• Title/Summary/Keyword: Fire ignition

Search Result 521, Processing Time 0.031 seconds

A Study on Fire Performance Evaluation of EIFS on Anti-Flaming Finish by Cone Calorimeter Test (콘칼로리미터에 의한 외단열시스템의 방염 화재성능평가를 위한 연구)

  • Min, Se-Hong;Sun, Ju-Seok;Kim, Sang-Chul;Choi, Yong-Mook;Lee, Seok-Ki
    • Fire Science and Engineering
    • /
    • v.26 no.3
    • /
    • pp.106-111
    • /
    • 2012
  • In this study, EIFS (Exterior insulation finish system) of exterior cladding was applied Cone calorimeter test to confirm the effect of flame retardant. As a results, the initial ignition points in accordance with the coated form and concentration of the flame retardant was delayed. But flame resistant treatment of EIFS cladding to control the fire will not affect confirmed that. In addition, EIFS that uses high-density and low-density due to difference in the density of the impact of the fire was no difference. The exterior of the ignition experiment occurred before and after 40 seconds, heat release rate to 100 seconds appears to occur about 90 % compared with the other exterior wall materials, the initial fire spread very fast was confirmed. EIFS cladding in order to prevent the spread of fire in the application of EIFS legally use is limited by the use of the building. And flame spread can be prevented, such as a vertical outer wall compartment measures are urgently needed.

A Study on the Combustion Characteristics of the Crown of Pine Trees in the Drying Season (건조기 소나무 수관부 부위별 연소특성에 관한 연구)

  • Hyuk Kwon;Jong Ho Lee
    • Journal of the Korean Society of Safety
    • /
    • v.38 no.4
    • /
    • pp.39-46
    • /
    • 2023
  • Pine trees, which account for 23% of the forested area of the Republic of Korea, are highly vulnerable to fire in comparison to broad-leaved trees due to the presence of consistent water tube sections throughout the year and resin that is composed of approximately 20% oil. In addition, the pattern of forest fires is determined by weather, topographic conditions, and fluctuation in moisture content. Therefore, when fire breaks out in pine tree forests during the dry season (January to March), it is difficult to extinguish, and it quickly spreads. In this study, the combustion characteristics of pine needles, pine cones, and pine branches in the water tube sections of living pine trees were compared and analyzed in accordance with the moisture content as per the ISO 5660-1. The monthly moisture content was analyzed from January to March, and it was found to be the lowest in March, with 53.6% for pine needles, 51.9% for pine branches, and 10.9% for pine cones. In particular, pine cones were more vulnerable to fire as compared to pine needles and pine branches because their moisture content was more than five times lower than that of pine needles and branches. The ignition time, which affects the speed of flame propagation, was the most rapid in March, and the fastest ignition time was for pine cones, at 19 seconds, followed by 34 seconds for pine needles, and 256 seconds for pine branches. The pine branches were the last to be ignited due to the effect of density, according to the thickness and specific gravity of the specimen. The peak heat release rate, which is a measurable index of fire intensity, was analyzed for pine cones and found to be 184.28 kW/m2 , while the mean effective heat of combustion was 19.79 MJ/kg, and the total heat release rate was 39.7 MJ/m2 , and these values were higher than those of pine branches and pine needles. Thus, we determined that the flame propagation speed and fire intensity according to the moisture content can be used to evaluate the risk of fire to the water tube section of pine trees. It is suggested that because of the combustion characteristics of the pine cone in March, that is when the forest is most vulnerable to fires.

Fire Performance of the Wood Treated with Inorganic Fire Retardants

  • Son, Dong-Won;Kang, Mee-Ran;Kim, Jong-In;Park, Sang-Bum
    • Journal of the Korean Wood Science and Technology
    • /
    • v.40 no.5
    • /
    • pp.335-342
    • /
    • 2012
  • To prepare the eco-friendly fire retardant wood, Japanese red pine (Pinus densiflora), Hemlock (Tsuga heterophylla), and Radiata pine (Pinus radiata) were treated with inorganic chemicals, such as sodium silicate, boric acid, ammonium phosphate, and ammonium borate. Different combination and concentration of those chemicals were impregnated by vacuum/pressure treatment methods. The electron-beam treatment was used to increase the chemical penetration into the wood. The fire performance of the fire retardant treated wood was investigated. The penetration of chemicals into the wood was enhanced after electron beam treatment. Ignition time of the treated wood was the most effectively retarded by sodium silicate, ammonium phosphate, and ammonium borate. The most effective chemical combination was found at 50% sodium silicate and 3% ammonium borate, which satisfied flammability criteria for a fire retardant material in the KS F ISO 5660-1 standards.

