• 제목/요약/키워드: Epitaxial Growth

검색결과 476건 처리시간 0.028초

CST 승화법을 이용한 p-type 4H-SiC(0001) 에픽텍셜층 성장과 이를 이용한 MESFET 소자의 전기적 특성 (Epitaxial Layer Growth of p-type 4H-SiC(0001) by the CST Method and Electrical Properties of MESFET Devices with Epitaxially Grown Layers)

  • 이기섭;박치권;이원재;신병철
    • 한국전기전자재료학회논문지
    • /
    • 제20권12호
    • /
    • pp.1056-1061
    • /
    • 2007
  • A sublimation epitaxial method, referred to as the Closed Space Technique (CST) was adopted to produce thick SiC epitaxial layers for power device applications. In this study, we aimed to systematically investigate surface morphologies and electrical properties of SiC epitaxial layers grown with varying a SiC/Al ratio in a SiC source powder during the sublimation growth using the CST method. The surface morphology was dramatically changed with varying the SiC/Al ratio. When the SiC/Al ratio of 90/1 was used, the step bunching was not observed in this magnification and the ratio of SiC/Al is an optimized range to grow of p-type SiC epitaxial layer. It was confirmed that the acceptor concentration of epitaxial layer was continuously decreased with increasing the SiC/Al ratio. 4H-SiC MESFETs haying a micron-gate length were fabricated using a lithography process and their current-voltage performances were characterized. It was confirmed that the increase of the negative voltage applied on the gate reduced the drain current, showing normal operation of FET device.

실리콘 선택적 기상 성장을 이용한 마이크로 센서에 응용되는 구조물 제조법 (Application of selective Epitaxial Growth of Silicon on MEMS Structure)

  • 박정호;김종관;김상영;성영권
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1025-1027
    • /
    • 1995
  • SEG(Selective Epitaxial Growth) and ELO(Epitaxial Lateral Growth) of Silicon offer new opportunities in the fabrication of MEMS(Micro Electro-Mechanical Systems) structures. SEG of silicon enables the stacking of junctions in addition to those resulting from the standard bipolar process and this properly was utilized for the fabrication of an improved-performance color sensor. When the crystalline growth takes place through the seed windows and proceeds over the dielectric, after reaching the surface, it form an ELO silicon layer and this ELO-Si can be modified into various structures for MEMS application such as cantilevers, beams, diaphragms.

  • PDF

초전도 박막의 에피택셜 성장에 관한 연구 (A Study on the Epitaxial Growth of Superconducting Thin Film)

  • 이희갑;박용필;김귀열
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 일렉트렛트 및 응용기술
    • /
    • pp.208-211
    • /
    • 2002
  • $Bi_2Sr_2CuO_x$(Bi-2201) thin films were fabricated by atomic layer-by-layer deposition using an ion beam sputtering method. 10 wt% and 90 wt% ozone mixed with oxygen were used with ultraviolet light irradiation to assist oxidation. At early stages of the atomic layer by layer deposition, two dimensional epitaxial growth which covers the substrate surface would be suppressed by the stress and strain caused by the lattice misfit, then three dimensional growth takes place. Since Cu element is the most difficult to oxidize, only Sr and Bi react with each other predominantly, and forms a buffer layer on the substrate in an amorphous-like structure, which is changed to $SrBi_2O_4$ by in-situ anneal.

  • PDF

Epitaxial Growth of Polyurea Film by Molecular Layer Deposition

  • 최성은;강은지;이진석
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.264.2-264.2
    • /
    • 2013
  • Molecular layer deposition (MLD) is sequential, self-limiting surface reaction to form conformal and ultrathin polymer film. This technique generally uses bifunctional precursors for stepwise sequential surface reaction and entirely organic polymer films. Also, in comparison with solution-based technique, because MLD is vapor-phase deposition based on ALD, it allows epitaxial growth of molecular layer on substrate and is especially good for surface reaction or coating of nanostructure such as nanopore, nanochannel, nanwire array and so on. In this study, polyurea film that consisted of phenylenediisocyanate and phenylenediamine was formed by MLD technique. In situ Fourier Transform Infrared (FTIR) measurement on high surface area SiO2 substrate was used to monitor the growth of polyurethane and polyurea film. Also, to investigate orientation of chemical bonding formed polymer film, plan-polarized grazing angle FTIR spectroscopy was used and it showed epitaxial growth and uniform orientation of chemical bones of polyurea films.

