• 제목/요약/키워드: 열사이클

검색결과 35건 처리시간 0.021초

Cu-Zn-AI 형상기억 합금의 열사이클에 따른 집합조직의 변화에 관한 연구 (A Study on Change of Texture During Thermal Cycling in Cu-Zn-AI Shape Memory Alloy)

  • 홍대원;박영구
    • 열처리공학회지
    • /
    • 제5권3호
    • /
    • pp.179-185
    • /
    • 1992
  • The shape memory effect results from the martensite transfomation of each individual grain. Thus it is necessary to study the texture and its variation. In this study the change of texture during thermal cycling and it's effect on shape memory ability are investigated. The major component of the rolling texture in the parent phase is identified (001) [110], and minor components are (112) [110], (111) [112], {hkl}<100> fiber texture is developed at $45^{\circ}$ from rolling direction. In the case of martensite phase, it is estimated that the major component is (011) [100] and the minor components are (105) [501], (010) [101] and (100) [001]. According to thermal cycling. severity of texture, especially (001) [110] component in parent phase and (011) [100] component in martensite phase are increased. The shape memory ability is increased with increase of thermal cycles and also increased as the direction of specimen approach to $45^{\circ}$ from rolling direction. After first thermal cycling the temperature of transformation can be define clearly and Ms and As are raised by thermal cycling.

  • PDF

153 FC-BGA에서 솔더접합부의 신뢰성 향상에 관한 연구 (A Study on the Improvement of Solder Joint Reliability for 153 FC-BGA)

  • 장의구;김남훈;유정희;김경섭
    • 마이크로전자및패키징학회지
    • /
    • 제9권3호
    • /
    • pp.31-36
    • /
    • 2002
  • PBGA에 비해 상대적으로 큰 칩을 실장하는 고속 SRAM용 153 FC-BGA을 대상으로 2차 솔더접합부의 신뢰성을 평가하였다. 실험은 열사이클 시험에서 발생하는 단면과 양면 실장, 패키지 구조, 언더 필 재료, 기판의 종류와 두께, 솔더 볼의 크기에 따른 영향을 분석하였다. BT기판의 두께가 0.95mm에서 1.20mm로 증가하고, 낮은 영률 의 언더 필 재료에서 솔더접합부의 피로 수명이 30% 향상됨을 확인하였다. 또한 솔더 볼의 크기가 0.76 mm에서 0.89mm로 증가하면, 솔더접합부에서 균열에 대한 저항성은 2배 정도 증가하였다.

  • PDF

동결/해동 열사이클이 PEFC의 GDL/MEA에 미치는 영향 (Freeze/Thaw cycle effects on GDLs and MEAs of PEFC)

  • 임남윤;박구곤;박진수;윤영기;이원용;임태원;김창수
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2006년도 춘계학술대회
    • /
    • pp.96-98
    • /
    • 2006
  • Proper water management is vital to achieve high performance and durability of PEFC (Polymer Electrolyte Fuel Cell). The effects of the residual water from PEFC after purge in shut-down processes on GDL/MEAs were investigated with freeze/thaw cycles Freeze/thaw cycle tests were conducted with single cells which were designed from transparent acryl plates. Single cells which contain several amount of residual water were cycles from $80^{\circ}C$ to $-28^{\circ}C$. The resistance changes of the single cells which have various amount of residual water were evaluated by ac-impedance analysis with 24 times of freeze/thaw cycles. Also, after the freeze/thaw cycles, the property changes were characterized by visual methods such as SEM, EPMA. Though it was difficult to observe noticeable property changes in the visual characterizations, the resistance of cells dramatically increased with the amount of remained water.

  • PDF

알루미나 시멘트에 기반한 복합재료의 열역학적 특성 (Thermal and Mechanical Properties of Alumina Cementitious Composite Materials)

  • 양인환;이정환;최영철
    • 한국건설순환자원학회논문집
    • /
    • 제3권3호
    • /
    • pp.199-205
    • /
    • 2015
  • 이 연구에서는 고온의 축열재료로 사용하기 위한 알루미나 시멘트 복합재료의 역학적 및 열적 특성을 파악하고자 하였다. 알루미나 시멘트를 기본 바인더로 하고 플라이애시, 실리카퓸, CSA (calcium sulfo-aluminate) 및 그라파이트의 치환에 따른 고온에서의 물성을 파악하였다. 알루미나 시멘트 기반 복합재료의 역학적 특성으로서 열사이클 전과 후의 압축강도 및 인장강도를 측정하였다. 또한, 복합재료의 열적 특성으로서 열전도율과 비열을 측정하였다. 열사이클링 적용 이후의 잔류압축강도 측정결과, 알루미나 시멘트만을 사용한 배합과 알루미나 시멘트를 실리카퓸으로 치환한 배합의 압축강도가 크게 나타나며, 이 두 배합의 잔류강도 비는 65%를 상회한다. 그라파이트를 혼합한 복합재료의 비열이 가장 크고 이는 그라파이트의 비열이 크기 때문이다. 연구결과는 콘크리트를 고온조건에서의 축열매체로 활용하기 위한 실제적인 기초실험 자료로 활용될 수 있을 것으로 사료된다.

