  • The paper proposes a technique for reconstructing the true hardening curve of isotropic materials from ring tensile tests. Neutron irradiated 42XNM alloy tensile properties were investigated. The calculation of the true hardening curve for tensile and compression tests of standard cylindrical samples was performed at the first step. After that, the FEM-model was developed and validated using the ring tension and compression tests (with the hardening curve defined in step 1). Finally, the true hardening curve was calculated by selecting the FEM-model parameters and its validation by ring sample tests in different states using an iterative method. For these samples, experimental and calculated gauge length values were obtained, and the corresponding material's constants were estimated.

공용중인 교량의 응력이력 계측 및 응력범주를 고려한 피로평가 (Fatigue Evaluation of a Steel Bridge in Service through Stress History Measurement and Consideration of Stress Category)

  • 나성옥;권민호;차철준;김인호
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제18권2호
    • /
    • pp.108-116
    • /
    • 2014
  • 강교의 정확한 피로균열의 발생원인 또는 교량의 피로안전성을 검토하기 위해서는 적합한 응력이력 측정이 요구된다. 그러나 실제 현장에서의 응력이력 측정은 현장 여건과 경제성, 작업성 등의 이유로 1개소의 스트레인게이지를 설치하여 계측을 실시한다. 이는 특정 구조물의 실제 치수와 게이지 길이 용접부 응력집중 등의 영향을 고려하지 못하고, 구조 모델링을 통한 응력해석에도 많은 어려움이 있다. 그러므로 본 연구에서는 용접단부에 다수의 게이지 설치, 최소 길이 게이지 사용, 설치 위치 등의 개선된 방법을 적용하여 용접단부와 스트레인게이지 설치 거리에 따른 변형률 진폭에 대한 상관식을 도출하고 국제용접협회 (IIW)의 제안식과 비교하였다. 또한 적합한 피로등급 상세범주 선정을 통해 공용중인 교량의 피로손상도 평가 및 잔존수명을 예측하고 분석하였다. 그 결과 피로균열 발생빈도가 높은 부재파악, 용접 단부와 게이지 설치 거리에 따른 변형률의 정량적 파악으로 정확한 피로손상도 평가 및 잔존수명 예측이 가능하므로 향후 교량의 응력이력 계측 시 개선된 방법을 적용해야 할 것이다.

서울지점 강우자료에 나타난 도시화의 간섭 분석 (Intervention Analysis of Urbanization Effect on Rainfall Data at the Seoul Rain Gauge Station)

  • 유철상;김대하;박상형;김병수;박창열
    • 한국수자원학회논문집
    • /
    • 제40권8호
    • /
    • pp.629-641
    • /
    • 2007
  • 본 연구에서는 우리나라 최대 도시인 서울지점에서의 도시화의 영향을 강우자료의 분석을 통해 파악하였다. 서울지점 강우의 도시화 영향을 파악하기 위해 관측길이가 길고 도시화의 정도가 상대적으로 덜한 전주지점과 관측 기록의 길이는 짧으나 서울 인근지점으로 도시화의 영향이 매우 적을 것으로 판단되는 이천지점의 강우자료를 비교 대상으로 이용하였다. 또한 도시화의 영향에 해당하는 서울지점과 전주지점의 강우량 차이를 간섭모형을 이용하여 정량화 하였다. 그 결과, 연최대치 호우사상의 최대강우강도는 점점 증가하는 추세이며, 총지속시간의 경우는 전체기간에 대해 감소하는 경향이고, 특히 1960년 이후에는 그 평균이 과거보다 현저히 감소하는 추세임을 확인할 수 있었다. 아울러 간섭분석을 통해 1960년 이후의 도시화가 강우에 미친 영향을 정량화한 결과 도시화에 의한 강우강도 및 강우량의 증가 양상이 지속되고 있음을 확인하였다.

CF8M 스테인리스 강 저주기 환경피로 실험의 주기적 변형률 경화 특성 (Characteristics of the Cyclic Hardening in Low Cycle Environmental Fatigue Test of CF8M Stainless Steel)

  • 정일석;하각현;김태룡;전현익;김영신
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회A
    • /
    • pp.17-22
    • /
    • 2007
  • Low-cycle environmental fatigue tests of cast austenitic stainless steel CF8M at the condition of fatigue strain rate 0.04%/sec were conducted at the pressure and temperature, 15MPa, $315^{\circ}C$ of a operating pressurized water reactor. The used test rig was limited to install an extensometer at the gauge length of the cylindrical fatigue specimen inside the small autoclave. So the magnet type LVDT's were used to measure the fatigue displacement at the specimen shoulders inside the high temperature and high pressure water autoclave. However, the displacement and strain measured at the specimen shoulders is different from the one at the gauge length for the geometry and the cyclic strain hardening effect. FEM calculated the displacement and the strain of the gauge length from the data measured at the shoulders. Tensile test properties in elastic and plastic behavior of CF8M material were used in the FEM analysis. A series of low cycle fatigue tests simulating the cyclic strain hardening effect verified that the FEM calculation was well agreed with the simulated tests. The process and method developed in this study would be so useful to produce reliable environmental fatigue curves of CF8M stainless steel in pressurized water reactors.

