비납계 $[Bi_{1-x}(Na_{0.7-x}K_{0.2}Li_{0.1})]_{0.5}Ba_xTiO_3$ 압전 세라믹의 압전-유전특성 (Piezoelectric and Ferroelectric Properties of $[Bi_{1-x}(Na_{0.7-x}K_{0.2}Li_{0.1})]_{0.5}Ba_xTiO_3$ Lead-Free Piezoelectric Ceramics)

  • 이대수;정순종;김민수;박언철;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.271-271
    • /
    • 2006
  • The structural, dielectric and piezoelectric properties of $[Bi_{1-x}(Na_{0.7-x}K_{0.2}Li_{0.1})]_{0.5}BaxTiO_3$ (BNKLBxT) ceramics were studied for the compositional range, x = 0-0.08. The samples were prepared by conventional sintering technique. The result of X-ray diffraction (XRD) suggest that $Ba^{2+}$ diffuse into the $[Bi(Na_{0.7}K_{0.2}Li_{0.1})]_{0.5}TiO_3$ (BNKLT) lattices to form a solid solution with a single phase perovskite structure. The ceramic show excellent piezoelectric and ferroelectric properties, and optimum properties measured are as follows: piezoelectric constant $d_{33}=230pC/N$, planar electromechanical coupling factor $k_p\;=\;40.3%$, remanent polarization $P_r\;=\;30\;{\mu}C/cm^2$, and coercive field $E_c\; =\;2.5\;kV/mm$, respectively.

  • PDF

Structural, Dielectric and Field-Induced Strain Properties of La-Modified Bi1/2Na1/2TiO3-BaTiO3-SrZrO3 Ceramics

  • Hussain, Ali;Maqbool, Adnan;Malik, Rizwan Ahmed;Zaman, Arif;Lee, Jae Hong;Song, Tae Kwon;Lee, Jae Hyun;Kim, Won Jeong;Kim, Myong Ho
    • 한국재료학회지
    • /
    • 제25권10호
    • /
    • pp.566-570
    • /
    • 2015
  • $Bi_{0.5}Na_{0.5}TiO_3$ (BNT) based ceramics are considered potential lead-free alternatives for $Pb(Zr,Ti)O_3$(PZT) based ceramics in various applications such as sensors, actuators and transducers. However, BNT-based ceramics have lower electromechanical performance as compared with PZT based ceramics. Therefore, in this work, lead-free bulk $0.99[(Bi_{0.5}Na_{0.5})_{0.935}Ba_{0.065}]_{(1-x)}La_xTiO_3-0.01SrZO_3$ (BNBTLax-SZ, with x = 0, 0.01, 0.02) ceramics were synthesized by a conventional solid state reaction The crystal structure, dielectric response, degree of diffuseness and electric-field-induced strain properties were investigated as a function of different La concentrations. All samples were crystallized into a single phase perovskite structure. The temperature dependent dielectric response of La-modified BNBT-SZ ceramics showed lower dielectric response and improved field-induced strain response. The field induced strain increased from 0.17%_for pure BNBT-SZ to 0.38 % for 1 mol.% La-modified BNBT-SZ ceramics at an applied electric field of 6 kV/mm. These results show that La-modified BNBT-SZ ceramic system is expected to be a new candidate material for lead-free electronic devices.

소결조재 변화에 따른 0.94$(K_{0.5}Na_{0.5})NbO_3$-0.06Ba$(Zr_{0.05}Ti_{0.95})O_3$ 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristics of 0.94$(K_{0.5}Na_{0.5})NbO_3$-0.06Ba$(Zr_{0.05}Ti_{0.95})O_3$ Ceramics System According to the variations of sintering aids)

