• 제목/요약/키워드: High Higher surfaces

검색결과 270건 처리시간 0.024초

A STUDY ON OSTEOBLAST-LIKE CELL RESPONSES TO SURFACE-MODIFIED TITANIUM

  • Hong Min-Ah;Kim Yung-Soo;Kim Chang-Whe;Jang Kyung-Su;Lee Jae-Il
    • 대한치과보철학회지
    • /
    • 제41권3호
    • /
    • pp.300-318
    • /
    • 2003
  • Statement of problem: The success of implants depends on intimate and direct contact of implant material on bone tissue and on functional relationship with soft tissue contact. Creation and maintenance of osseointegration depend on the understanding of the tissue's healing, repairing, and remodeling capacity and these capacities rely on cellular behavior. Altering the surface properties can modify cellular responses such as cell adhesion, cell motility, bone deposition, Therefore, various implant surface treatment methods are being developed for the improved bone cell responses. Purpose: The purpose of this study was to evaluate the responses of osteoblast-like cells to surface-modified titanium. Materials and Methods: The experiment was composed of four groups. Group 1 represented the electropolished surface. Group 2 surfaces were machined surface. Group 3 and Group 4 were anodized surfaces. Group 3 had low roughness and Group 4 had high roughness. Physicochemical properties and microstructures of the discs were examined and the responses of osteoblast-like cells to the discs were investigated. The microtopography was observed by SEM. The roughness was measured by three-dimension roughness measuring system. The microstructure was analyzed by XRD, AES. To evaluate cell responses to modified titanium surfaces, osteoblasts isolated from calvaria of neonatal rat were cultured. Cell count, morphology, total protein measurement and alkaline phosphatase activities of the cultures were examined. Results and Conclusion: The results were as follows 1. The four groups showed specific microtopography respectively. Anodized group showed grain structure with micropores. 2. Surface roughness values were, from the lowest to the highest, electropolished group, machined group, low roughness anodized group, and high roughness anodized group. 3. Highly roughened anodized group was found to have increased surface oxide thickness and surface crystallinity. 4. The morphology of cells, flattened or spherical, were different from each other. In the electropolished group and machined group, the cells were almost flattened. In two anodized groups, some cells were spherical and other cells were flattened. And the 14 day culture cells of all of the groups were nearly flattened due to confluency. 5. The number of attached cells was highest in low roughness anodized group. And the machined group had significantly lower cell count than any other groups(P<.05). 6. Total protein contents showed no difference among groups. 7. The level of alkaline phosphatase activities was higher in the anodized groups than electropolished and machined groups(P<.05).

치과용 지르코니아 이장재 처리에 따른 지르코니아와 도재의 전단결합강도 비교 (Shear bond strength of a layered zirconia and porcelain according to treatment of zirconia liner)

  • 서정일;박원욱;김양근
    • 대한치과기공학회지
    • /
    • 제39권1호
    • /
    • pp.43-52
    • /
    • 2017
  • Purpose: Physical and chemical properties of gold is most suitable to be restored of teeth to its original state. Recently zirconia was used instead of gold because of esthetical and intimacy of human body. Because of high strength and high abrasion resistance of zirconia, all zirconia artificial tooth lead to wear the original tooth of opposite site. To preserve this original tooth, zirconia artificial tooth covered with dental ceramic glass was used. When joining the zirconia core and dental ceramic glass, difference of their thermal expansion coefficient and wetting ability is generated the residual stress at interface lead to crack. In order to solve this problem, intermediate layer what is called zir-liner was imported to decrease the residual stress and increase the bonding strength. Methods: In this study, to identify the optimum conditions for manufacturing process, various methods to rough the surface of zirconia core were adopted, and vary the thickness of interlayer, and analyzed bond strength. Results: Bond strength of sanding specimens group showed higher than that of non-sanding specimens group, and once applied intermediate layer with sanding specimens showed highest bond strength with 28 MPa. SEM photomicrographs of zirconia cores fired at $1500^{\circ}C$ showed parallel straight lines in sanding and pockmarked surface in blasting surfaces as abrasion traces. Observation of the destruction section after shear test by SEM were carried out. Liner applied non-sanding group and non-liner applied sanding group all showed interfacial crack. Sandblasting group with non-liner showed remained dental ceramic glass on the surface of zirconia. Sandblasting group with once applied liner showed partially remained liner and dental ceramic glass on the surface of zirconia. XRD analysis revealed that sandblasting group showed higher monoclinic peaks than other specimens group and this result was due to the high collision energy for stress induced phase transformation. Conclusions: A study on the improvement of bonding strength between zirconia and dental ceramic glass steadily carried out for the future to practical use.