A study of the Influence of Forest Fire on Polymer Insulator for UHV (초고압용 폴리머 애자의 산불영향 연구)

  • Choi, In-Hyuk;Choi, Jang-Hyun;Jung, Yoon-Hwan;Lee, Dong-Il
    • Proceedings of the Korean Institute of IIIuminating and Electrical Installation Engineers Conference
    • /
    • 2005.05a
    • /
    • pp.254-259
    • /
    • 2005
  • Big fire such as mountain fire my cause the prevention of the functions of the overhead cables and insulators, which may affect the operation of the transmission lines. Therefore, in order to understand the effect of the mountain fire on the polymeric insulator for transmission lines, the author observed the deformation of the sheds of the polymeric insulators and the change of the discs of the porcelain insulators under fire, and investigated the electrical and mechanical characteristics of the insulators after the ignition test. As the result the following conclusions were obtained. First, the porcelain insulator was degraded in electrical characteristics when the insulator was subjected to the fire for approximately 5 minutes; whereas, the polymeric insulator was not degraded though there were some damage on its sheds. Second, after 20 minute exposure to the fire, the polymeric insulator lost a lot of parts of sheds, but the electrical characteristics was lowered by around 20%, but the porcelain insulators were electrically degraded by more than 80%.

  • PDF

ANALYSIS OF STEADY FIRE-DRIVEN FLUID FLOW FOR RAILWAY TUNNEL BY DIFFERENT VELOCITY CONDITIONS AT THE END OF TUNNEL (종단부 유속조건 변화에 따른 철도터널 내 정상상태 화재유동해석)

  • Lee, D.C.;Lee, D.H.;Jung, W.S.;Park, S.H.
    • 한국전산유체공학회:학술대회논문집
    • /
    • 2010.05a
    • /
    • pp.208-213
    • /
    • 2010
  • In this study CFD(Computational Fluid Dynamics) analysis of the steady fire-driven fuid flow for the performance test of ventilation at railway tunnel between Heuksok and Nodeul Station from Seoul Metro 9 is performed. There were fans with exhaust and intake modes and each was installed at the middle and both ends of the tunnel. For this test, the pool fire source of methyl alcohol with 1.5MW and smoke generators were installed between the middle of tunnel and Heuksok Station. In this test, the smoke behavior from natural convection was observed for 10 minutes from the ignition of pool fire and then fans with intake-modes at both sides of Heuksok effect of fan-on with intake mode located in the opposite side of the tunnel nearby Heuksok Station on fire-driven fluid flow is studied on when the boundary conditions of fan-on at the tunnel between Heuksok and Nodeul Station are the same as test. FLUENT, a commercial CFD code, is used for this analysis.

  • PDF

Study on the Application of Cone Calorimeter for Building of Data-Bases for Fire Safety (화재안전 데이터베이스 구축을 위한 콘칼로리미터의 활용성 연구)

  • Hong, Hwa-Young;Lee, Jong-Sung;Park, Su-Jin;Kwon, In-Kyu
    • Proceedings of the Korea Institute of Fire Science and Engineering Conference
    • /
    • 2011.04a
    • /
    • pp.325-329
    • /
    • 2011
  • Fire has developed from the inter-action of heat at the early state and it is very difficult to estimate the magnitude of the fire. Cone Calorimeter can obtain the important material properties from the exposed part of it. It can be contained that ignition, loss of mass, heat release rate, smoke generation, and gas analysis. The purpose of this study is emphasize on the properties of structural steels in terms of physical, mechanical and that will be important way to build the databases of fire safety.

