• 제목/요약/키워드: 포러스 콘크리트

검색결과 68건 처리시간 0.031초

조장조성용 포러스콘크리트의 물리${\cdot}$역학적 특성에 관한 실험적 연구 (A Study on the Physical and Mechanical Properties of Kelp Forest Regeneration Porous Concrete)

  • 서대석;박승범;조광연;이준;장영일;이윤선
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.521-524
    • /
    • 2004
  • The Purpose of this study is to develope the method for early recovery of the biodiversity in the oligotrophical costal area, it is important in the recovery of the biodiversity to make kelp forest grow in the concerned area. In order for it, sufficient nutrient is required as well as the proper seedbed, Hence in this study, granulated fertilizer, which contains nutrient, such as nitrogen, phosphorus and etc, is coated by cement paste, and then is mixed in to the porous concrete in order to provide seedbed and nutrient simultaneously. The physical and mechanical properties, such as water permeability, void ratio, compressive strength of porous concrete with granulated fertilizer are discussed.

  • PDF

폴리프로필렌섬유보강 포러스 폴리머 콘크리트의 특성 (Properties of Porous Polymer Concrete Reinforced Polypropylene Fiber)

  • 김영익;성찬용
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.723-726
    • /
    • 2004
  • Porous polymer concrete can be applied to roads, sidewalks, river embankment, drain pipes, conduits, retaining walls, yards, parking lots, plazas, interlocking blocks, etc. This study is to examine a content ratio of polypropylene fiber to improve bending strength, impact resistance and freezing and thawing rssistance of porous polymer concrete. Also, this study is performed to develop the porous polymer concrete using recycled coarse aggregate and blast furnace slag for application of structures needed permeability. At 7 days of curing, compressive strength, flexural strength, water permeability and flexural load are in the ragge of $17\~21MPa,\;5\~7MPa,\;4.1\times10^{-2}\~7.7\times10^{-2}cm/s$, respectively. It is concluded that the recycled aggregate can be used in the porous polymer concretes.

  • PDF

특수처리 입상비료를 이용한 포러스콘크리트의 해양식물 부착특성에 관한 연구 (Marine Plant Adhesion Properties of Porous Concrete Using Specially Treated Granular Fertilizer)

  • 이병재;박승범;이준;손성우;조광연
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.893-896
    • /
    • 2006
  • This study examined plant adhesion characteristics of the porous concrete that used specially treated granular fertilizer for field application, which was used for the restoration of the marine ecosystem. The results of the experiment showed that nutrient eruption amount, the destruction and dissolution ratio tended to decrease when the coating thickness was increased. The void ratio and compressive strength tended to decrease when the specially treated granular fertilizer mixing ratio was increased. According to these results, the appropriate thickness of coating for cement coated granular fertilizer was 1.0mm. The adhesion ability of marine plant to porous concrete was superior when the cement coated granular fertilizer was mixed. Therefore, the appropriate cement coated granular fertilizer mixing ratio of 20% with a coating thickness of 1.0mm is thought to be a factor when considering the strength of the porous concrete for marine ecosystem restoration and the adhesion characteristics of marine plant.

  • PDF

다짐방법에 따른 포러스콘크리트의 물리.역학적 특성에 관한 연구 (The Study on the Physical and Mechanical Properties of Porous Concrete according to Compaction Method)

  • 송재립;박승범;서대석;이준;장영일
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.813-816
    • /
    • 2006
  • Recently, improvements in the standard of living in industrial area require the establishment of a convenient residential environment in order to enhance the quality of living. To achieve such an environment, it is necessary to effectively reduce or prevent various environmental problems occurring in and around residential areas. Although conventional concrete has been regarded as a destroyer of nature, water and air can pass freely through concrete when it is made porous concrete by forming continuous void. In view of the harmony between nature and concrete, various research paths are being taken focusing on coarse aggregates to make porous concrete having continuous voids so as to improve water and air permeability, acoustic absorption, water purification, and applicability to vegetation. In this study, the Physical and Mechanical Properties of porous concrete according to compaction method analyzed by void ratio, coefficient of permeability and compressive strength.