탈접착 후처치시 핸드피스(handpiece) 속도가 치아에 미치는 영향에 대한 비교 연구 (A comparison study of the effects of handpiece speed on teeth in debonding procedure)

  • 박수병;김구호;하만희
    • 대한치과교정학회지
    • /
    • 제34권1호
    • /
    • pp.83-91
    • /
    • 2004
  • 본 연구는 탈접착 후처치시 사용된 핸드피스(handpiece)속도에 따른 처치 효율성과 환자 불편감 정도를 알아보기 위하여 시행되었다. 발거된 소구치(50개)에 브라켓을 접착하고 제거한 후 tungsten carbide bur를 장착한 저속 핸드피스와 ultra-fine diamond finishing bur를 장착한 고속 핸드피스로 각각 25개씩 탈접착 후처치를 시행했으며, 이때 각 실험군내 치아의 진동정도와 치수강내 온도 변화를 측정하였다. 이후 각 실험군(저속, 고속 핸드피스군)에서 임으로 10개씩의 치아를 선택하여 주사전자현미경으로 법랑질 표면에 대한 평가를 시행하여, 다음과 같은 결론을 얻었다. 1. 저속 핸드피스를 사용한 레진 제거시 다양한 진폭의 치아 진동이 고속 핸드피스를 이용한 경우보다 많이 나타났다. 2. 고속 핸드피스를 이용한 경우의 치수강내 온도변화가 저속 핸드피스를 사용한 경우보다 유의성 있게 높았으며, 레진 제거 시간 역시 두 배정도 길게 걸렸다. 3. 레진 제거 후 법랑질 표면에 대한 주사전자현미경상은 고속 핸드피스를 사용한 경우에서 절흔들(notches)과 잔여레진들이 저속 핸드피스를 사용한 경우보다 많은 것을 보여주었다.

Double Step Fabrication of Ag Nanowires on Si Template

  • Zhang, J.;Cho, S.H.;Quan, W.X.;Zhu, Y.Z.;Mseo, J.
    • Journal of Korean Vacuum Science & Technology
    • /
    • 제6권2호
    • /
    • pp.79-83
    • /
    • 2002
  • As Ag does not form my silicide on Si surfaces, Ag wire is a candidate for self-assembled nanowire on the reconstructed and single-domain Si(5 5 12)-2 $\times$ 1. In the present study, various Ag coverages and post-annealing temperatures had been tested to fabricate a Ag nanowire with high aspect ratio. When Ag coverage was less than 0.03 ML and the post-annealing temperature was 500(C, Ag atoms preferentially adsorbed on the tetramer sites resulting in Ag wires with an inter-row spacing of ~5 nm. However, its aspect ratio is relatively small and its height is also not even. On the other hand, the Ag-posited surface completely loses its reconstruction even with the same annealing at 500 $\^{C}$ if the initial coverage exceeds 0.05 ML. But the additional subsequent annealing at 700$\^{C}$ and slow-cooling process recovers the well-ordered Ag chain with relatively high aspect ratio on the same tetramer sites. It can be understood that, in the double step annealing process, the lower temperature annealing is required for cohesion of adsorbed Ag atoms and the higher temperature annealing is for providing Ag atoms to the tetramer sites.