  • 서병호;김도형;이유형;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.205-205
    • /
    • 2008
  • PZT 세라믹은 우수한 유전 및 압전특성을 갖고 있어 변압기, 센서 및 엑츄에이터 등에 널리 응용되고 있다. 그러나, 우수한 특성에도 불구하고 PZT세라믹스의 소결시 PbO의 높은 유독성 및 휘발로 인하여 환경오염을 야기 시킨다. 그러므로 PbO로 구성된 세라믹을 대체하기 위한 우수한 압전특성을 가진 비납계 세라믹스 개발이 연구의 주류를 이루고 있다. 그 중 비납계 NKN와 BZT는 대체물질로 많이 관심을 받고 있다. 이는 일반적인 NKN조성은 우수한 압전성과 높은 큐리온도를 가지고 있을 뿐만 아니라, BZT조성의 Zr성분이 큐리온도를 낮추거나 유전특성을 졸게 하여 유전율 곡선을 완화하게 하는 특징이 있다. 하지만 NKN은 $1140^{\circ}C$이상의 소결온도에서 K의 휘발특성으로 인해 소성 후에도 주변의 수분을 흡수하는 조해성이 발생하는 문제가 발생한다. 그래서 본 연구에서는 낮은 온도에서 NKN계 세라믹스의 밀도를 증가시킬 뿐만 아니라, 우수한 유전 및 압전특성을 갖는 세라믹스를 제조하고자 비납계 $0.94(K_{0.5}Na_{0.5})NbO_3-0.06Ba(Zr_{0.05}Ti_{0.95})O_3$ (NKN-BZT)의 조성을 사용하였고 소결조제로는 $MnO_2$, NiO, $Bi_2O_3$, ZnO, $Li_2CO_3$, CuO등을 변화주어 유전 및 압전 특성을 알아보았다.

  • PDF

비납계 (Bi1/2Na1/2)TiO3-Ba(Cu1/3Nb2/3)O3 세라믹의 압전 및 변위 특성 (Piezoelectric and Strain Properties of Lead-free (Bi1/2Na1/2)TiO3-Ba(Cu1/3Nb2/3)O3 Ceramics)

  • 류정호;정대용
    • 한국재료학회지
    • /
    • 제21권11호
    • /
    • pp.628-633
    • /
    • 2011
  • Studies on lead-free piezoelectrics have been attractive as means of meeting environmental requirements. We synthesized lead-free piezoelectric $(Bi_{1/2}Na_{1/2})TiO_3-Ba(Cu_{1/3}Nb_{2/3})O_3$ (BNT-BCN) ceramics, and their dielectric, piezoelectric, and strain behavior were characterized. As BCN with a tetragonal phase was incorporated into the rhombohedral BNT lattice, the lattice constant increased. A small amount of BCN increased the density and dielectric constant forming the complete solid solution with BNT. However, BCN above 10 mol% was precipitated into a separate phase, and which was detected with XRD. In addition, EDX measurement revealed that Cu in BCN was not distributed homogeneously but was accumulated in a certain area. A lower density with a large amount of BCN was attributed to the nonsinterable property of BCN with large tetragonaliy. The dielectric constant vs the temperature change and the strain vs the electric field indicated that the ferroelectric property of BNT was diminished and paraelectric behavior was enhanced with the BCN addition. BNT-7.5BCN showed a 0.11% unimorph strain with a 9.0 kV/mm electric field with little hysteresis.

Processing, structure, and properties of lead-free piezoelectric NBT-BT

  • Mhin, Sungwook;Lee, Jung-Il;Ryu, Jeong Ho
    • 한국결정성장학회지
    • /
    • 제25권4호
    • /
    • pp.160-165
    • /
    • 2015
  • Lead-free piezoelectric materials have been actively studied to substitute for conventional PZT based solid solution, $Pb(Zr_xTi_{1-x}O_3)$, which occurs unavoidable PbO during the sintering process. Among them, Bismuth Sodium Titanate, $Na_{0.5}Bi_{0.5}TiO_3$ (abbreviated as NBT) based solid solution is attracted for the one of excellent candidates which shows the strong ferroelectricity, Curie temperature (Tc), remnant polarization (Pr) and coercive field (Ec). Especially, the solid solution of rhombohedral phase NBT with tetragonal perovskite phase has a rhombohedral - tetragonal morphotropic phase boundary. Modified NBT with tetragonal perovskite at the region of MPB can be applied for high frequency ultrasonic application because of not only its low permittivity, high electrocoupling factor and high mechanical strength, but also effective piezoelectric activity by poling. In this study, solid state ceramic processing of NBT and modified NBT, $(Na_{0.5}Bi_{0.5})_{0.93}Ba_{0.7}TiO_3$ (abbreviated as NBT-7BT), at the region of MPB using 7 % $BaTiO_3$ as a tetragonal perovskite was introduced and the structure between NBT and NBT-7BT were analyzed using rietveld refinement. Also, the ferroelectric and piezoelectric properties of NBT-7BT such as permittivity, piezoelectric constant, polarization hysteresis and strain hysteresis loop were compared with those of pure NBT.

