Practical Application of GGBS-Based Alkali-Activated Binder to Secondary Products of Concrete (고로슬래그 기반 알카리 활성 결합재의 콘크리트 2차 제품 적용성 평가)

  • Sim, Jae-Il;Yang, Keun-Hyeok
    • Journal of the Korea Institute of Building Construction
    • /
    • v.10 no.5
    • /
    • pp.37-44
    • /
    • 2010
  • This study examined the practical application of ground granulated blast-furnace slag (GGBS) based alkali-activated (AA) binders for the development of cementless environmental-friendly secondary products of concrete, such as brick, shore protection blocks and interlocking blocks. The addition amount and type of alkaline ion to activate GGBS varied according to the diverse qualities of the secondary products of concrete required in Korean industrial standards (KS) and other specifications. Test results showed that the secondary products of concrete using GGBS-based AA binders surpassed the demanded capacities of KS and other specifications. In addition, shore protection block had a pH value close to neutral, enabling an advantageous environment for marine life. Therefore, the GGBS-based AA binders can be effectively applied to develop eco-friendly secondary products of concrete with reduced $CO_2$.

Evaluation of Flexural Performance of Eco-Friendly Alkali-Activated Slag Fiber Reinforced Concrete Beams Using Sodium Activator (나트륨계 알칼리 활성화제를 사용한 친환경 알카리활성 슬래그 섬유보강콘크리트 보의 휨성능 평가)

  • Ha, Gee-Joo;Yi, Dong-Ryul;Ha, Jae-Hoon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.2
    • /
    • pp.170-178
    • /
    • 2015
  • In this study, it was developed eco-friendly alkali-activated slag fiber reinforced concrete using ground granulated blast furnace slag, alkali activator (water glass, sodium hydroxides), and steel fiber. Eight reinforced concrete beam using alkali-activated slag concrete were constructed and tested under monotonic loading. The major variables were mixture ratio of alkali activator, mixed/without of steel fiber. Experimental programs were carried out to improve and evaluate the flexural performance of such test specimens, such as the load-displacement, the failure mode, the maximum load carrying capacity, and ductility capacity. All the specimens were modeled in scale-down size. The reinforced concrete beams using the eco-friendly alkali-activated slag fiber reinforced concrete was failed by the flexure or flexure-shear in general. In addition, the maximum strength increased with the adding the mol of sodium hydroxide, and the specimen reinforced the steel fiber showed the value of maximum strength which is increased by 15.8% through 25.9%. It is thought that eco-friendly alkali-activated slag fiber reinforced concrete can be used with construction material and product to replace normal concrete. If there is applied to structures such as precast concrete member and production of 2nd concrete product, it could be improved the productivity and reduction of construction duration etc.

Quality Characteristics and Environmental Impact Assessment of Alkali-Activated Foamed Concrete (알카리활성 기포콘크리트의 품질특성 및 환경영향 평가)

  • Yang, Keun-Hyeok;Yoo, Sung-Won;Lee, Hyun-Ho;Kim, Sang-Chel
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.1 no.2
    • /
    • pp.114-119
    • /
    • 2013
  • The present study tested 5 concrete mixes to develop reliable mixing proportions for the sustainable alkali-activated(AA) foamed concrete as a thermal insulation material for the floor heating system of buildings. The AA binder used was composed of 73.5% ground granulated blast-furnace slag, 15% fly ash, 5% calcium hydroxide, and 6.5% sodium silicate. As a main variable, the unit binder content varied from $325kg/m^3$ to $425kg/m^3$ at a space of $25kg/m^3$. The test results revealed that AA foamed concrete has considerable potential for practical applications when the unit binder content is close to $375kg/m^3$, which achieves the minimum quality requirements specified in KS F 4039 and ensures economic efficiency. In addition, lifecycle assessment demonstrated the reduction in the environmental impact profiles of all specimens relative to typical ordinary portland cement foamed concrete as follows: 99% for photochemical oxidation potential, 87~89% for global warming potential, 78~82% for abiotic depletion, and 70~75% for both acidification potential and human toxicity.

