• Title/Summary/Keyword: 입도조정

Search Result 61, Processing Time 0.035 seconds

A Study on the Electrical and Physical Properties of Cement Mortar used Carbon Material Industrial by-product (탄소소재 산업부산물을 사용한 시멘트 모르타르의 전기·물리적 특성 연구)

  • Jo, Jeong-Hoon;Kim, Nam-Il;Lee, Young-Jun;Seo, Sung-Kwan;Chu, Yong-Sik
    • Resources Recycling
    • /
    • v.30 no.6
    • /
    • pp.19-27
    • /
    • 2021
  • Electrically conductive mortar used in industrial carbon material byproducts was manufactured and analyzed in this study. The contents of the carbon material and mixed water were controlled, and the distance between electrodes was set to 0.42 m and 0.88 m. The carbon material was graphite with a layered structure. The carbon material was used as fine powder and aggregate substitutes according to particle size. The average particle sizes of each materials were 18.4㎛ and 546.1 ㎛ and the electrical conductivities were 62.3 S/m and 32.5 S/m, respectively. To maintain similar mortar flow in each sample, the water content was increased with increasing carbon material, and accordingly, the porosity showed an increasing trend. When electrode distance of the mortar (week 6) was 0.42 m, the voltage-current values were 342 V-1.48 A (S20) and 349 V-1.44 A (S30). For electrode distance of 0.88 m, these values were 513 V-0.98 A (S20) and 500 V-1.01 A (S30). The exothermic properties improved with increasing carbon material content and decreasing electrode distance.

Characterization of relationship between particle size and powder properties for $BaTiO_3$ ($BaTiO_3$의 입도와 분체특성과의 상관 관계 연구)

  • Chun, M.P.;Cho, J.H.;Kim, B.I.
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.6
    • /
    • pp.244-251
    • /
    • 2005
  • The relationship between particle size of hydro-thermally synthesized barium titanate powders (BT01, BT02, BT03, BT04, BT05) and the powder properties was investigated by means of particle size, specific surface area, zeta potential, XPS, XRD and SEM. Particle size determined by laser light scattering is closely related with specific surface area and the tetragonality (c/a) obtained from XRD. The specific surface area of the samples inversely decreased with increasing particle size except BT03 powder. BT03 sample showed higher surface area than BT04 sample of equivalent particle size, which was attributed mostly to the agglomeration of particles in terms of SEM image and XRD analysis. Zeta potential increased with increasing particle size with the exception of BT02 and BT03 which showed larger minus value of zeta potential in comparison with other BT powders. Beta potential results of BT02 and BT03 are considered to be related with the dissolution of $Ba^{2+}$ ion in these powers which was examined by XPS.

Experimental Study on Long-Term Performance Evaluation of Geosynthetic Strip Reinforcement (띠형 섬유보강재의 장기성능 평가를 위한 실험적 연구)

  • Lee, Kwang-Wu;Kim, Ju-Hyeung;Cho, Sam-Deok;Han, Jung-Geun;Yoon, Won-Il;Hong, Ki-Kwon
    • Journal of the Korean Geosynthetics Society
    • /
    • v.9 no.4
    • /
    • pp.75-84
    • /
    • 2010
  • In this study, the long-term performance tests, which have extensibility, creep deformation, installation resistance and durability characteristic, is conducted to apply geosynthetic strip in field. The strength reduction factors using the test results are evaluated in order to calculate long-term design tensile strength. First, the creep deformation was evaluated by both the stepped isothermal method(SIM) and the time-temperature superposition(TTS) method. The creep reduction factor is reasonable to apply 1.6. Second, the result of installation damage test had little damage of yarn, which affected strength of reinforcement. Therefore, it can be analyzed that the installation damage of geosynthetic strip has little effect of long-term design tensile strength. Finally, the durability reduction factor considering chemical, biological and outdoor exposure resistance is reasonable to apply 1.1, which is considered the stability and economic efficiency of reinforced earth wall using geosynthetic strip.