  • PDF

Sulphate Reducing Bacteria and Methanogenic Archaea Driving Corrosion of Steel in Deep Anoxic Ground Water

  • Rajala, P.;Raulio, M.;Carpen, L.
    • Corrosion Science and Technology
    • /
    • 제18권6호
    • /
    • pp.221-227
    • /
    • 2019
  • During the operation, maintenance and decommissioning of nuclear power plant radioactive contaminated waste is produced. This waste is stored in an underground repository 60-100 meters below the surface. The metallic portion of this waste comprises mostly carbon and stainless steel. A long-term field exposure showed high corrosion rates, general corrosion up to 29 ㎛ a-1 and localized corrosion even higher. High corrosion rate is possible if microbes produce corrosive products, or alter the local microenvironment to favor corrosion. The bacterial and archaeal composition of biofilm formed on the surface of carbon steel was studied using 16S rRNA gene targeting sequencing, followed by phylogenetic analyses of the microbial community. The functional potential of the microbial communities in biofilm was studied by functional gene targeting quantitative PCR. The corrosion rate was calculated from weight loss measurements and the deposits on the surfaces were analyzed with SEM/EDS and XRD. Our results demonstrate that microbial diversity on the surface of carbon steel and their functionality is vast. Our results suggest that in these nutrient poor conditions the role of methanogenic archaea in corrosive biofilm, in addition to sulphate reducing bacteria, could be greater than previously suspected.

다공성 금속 샤워헤드가 적용된 상압플라즈마 화학기상증착법을 이용한 저온 다결정 실리콘 증착 공정 (Low Temperature Polycrystalline Silicon Deposition by Atmospheric Pressure Plasma Enhanced CVD Using Metal Foam Showerhead)

  • 박형규;송창훈;오훈정;백승재
    • 한국전기전자재료학회논문지
    • /
    • 제33권5호
    • /
    • pp.344-349
    • /
    • 2020
  • Modern thin film deposition processes require high deposition rates, low costs, and high-quality films. Atmospheric pressure plasma-enhanced chemical vapor deposition (AP-PECVD) meets these requirements. AP-PECVD causes little damage on thin film deposition surfaces compared to conventional PECVD. Moreover, a higher deposition rate is expected due to the surface heating effect of atomic hydrogens in AP-PECVD. In this study, polycrystalline silicon thin film was deposited at a low temperature of 100℃ and then AP-PECVD experiments were performed with various plasma powers and hydrogen gas flow rates. A deposition rate of 15.2 nm/s was obtained at the VHF power of 400 W. In addition, a metal foam showerhead was employed for uniform gas supply, which provided a significant improvement in the thickness uniformity.

Top-GaP 상부에 나노 크기의 Roughness 처리에 의한 AlGaInP 고휘도 LED의 휘도 향상 (Improvement of Brightness for AlGaInP High-brightness LEDs with Nano-scale Roughness on Top-GaP Surface)

  • 소순진;하헌성;박춘배
    • 한국전기전자재료학회논문지
    • /
    • 제21권1호
    • /
    • pp.68-72
    • /
    • 2008
  • AlGaInP high-brightness LEDs(HB-LEDs) have gained importance a variety of application operating in the red, orange, yellow and yellow-green wavelength. The light generated from inside LED chips should be emitted to the air through the surfaces of the chips. However, because of the differences between the semiconductor and air or epoxy's refractive index, some of the light was blocked so that caused lowering external quantum efficiency. In this study, nano-scale roughness on the top-GaP layer of AlGaInP epitaxial wafer was fabricated to improve' the brightness of AlGaInP LEDs. Nano-scale roughness was made by ICP dry etcher. Our AlGaInP LEDs with nano-scale roughness has higher brightness (about 28.5 %) than standard AlGaInP LEDs.