석탄 촤-수증기 가스화반응에서 알카리 금속염과 전이금속염 혼합물의 촉매활성

  • 이운재;김상돈
    • Proceedings of the Korea Society for Energy Engineering kosee Conference
    • /
    • 1994.05a
    • /
    • pp.9-14
    • /
    • 1994
  • 알카리금속염 (K$_2$CO$_3$, $K_2$SO$_4$). 알카리 토금속염 (Ba(NO$_3$)$_2$), 철족금속염(Ni(NO$_3$)$_2$, FeSO$_4$) 으로 이루어진 여러가지 혼합물들이 반응온도 700~85$0^{\circ}C$ 하의 촤-수증기 가스화반응에서 나타내는 촉매활성을 열천칭 반응기를 사용하여 측정하였다. 비촉매 가스화반응에서 초기반응성은 수증기 분압에 비례하였다. 촉매 가스화반응에서 단일염 촉매의 경우 $K_2$CO$_3$ 가 가장 큰 활성을 나타내었으며, 다른 염들은 낮은 활성을 보였다. 혼합염의 경우 $K_2$SO$_4$에 철족염을 부가함에 따라 반응속도가 향상되었으며, $K_2$SO$_4$+Ni(NO$_3$)$_2$가 가장 큰 촉매활성을 나타내었다. $K_2$SO$_4$와 Ni(NO$_3$)$_2$ 의 촉매 활성은 담지량에 따라 증가하며, 석탄의 등급에 따라 감소하였다. $K_2$SO$_4$와 Ni(NO$_3$)$_2$의 혼합비는 같은 몰비로 혼합하였을때 가장 큰 활성을 나타내었다.

  • PDF

Resistance to Freezing and Thawing of Alkali-Activated Slag Concrete (알카리활성 슬래그 콘크리트의 동결융해 저항성)

  • Mun, Jae-Sung;Cho, Ah-Ram;Sim, Jae-Il;Yang, Keun-Hyeok
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2011.11a
    • /
    • pp.105-106
    • /
    • 2011
  • The present tests examined the resistance to freezing and thawing of alkail-activated (AA) slag concrete having compressive strength between 30~56 MPa. To enhance the compressive strength and resistance to freezing and thawing of AA slag concrete, Na ions were used for an activator. Test results revealed that the resistance to freezing and thawing of AA slag concrete is comparable to that of cement concrete when compressive strength is more than 50 MPa.

  • PDF

Postmorten Changes in the Myofibrillar Proteins of Alkaline and Acid Rigor Rabbit Muscle during Storage (사후강직형태에 따른 근원섬유 단백질의 이화학적 성질변화)

  • Kim, Dae-Gon;Sung, Sam-Kyung
    • Journal of the Korean Society of Food Science and Nutrition
    • /
    • v.21 no.6
    • /
    • pp.712-718
    • /
    • 1992
  • This experiment was carried out to investigate some physico-chemical properties of myofibrillar proteins isolated from alkaline and acid rigor muscles of rabbit. The degree of fragmentation was about 0.35 at 3 days of postmortem in acid rigor muscle fiber, whereas it was only 0.3 at 7 days of postmortem in alkaline rigormuscle fiber. $Mg^{2+}$-activated ATPase activities of actomyosin were increased to the highest level at 1st day in acid rigor and at 3rd day in alkaline rigor muscle fiber. $Ca^{2+}$-activated ATPase activities of actomyosin were slightly increased at postmortem. $Mg^{2+}$-, and $Ca^{2+}$-activated ATPase activities were higher in alkaline rigor muscle than those in acid rigor muscle at postmortem. Solubility of actomyosin increased with postmortem but no differences were observed in rigor types. SDS-PAGE(sodium dodecyl sulfate polyacrylamide gel electrophoresis) band patterns of myofibrils did not show significant differences between rigor types, but newly 30.000 dalton proteins were appeared at 3 day postmortem in both rigor types.

