• Title/Summary/Keyword: Ag migration

Search Result 33, Processing Time 0.027 seconds

Investigation of Ag Migration from Ag Paste Bump in Printed Circuit Board (Ag Paste bump 구조를 갖는 인쇄회로기판의 Ag migration 발생 안전성 평가)

  • Song, Chul-Ho;Kim, Young-Hun;Lee, Sang-Min;Mok, Jee-Soo;Yang, Yong-Suk
    • Korean Journal of Materials Research
    • /
    • v.20 no.1
    • /
    • pp.19-24
    • /
    • 2010
  • The current study examined Ag migration from the Ag paste bump in the SABiT technology-applied PCB. A series of experiments were performed to measure the existence/non-existence of Ag in the insulating prepreg region. The average grain size of Ag paste was 30 nm according to X-ray diffraction (XRD) measurement. Conventional XRD showed limitations in finding a small amount of Ag in the prepreg region. The surface morphology and cross section view in the Cu line-Ag paste bump-Cu line structure were observed using a field emission scanning electron microscope (FE-SEM). The amount of Ag as a function of distance from the edge of Ag paste bump was obtained by FE-SEM with energy dispersive spectroscopy (EDS). We used an electron probe micro analyzer (EPMA) to improve the detecting resolution of Ag content and achieved the Ag distribution function as a function of the distance from the edge of the Ag paste bump. The same method with EPMA was applied for Cu filled via instead of Ag paste bump. We compared the distribution function of Ag and Cu, obtained from EPMA, and concluded that there was no considerable Ag migration effect for the SABiT technology-applied printed circuit board (PCB).

Electrochemical Migration Characteristics of Sn-3.0Ag-0.5Cu Solder Alloy in NaBr and NaF Solutions (NaBr 및 NaF 용액에 대한 Sn-3.0Ag-0.5Cu 솔더 합금의 Electrochemical Migration 특성)

  • Jung, Ja-Young;Jang, Eun-Jung;Yoo, Young-Ran;Lee, Shin-Bok;Kim, Young-Sik;Joo, Young-Chang;Chung, Tai-Joo;Lee, Kyu-Hwan;Park, Young-Bae
    • Journal of Welding and Joining
    • /
    • v.25 no.3
    • /
    • pp.57-63
    • /
    • 2007
  • Electrochemical migration characteristics of Pb-free solder alloys are quantitatively correlated with corrosion characteristics in harsh environment conditions. In-situ water drop test and corrosion resistance test for Sn-3.0Ag-0.5Cu solder alloys were carried out in NaBr and NaF solutions to obtain the electrochemical migration lifetime and pitting potential, respectively. Sn-3.0Ag-0.5Cu solder alloy shows similar ionization and electrochemical migration behavior with pure Sn because of Ag and Cu do not migrate due to the formation of resistant intermetallic compounds inside solder itself. Electrochemical migration lifetime in NaBr is longer than in NaF, which seems to be closely related to higher pitting potential in NaBr than NaF solution. Therefore, it was revealed that electrochemical migration lifetime of Sn-3.0Ag-0.5Cu solder alloys showed good correlation to the corrosion resistance, and also the initial ionization step at anode side is believed to be the rate-determining step during electrochemical migration of Pb-free solders in these environments.

Improving quality of keyboard by analyzing Ag ion migration (키보드에서의 Ag Ion Migration 불량 개선사례)

  • 하종신;최완수;이성수;김영복
    • Proceedings of the Korean Reliability Society Conference
    • /
    • 2001.06a
    • /
    • pp.489-496
    • /
    • 2001
  • 컴퓨터 키보드의 시장 불량품을 분석한 결과 여러 키가 동시에 입력되는 현상이 다수 발생되는 것을 알 수 있었다. 정밀분석결과 이의 원인이 키보드 membrane의 패턴을 구성하는 은(Ag) paste의 ion migration발생에 의한 것임을 알 수 있었다. 재현실험을 통해 고온 고습한 환경에서 장시간 사용하다보면 membrane내부로 수분이 침투하여 패턴간에 Ag ion migration이 발생되어 키 동작 오류를 유발시킴을 알 수 있었다. 이에 대한 대책안으로 제조 원가에 크게 영향을 주지 않으면서 migration을 크게 억제할 수 있는 준방수 방식의 membrane을 채택하여 4$0^{\circ}C$, 90%RH 환경에서 최소 5년을 보증할 수 있는 키보드를 제작하였다. 또한, 키보드 membrane의 ion migration 시험시 정상사용 조건을 가속시킬 수 있는 재현 및 검증시험법(85$^{\circ}C$, 85%RH, 가속계수 17배)을 개발하였다.

