  • Two types of advanced cold-work tool steels were characterized and compared. A higher-alloyed ledeburitic steel with primary carbides (denoted as 9Cr) and a lower-alloyed steel without primary carbides (5Cr) were fabricated by vacuum induction melting and subsequent hot forging. They were spheroidizing-annealed at $870^{\circ}C$, quenched at $1030^{\circ}C$ and tempered at 180 or $520^{\circ}C$. Their machinability after annealing and hardness, impact toughness, wear resistance after tempering were compared and interpreted in association with their characteristic microstructures. After annealing, 5Cr showed higher resistance to machining due to higher ductility and toughness in spite of lower strength and smaller carbide volume. Owing to smaller carbide volume fraction and the absence of coarse primary carbides, 5Cr showed even better impact toughness although the hardness was lower. The improved toughness of 5Cr resulted in excellent wear resistance, while smaller volume fraction of retained austenite also contributed to it.

Finite element analysis of unconstrained axisymmetric piercing (구속이 없는 축대칭 피어싱 공정의 유한요소해석)

  • 양동열;유요한;이종수
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.6
    • /
    • pp.876-888
    • /
    • 1986
  • The Study is concerned with the analysis of unconstrained axisymmetric piercing as a nonsteady forging process by the rigid-plastic finite element method. In the numerical analysis of axisymmetric piercing, the initial velocity field is generated by assuming the material as a linear viscous material to begin with in order to facilitate the input handling and to ensure better convergencey. The strain-hardening effect for nonsteady deformation and the friction of the die-material interial interface are considered in the formulation. Rigid body treatment is also incorporated in the developed program. The experiments are carried out for aluminum alloy specimens (A1204) with different specimen heights. It is shown that the experimental results are in excellent agreement with the finite element simulations is deformed configuration. For load prediction the theoretical prediction shows excellent agreement with th eexperimental laod in the initial stage of loading before fracture of the specimen is not initiated. Distribution of stresses, strains and strain rates has been found for the given cases in computation. On this basis several fracture criteria are introduced in order to check the fracture initiation. It is found that maximum shear criterion is capable of good fracture prediciton.

Effect of Boron on the Manufacturing Properties of Ti-2Al-9.2Mo-2Fe Alloy (Ti-2Al-9.2Mo-2Fe 합금의 후공정 특성에 미치는 보론의 영향)

  • Kim, Tae-Yong;Lim, Ka-Ram;Lee, Yong-Tai;Cho, Kyung-Mok;Lee, Dong-Geun
    • Korean Journal of Materials Research
    • /
    • v.25 no.11
    • /
    • pp.636-641
    • /
    • 2015
  • Titanium has many special characteristics such as specific high strength, low elastic modulus, excellent corrosion and oxidation resistance, etc. Beta titanium alloys, because of their good formability and strength, are used for jet engines, and as turbine blades in the automobile and aerospace industries. Low cost beta titanium alloys were developed to take economic advantage of the use of low-cost beta stabilizers such as Mo, Fe, and Cr. Generally, adding a trace of boron leads to grain refinement in casted titanium alloys due to the pinning effect of the TiB phases. This study analyzed and evaluated the microstructural and mechanical properties after plastic deformation and heat treatment in boron-modified Ti-2Al-9.2Mo-2Fe alloy. The results indicate that a trace of boron addition made grains finer; this refinement effect was found to be maintained after subsequent processes such as hot forging and solution treatment. This can effectively reduce the number of required manufacturing process steps and lead to savings in the overall cost as well as low-cost beta elements.

Estimaion of the sintering and forging characteristics of the W/Cu nanocomposite powders produced by the spray conversion process (Spray conversion 법으로 제조된 W/Cu 나노복합분말의 소결특성 및 단조특성 평가)

