수립되어 있다. 그러나, 발전소 배관은 다양한 침식손상 메커니즘에 의해 여전히 손상을 받고 있다. 대표적인 침식 메커니즘은 캐비테이션, 액적충돌침식(LDIE), 플래싱, 고체입자침식(SPE)이다. 본 논문에서 기술하는 액적충돌침식 은 손상예측이 어렵고, 관리를 위한 체계적인 방안도 수립되어 있지 않다. 본 논문에서는 실제 발전소 현장에서 발생한 사례를 바탕으로 기존에 개발된 예측 모델과 실험을 통해 얻어진 상관식을 비교하여 액적충돌침식으로 인한 손상을 평가할 수 있는 방법을 제시하였다.

B-Scan 초음파 측정장비를 이용한 원전 배관 침식손상 검사법 개발 (Development of Inspection Methodology for a Nuclear Piping Wall Thinning Caused by Erosion Using Ultrasonic B-Scan Measurement Device)

  • 이대영;서혁기;황경모
    • Corrosion Science and Technology
    • /
    • 제11권3호
    • /
    • pp.89-95
    • /
    • 2012
  • U.S. Electric Power Research Institute (EPRI) has developed CHECWORKS program and applied it to power plant piping lines since some lines were ruptured by flow-accelerated corrosion (FAC) in 1978. Nowadays the CHECWORKS program has been used to manage pipe wall thinning phenomena caused by FAC. However, various erosion mechanisms can occur in carbon-steel piping. Most common forms of erosion are cavitation, flashing, liquid droplet impingement erosion (LDIE), and Solid Particle Erosion (SPE). Those erosion mechanisms cause pipe wall thinning, leaking, rupturing, and even result in unplanned shutdowns of utilities. Especially, in two phase condition, LDIE damages a wide scope of plant pipelines. Furthermore, LDIE is the major culprit to cause such as power runback by pipe leaking. This paper describes the methodologies that manage wall thinning and also predict LDIE wall thinning area. For this study, current properties of two-phase condition are investigated and LDIE areas are selected. The areas are checked by B-Scan method to detect the effect of wall thinning phenomena.