  • PDF

Effects of Ag and Cu Additions on the Electrochemical Migration Susceptibility of Pb-free Solders in Na2SO4 Solution

  • Yoo, Y.R.;Nam, H.S.;Jung, J.Y.;Lee, S.B.;Park, Y.B.;Joo, Y.C.;Kim, Y.S.
    • Corrosion Science and Technology
    • /
    • v.6 no.2
    • /
    • pp.50-55
    • /
    • 2007
  • The smaller size and higher integration of advanced electronic package systems result in severe electrochemical reliability issues in microelectronic packaging due to higher electric field under high temperature and humidity conditions. Under these harsh conditions, electronic components respond to applied voltages by electrochemical ionization of metal and the formation of a filament, which leads to short-circuit failure of an electronic component, which is termed electrochemical migration. This work aims to evaluate electrochemical migration susceptibility of the pure Sn, Sn-3.5Ag, Sn-3.0Ag-0.5Cu solder alloys in $Na_{2}SO_{4}$. The water drop test was performed to understand the failure mechanism in a pad patterned solder alloy. The polarization test and anodic dissolution test were performed, and ionic species and concentration were analyzed. Ag and Cu additions increased the time to failure of Pb-free solder in 0.001 wt% $Na_{2}SO_{4}$ solution at room temperature and the dendrite was mainly composed of Sn regardless of the solders. In the case of SnAg solders, when Ag and Cu added to the solders, Ag and Cu improved the passivation behavior and pitting corrosion resistance and formed inert intermetallic compounds and thus the dissolution of Ag and Cu was suppressed; only Sn was dissolved. If ionic species is mainly Sn ion, dissolution content than cathodic deposition efficiency will affect the composition of the dendrite. Therefore, Ag and Cu additions improve the electrochemical migration resistance of SnAg and SnAgCu solders.

Flux residue effect on the electrochemical migration of Sn-3.0Ag-0.5Cu (Sn-3.0Ag-0.5Cu 솔더링에서 플럭스 잔사가 전기화학적 마이그레이션에 미치는 영향)

  • Bang, Jung-Hwan;Lee, Chang-Woo
    • Journal of Welding and Joining
    • /
    • v.29 no.5
    • /
    • pp.95-98
    • /
    • 2011
  • Recently, there is a growing tendency that fine-pitch electronic devices are increased due to higher density and very large scale integration. Finer pitch printed circuit board(PCB) is to be decrease insulation resistance between circuit patterns and electrical components, which will induce to electrical short in electronic circuit by electrochemical migration when it exposes to long term in high temperature and high humidity. In this research, the effect of soldering flux acting as an electrical carrier between conductors on electrochemical migration was investigated. The PCB pad was coated with OSP finish. Sn3.0Ag0.5Cu solder paste was printed on the PCB circuit and then the coupon was treated by reflow process. Thereby, specimen for ion migration test was fabricated. Electrochemical migration test was conducted under the condition of DC 48 V, $85^{\circ}C$, and 85 % relative humidity. Their life time could be increased about 22% by means of removal of flux. The fundamentals and mechanism of electrochemical migration was discussed depending on the existence of flux residues after reflow process.

Electrochemical Ion Migration Sensitivity of Printed Circuit Board Plated with Sn-3.0Ag-0.5Cu and Sn-37Pb (Sn-3.0Ag-0.5Cu, Sn-37Pb 표면처리 기판의 전기화학적 이온 마이그레이션 민감도)

  • Hong, Won-Sik;Park, No-Chang;O, Cheol-Min;Kim, Gwang-Bae
    • Proceedings of the KWS Conference
    • /
    • 2006.10a
    • /
    • pp.136-138
    • /
    • 2006
  • Recently a lots of problems have observed in high densified and high integrated electronic components. One of them is ion migration phenomena, which induce the electrical short of electrical circuit. Ion migration phenomena has been observed in the field of exposing the specific environment and using for a long time. Also as the RoHS restriction was started in July 1st, 2006, Pb-free solder was utilized in electronics assemblies. In this case, it is very important to compatible between components and printed circuit board(PCB), thus surface treatment materials of PCB was changed to Sn, Sn-3.0Ag-0.5Cu, Cu. Therefore these new application become to need to reevaluate the sensitivity about electrochemical ion migration. This study was evaluated the occurrence time of electrochemical ion migration using by water drop test. We utilized PCB(printed circuit board) having a comb pattern as follows 0.1, 0.318, 0.5, 1.0 mm pattern distance. Sn-3.0Ag-0.5Cu and Sn-37Pb were electroplated on the comb pattern. 6.5V and 15.0V were applied in the comb pattern and then we measured the electrical short time causing by occurring the ion migration. In these results, we evaluate the sensitivity and derived the prediction models of ion migration occurrence time depending on the pattern materials, applied voltage and pattern spacing of PCB conductor.