  • PDF

하이브리드 이산화티탄의 자기조직체 형성공법을 이용하여 제조된 하이브리드 이산화티탄의 자외선차단 상승효과

  • Jo, Hyeon-Dae
    • Ceramist
    • /
    • v.19 no.3
    • /
    • pp.26-35
    • /
    • 2016
  • The purpose of this study is to find the optimum conditions for manufacturing titanium dioxide using a hybrid self-assembly forming method, to confirm the shape, properties and synergy effect of UV protection for hybrid titanium dioxide. Hybrid titanium dioxide, manufactured by forming self-assembly of different sizes consisting of two kinds of titanium dioxides, has micro titanium dioxide (250nm~300nm) for support material, Nano titanium dioxide (20~30nm) for surface material, coating support material. Adjustment experiments of $AlCl_3$ concentration and both titanium dioxide ratio were conducted to find the optimized conditions for the surface coating of titanium dioxide striking a negative charge, a sample made of the optimized process was confirmed through an optical analysis, particle size analysis, and potentiometric analysis. The SPF in-vitro value of the cosmetics samples containing hybrid titanium dioxide showed 15~30% higher levels than the cosmetics samples containing both titanium dioxides mixture.

Blast Design for Improvement of Limestone Fragmentation (석회석 파쇄도 향상을 위한 발파 설계)

  • Piyush, Rai;Yang, Hyung-Sik
    • Explosives and Blasting
    • /
    • v.28 no.1
    • /
    • pp.19-26
    • /
    • 2010
  • The paper presents a case study of a limestone quarry of the Philippines, where major problems in terms of improper fragmentation, poor wall control, and poor heave of the muck pile were witnessed. The paper highlights the significant role of switching over from diagonal firing pattern to V-type firing pattern, and also of making suitable adjustments in the stemming column length for improved confinement and gas retention. The study revealed that by making aforesaid design modifications in the blast round, marked improvement in blasting results was registered. Looking at the results, it was further contemplated to expand the mesh area in the subsequent blast rounds. The mesh area was incremented from the existing $8.96m^2$ to $12m^2$. The results were meticulously registered in the field, and clearly depicted definite improvements in the blast results in terms of increased P.F., reduced boulder count, reduced FEL cycle time, reduced dozing hours and improved heave.

Effects of Crystallite Size on Gas Sensitivity and Surface Property of Oxide Semiconductor (산화물 반도체의 결정입도가 가스감도와 표면특성에 미치는 영향)

  • Song, Guk-Hyeon;Park, Sun-Ja
    • Korean Journal of Materials Research
    • /
    • v.3 no.4
    • /
    • pp.319-326
    • /
    • 1993
  • The effects of $SnO_2$ crystallite size on the powder characteristics, the resistance in air and the sensitivity to 0.5 vol % $H_2$, CO-air mixture were observed. The size of SnO, powder was controlled by calcining temperature variation ($500^{\circ}C$ ~$1100^{\circ}C$) of $\alpha$-stannic acid fabricated from $SnCl_4 \cdot xH_2O$. Its crystallite size. evaluated from TEM image, was in the range of 8-54nm. With the reduction of crystallite size, the adsoption peak of $H_2O$ on FTIR curve became more clear while the lattice parameters were invariable. As the crystallite size decreased, with elements of thick film, the temperatures showing a minimum resistance in air and a maximum sensitivity to H, gas reduced. The temperature variations were assigned to the changes of activation energy of the active adsorbates, and it was suggested that the decrease of activation energy can be one of the reasons for the' sensitivity increase with the' fine powder.