고체산화물 연료전지의 Samarium Oxide 혼합 공기극에 대한 열특성 분석 (Thermal Characteristics of Samarium-based Composite Cathode ($Sm_{0.5}Sr_{0.5}CoO_{3-\delta}/ Sm_{0.2}Ce_{0.8}O_{1.9}$) for Intermediate Temperature-operating Solid Oxide Fuel Cell)

  • 백승욱;배중면
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회B
    • /
    • pp.2021-2025
    • /
    • 2007
  • Performance of single cell at solid oxide fuel cell (SOFC) system is largely affected by electrocatalytic and thermal properties of cathode. Samarium-based perovskite oxide material is recently recognized as promising cathode material for intermediate temperature-operating SOFC due to its high electrocatalytic property. Perovskite structured $Sm_{0.5}Sr_{0.5}CoO_{3-\delta}$ and its composite material, $Sm_{0.5}Sr_{0.5}CoO_{3-\delta}/Sm_{0.2}Ce_{0.8}O_{1.9}$ were investigated in terms of area specific resistance (ASR), thermal expansion coefficient (TEC), thermal cycling and long term performance. $Sm_{0.2}Ce_{0.8}O_{1.9}$ was used as electrolyte material. Electrochemical ac impedance spectroscopy (EIS) and dilatometer were used to measure the cathodic properties. Composite cathode ($Sm_{0.5}Sr_{0.5}CoO_{3-\delta}$: $Sm_{0.2}Ce_{0.8}O_{1.9}$ = 6:4) showed a good ASR of 0.13${\Omega}$ $cm^2$ at 650$^{\circ}C$ and its TEC value was 12.3${\times}$10-6/K at 600$^{\circ}C$ which is similar to the value of ceria-based electrolyte of 11.9${\times}$10-6/K. Performance of composite cathode was maintained with no degradation even after 13 times thermal cycle test.

  • PDF

모아레 간섭계와 모델교정법을 이용한 솔더 합금의 점소성 물성치 역추정 (Inverse Estimation of Viscoplastic Properties of Solder Alloy Using Moir$\acute{e}$ Interferometry and Computer Model Calibration)

  • 강진혁;이봉희;주진원;최주호
    • 한국전산구조공학회논문집
    • /
    • 제24권1호
    • /
    • pp.97-106
    • /
    • 2011
  • 본 연구에서는 전자패키지에 사용되는 솔더 재료의 점소성 물성치를 규명하였다. 이를 위해 전자패키지와 비슷한 변형을 보이는 시편을 제작하였고 모아레 간섭계를 이용하여 열사이클 하에서의 변형을 측정한 뒤 시편의 굽힘 변위와 솔더의 전단 변형률을 구하였다. 시편에 대해 점소성 유한요소해석을 실시하였고 해석 결과가 실험 결과에 일치하도록 물성치를 역으로 추정하였다. 실험에서 발생한 측정오차와 실험횟수 부족 등의 불확실성을 고려하기 위해 컴퓨터 모델 교정법을 이용하였고, 그 결과 추정된 물성치는 평균 및 신뢰구간으로 표현되었으며, 이로 인한 유한요소해석 결과도 마찬가지로 평균 및 신뢰구간으로 표현되었다.

[$CO_2$] 용접이음재의 대기 및 해수중에서의 회전굽힘 피로강도에 관한 연구 (A Study on Rotary Bending Fatigue Strength of the $CO_2$ Gas Welded Joint in Air and Sea Water)

  • 강성원;이승윤
    • 대한조선학회논문집
    • /
    • 제37권2호
    • /
    • pp.118-126
    • /
    • 2000
  • 용접이음재에서는 용착금속, 열영항부 및 모재가 열사이클 및 조직의 변화에 의하여 각종 기계적 성질의 차이가 있으며, 특히 부식환경에서는 이들의 영향이 현저하게 나타나는 경우가 많다. 또 용접이음재의 피로강도는 이음형식, 용접금속 및 열영향부의 특성, 사용환경과 응력의 종류에 따라 변화한다. 따라서 본 연구에서는 현재 선박 및 해양구조물의 건조에 많이 채용되고 있는 TMCP 강재의 $CO_2$ 가스 용접이음재의 열영향부에 대한 대기중 및 부식환경중에서의 회전굽힘피로시험을 실시하여 피로균열의 발생 및 성장거동을 조사 검토하였다. 또한 대기중의 피로강도와 부식환경중의 피로강도를 비교함으로써 부식효과 및 응력집중효과 등을 고려한 용접이음재의 부식환경중에서의 피로강도 평가법 및 피로강도 설계곡선을 검토하였다.