항공기 브레이크 재료용 탄소/탄소 복합재료의 마찰 및 마모 거동 (Friction and Wear Behavior of Carbon/Carbon Composites for Aircraft Brake Material)

  • 우성택;윤재륜
    • Tribology and Lubricants
    • /
    • 제9권1호
    • /
    • pp.62-69
    • /
    • 1993
  • Friction and wear behavior of a carbon/carbon composite material for aircraft brake material was experimentally investigated. Friction and wear test setup was designed and built for the experiment. Friction and wear tests were conducted under various sliding conditions. Friction coefficients were measured and processed by a data acquisition system and amount of wear measured by a balance. Stainless steel disk was used as the counterface material. Temperature was also measured by inserting thermocouple 2.5 mm beneath the sliding surface of the carbon/carbon composite specimen. Wear surfaces were observed by SEM, and analyzed by EDAX. The experimental results showed that sliding speed and normal force did not have significant effects on friction coefficient and wear factor of the composite. Temperature increase just below the surface was not large enough to cause any thermal degradation or oxidation which occurred at higher temperature when tested by TGA. Wear film was generated both on the specimen and on the counterface at relatively low sliding speed but cracks, grooves, and wear debris were observed at high sliding speed. Friction coefficient remained almost constant when the sliding speed or normal load was varied. It is believed that the adhesive and abrasive components contributed mainly to the friction coefficient. Wear behavior at low sliding speed was governed by wear film formation and adhesive wear mechanism. At high speed, fiber orientation, ploughing by counterface asperities, and fiber breakage dominated wear of the carbon/carbon composite.

선박용 연료유와 윤활유의 조합에 의한 락커 형성에 관한 연구 (Study on Lacquer Formation in Combined of Marine Fuel Oil and Marine Lubricant Oil)

  • 홍성호;박종국;류영석
    • Tribology and Lubricants
    • /
    • 제31권3호
    • /
    • pp.86-94
    • /
    • 2015
  • We perform lacquer formation experiments with various combinations of marine fuel oils and lubricant oils. We also investigate the influences of base number (BN) in lubricant oil and sulfur content in fuel oil. A dissolution test with 10% dilute sulfuric acid and pull-off force test are accomplished to distinguish whether the residual layers are lacquering or not. The lacquering layers are dissolved by dilute sulfuric acid and have a strong pull-off force. Moreover, the calcium content detected in the residual layers is compared by energy dispersive x-ray spectroscopy (EDS). More calcium is detected in the lacquer layers than in other residual layers. Distillate fuels containing low sulfur levels are more prone to lacquering when mixed with lubricant oil with a high BN. On the other hand, residual fuels with a high sulfur content do not form lacquer. We investigate the effect of mixture volume ratio. The mixture with higher fuel oil content is more prone to generate lacquer. These experiments indicate that a lubricant with an appropriate BN should be used to prevent lacquer forming on the surfaces such as cylinder liners depending on the sulfur content of fuel oil.

Assessment of Non-point Pollutants and Runoff Characteristics in Urban Area, Korea

  • Park, Jae-Young;Choi, I-Song;Oh, Jong-Min
    • 생태와환경
    • /
    • 제38권spc호
    • /
    • pp.67-75
    • /
    • 2005
  • The objectives of this study were to understand the runoff characteristics of the non-point sources originating from impervious surfaces and to assess their effect on the aquatic environment in the urban areas. The concentration of pollutants (SS, BOD, COD and T-P) except for T-N showed the highest value in runoff from road, and event mean concentration (EMC) also showed high value from road. The pollutants discharged from road showed a higher concentration in the beginning stage (0 ${\sim}$ 30%) of progressive percentage of rainfall. The contribution percentages of non-point sources by load were 44.9% for SS, 11.2% for BOD, 21.4% for COD, 11.4% for T-N and 8.1% for T-P in the total load of pollutant discharged through sewer. From our results, the road was a significant potential source that deteriorated water quality of the streams and lakes in the vicinity of the urban area during the rain period. Therefore, counter plan is required to reduce pollutant concentration on the road from non-point sources in the urban area. Also, since pollutant concentration in the beginning stage of rainfall was quite high, road cleaning seems to be one of the very useful methods to prevent inflowing of pollutants to the aquatic environment.