  • PDF

Upward Flame Spread for Fire Risk Classification of High-Rise Buildings

  • McLaggan, Martyn S.;Gupta, Vinny;Hidalgo, Juan P.;Torero, Jose L.
    • International Journal of High-Rise Buildings
    • /
    • v.10 no.4
    • /
    • pp.299-310
    • /
    • 2021
  • External fire spread has the potential to breach vertical compartmentation and violate the fire safety strategy of a building. The traditional design solution to this has been the use of non-combustible materials and spandrel panels but recent audits show that combustible materials are widespread and included in highly complex systems. Furthermore, most jurisdictions no longer require detailing of spandrel panels under many different circumstances. These buildings require rapid investigation using rational scientific methods to be able to adequately classify the fire risk. In this work, we use an extensive experimental campaign of material-scale data to explore the critical parameters driving upward flame spread. Two criteria are outlined using two different approaches. The first evaluates the time to ignition and the time to burnout to assess the ability for a fire to spread, and can be easily determined using traditional means. The second evaluates the preheated flame length as the critical parameter driving flame spread. A wide range of cladding materials are ranked according to these criteria to show their potential propensity to flame spread. From this, designers can use conservative approaches to perform fire risk assessments for buildings with combustible materials or can be used to aid decision-making. Precise estimates of flame spread rates within complex façade systems are not achievable with the current level of knowledge and will require a substantial amount of work to make progress.

A Study on the Improvement of Life Safety Code for Logistics Warehouse Facilities (물류창고 시설의 인명안전기준 개선 방안에 관한 연구)

  • Kim, Yun-Seong;Jin, Seung-Hyeon;Lee, Byeong-Heun;Kwon, Yeong-Jin
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.98-99
    • /
    • 2021
  • The number of fires in the Korean distribution warehouse increased by about 350 from 1,070 in 2014 to 1,416 in 2020. In addition, the fire load increases with the scale of the distribution warehouse, and even if the automatic sprinkler operates, there is a limit to the direct intrusion of the water source into the ignition source, and the detector is often installed on a high ceiling. The sensing time is often delayed. In order to improve the fire safety of such distribution warehouses, the US NFPA stipulates in detail the contents related to the facility, such as sprinkler water discharge standards, rack-type warehouse installation height restrictions, and regulations on collection and equipment. However, in Japan, the goods loaded inside the distribution warehouse are not classified in detail, and it is considered that the fire safety for the distribution warehouse is low due to the relaxation regulations of the fire prevention section. Therefore, in this study, common problems are classified into material, spatial, and safety management characteristics through the cases of distribution warehouse fires that occurred in Korea and abroad, and the problems related to distribution warehouses in Korea and abroad are compared and analyzed. And present basic materials for improving the life safety standards of future distribution warehouse facilities.

  • PDF

Measurement and Prediction of Autoignition Temperature of n-Butanol and sec-Butanol System (노말부탄올과 2차부탄올 계의 최소자연발화온도의 측정 및 예측)

  • Ha, Dong-Myeong
    • Fire Science and Engineering
    • /
    • v.26 no.5
    • /
    • pp.48-53
    • /
    • 2012
  • The autoignition temperature (AIT) is important index for the safe handling of flammable liquids which constitute the solvent mixtures. This study measured the AITs and ignition delay time for n-Butanol+sec-Butanol system by using ASTM E659 apparatus. The AITs of n-Butanol and sec-Butanol which constituted binary system were $340^{\circ}C$ and $447^{\circ}C$, respectively. The experimental AITs of n-Butanol+sec-Butanol system were a good agreement with the calculated AITs by the proposed equations with a few A.A.D. (average absolute deviation).

A Study of Minimum Autoignition Temperature Behavior (MAITB) of Benzene and n-Hexane Mixture (벤젠과 노말헥산 혼합물의 최소자연발화온도 거동에 관한 연구)

  • Ha, Dong-Myeong;Kim, Kyu-Hyun
    • Fire Science and Engineering
    • /
    • v.27 no.1
    • /
    • pp.8-13
    • /
    • 2013
  • The autoignition temperature (AIT) is important index for the safe handling of flammable liquids which constitute the solvent mixtures. This study measured the AITs and ignition delay time for Benzene and n-Hexane system by using ASTM E659 apparatus. The AITs of Benzene and n-Hexane which constituted binary system were $583^{\circ}C$ and $240^{\circ}C$, respectively. The experimental AITs of Benzene and n-Hexane system were a good agreement with the calculated AITs by the proposed equations with a few A.A.D. (average absolute deviation).