  • 김태형;노준웅;김은표
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2002.11a
    • /
    • pp.36-36
    • /
    • 2002
  • 최근 한국기계연구원에서 개발된 Mechanochemical process (MCP)는 Spray conversion 법에 의하여 나노크기의 W/Cu 복합 분말을 제조하는 방법으로서, 현재 (주)나노테크에서 산업화를 위한 시험/개발이 진행 중이다. 이 방법에 의하여 W /1 0 ~ 40wt. %Cu 조성의 초미렵 W/Cu 복합 분말의 양산화가 가능하게 됨으로써, 나노복합분말을 사용한 초미립 W/Cu 합금의 소결 제조 연구 역시 나 노태크에서 분말사업화와 동시에 수행되고 있다. 현재 Spray conversion 법으로 제조되고 있는 W/Cu 나노복합분말 및 그 소결체는 Cu의 조성범 위에 따라 민수용 및 군수용 제품으로의 적용이 시도되고 있으며, 각기 특성향상을 목표로 각 적용 분야에서 요구되는 제반 성능에 대한 검토가 이루어지고 있다. 특히 군수용의 목적으로 사용될 경우, 정적 및 동적부하상태에서 재료의 균일한 변형이 가장 중요한 특성이다. 현 개발품의 경우, 일반 W 빛 Cu 원료에 비하여 상대적으로 높은 순도의 원료를 사용하였기 때문에 분말 및 소재상태 에서의 순도가 높아서, 연성을 저하시키는 것으로 알려진 기지상내 합금원소 또는 interface 게재물 이 존재할 가능성이 매우 낮다. 또한 초미립 W 입자들과 Cu 상의 혼합도가 극대화된 상태이기 때문에 상대적으로 저옹에서도 완전치밀화된 미세조직을 얻을 수 있는데, 이는 분말상태의 균일한 미세구조를 유지할 수 있으며, 동시에 W 업자간의 과도한 neck 형성을 방지함으로써 기계적 변형시 재료의 연성 향상이 기대된다. 이러한 W/Cu 나노복합분말 소결체의 특성은 균일한 밀도분포와 동시에 과도한 동적 부하상태에서 균일한 변형이 보장되어야만 하는 특정 군수용 목적에 잘 부합하는 것으로 판단된다. 본 고에서는 상기한 W/Cu 나노복함분말을 사용하여 균일한 미세구조를 가지는 완전치밀화된 소결재를 제조하는 과정과 제조된 소결재를 향후 군수용 제품에 척용시키기 위하여 진행된 단조특성에 대한 연구결과틀을 재료의 미세구조척 관점에서 논의하였다.

  • PDF

High-Temperature Oxidation Behavior of Fe-22%Cr-5.8%Al Alloy (Fe-22%Cr-5.8%Al 합금의 고온 산화 거동)

  • Kim, Song-Yi;Choi, Sung-Hwan;Yun, Jung-Yeul;Kong, Young-Min;Kim, Byoung-Kee;Lee, Kee-Ahn
    • Journal of the Korean institute of surface engineering
    • /
    • v.44 no.1
    • /
    • pp.13-20
    • /
    • 2011
  • This study investigated the high temperature oxidation behavior of Fe-22%Cr-5.8%Al alloy and the oxidation kinetics of the alloy were discussed. Bulk samples were prepared by VAM (vacuum arc melting) and hot forging. High temperature oxidation testes were isothermally conducted up to 100 hours in 79%$N_2$+21%$O_2$ environment at three different temperatures ($900^{\circ}C$, $1000^{\circ}C$, $1100^{\circ}C$). The weight gain was measured after oxidation according to oxidation time (2, 4, 6, 8, 10, 15, 20, 25, 30, 60, 80, 100 hours). The weight gain significantly increased with increasing oxidation temperature. As the temperature increased, the oxidized samples showed sequential formation of $Al_2O_3$, Cr-rich oxide, Fe-rich oxide. The activation energy of high temperature oxidation was obtained as 306.63 KJ/mol. $Al_2O_3$ were developed on the surface in the early stage of oxidation, representing protective role of oxidation. However, Fe-based and Cr-based oxides leaded to breakaway of oxide layer, thus resulted in the significant increase of additional oxidation.

