Effect of Environmental Conditions on Expansion of Mortar-bar by Alkali-Silica Reaction (환경조건이 알칼리-실리카 반응에 의한 모르타르 봉 길이 팽창에 미치는 영향)

  • Kim, Seong-Kwon;Yun, Kyong-Ku;Hong, Seung-Ho;Kang, Moon-Sik
    • International Journal of Highway Engineering
    • /
    • v.13 no.3
    • /
    • pp.1-6
    • /
    • 2011
  • The possibility of ASR(alkali-silica reaction) for coarse aggregates had known to be low up to recently in Korea. But the distress of ASR was identified and reported by ASTM C 1260 test. The purpose of this paper was to identify the effect of environmental conditions on length expansion of mortar-bar by alkali-silica reaction with KS F 2546 and ASTM C 1260 test. The results of this study were as following; The result of KS F 2546 test for five kinds of aggregates shows that all of them are non-reactive. But that of ASTM C 1260 test shows that all of aggregates except Andesite-2 are over possible reactive because of environmental condition such as external alkali ion by 1N NaOH, high temperature and humidity. The result of variety of NaOH concentration on ASTM C 1260 using Siltstone indicates that length expansion rate increases highly as NaOH concentration increases. And, comparison results of KS F 2546 for Siltstone with that of 0.00N NaOH experiment indicates that length expansion rate increases as temperature and humidity increases.

Application of ASTM C 1260 for Cement Matrix Mixed with FlyAsh and Lithium Nitrate (플라이애시와 질산리튬을 사용한 시멘트 경화체의 ASTM C 1260 적용성 검토)

  • Kim, Seong-Kwon;Yun, Kyong-Ku;Hong, Seung-Ho;Kang, Moon-Sik
    • International Journal of Highway Engineering
    • /
    • v.14 no.3
    • /
    • pp.1-7
    • /
    • 2012
  • The purpose of this study was to review application of ASTM C 1260 for cement matrix with flyash and lithium nitrate using reactive aggregate. The experimental program included the accelerated mortar bar test (AMBT: ASTM C 1260) for the slate which was evaluated as reactive aggregate by ASTM C 1260 at the previous study. The cement, which was substituted by 10, 20, 30% flyash containing less than 10% CaO, could control ASR expansion. From the experiment applying lithium nitrate to control ASR, the mortar bar containing lithium nitrate showed more than 0.1% expansion at 14 days. This is probably due to dissolution of lithium nitrate in NaOH solution during test periods. Thus, it is necessary to adopt another test method to verify the control effect of lithium nitrate against alkali-silica reaction.

Evaluation of Alkali-Silica Reactivity for Aggregates in Korea according to Test Methods (시험방법에 따른 국내 골재의 알칼리-실리카 반응성 평가)

  • Yun, Kyong-Ku;Kim, Seong-Kwon;Hong, Seung-Ho;Han, Seung-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.6
    • /
    • pp.689-696
    • /
    • 2008
  • The purpose of this study was to evaluate the alkali-silica reactivity for aggregates in Korea according to test methods: accelerated mortar bar test (AMBT) by ASTM C 1260; chemical test by KS F 2545 (ASTM C 289). The results are as follows: The AMBT (ASTM C 1260) results showed that two (2) igneous rocks (two mica granite and felsite), three (3) sedimentary rocks (arkose, red sandstone and shale), two (2) metamorphic rock (slate and vitric tuff), one (1) mineral (quartz) showed more expansion than 0.1% at 14 days. But, some sedimentary rocks and metamorphic rocks expanded more than 0.1% at 28 days even though they were less than 0.1% at 14 days. Therefore, it is necessary to extend the experimental dates more than 14 days to evaluate the possibility of alkali-aggregate reactivity. The chemical test (KS F 2545) results showed that five (5) igneous rocks (andesite, diabase, granite porphyry, muscovite granite and diorite) were indicative of potentially deleterious expansion, while two (2) igneous rocks (diorite porphyry and quartz porphyry) were possible indicative of expansion, and three (3) igneous rocks (biotite granite, two mica granite and felsite) were indicative of innocuous reactivity. The above results showed that the results from chemical method (KS F 2545) and AMBT (ASTM C 1260) had little relationship.