  • PDF

Si-Ge-H-Cl 계를 이용한 자기정렬 HBT용 Si 및 SiGe의 선택적 에피성장 (Selective Epitaxial Growth of Si and SiGe using Si-Ge-H-Cl System for Self-Aligned HBT Applications)

  • 김상훈;박찬우;이승윤;심규환;강진영
    • 한국전기전자재료학회논문지
    • /
    • 제16권7호
    • /
    • pp.573-578
    • /
    • 2003
  • Low temperature selective epitaxial growth of Si and SiGe has been obtained using an industrial single wafer chemical vapor deposition module operating at reduced pressure. Epitaxial Si and heteroepitaxial SiGe deposition with Ge content about 20 % has been studied as extrinsic base for self-aligned heterojunction bipolar transistors(HBTs), which helps to reduce the parasitic resistance to obtain higher maximum oscillation frequencies(f$\_$max/). The dependence of Si and SiGe deposition rates on exposed windows and their evolution with the addition of HCl to the gas mixture are investigated. SiH$_2$Cl$_2$ was used as the source of Si SEG(Selective Epitaxial Growth) and GeH$_4$ was added to grow SiGe SEG. The addition of HCl into the gas mixture allows increasing an incubation time even low growth temperature of 675∼725$^{\circ}C$. In addition, the selectivity is enhanced for the SiGe alloy and it was proposed that the incubation time for the polycrystalline deposit on the oxide is increased probably due to GeO formation. On the other hand, when only SiGe SEG(Selective Epitaxial Growth) layer is used for extrinsic base, it shows a higher sheet resistance with Ti-silicide because of Ge segregation to the interface, but in case of Si or Si/SiGe SEG layer, the sheet resistance is decreased up to 70 %.

Epitaxial growth of Tin Oxide thin films deposited by powder sputtering method

  • 백은하;김소진;강현철
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2015년도 제49회 하계 정기학술대회 초록집
    • /
    • pp.185.2-185.2
    • /
    • 2015
  • Tin Oxide (SnO2) has been widely investigated as a transparent conducting oxide (TCO) and can be used in optoelectronic devices such as solar cell and flat-panel displays. In addition, it would be applicable to fabricating the wide bandgap semiconductor because of its bandgap of 3.6 eV. There have been concentrated on the improvement of optical properties, such as conductivity and transparency, by doping Indium Oxide and Gallium Oxide. Recently, with development of fabrication techniques, high-qulaity SnO2 epitaxial thin films have been studied and received much attention to produce the electronic devices such as sensor and light-emitting diode. In this study, powder sputtering method was employed to deposit epitaxial thin films on sapphire (0001) substrates. A commercial SnO2 powder was sputtered. The samples were prepared with varying the growth parameters such as gas environment and film thickness. Then, the samples were characterized by using XRD, SEM, AFM, and Raman spectroscopy measurements. The details of physical properties of epitaxial SnO2 thin films will be presented.

  • PDF

LSI급 소자 제작을 위한 3인치 GaAs MBE 에피택셜 기판의 균일도 특성 연구 (A Study on Characteristics of Si doped 3 inch GaAs Epitaxial Layer Grown by MBE for LSI Application)

  • 이재진;이해권;맹성재;김보우;박형무;박신종
    • 전자공학회논문지A
    • /
    • 제31A권7호
    • /
    • pp.76-84
    • /
    • 1994
  • The characteristics of 3 inch wafer scale GaAs epitaxial wafer grown by molecular beam epitaxy for LSI process application were studied. The thickness and doping uniformity are characterized and discussed. The growth temperature and growth rate were $600^{\circ}C$ by pyrometer, and 1 $\mu$m/h, respectively. It was found that thickness and doping uniformity were 3.97% and 4.74% respectively across the full 3 inch diameter GaAs epitaxial layer. Also, ungated MESFETs have been fabricated and saturation current measurement showed 4.5% uniformity on 3 inch, epitaxial layer, but uniformity of threshold voltage increase up to 9.2% after recess process for MESFET device.

  • PDF

Crystal structure of the epitaxial $BaTiO_{3}$ thin film on the MgO (100) substrate prepared by the coating-pyrolysis process

  • Kim, S.;Kwon, O.Y.;Choi, S.W.;Manabe, T.;Yamaguchi, I.;Kumagai, T.;Mizuta, S.
    • 한국결정성장학회지
    • /
    • 제10권6호
    • /
    • pp.378-380
    • /
    • 2000
  • The epitaxial $BaTiO_{3}$ thin film was prepared on the MgO substrate by the coating-pyrolysis process using a mixed solution of Ba-naphthenate and Ti-naphthenate. The crystal structure of the epitaxial $BaTiO_{3}$ thin film was characterized by XRD ${\theta}/2{\theta}$ scan and asymmetric {303} rocking curve scan. The epitaxial $BaTiO_{3}$ thin film had the cubic phase with the lattice parameter of a = c = 0.4018 nm.