  • PDF

골재의 종류에 따른 포러스콘크리트의 특성에 관한 실험적 연구 (An Experimental Study on the Characteristic of Porous Concrete using different Aggregates)

  • 정시진
    • 한국건축시공학회지
    • /
    • 제4권1호
    • /
    • pp.89-96
    • /
    • 2004
  • Porous concrete is used of various parts by advantage of porous. Example of growing of plant is possible, and dwelling of creature, and filter functions of various contaminant, and decrease of noise, and so on. This research is for porous concretes that were used by four aggregate rubble, refreshing aggregate, expanded clay, orchid stone. This research estimate that physical and mechanical characteristics of fresh concrete and hardened concrete. The purpose of this research is to make environment-friendly porous concrete. This research's conclusion is as following : 1. Porous Concrete's slump was measured 12~14cm with rubble, 12~16cm with refreshing aggregate, 11~13cm with expanded clay, 11~13cm with orchid stone. Weight of aggregate was bigger, slump price appeared by bigger thing. Because placed Porous Concrete is low viscosity and small resistance between aggregate, it estimated that have high workability. 2. Porous Concrete's unit weight was measured 1.71~1.75t/$\textrm{m}^3$ with rubble, 1.58~1.62t/$\textrm{m}^3$ with refreshing aggregate, 1.19~1.20t/$\textrm{m}^3$ with expanded clay, 0.98~1.06t/$\textrm{m}^3$ with orchid stone. Showed aspect such as weight of aggregate. 3. Porous Concrete's compressive strength was measured 76~102kgf/$\textrm{cm}^2$ with rubble, 51~60kgf/$\textrm{cm}^2$ with refreshing aggregate, 30~40kgf/$\textrm{cm}^2$ with expanded clay, 13~16kgf/$\textrm{cm}^2$ with orchid stone. 4. Tendency of tensile strength and bending strength showed generally similarly with compressive strength, but showed low value fewer than 15kgf/$\textrm{cm}^2$ Therefore, wire mesh, reinforcing rod, such as establishment of frame is considered to need in reinforcement about tensility or flexures in case receive tensility or produce product of thin absence form. It concludes by speculating on the consequences of extrapolating the results of study to remodelling the office building being already existence.

시멘트체이스트의 유동성 및 진동다짐시간이 포러스콘크리트의 기초물성에 미치는 영향 (Influence of Paste Fluidity and Vibration Time for Fundamental Properties of Porous Concrete)

  • 이성일;유범재;장종호;김재환;백용관;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.311-316
    • /
    • 2001
  • This study analyzed the influence of paste fluidity and vibration time for fundamental properties of porous concrete. Results of this study were shown as follows; 1) Even if target void ratio is same, void ratio and compressive strength of porous concrete is different according to w/c, paste flow and vibration time. So, In case of target void ratio, we must consider the influence of w/c, paste flow, and vibration time. 2) Though w/c and vibration time are same, as paste flow increase, all void ratio, continuous void ratio, and compressive strength decrease and difference between upper and lower void ratio increase. 3) Though w/c and paste flow are same, as vibration time increase, all void ratio and continuous void ratio decrease and difference between upper and lower void ratio increase. Also, compressive strength increase by 10 seconds and decease after 10 seconds. 4) As types of superplasticizer is different, all void ratio, continuous void ratio, and compressive strength are different. So, we must give consideration to paste fluidity and vibration time in order that increase of strength of porous concrete and distribution of uniform void.