  • PDF

가스터빈 단결정 블레이드 사용품의 특성변화 (Changes in Material Properties of Used Gas Turbine Blade Made of Single- Crystal Superalloy)

  • 유근봉;이한상;송규소;이규호
    • 대한기계학회논문집A
    • /
    • 제34권12호
    • /
    • pp.1909-1915
    • /
    • 2010
  • 고온의 연소가스에서 운전되는 국내 가스터빈 부품들은 매일 기동정지를 반복함으로써 열사이클에 의해 재료특성에 변화가 발생한다. 최근 많은 가스터빈 고온부품들이 단결정 초내열 합금으로 제작되어 지지만 재료열화 예측을 통한 부품 교체와 정비에 대한 기준이 없어서 대부분 제작사에 의존하고 있는 실정이다. 본 연구에서는 향후 수명평가와 손상분석의 기초자료로 활용하기 위해 실제 운전된 가스터빈 1 단 블레이드의 열화상태를 조사하였다. 사용한 블레이드는 25,000 및 52,000 의 등가운전시간(EOH : Equivalent Operating Hour)을 가졌으며, 재질은 단결정 초내열합금인 CMSX-4 이다. 사용된 블레이드에서 직접 시험편을 채취하여 기계적특성 시험 및 미세조직을 관찰하였다.

고로슬래그 혼입 콘크리트의 고온 조건에서의 열역학 성능 (Thermal Characteristics of Concrete Fabricated with Blast Furnace Slag Subjected to Thermal Cycling Condition)

  • 양인환;박지훈
    • 한국건설순환자원학회논문집
    • /
    • 제5권4호
    • /
    • pp.414-420
    • /
    • 2017
  • 이 연구에서는 고온의 태양열 에너지를 저장하기 위한 고로슬래그 콘크리트의 열역학적 특성을 파악하였다. 고로슬래그 콘크리트의 열역학적 특성에 미치는 영향을 파악하기 위한 실험연구를 수행하였다. 실험변수로써 고로슬래그 함유량과 물-바인더 비를 고려하였다. 고로슬래그 콘크리트의 역학적 특성으로써 열사이클 전과 후의 압축강도 및 인장강도를 측정하고, 열적 특성으로써 열전도율과 비열을 측정하였다. 고로슬래그를 포함한 콘크리트의 열싸이클 적용 후의 잔류압축강도가 고로슬래그를 포함하지 않은 콘크리트의 잔류압축강도보다 크다. 또한, 고로슬래그를 혼입한 콘크리트의 열전도율이 고로슬래그를 포함하지 않은 콘크리트의 열전도율보다 더욱 크다. 이는 고로슬래그 콘크리트가 열에너지의 축열과 방열에 효과적인 것을 나타낸다. 실험연구 결과는 콘크리트 열저장 축열 모듈 설계에 효율적으로 활용될 수 있다.

세라믹/금속접합재의 고온 열사이클에 따른 잔류응력분포 및 굽힘강도 특성 (Characteristics of bending strength and residual stress distribution on high thermal cycle of ceramic and metal joint)

  • 박영철;허선철;부명환;김현수;강재욱
    • 대한기계학회논문집A
    • /
    • 제21권10호
    • /
    • pp.1541-1550
    • /
    • 1997
  • Since the ceramic/metal joint material is made at a high temperature, the residual stress develops when it is cooled from bonding temperature to room temperature due to remarkable difference of thermal expansion coefficient between ceramic and metal. As residual stress at ceramic/metal joints influences the strength of joints, it is important to estimate residual stress quantitatively. In this study, it is attempted to estimate joint residual stress of Si$_3$N$_4$STS304 joints quantitatively and to compare the strength of joints. The difference of residual stress is measured when repeated thermal cycl is loaded, under the conditions of the practical use of the ceramic/metal joint. The residual stress increases at 1 cycle of thermal load but decreases in 3 cycles to 10 cycles of thermal load. And 4-point bending test is performed to examine the influence of residual stress on fracture strength. As a result, it is known that the stress of joint decreases as the number of thermal cycle increases.