Effects of Pre-synthesized $BaTiO_3$ Addition on the Microstructure and Dielectric/ Piezoelectric Properties of $(Bi_{0.5}Na_{0.5})_{0.94}Ba_{0.06}TiO_3$ Piezoelectric Ceramics

  • Khansur, Neamul Hayet;Yoon, Man-Soon;Kweon, Soon-Yong;Lee, Young-Geun;Ur, Soon-Chul
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.189-189
    • /
    • 2008
  • Due to the environmental issue vast research is going on to replace the widely used lead contented piezoelectric materials. Bismuth sodium titanate (abbreviated as BNT) based bismuth sodium titanate-barium titanate (abbreviated as BNBT) ceramic was prepared by using modified method rather than conventional mixed oxide method. This modification was made to improve the properties of BNT based ceramic. In this procedure $BaTiO_3$ (abbreviated as BT) was prepared using conventional mixed oxide method. Analytical grade raw materials of $BaCO_3$ and $TiO_2$ were weighted and ball milled using ethanol medium. The mixed slurry was dried and sieved under 80 mesh. Then the powder was calcined at $1100^{\circ}C$ for 2 hours. This calcined BT powder was used in the preparation of BNBT. Stoichiometric amount of $Bi_2O_3$, $Na_2CO_3$, $TiO_2$ and BT were weighted and mixed by using ball mill. The used calcination temperature was $850^{\circ}C$ for 2 hours. Calcined powder was taken for another milling step. BNBT disks were pressed to 15 mm of diameter and then cold isostatical press (CIP) was used. Pressed samples were sintered at $1150^{\circ}C$ for 2 hours. The SEM microstructure analysis revealed that the grain shape of the sintered ceramic was polyhedral and grain boundary was well matched where as the sample prepared by conventional method showed irregular arrangement and grain boundary not well matched. And sintered density was better (5.78 g/cc) for the modified method. It was strongly observed that the properties of BNBT ceramic near MPB composition was found to be improved by the modified method compare to the conventional mixed oxide method. The piezoelectric constant dB of 177.33 pC/N, electromechanical coupling factor $k_p$ of 33.4%, dielectric constant $K_{33}^T$ of 688.237 and mechanical quality factor $Q_m$ of 109.37 was found.

  • PDF

무연 BNBT 세라믹스의 압전특성에 미치는 La2O3의 영향 (Effects of La2O3 on the Piezoelectric Properties of Lead-Free (Bi0.5Na0.5)0.94Ba0.06TiO3 Piezoelectric Ceramics)

  • 손영진;윤만순;어순철
    • 한국재료학회지
    • /
    • 제15권12호
    • /
    • pp.756-759
    • /
    • 2005
  • A lead free piezoelectric material, bismuth sodium barium titanate $(Bi_{0.5}Na_{0.5})_{0.94}Ba_{0.06}TiO_3$ (BNBT), was considered as an environment-friendly alternatives for the current PZT system. A perovskite BNBT was synthesized by conventional bulk ceramic processing technique. In order to improve piezoelectric properties, $La_2O_3$ as a dopant was incorporated into the BNBT system up to 0.025 moi, ana the effects on subsequent the piezoelectric ana dielectric properties were systematically investigated. With increasing $La_2O_3$ contents, the equilibrium grain shape was remarkably evidenced and sintered density was increased. Piezoelectric and dielectric properties were s]town to have maximum values at the $La_2O_3$ contents of 0.02 mol. $La^{3+}$ ions seemed to act as a softener in the BNBT system and to enhance dielectric and piezoelectric properties in this study.

