Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.21
no.11
/
pp.973-976
/
2008
In addition to its similarity to genuine diamond film, diamond-like carbon (DLC) film has many advantages, including its wide band gap and variable refractive index. In this study, DLC films were prepared by the RF PECVD (Plasma Enhanced Chemical Vapor Deposition) method on silicon substrates using methane ($CH_4$) and hydrogen ($H_2$) gas. We examined the effects of the RF power on the electrical properties of the DLC films. The films were deposited at several RF powers ranging from 50 to 175 W in steps of 25 W. The leakage current of DLC films increased at higher deposition RF power. And the resistivities of DLC films grown at 50 W and 175 W were $5\times10^{11}$${\Omega}cm$ and $2.68\times10^{10}$${\Omega}cm$, respectively.
An experimental study was performed to discover the effect of environment on the tribological behavior of Si-incorporated diamond-like carbon(Si-DLC) film slid on a steel ball. The films were deposited on Si(100) wafers by a radio-frequency glow discharge of mixtures of benzene and dilute silane gases. Experiments using a ball-on-disk test-rig was performed in vacuum, dry air and ambient air conditions. It was observed that coefficient of friction decreased as the environment changed from vacuum, to dry air. Chemical analyses of debris suggested that low and stable friction is closely related to the formation of silicon-rich oxide debris and the rolling action.
Proceedings of the Korean Vacuum Society Conference
/
2000.02a
/
pp.126-126
/
2000
다이아몬드상 카본(DLC) 필름은 경도가 높고, 마찰계수가 낮다는 장점을 가지고 있기 때문에 내마모성 코팅이나 윤활성코팅에 응용을 위한 연구가 활발히 진행중이다. 하지만 마찰계수가 주변환경에 매우 큰 영향을 받는다는 단점이 있다. 이러한 단점은 DLC필름의 응용에 대한 저해 요인이 되며, 이 점을 보완하기 위해서 DLC 필름에 Si을 첨가하는 연구들이 진행되고 있다. 본 실험에서는 r.f-PACVD 법을 이용하여 Si이 첨가된 DLC 필름의 주위 환경 변화에 따른 마찰특성의 변화를 연구하였다. 사용한 반응 가스는 벤젠(C6H)과 희석된 Silane(SiH4 : H2 = 10 : 90)이며, 희석된 Silane과 벤젠의 첨가비율을 조절하여 필름내 Si의 함량을 조절하였고, 증착시 바이아스의 전압은 -400V로 하였다. 마찰테스트는 Ball-on-Disk type의 조건에서 대기, 건조공기, 진공의 세가지 분위기에서 마찰테스트를 실행하였다. 실험결과 마찰계수는 건조공기, 대기, 진공의 순으로 증가하였고, 필름내에 포함되어 있는 Si의 양이 증가할수록 마찰계수는 낮고 안정한 값을 나타내었다. Tribochemiacal 분석과, ball과 track의 전자현미경 사진 분석 결과, 진공에 비해서 건조공기와 대기중에서 마찰계수가 낮은 것은 DLC 필름내에 마모 track 중심부에 Si-C-O 계의 화합물이 형성되어, 이 화합물이 마찰계면에 존재하여 마찰계수를 낮추었음을 확인하였다. 그리고 대기중에서 실험한 경우, 습기의 존재로 인해 마모입자가 볼의 표면에서 엉김으로써 건조공기의 상태에서 보다 높은 마찰저항을 갖게 됨으로 인하여 마찰계수가 높아짐을 알 수 있었다.a)는 as-deposit 상태이며, 그림 1(b)는 45$0^{\circ}C$, 60min 열처리한 plan-view TEM 사진이다.dical의 영향을 조사하였으며 oxygen radical의 rf power에 따른 변화는 OES(Optical emission spectroscopy)를 사용하였다. 너무 적은 oxygen ion beam flux나 oxygen radical은 film의 전도도 및 투과도를 저하시켰고 반면 너무 과도한 flux의 증가 시는 전도도는 감소하였고 투과도는 증가하는 경향을 보였다. 기판에 도달하는 oxygen ion flux는 faraday cup을 이용하여 측정하였으며 증착된 ITO film은 XPS, UV-spectrometer, 4-point probe를 이용하여 분석하였다. 때문으로 생각되어진다. 또한, 성장 온도가 낮아짐에 따라 AlGaN의 성장을 저해하기 때문으로 판단된다. 성장 온도 변화에 따라 성장된 V의 구조적 특성 및 표면 거칠기 변화를 관찰하여 AlGaN의 성장 거동을 논의하겠다.034, 0.005 정도로 다시 감소하였다. 박막의 유전율은 약 35 정도의 값을 나타내었으며 X-선 회절 data로부터 분석한 박막의 변형은 증온도에 따라 7.2%에서 0.04%로 감소하였고 이 이경향은 유전손실은 감소경향과 일치하였다.는 현저하게 향상되었다. 그 원인은 SB power의 인가에 의해 활성화된 precursor 분자들이 큰 에너지를 가지고 기판에 유입되어 치밀한 박막이 형성되었기 때문으로 사료된다.을수 있었다.보았다.다.다양한 기능을 가진 신소재 제조에 있다. 또한 경제적인 측면에서도 고부가 가치의 제품