  • PDF

CF8M 스테인리스 강 저주기 환경피로 실험의 주기적 변형률 경화 특성 (Characteristics of the Cyclic Hardening in Low Cycle Environmental Fatigue Test of CF8M Stainless Steel)

  • 정일석;하각현;김태룡;전현익
    • 대한기계학회논문집A
    • /
    • 제32권2호
    • /
    • pp.177-185
    • /
    • 2008
  • Low-cycle environmental fatigue tests of cast austenitic stainless steel CF8M at the condition of fatigue strain rate 0.04%/sec were conducted at the pressure and temperature, 15MPa, $315^{\circ}C$ of a operating pressurized water reactor (PWR). The used test rig was limited to install an extensometer at the gauge length of the cylindrical fatigue specimen inside a small autoclave. So the magnet type LVDT#s were used to measure the fatigue displacement at the specimen shoulders inside the high temperature and high pressure water autoclave. However, the displacement and strain measured at the specimen shoulders is different from the one at the gauge length for the geometry and the cyclic strain hardening effect. Displacement of the fatigue specimen gauge length calculated by FEM (finite element method) used to modify the measured displacement and fatigue life at the shoulders. A series of low cycle fatigue life tests in air and PWR conditions simulating the cyclic strain hardening effect verified that the FEM modified fatigue life was well agreed with the simulating test results. The process and method developed in this study for the environmental fatigue test inside the small sized autoclave would be so useful to produce reliable environmental fatigue curves of CF8M stainless steel in pressurized water reactors.

개교환자의 발성에 관한 언어 음성학적 연구 (A SPEECH-PHONETIC STUDY ON THE PRONUNCIATION OF THE OPENBITE PATIENTS)

  • 김기달;양원식
    • 대한치과교정학회지
    • /
    • 제21권2호
    • /
    • pp.287-307
    • /
    • 1991
  • This study aimed at examining speech defects of openbite patients, which were analized in terms of formant frequency for vowels and word pronunciation length for consonants. In addition, the upper and lower lip (perioral m.) activity was tested by the EMG. The tongue force was measured by the strain gauge, and the speech discrimination test was carried out. One experimental group and one control group were used for this study and they were respectively composed of six female openbite patients and six normal-occlusion females. Eight monophthongs, two fricatives and two affricatives were chosen for speech analysis. Speeches of the above-mentioned groups were recorded and then analized by the ILS/PC-1 software. Four hundred most frequently used monosyllables were also chosen for discrimination score. Openbite patients showed the following characteristics: 1. Abnormality in case of /a/, $/\varepsilon/$, /e/, /i/ $F_2$ and /e/, /a/ $F_1$. 2. Significantly elongated length in their pronunciation of /h/ and $/C^h/$ and somewhat elongated length also in their pronunciation of /s/ and /c/. 3. Significant upper lip activity according to the EMG test during pronunciation of the bilabial consonants. 4. Relatively weak tongue force according to the strain gauge measurement. 5. According to the speech discrimination test, high rate of misarticulation in case of (a) initial /p/ /s'/ and /ts'/, (b) /a/,$/\varepsilon/$,/e/,/je/,/o/, $/\phi/$,/jo/,/u/,/we/, and /i/ (c) final (equation omitted).

  • PDF

디지탈 화상처리를 이용한 사출제품의 길이측정용 시각검사시스템 개발에 관한 연구

  • 김재열;박환규;오보석
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 춘계학술대회 논문집
    • /
    • pp.281-285
    • /
    • 1996
  • In this paper, I made visual inspection system using Vision Board and it is consist of an illuminator (a fluorescent lamp), image input device(CCD(Charge)Coupled Device) camera), image processing system(Vision Board(FARAMVB-02), image output device(videomonitor, printer), a measuring instrument(TELMN1000). Length measurement by visual inspection system is used 100mm gauge block instead of calculating distance between camera and object, it measured horizontal and vertical length factor from 400mm to 650mm by increasing 50mm. In this place, measured horizontal and vertical length factor made use of length measurement of a injection. A measuring instrument used to compare a measured length of a injection visual inspection system with it. In conclusion, length measurement of a injection compared a measuring instrument withvisual inspecion system using length factor of 100mm guage block. Maximum error of length compared two devices a measuring instrument with visual inspection system is 0.55mm. And operation program is made up Borland C++ 3.1. By changing, it is applied to various uses.

  • PDF

레이저간섭계와 미터표준 (Laser Interferometer and Length Standards)

  • 엄태봉;서호성
    • 한국정밀공학회지
    • /
    • 제17권6호
    • /
    • pp.17-24
    • /
    • 2000
  • 1960년 Jawan 등이 1.15㎛ 파장을 포함한 6개의 발진파장을 갖는 He-Ne 레이저의 연속 발진을 성공시킨 이후 레이저는 단색성이나 빛의 진직성을 이용하는 계측에서 특히 정밀길이측정에서 매우 중요하게 사용되고 있다. He-Ne 레이저의 발진선폭은 80㎑로써 길이표준기로 사용되었던 Kr-86 스펙트럼선의 선폭(400㎒)의 5,000 분의 1에 해당되는 매우 좁은 선폭을 갖고 있다.(중략)

  • PDF