Concentration dependent dielectric properties of Barium Titanate/Polyvenylidene Fluoride (PVDF) and (Bi0.5Na0.5)0.94Ba0.06TiO3/Poly(VDF-TrFE) composite

  • Roy, Ansu K.;Ahmad, Z.;Prasad, A.;Prasad, K.
    • Advances in materials Research
    • /
    • 제1권4호
    • /
    • pp.285-297
    • /
    • 2012
  • The present study addresses the problem of quantitative prediction of effective complex relative permittivity of Barium Titanate/Polyvenylidene Fluoride (PVDF) and $(Bi_{0.5}Na_{0.5})_{0.94}Ba_{0.06}TiO_3$/Poly(VDF-TrFE) biphasic ceramic-polymer composites. Theoretical results for effective relative permittivity derived from several dielectric mixture equations were fitted to the experimental data taken from the works of Prasad et al. (2010), Wang et al. (2004), Takenaka et al. (1991) and Yamada et al. (1982). The study revealed that out of the different test equations, only a few equations like modified Rother-Lichtenecker equation, Dias-Dasgupta equation or Rao equation for the real part and Bruggeman equation for the imaginary part of complex permittivity well fitted the corresponding experimental results. In the present study, some of the equations were used in their original forms, while some others were modified by choosing suitable shape-dependent parameters in order to get reasonably good agreement with experimental results. Besides, the experimental results have been proposed in the form of a mathematical model using first order exponential growth, which provided excellent fits.

NKN-(1-x)BNT-xBT 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Properties of NKN-(1-x)BNT-xBT Ceramics)

  • 이승환;남성필;이성갑;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제23권10호
    • /
    • pp.771-775
    • /
    • 2010
  • In this study, piezoelectric and dielectric properties of the $(Na_{0.5}K_{0.5})NbO_3-(1-x)(Bi_{0.5}Na_{0.5})TiO_3-xBaTiO_3$ [NKN-(1-x)BNT-xBT] ceramics were investigated. The lead-free NKN-(1-x)BNT-xBT ceramics were fabricated by a conventional mixed oxide method. The results indicate that the addition of $BaTiO_3$ significantly influences the sintering, microstructure, phase transition and electrical properties of NKN-BNT ceramics. A gradual change in the piezoelectric and dielectric properties was observed with the increase of BT contents. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased at the morphotropic phase boundary (MPB). The $d_{33}$=184 pC/N, $k_p$=0.38, dielectric constant=1455 with dielectric loss value of less than 1% were obtained for the NKN-0.95BNT-0.05BT ceramics sintered at $1150^{\circ}C$ for 2h. These results demonstrate that the NKN-(1-x)BNT-xBT ceramics is an attractive candidate for lead-free piezoelectric materials.

[100]-Texturing of Barium Titanate Ceramics Using Sodium Bismuth Titanate Templates: Challenges and Insights

  • Nu-Ri Ko;Temesgen Tadeyos Zate;Wook Jo
    • 한국전기전자재료학회논문지
    • /
    • 제37권3호
    • /
    • pp.328-331
    • /
    • 2024
  • This research explores the development of [100]-textured barium titanate (BaTiO3, BT) ceramics using sodium bismuth titanate (Na0.5Bi4.5Ti4O15, NBiT) templates, aimed at leveraging the inherent high dielectric property of BT. However, the attempted texturing was unsuccessful, primarily due to bismuth diffusion from the NBiT templates into the BT matrix below the sintering temperature, at 1,000℃. Systematical exploration about the cause of the failure is involved and alternative approaches are proposed in detail to overcome the challenge. These findings contribute to the understanding of techniques and conditions for textured ceramic fabrication and highlight the need for further research in this area.