Evaluation of Flexural Performance of Eco-Friendly Alkali-Activated Slag Fiber Reinforced Concrete Beams Using Sodium Activator

나트륨계 알칼리 활성화제를 사용한 친환경 알카리활성 슬래그 섬유보강콘크리트 보의 휨성능 평가

  • Received : 2015.01.16
  • Accepted : 2015.03.15
  • Published : 2015.03.30

Abstract

In this study, it was developed eco-friendly alkali-activated slag fiber reinforced concrete using ground granulated blast furnace slag, alkali activator (water glass, sodium hydroxides), and steel fiber. Eight reinforced concrete beam using alkali-activated slag concrete were constructed and tested under monotonic loading. The major variables were mixture ratio of alkali activator, mixed/without of steel fiber. Experimental programs were carried out to improve and evaluate the flexural performance of such test specimens, such as the load-displacement, the failure mode, the maximum load carrying capacity, and ductility capacity. All the specimens were modeled in scale-down size. The reinforced concrete beams using the eco-friendly alkali-activated slag fiber reinforced concrete was failed by the flexure or flexure-shear in general. In addition, the maximum strength increased with the adding the mol of sodium hydroxide, and the specimen reinforced the steel fiber showed the value of maximum strength which is increased by 15.8% through 25.9%. It is thought that eco-friendly alkali-activated slag fiber reinforced concrete can be used with construction material and product to replace normal concrete. If there is applied to structures such as precast concrete member and production of 2nd concrete product, it could be improved the productivity and reduction of construction duration etc.

이 연구에서는 산업부산물인 알카리활성 슬래그와 알칼리 활성화제 (물유리, 수산화나트륨)에 강섬유를 사용하였으며, 이를 철근콘크리트 보에 적용하여 휨성능 평가를 하였다. 주요변수는 알칼리 활성화제의 혼입비율 및 강섬유를 혼입으로 총 8개의 실험체를 제작하였으며, 재료 및 구조성능 평가를 위한 실험을 수행한 결과 다음과 같은 결론을 얻었다. 친환경 알카리활성 슬래그 섬유보강콘크리트를 사용한 철근콘크리트 보는 전반적으로 휨 또는 휨-전단에 의하여 파괴되었다. 그리고 수산화나트륨의 몰 증가와 강섬유를 보강한 결과 최대내력이 15.8~25.9% 증가한 값이 나타났으며, 연성 또한 높게 나타났다. 친환경 알카리활성 슬래그 섬유보강콘크리트는 기존의 콘크리트를 대체할 수 있는 기초연구로서 향후 건설소재 및 재료분야에 활용할 수 있을 것으로 사료되며, 이러한 특성을 바탕으로 콘크리트 2차 제품 생산과 구조부재를 PC화하여 활용할 경우 생산성 향상, 공기단축 등 효율이 상승될 것으로 보인다.

Keywords

References

  1. Cho, C. G., Kim, B. J., Yang, K. H., and Song, J. K. (2012), Strength Development of Blended Sodium Alkali-Activated Ground Granulated Blast-Furnace Slag (GGBS) Mortar, Journal of the Korea Concrete Institute, 24(2), 137-145. https://doi.org/10.4334/JKCI.2012.24.2.137
  2. Djwantoro Hardjito, Shaw Shen Fung (2010), Fly Ash-Based Geopolymer Mortar Incoporating Bottom Ash, Modern Applied Science, 4(1), 44-52.
  3. Gweok, G. H., Jee, N. Y., Yoon, S. C. (2007), The Experimental Study on The Practical Use of Secondary Product of Concrete Contained Alkali-Activated Slag, Journal of the Architectural Institute of Korea, 23(1), 121-128.
  4. Ha, G. J., Kim, J. H., Jang, K. C. (2013), Evaluation of Flexural Performance of Eco-Friendly Inorganic Binding Material R/C Beams using Sodium Activator, Journal of the Korea Concrete Institute, 25(3), 261-269. https://doi.org/10.4334/JKCI.2013.25.3.261
  5. J. S. Damtoft. (2007), Sustainable Development and climate Change Initiative.
  6. Kim, B. J. (2010), Properties of tensile strength of non-cement concrete using GGBS binder activated by sodium silicate, Department of Architectural Engineeing Graduate Schol Chonnam National University, 12-13.
  7. Lee, H. S. (2006), Experimental study on strength properties of alkali activated slag mortars with different activator type and curing temperature, Department of Architectural Engineering Graduate School of the Hanyang University, 25.
  8. Lee, H. Y., Jang, H. S., So, S. Y., So, Y. S. (2006), The Improvement of Compressive Strength of Non-Sintered Cement Mortar with Alkali activator, Proceedings of the Architectural Institute of Korea, 26(1), 677-680.
  9. Lee, J. G. (2010), New material sufficing modern social demands-Geopolymer, Journal of the korea institute of building construction, 10(6), 27-31. https://doi.org/10.5345/JKIC.2010.12.6.027
  10. Lee, K. P,, Do, Y. S,, Lee, S. S., Song, H. Y. (2009), A Study on Optimum Mixing Derivation of the Enviroment-friendly high performance geopolymer paste, Proceedings of the Korea Institute of Building Construction, 9(2), 107-110.
  11. Park, C. W. (2010), Asian Concrete Federation, presentation material of business presentation.
  12. Son, S. G., Lee, J. H., Lee, S. H., Kim, Y. D. (2009), Low Temperature Synthesis of Forsterite Powders by the Geopolymer Technique, Journal of the Korean ceramic society, 46(3), 242-248. https://doi.org/10.4191/KCERS.2009.46.3.242
  13. T. Bakharev (2003), Resistance of Alkali-Activated Slag Concrete to Acid Attack, Cement and Concrete Research, 33, 1607-1611. https://doi.org/10.1016/S0008-8846(03)00125-X
  14. Yang, K. H., Song, J. G. (2007), The Properties and Applications of Alkali-Activated Concrete with No Cement, Magazine of the Korea Concrete Institute, 19(2), 42-48. https://doi.org/10.22636/MKCI.2007.19.2.42