  • PDF

Permeability Variation With Lift Thickness of Asphalt Pavement (아스팔트 포장의 시공 포설두께에 따른 투수계수 변화특성)

  • Park, Sang Hyun;Moon, Jun Ho;Bae, Seok Il;Kim, Young Uk
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.3
    • /
    • pp.2229-2233
    • /
    • 2015
  • The permeability of HMA(hot mixed asphalt) is a major influencing factor for long-term performance of the pavement. Especially, the lift thickness of the pavement during construction causes a wide range of physical properties of HMA. This study investigates the correlationship between the lift thickness and the physical properties of HMA through a series of laboratory experiments. The specimens were cored from a construction site of the dense graded asphalt pavement. The cored samples have various lift thickness and the number of compaction for the study. The results of the study show that the permeability of the sample decreases with the apperant density and t/NMAS, and the air void ratio. Therefore, the commonly used construction method as a constant lift thickness regardless of conditions needs to be reconsidered.

Policy System of Data Access Control for Web Service (웹 서비스를 위한 데이터 접근 제어의 정책 시스템)

  • Jo, Sun-Moon;Chung, Kyung-Yong
    • The Journal of the Korea Contents Association
    • /
    • v.8 no.11
    • /
    • pp.25-32
    • /
    • 2008
  • Access control techniques should be flexible enough to support all protection granularity levels. Since access control policies are very likely to be specified in relation to document types, it is necessary to properly manage a situation in which documents fail to be dealt with by the existing access control policies. In terms of XML documents, it is necessary to describe policies more flexibly beyond simple authorization and to consider access control methods which can be selected. This paper describes and designs the access control policy system for authorization for XML document access and for efficient management to suggest a way to use the capacity of XML itself. The system in this paper is primarily characterized by consideration of who would exercise what access privileges on a specific XML document and by good adjustment of organization-wide demands from a policy manager and a single document writer.

Synergy Effect of Sun Protection Factor Using Method of Forming Self-Assembly of Hybrid Titanium Dioxide (하이브리드 이산화티탄의 자기조직체 형성공법을 이용하여 제조된 하이브리드 이산화티탄의 자외선차단 상승효과)

  • Cho, Hyun Dae;Park, Soo Nam
    • Journal of the Korean Applied Science and Technology
    • /
    • v.31 no.4
    • /
    • pp.748-758
    • /
    • 2014
  • The purpose of this study is to find the optimum conditions for manufacturing titanium dioxide using a hybrid self-assembly forming method, to confirm the shape, properties and synergy effect of UV protection for hybrid titanium dioxide. Hybrid titanium dioxide, manufactured by forming self-assembly of different sizes consisting of two kinds of titanium dioxides, has micro titanium dioxide (250nm~300nm) for support material, Nano titanium dioxide (20~30nm) for surface material, coating support material. Adjustment experiments of $AlCl_3$ concentration and both titanium dioxide ratio were conducted to find the optimized conditions for the surface coating of titanium dioxide striking a negative charge, a sample made of the optimized process was confirmed through an optical analysis, particle size analysis, and potentiometric analysis. The SPF in-vitro value of the cosmetics samples containing hybrid titanium dioxide showed 15~30% higher levels than the cosmetics samples containing both titanium dioxides mixture.

Mechanical Characteristics of Porous Concrete using Recycled-Aggregate (순환골재를 이용한 투수성 콘크리트의 역학특성)

  • You, Seung-Kyong;Yu, Nam-Jae;Cho, Sung-Min;Shim, Min-Bo
    • Journal of the Korean Geosynthetics Society
    • /
    • v.6 no.2
    • /
    • pp.17-20
    • /
    • 2007
  • In this study, a series of uniaxial unconfined compression test and constant-head test were performed to investigate the mechanical characteristics of porous concrete using recycled-aggregate for the varying unit weight and water-cement ratio. To enhance the permeability of the porous concrete, the recycled-aggregate with similar grain size in the range of $40{\pm}5mm$ was used and water-cement ratio that leads to the lean-mix was adapted. The mechanical characteristics of the porous concrete cured for 3 days were examined; the compressive strength and $E_{50}$ showed their maximum values with 40% water-cement ratio and $1.8t/m^3$ unit weight and the permeability coefficient was averagely measured in the range of $0.9{\times}10^0cm/sec$ regardless of water-cement ratio and unit weight.

  • PDF