  • PDF

X-ray Absorption Spectra Analysis for the Investigation of the Retardation Mechanism of Iodine Migration by the Silver Ion Added to Bentonite (벤토나이트에 첨가한 은 이온에 의한 아이오딘 이동 저지 메커니즘 규명을 위한 X-선 흡수 스펙트라 분석)

  • Kim, Seung-Soo;Kim, Min-Gue;Baik, Min-Hoon;Choi, Jong-Won
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.8 no.3
    • /
    • pp.201-205
    • /
    • 2010
  • Most of iodine was captured by the block when NaI solution flowed through a bentonite block sorbed silver to retard the migration of iodine released from high-level radioactive wastes. In order to understand in detail the mechanism for the retardation of the iodine by the silver ion, X-ray Absorption Near Edge Structure (XANES) and Extended X-ray Absorption Fine Structure (EXAFS) spectra of the silver sorbed bentonite before and after the contact with iodide were compared with those of AgO, $Ag_2O$ and AgI as references. This examination suggests that the silver ion sorbed on the bentonite is desorbed, and then it retards the migration of iodine by forming the cluster of AgI precipitate.

Behavior of Ag+ and Sn2+ After Reaction Between the Transparent Dielectric PbO-B2O3-SiO2-Al2O3 and Ag Electrodes (투명 유전체 (PbO-B2O3-SiO2-Al2O3 계)와 Ag 전극과의 반응에 의한 Ag+과 Sn2+의 거동)

  • Hong, Gyeong-Jun;Park, Jun-Hyeon;Heo, Jeung-Su;Kim, Hyeong-Jun
    • Korean Journal of Materials Research
    • /
    • v.12 no.5
    • /
    • pp.347-352
    • /
    • 2002
  • A transparent dielectric of the $PbO-B_2O_3-SiO_2-A1_2O_3$ system which was a low melting glass has been used for PDP (Plasma Display Panel), but it has a problem which is a reaction to be occurred between a transparent dielectric layer and electrodes (Ag, ITO) after firing. This research was conducted for ion migration of $Ag^+\$ and $Sn^ {2+}$ during firing three different frits of low melting glass. The result showed that yellowing phenomena occurred through a chemical reaction between $Ag^+\$and $Sn^ {2+}$ at 550~58$0^{\circ}C$ for 20~60 min. In addition, it was confirmed that the migration of $Sn^{2+}$ from ITO electrode made a strong effect on the yellowing phenomena.

A Study on Development of Flux to Restrict Occurrence of ion Migration in Lead-Free Solder (무연솔더 내 마이그레이션 플럭스개발에 관한 연구)

  • Ryu Dong Su;Lim Jae Hoon;Woo Seong Woo
    • Proceedings of the Korean Reliability Society Conference
    • /
    • 2005.06a
    • /
    • pp.385-392
    • /
    • 2005
  • The restriction of the use of hazardous substances in electrical and electronic equipment legislation mandates the substitution of lead and other hazardous substances in electronics products by July 2006. Due to this legislative pressure, the electronics industry is moving to adoption of lead free solders. In this paper, we investigated a flux to restrict generating electrochemical migration in lead-free solder. The lead-free solders used in this study were Sn-0.7Cu-0.01P and Sn-3.0Ag-0.5Cu. To measure the resistance of electrochemical migration, the dew-cycle test and water drop test were adopted. As the result, now flux having high durable of electrochemical migration was developed.

  • PDF

Electrical Conductance and Electrode Reaction of $RbAg_4I_5$ Single Crystals (고체전해질 $RbAg_4I_5$ 단결정의 전기전도성과 전극반응)

  • Jong Hee Park;Woon-Kie Paik
    • Journal of the Korean Chemical Society
    • /
    • v.24 no.4
    • /
    • pp.295-301
    • /
    • 1980
  • The electrical conductivity of solid electrolyte $RbAg_4I_5$ single crystal was studied at various temperatures. The four-probe method was used in measuring the conductance with an ac signal imposed on the specimen. The ionic conductivity was $0.284 ohm^{-1} cm^{-1}\;at\;25^{\circ}C$, and the activation energy for $Ag^+$ ion migration was calulated to be 1.70 kcal/mole. These values agree well with those reported for polycrystalline samples. Reactions at $Ag/RbAg_4I_5$ interface were studied by cyclic voltammetry with a silver reference electrode. It was found that silver ion is reversibly reduced at silver surfaces below zero volt, and iodide was oxidized above +0.67 volt.The anodic current arising from the oxidation of the electrode was small in magnitude initially over a wide range of potential, but, after silver was cathodically deposited on the electrode, reversing the potential sweep to the anodic direction resulted in a sharp peak of anodic current.

  • PDF