A Study on Development of Flux to Restrict Occurrence of ion Migration in Lead-Free Solder (무연솔더 내 마이그레이션 플럭스개발에 관한 연구)

  • Ryu Dong Su;Lim Jae Hoon;Woo Seong Woo
    • Proceedings of the Korean Reliability Society Conference
    • /
    • 2005.06a
    • /
    • pp.385-392
    • /
    • 2005
  • The restriction of the use of hazardous substances in electrical and electronic equipment legislation mandates the substitution of lead and other hazardous substances in electronics products by July 2006. Due to this legislative pressure, the electronics industry is moving to adoption of lead free solders. In this paper, we investigated a flux to restrict generating electrochemical migration in lead-free solder. The lead-free solders used in this study were Sn-0.7Cu-0.01P and Sn-3.0Ag-0.5Cu. To measure the resistance of electrochemical migration, the dew-cycle test and water drop test were adopted. As the result, now flux having high durable of electrochemical migration was developed.

  • PDF

The Oxidation Study of Lead-Free Solder Alloys Using Electrochemical Reduction Analysis (전기화학적 환원 분석을 통한 무연 솔더 합금의 산화에 대한 연구)

  • Cho Sungil;Yu Jin;Kang Sung K.;Shih Da-Yuan
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.1 s.34
    • /
    • pp.35-40
    • /
    • 2005
  • The oxidation of pure Sn and Sn-0.7Cu, Sn-3.5Ag, Sn-lZn, and Sn-9Zn alloys at $150^{\circ}C$ was investigated. Both the chemical nature and the amount of oxides were characterized using electrochemical reduction analysis by measuring the electrolytic reduction potential and total transferred electrical charges. X-ray photoelectron spectroscopy (XPS) was also conducted to support the results of reduction analysis. The effect of Cu, Ag and Zn addition on surface oxidation of Sn alloys is reported. For Sn, Sn-0.7Cu and Sn-3.5Ag, SnO grew first and then the mixture of SnO and $SnO_2$ was found. $SnO_2$ grew predominantly for a long-time aging. For Zn containing Sn alloys, both ZnO and $SnO_2$ were formed. Zn promotes the formation of $SnO_2$. Sn oxide growth rate of Pb-free solder alloys was also discussed in terms of alloying elements.

  • PDF

Effects of Microstructure on the Creep Properties of the Lead-free Sn-based Solders (미세조직이 Sn계 무연솔더의 크리프 특성에 미치는 영향)

  • Yoo, Jin;Lee, Kyu-O;Joo, Dae-Kwon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.10 no.3
    • /
    • pp.29-35
    • /
    • 2003
  • The Sn-based lead-free solders with varying microstructure were prepared by changing the cooling rate from the melt. Bulky as-cast SnAg, SnAgCu, and SnCu, alloys were cold rolled and thermally stabilized before the creep tests so that there would be very small amount of microstructural change during creep (TS), and thin specimens were water quenched from the melt (WQ) to simulate microstructures of the as-reflowed solders in flip chips. Cooling rates of the WQ specimens were 140∼150 K/sec, and the resultant $\beta-Sn$ globule size was 5∼10 times smaller than that of the TS specimens. Subsequent creep tests showed that the minimum strain rate of TS specimens was about $10_2$ times higher than that of the WQ specimens. Fractographic analyses showed that creep rupture of the TS-SnAgCu specimens occurred by the nucleation of voids on the $Ag_3Sn$ Sn or $Cu_6Sn_5$ particles in the matrix, their subsequent growth by the power-law creep, and inter-linkage of microcracks to form macrocracks which led to the fast failure. On the other hand, no creep voids were found in the WQ specimens due to the mode III shear rupture coming from the thin specimens geometry.