Controlling Effect of Alkali-Aggregate Reactivity using Mineral Admixtures (광물성 혼화재를 이용한 알칼리-골재 반응 억제 효과)

  • Yun, Kyong-Ku;Kim, Seong-Kwon;Seo, Jae-Yeop;Hong, Seung-Ho;Han, Seung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.255-256
    • /
    • 2009
  • This purpose of this study was to evaluate the controlling effect of alkali-aggregate reactivity using mineral admixtures for aggregates in Korea according to test methods: chemical test by KS F 2545; mortar bar test by KS F 2546; accelerated mortar bat test by ASTM C 1260.

  • PDF

Characteristics of Alkali-Silica Reaction according to Types and Substitution Ratios of Mineral Admixtures in Korea (국내 광물성 혼화재의 종류 및 혼입률에 따른 알칼리-실리카 반응 특성)

  • Kim, Seong-Kwon;Hong, Seung-Ho;Hur, In;Yun, Kyong-Ku
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.1
    • /
    • pp.49-55
    • /
    • 2011
  • The distresses of alkali-silica reaction (ASR) was recently reported at highway cement concrete pavement in Korea, which showed typical cracking and spalling patterns of ARS. Korea is was no longer safe zone against ASR, needding to find a control methodology against ASR. The purpose of this research was to provide a control methodology against ASR using mineral admixtures through a series of laboratory test program. Laboratory works included the accelerated mortar bar test (AMBT) by ASTM C 1260 regulation with five types of aggregate and three types of mineral admixtures (fly ash, ground granulated blast-furnace slag and silica fume). The result of ASTM C 1260 test for five types of aggregates without mineral admixtures showed that Siltstone and Mudstone were found to be "reactive." Tuff and Andesite-1 were found to be "possiblely reactive." In case of concrete mixed with 10, 20, and 30% fly ash, all specimens except Mudstone mixed with 10% FA were found to be "non-reactive". In cases of concrete mixed with 30, 40, and 50% ground granulated blast-furnace slag and 5, 7.5, and 10% silica fume, all specimens were found to be "non-reactive." These results could be selectively applied in constructions in Korea.

Preventive Measures on Alkali-Silica Reaction of Crushed Stones (쇄석 골재의 알칼리-실리카 반응 방지 대책)

  • Jun Ssang-Sun;Lee Hyo-Min;Seo Ki-Young;Hwang Jin-Yeon;Jin Chi-Sub
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.1 s.85
    • /
    • pp.129-137
    • /
    • 2005
  • In Korea, due to the insufficiency of natural aggregates and increasing needs of crushed stones, it is necessary to examine the alkali-silica reaction of the crushed stones. The reaction produces an alkali-silica reaction gel which can imbibe pore solution and swell to generate cracks that are visible In affected concrete. In general, crushed stones are tested by petrograptuc examination, chemical method and mortar-bar method, but the most reliable method Is mortar-bar test. This study tested alkali-silica reactivity of crushed stones of various rock types using ASTM C 227 and C 1260, and compared the results of two test methods. This study also analyzed effects of particle size and grading of reactive aggregate on alkali-silica reaction expansion of mortar-bar. The effectiveness of mineral admixtures to reduce detrimental expansion caused by alkali-silica reaction was investigated through the ASTM C 1260 method. The mineral admixtures used were nv ash, silica fume, metakaolin and ground granulated blast furnace slag. The replacement ratios of 0, 5, 10, 15, 25 and $35\%$ were commonly applied for all the mineral admixtures and the replacement ratios of 45 and $55\%$ were additional applied for the admixtures that could maintain workability. The results indicate that replacement ratios of $25\%$ for ay ash, $10\%$ for silica fume, $25\%$ for metakaolin or $35\%$ for ground granulated blast furnace slag were most effective to reduce alkali-silica reaction expansion under the experimental conditions.