  • PDF

Physiological properties and transformation of alkaline-tolerant bacteria (알카리내성 세균의 생리적 특성 및 형질전환)

  • 유주현;정용준;정건섭;오두환
    • Microbiology and Biotechnology Letters
    • /
    • v.14 no.3
    • /
    • pp.239-244
    • /
    • 1986
  • To develop the potential use as new host strain for gene cloning, alkaline-tolerant isolates from soil were examined for amylase activity, protease activity, antimicrobial activity and transformability by using plasmid pUB 110. Of these strains, one was selected and identified as Bacillus sp. YA-14. in the enzymatic properties of Bacillus sp. YA-14 the optimal conditions for the reaction of amylase and protease were at pH 0.8 and pH 7.5 respectively. The antimicrobial activity of Bacillus sp. YA-14 was also found. For the transformation, Bacillus sp. YA-14 was cultured to late logarithmic growth phase ai 37$^{\circ}C$ in modified SPI medium (pH 8.0) containing 0.4% MgSO$_4$. The presence of pUB 110 plasmid DNA in transformants was confirmed by electrophoresis and stably maintained in the new host.

  • PDF

Cloning of Promoters from Alkali-tolerant Bacillus sp. (알카리 내성 Bacillus속 Promoter의 Cloning)

  • 유주현;구본탁;공인수;정용준;박영서
    • Microbiology and Biotechnology Letters
    • /
    • v.16 no.2
    • /
    • pp.126-130
    • /
    • 1988
  • Promoters of an alkali-tolerant Bacillus sp. isolated from soil have been cloned in Bacillus subtilis using promoter probe vector pPL703. The CAT specific activity of a clone harboring the strongest promoter activity among these transformants was 8.01. This activity was 2.5 times higher than that of Bacillus subtilis harboring expression vector pPL708 and was increased after the end of the logarithmic growth phase. In the 2.8kb of inserted DNA fragment, BamHI and Sal I recognition sites were located.

  • PDF

Antioxidant and anticariogenic activities of enzymatic hydrolysate from spent coffee grounds (커피박 효소분해물의 항산화 및 항충치균 활성)

  • Man-Jin In;Yu Min Jang;Min Young Jo;Hee Jeong Kim;Dong Chung Kim
    • Journal of Applied Biological Chemistry
    • /
    • v.66
    • /
    • pp.462-466
    • /
    • 2023
  • After treating spent coffee grounds with alkali, extracts were prepared by using Viscozyme and Alcalase, respectively. Treatment of spent coffee grounds with alkali and enzymes increased the content of phenolic compounds in the extracts, thus possessing the good scavenging activities on free and cation radicals. In particular, the extract obtained by continuous treatment with alkali and Alcalase on spent coffee grounds had the best content of phenolic compounds and antioxidant activity, and inhibited the growth of Streptococcus mutans in proportion to the concentration. In conclusion, the Alcalase-enzymatic hydrolysate of alkali-treated spent coffee grounds showed excellent antioxidant and anticariogenic effects.

Expression of Developmentally Regulated Promoter of Alkali-tolerant Bacillus sp. YA-I4 (알칼리 내성 Bacillus sp. YA-14에서 유래된 생육단계 조절 promoter의 발현)

  • 박영서;구본탁;박희경;유주현;김진만
    • Microbiology and Biotechnology Letters
    • /
    • v.18 no.4
    • /
    • pp.429-432
    • /
    • 1990
  • The promoter isolated from chromosomal DNA of an alkali-tolerant Bacillus sp. YA-14 was subcloned and biochemically characterized. Also the relationships between the promoter activity and sporulation were investigated. In alkali-tolerant Bacillus sp. and Bacillus subtilis, the activity of promoter began to increase at the onset of sporulation with the same mode, and repressed in the presence of 1.0% (wtv) glucose. Among five spoO genes, three epoO genes (spoOB, spoH, spoOJ) were required for promoter expression.

  • PDF