  • PDF

Alloy Design and Evaluation of Sn-Bi-In-Zn Solder Alloys through Thermodynamic Calculation (무연 솔더 Sn-Bi-In-Zn 합금의 열역학적 설계 및 특성 평가)

  • Yun, Seung-Uk;Lee, Byeong-Ju;Lee, Hyeok-Mo
    • Korean Journal of Materials Research
    • /
    • v.7 no.4
    • /
    • pp.303-309
    • /
    • 1997
  • 기존의 전자 기판에서 땜납으로 사용되고 있는 Sn-Pb계 합금을 대체하기 위한 새로운 합금을 개발하기 위하여 열역학을 이용한 상평형계산을 통해 얻은 다원계 상태도를 바탕으로 적정한 녹는점과 용융구간을 가지는 Sn-Bi-In-Zn계 솔더합금을 설계하였다. 설계된 합금을 제작하여 XRD, DSC및 EDX로 분석하여 상의 확인,조성분석 및 고상점과 액상점 등의 녹음 거동을 확인하였다. 또한 열처리에 따른 미세구조의 변화를 관찰하였고, 이러한 조직변화가 기계적 성질에 미치는 영향을 경도실험과 인장실험을 통해 연구하였다.

  • PDF

Simulation of Thermal Fatigue Life Prediction of Flip Chip with Lead-free Solder Joints by Variation in Bump Pitch and Underfill (무연 솔더 접합부을 갖는 플립칩에서의 언더필 및 범프 피치 변화에 의한 열 피로 수명 예측 해석)

  • Kim, Seong-Keol;Kim, Joo-Young
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.19 no.2
    • /
    • pp.157-162
    • /
    • 2010
  • This paper describes the thermal fatigue life prediction models for 95.5Sn-4.0Ag-0.5Cu solder joints of Flip chip package considering Under Bump Metallurgy(UBM). A 3D Finite element slice model was used to simulate the viscoplastic behavior of the solder. For two types of solder bump pitches, simulations were analyzed and the effects of underfill packages were studied. Consequently, it was found out that solder joints with underfill had much better fatigue life than solder joints without underfill, and solder joints with $300{\mu}m$ bump pitch had a longer thermal fatigue life than solder joints with $150{\mu}m$ bump pitch. Through the simulations, flip chip with lead-free solder joints should be designed with underfill and a longer bump pitch.

A Study on the Characteristics of Sn-Ag-X Solder Joint -The Wettability of Sn-Ag-Bi-In Solder to Plated Substrates- (Sn-Ag-X계 무연솔더부의 특성 연구 -기판 도금층에 따른 Sn-Ag-Bi-In 솔더의 젖음특성-)

  • 김문일;문준권;정재필
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.1
    • /
    • pp.11-16
    • /
    • 2002
  • As environmental concerns increasing, the electronics industry is focusing more attention on lead free solder alternatives. In this research, we have researched wettability of intermediate solder of Sn3Ag9Bi5In, which include In and Bi and has similar melting temperature to Sn37Pb eutectic solder. We investigated the wetting property of Sn3Ag9Bi5In. To estimate wettability of Sn3Ag9Bi5In solder on various substrates, the wettability of Sn3Ag9Bi5In solder on high-pure Cu-coupon was measured. Cu-coupon that plated Sn, Ni and Au/Ni and Si-wafer adsorbed Ni/Cu under bump metallurgy on one side. As a result, the wetting property of Sn3Ag9Bi5In solder is a little better than that of Sn37Pb and Sn3.5Ag.

The micorstructure and strength of SnCuX Solder joint (SnCuX계 솔더를 이용한 무연 솔더링에서의 계면구조와 기계적 특성)

  • 이재식;박지호;문준권;정재필
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2002.11a
    • /
    • pp.55-58
    • /
    • 2002
  • The possibility of SnCuX Solder as alternative for Pb-free Solder have been investigated in this study. SnCuX Solder balls(500${\mu}{\textrm}{m}$) were placed on Si-wafer which is Al/Ni/Cu(500nm/$4{\mu}{\textrm}{m}$/$4{\mu}{\textrm}{m}$)UBM layer. After reflow soldering at $250^{\circ}C$, shear strength and microstructure were analyzed. The results showed that the shear strength(500gf) of SnCuX was higher than that of SnCuX at $230^{\circ}C$ and $Cu_6Sn_5$ intermetallic compounds were formed between Cu and SnCuX Solder layers