  • PDF

산업부산물을 사용한 포러스 콘크리트의 수질정화 특성에 관한 실험적 연구 (An Experimental Study on Water-Purification Properties of Porous Concrete Using Industrial By-Products)

  • 조영수;김정환;권혁준;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.717-722
    • /
    • 2002
  • The results of an experiment on the water purification of the porous concrete and its influence on the compressive strength are reported in this paper. Two different sizes of coarse aggregate of 5-10, and 10-20mm, and three absolute volume ratios of paste to aggregate of 30, 40 and 50 percent for a given size of aggregate were used. For the compressive strength, the concrete with the aggregate size of 5-10mm showed much higher strength than that with the aggregate size of 10-20mm. But, the compressive strength is higher when the ratio of paste to aggregate is smaller. In the water purification experiment, the amount of attached an organism on the porous concrete surface indirectly is examined by measuring the consumption of the Dissolved Oxygen (DO). The ability of the water purification is evaluated by the removal amount of the Total Phosphorus(T-P) and Total Nitrogen(T-N). The ability of the removal of the T-N and T-P in the test water is superior to a porous concrete with a smaller size of aggregate and a higher void content. These results are owing to a large specific surface area of the specimen. As a result, porous concrete using by-products has sufficient performance of water purification.

  • PDF

랜덤입사방법에 의한 포러스 콘크리트의 흡음특성에 관한 실험적 연구 (The Study on Sound Absorbing Characteristics of Porous Concrete according to Reverberation Room Methods)

  • 서대석;박승범;조광연;장영일;김형석;이윤선
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.568-571
    • /
    • 2004
  • This research estimated the physical. mechanical characteristic and the character of sound absorption according to target void ratio of porous concrete and the mixing ratio of recycled aggregate for the valid utilization of recycled aggregate using waste concrete and sound reduction out of a road, a railway, a residential street, and a downtown area. As a result of the test, compressive strength tended to be a radical strength fall when target void ratio was $25\%$ and contents of recycled aggregate exceeded over $50\%$. Also, the character of sound absorption of porous concrete which used recycled aggregate using waste concrete was the most excellent when target void ratio was $25\%$, and the influence by contents of recycled aggregate was trivial. Therefore, when the strength and the character of sound absorption of porous concrete are considered, it is proved valid that proper target void ratio was $25\%$ and contents of recycled aggregate using waste concrete was $50\%$ or so.

  • PDF

섬유보강 포러스 콘크리트의 공극률과 투수계수 특성에 관한 연구 (A Study on the Void Ratio and Permeability Coefficient Properties of fiber Reinforced Porous Concrete)

  • 김정환;조광연;이준;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.677-682
    • /
    • 2000
  • Porous concrete is defined as d type of concrete for which the fine aggregate component the matrix is entirely omitted. Although it had been used as a building material in Europe for over 60 years, low strength and high void ratio limited its application in the past. In recent years, however high void ratio of concrete has been recognized again and can be used as an environmental conscious material, for example, parking lots, draining light-traffic-volume pavements and as sea water purifying material. The result of an experiment on the void ratio of fiber reinforced porous concrete and its influence on the compressive strength and permeability relationship of concrete are reported in this paper. One-sized coarse aggregate of 5-10mm, and three absolute content of fiber(steel fiber, polyprophylen fiber) were used. The result of measured void ratio, permeability coefficient and compressive strength show a small variation. Void ratio, permeability coefficient and compressive strength of fiber reinforced porous concrete depend on contents of fiber and absolute volume ratios of paste to aggregate.

  • PDF

환경친화 식생용 포러스콘크리트의 현장적용성에 관한 연구 (A Study on the Filed Application of Environmental Friendly Porous Concrete For Planting)

  • 김정환;이남익;이용희;권혁준;이준;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.769-772
    • /
    • 2005
  • The river environments of many streams in korea have been deteriorate through the rapid industrialization and urbanization since the 1960s. In Germany and Japan, on the other hand, much efforts on the research and project have been made for the restoration of the deteriorated streams to close-to-nature. in order to restore the deteriorated streams, therefore, it is necessary to investigate such advanced technologies and materials. In view of this requirement, various research paths are being taken focusing on coarse aggregates to make multi-functional porous concrete having continuous voids so as to improve water and air permeability, acoustic absorption, water purification, and applicability to vegetation. The Purpose of this study is to investigate the method for recovery of the environment in the streams area using porous concrete block. the porous concrete block applies for test in the cheonggae-cheon have been monitored planting during six month. after 6 months, plant grows flourishing and reconstructed in state such as nature rivers.

  • PDF