Effects of Annealing on the Texture Development and Abnormal Grain Growth in a Commercial AZ31B Mg Alloy Sheet (상용 AZ31B Mg합금 판재의 어닐링에 따른 집합조직 변화 및 결정립 이상 성장)

  • Yang, G.S.;Yoon, S.S.;Jang, W.Y.;Kang, J.W.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.21 no.6
    • /
    • pp.293-299
    • /
    • 2008
  • In order to provide with fundamental data of the wrought Mg alloy for press forging, the effect of annealing temperature on the microstructure, texture development and tensile properties is studied in a commercial AZ31B Mg alloy sheet. Basal texture i.e. $(0001){\pm}5^{\circ}$[21$\bar{3}$0] is developed in a commercial AZ31B Mg sheet, and the texture is not changed considerably by annealing over $400^{\circ}C{\times}30min$, while (10$\bar{3}$0) component with high intensity can be observed due to abnormal grain growth. When the sheet is tensile-deformed with RD, $45^{\circ}$ and TD directions at room temperature, fracture strains are given by 25.8, 21.4 and 11.9% in the order of RD, $45^{\circ}$ and TD directions, respectively. With increasing annealing temperature up to $450^{\circ}C{\times}30min$, little change in mean grain size can be revealed by annealing below $300^{\circ}C{\times}30min$ but an abnormal grain growth, where some grains become significantly coarser than the rest, occurs by annealing above $400^{\circ}C{\times}30min$. The maximum tensile strain of around 25% is obtained by annealing below $300^{\circ}C{\times}30min$, but it is abruptly decreased to 16% by annealing above $400^{\circ}C{\times}30min$ owing to intergranular fracture of abnormal grown grains.

Manufacturing Technique of Gilt-Bronze Objects Excavated from Tomb No.1(Donghachong) in Neungsan-ri, Buyeo

  • Shin, Yong-bi;Lee, Min-hee;Kim, Gyu-ho
    • Korean Journal of Materials Research
    • /
    • v.30 no.9
    • /
    • pp.453-457
    • /
    • 2020
  • Tomb No. 1 (Donghachong) of the Buyeo Neungsan-ri Tomb complex (listed as UNESCO World Heritage Site), is a royal tomb of the Baekje Sabi Period. One wooden coffin unearthed there is an important relic of the funerary culture of the Baekje. This study examines the production techniques of gilt-bronze objects attached to the wooden coffin excavated from Donghachong. The base metal of the gilt-bronze object is pure copper, with single α phase crystals in a heterogeneous form containing annealing twins; Au and Hg are detected in the gilt layer. We suggest that the surface of the forging copperplate is gilded using a mercury amalgam technique; it is thought that the annealing twins of the base material formed during the heat treatment process for the sheet metal. The gilt layer is three to five times thicker for the gilt-bronze objects found near the foot of the coffin than those near the head. We estimate the plating process is carried out at least three times because three layers are identified on the plate near the head. Therefore, it is likely that the materials and methods used to construct the gilt-bronze objects found in different parts of the coffin are the same, but the number of platings is different. This research confirms the metal crafting techniques used in Baekje by the examination of production techniques of these gilt-bronze objects. Further, our paper presents an important example of restoration and reconstruction for a museum exhibition, through effective use of scientific analysis and investigation.

Piezoelectric and Dielectric Characteristics of (Na,K)$NbO_3$ Ceramics System According to Variations of Sintering Time (소결시간변화에 따른 (Na,K)$NbO_3$계 세라믹스의 유전 및 압전특성)

  • Kim, Do-Hyung;Yoo, Ju-Hyun;Jeong, Young-Ho;Hong, Jae-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.48-48
    • /
    • 2008
  • 현재 압전재료로써 사용되고 있는 PZT계 세라믹스는 우수한 압전 및 유전특성으로 초음파 센서, 압전변압기, 액츄에이터, 필터, 레조네이터와 같은 여러 응용분야에 널리 사용되어지고 있다. 그러나 납을 60%이상 포함하므로 환경오염에 의하여 그 사용에 대한 규제가 강화되고 있어 최근에는 납을 함유하지 않은 무연 환경친화형 압전세라믹스가 주목받고 있다. 현재 무연 조성 세라믹스에는 텅스텐-브론즈 형, 비스머스 레이어형, 페로브스카이트 형 등이 이으며, 그 중 페로보스카이트 혈을 제외하고는 보통 소성법 조제시 낮은 압전특성을 갖는다. 그러므로 압전특성을 증가시키기 위하여 Hot pressing, Hot forging, RTGG(Reactive Template Grain Growth), SPS(Spark Plasma Sintering), 그러나 이는 무연 세라믹스의 대량생산 과정에서 어려운 문제를 가지고 있고, 저가격 관점에서 볼 때 보통소성법이 보다 바람직하다. 그래서 보통소성법으로 NKN세라믹스의 소결성을 향상 시키고 비교적 높은 압전특성을 얻기 위해서 $LiSbO_3$, $LiNbO_3$, $LiTaO_3$, alkaline-earth(Mg, Ca, Sr, Ba) 등을 첨가한 논문들이 보고되고 있으며, 이러한 재료들의 kp는 대략 0.3-0.4를 나타내고 있다. 따라서, 본 연구에서는 소결온도를 낮추고자 $Ag_2O$를 소결조제로 사용하였고 유전 및 압전특성을 높이고자 소결시간 변화시켜 시편을 제작하여 NKN 세라믹스의 유전 및 압전특성을 조사하였다.