  • PDF

Effect of Aging treatment and Epoxy on Bonding Strength of Sn-58Bi solder and OSP-finished PCB (Sn-58Bi Solder와 OSP 표면 처리된 PCB의 접합강도에 미치는 시효처리와 에폭시의 영향)

  • Kim, Jungsoo;Myung, Woo-Ram;Jung, Seung-Boo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.21 no.4
    • /
    • pp.97-103
    • /
    • 2014
  • Among various lead-free solders, the Sn-58Bi solders have been considered as a highly promising lead-free solders because of its low melting temperature and high tensile strength. However, Sn-58Bi solder has the poor ductility. To enhance the mechanical property of Sn-58Bi solder, epoxy-enhanced Sn-58Bi solders have been studied. This study compared the microstructures and the mechanical properties of Sn-58Bi solder and Sn-58Bi epoxy solder with aging treatment. The solders ball were formed on the printed circuit board (PCB) with organic solderability preservative (OSP) surface finish, and then the joints were aged at 85, 95, 105 and $115^{\circ}C$ for up to 100, 300, 500 and 1000 hours. The shear test was conducted to evaluate the mechanical property of the solder joints. $Cu_6Sn_5$ intermetallic compound (IMC) layer grew with increasing aging time and temperature. The IMC layer for the Sn-58Bi epoxy solder was thicker than that for the Sn-58Bi solder. According to result of shear test, the shear strength of Sn-58Bi epoxy solder was higher than that of Sn-58Bi solder and the shear strength decreased with increasing aging time.

A Study on electrical and mechanical reliability assessment of Sn-3.5Ag solder joint (Sn-3.5Ag BGA 솔더 조인트의 전기적, 기계적 신뢰성에 관한 연구)

  • Sung, Ji-Yoon;Lee, Jong-Gun;Yun, Jae-Hyeon;Jung, Seung-Boo
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.80-80
    • /
    • 2009
  • 패키징 구조의 발전이 점차 중요한 문제로 대두되어, 칩의 집적 기술의 발전에 따라 실장기술에서도 고속화, 소형화, 미세피치화, 고정밀화, 고밀도화가 요구되고있다. 최근 선진국을 중심으로 전자 전기기기 및 부품의 실장기술에서도 환경 친화적인 기술을 요구함에 따라, 저에너지 공정 및 무연 실장 기술에 대한 연구가 활발하게 진행되고 있다. 기존의 SOP(Small Out-line Package), QFP(Quad Flat Package) 등은 소형화, 다핀화, 고속화, 실장성에 한계가 있기 때문에, SMT(Surface Mount Technology) 형식으로 된 BGA(Ball Grid Array)가 휴대형 전화를 비롯한 기타 전자 부품 실장에 널리 사용되고 있다. BGA ball shear 법은 BGA 모듈의 생산 및 취급 중에 발생할지도 모르는 기판에 수평으로 작용하는 기계적인 전단력에 BGA solder ball이 견딜 수 있는 정도를 측정하기 위해 사용되는 시험법이다. 전단 시험에 의한 전단 강도의 측정 외에 전기전도도 측정, 파면 관찰, 이동거리(displacement), 유한요소 해석법 등을 병행하여 시험법의 신뢰성 향상에 대한 연구가 이루어지고 있다. 본 실험에서는 지름이 $500{\mu}m$인 Sn-3.5Ag 솔더볼을 이용하여 세라믹 기판을 접합하여 BGA 패키지를 완성하였다. 상부 기판에 솔더볼을 정렬시켜 리플로우 방법으로 접합 한 후 솔더볼이 접합된 상부 기판과 하부 기판을 접합 하여 시편을 제작하였다. 접합된 시편들은 $150^{\circ}C$에서 0~800시간 열처리를 실시하였고, 열처리를 하면서 각각 $3{\times}10^2A/cm^2,\;5{\times}10^3A/cm^2$의 전류를 인가하였다. 시편들을 전단 시험기를 이용하여 솔더볼의 기계적 특성 평가를 하였으며, 계면 반응을 관찰하였다.

  • PDF