  • PDF

Dielectric and piezoelectric properties of (1-x)$(Na_{0.5}K_{0.5})NbO_3$ - $x(Ba_{(1-y)}Sr_y)TiO_3$ ceramics ((1-x)$(Na_{0.5}K_{0.5})NbO_3$ - $x(Ba_{(1-y)}Sr_y)TiO_3$의 유전 및 압전 특성)

  • Kim, Mi-Ro;Song, Hyun-Cheol;Choi, Ji-Won;Cho, Young-Soo;Kim, Hyun-Jai;Yoon, Seok-Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.59-59
    • /
    • 2008
  • Pb(Zr,Ti)$O_3$(PZT)는 현재 가장 우수한 압전특성을 가진 압전 재료로써, 압전효과와 역압전효과를 이용한 압전 액추에이터, 압전 트랜스듀서, 센서, 레조네이터 등의 활동에 대한 연구과 활발하게 이루어 지고 있다. 그러나 압전성이 우수한 PZT 세라믹스들은 Pb 성분이 포함되어 있기 때문에 환경오염뿐 아니라, 경제적인 측면에서도 많은 문제점을 가지고 있어 최근에는 유해원소인 Pb를 포함하지 않는 친환경 압전 세라믹스에 관한 연구가 활발히 진행되고 있다. (Na, K)$NbO_3$은 뛰어난 특성을 가지고 있어 Pb를 기본조성으로 하는 압전세라믹스를 대체할 수 있는 대표적인 물질중의 하나로 알려져 있다. 그러나, potassium의 수분과의 반응성과, 소결시 휘발로 인해 높은 소결밀도의 NKN을 제조하기 어렵다. 이러한 단점을 보안하기 위해 Hot pressing, Hot forging, SPS 등 여러가지 방법을 이용하여 연구가 수행되고 있지만, 고가의 제조공정을 이용해야만 한다. 본 연구에서는 $BaSrTiO_3$의 새로운 고용체를 추가시켜 기본 NKN 조성보다 소결밀도, 유전 및 압전특성을 향상시키고자 하였다.

  • PDF

A Study on Applet Control on the Internet Communication using Java Bytecode (자바 바이트 코드를 이용한 인터넷 통신의 애플릿 제어)

  • 김문환;나상동
    • The Journal of Korean Institute of Communications and Information Sciences
    • /
    • v.28 no.5C
    • /
    • pp.523-531
    • /
    • 2003
  • Java applets are downloaded from web server through internet and executed in Java Virtual Machine of clients'browser. Before execution of java applets, JVM checks bytecode program with bytecode verifier and performs runtime tests with interpreter. However, these tests will not protect against undesirable runtime behavior of java applets, such as denial of service attack, email forging attack, URL spoofing attack, or annoying sound attack. In order to protect malicious applets, a technique used in this paper is java bytecode modification. This technique is used to restrict applet behavior or insert code appropriate to profiling or other monitoring efforts. Java byte modification is divided into two general forms, class-level modification involving subclassing non-final classes and method-level modification used when control over objects from final classes or interface. This paper showed that malicious applets are controlled by java bytecode modification using proxy server. This implementation does not require any changes in the web sever, JVM or web browser.