Multi-layer diamond-like carbon (DLC) films were deposited by 13.56 MHz r.f. PACVD method. Multi-layer DLC film was composed of 2.5 $mu extrm{m}$ thick pure DLC filml and 0.2$\mu\textrm{m}$ thick Si incorporated DLC (Si-DLC) film as a surface layer. Tribological behaviors of the multi-layer DLC film were investigated with a ball-on-disk type tribometer in ambient atmosphere using AISI 52100 steel ball. Low friction coefficient (<0.1) period increased with increasing the Si content in the surface Si-DLC film. The wear rate after 44,000 cycles and 158,400 cycles were the $2.5\times10^{-8}\sim1.8\times10^{-7}\textrm{mm}^3$/rev. and $7.1\times10^{-9}\sim1.8\times10^{-8}\textrm{mm}^3$/rev.,respectively. The wear rate of the multi-layer DLC film after 158,400 cycles was about 2 times smaller than that of pure DLC films of 2.7 $\mu\textrm{m}$ thickness. This high wear resistance and low friction coefficient was caused by the formation of Si oxide layer on the wear scar surface, as confirmed by the debris composition analysis. It was further shown that this si oxide debris layer on the wear scar surface is formed again even after removing the debris of the steel ball, which maintain the low friction coefficient between multi-layer DLC films and steel ball.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.19
no.7
/
pp.618-623
/
2006
Hydrogenated Diamond-like carbon (DLC) films were prepared by the radio frequency plasma enhanced chemical vapor deposition (RF PECVD) method on silicon substrates using methane $(CH_4)$ and hydrogen $(H_2)$ gas. The wear track on the DLC films was examined after the ball-on disk (BOD) measurement with a Raman mapping method. The BOD measurement of the DLC films was performed for 1 to 3 hours with a 1-hour step time. The sliding traces on the hydrogenated DLC film after the BOD measurement were also observed using an optical microscope. The surface roughness and cross-sectional images of the wear track were obtained using an atomic force microscope (AFM). The novel Raman mapping method effectively shows the graphitization of DLC films of $300{\mu}m\times300{\mu}m$ area according to the sliding time by G-peak positions (intensities) and $I_D/I_G$ ratios.
Transactions of the Korean Society of Mechanical Engineers A
/
v.26
no.9
/
pp.1842-1848
/
2002
Although DLC coatings have good tribological properties, these are dependant on the deposition method, the property of contact surface, and test condition. Humidity, which has little influence on tribological behavior in macro scale, is an important factor of tribological behavior in small devices like MEMS. The objective of this study is to investigate the tribological behavior of DLC coatings with particular attention to their wettability at various humidities. DLC coatings were deposited on Si substrates and tested using a reciprocating friction tester against Si$_3$N$_4$balls at various humidities. The results showed that the tribological behavior of DLC coatings was dependant on relative humidity and wettablility of DLC coatings. Friction coefficient at high relative humidity was higher thar that at low relative humidity. The tungsten-containing DLC coatings had a good wear resistance at low relative humidity whereas DLC coatings derived from argon(Ar)+cesium(Cs) gases showed a good wear resistance at high relative humidity.
Park, Jung-Ho;Lim, Dae-Soon;Jung, Suk-Koo;Chang, Hoon;Shin, Jong-Han
Journal of the Korean Institute of Telematics and Electronics A
/
v.33A
no.11
/
pp.97-104
/
1996
Because of the novel characteristics such as chemical stability, hardness, electrical resistivity and thermal conductance, diamond-like carbon (DLC) film is a suitable materials for the passivation layers. For this purpose, DLC films are synthesized under various conditions and are characterized. Adhesive stregth is excellent and increased with the increase of the hydrogen gas flow rate. The resistivity of approximately 5.3X10$^{8}{\Omega}{\cdot}cm$ is measured by automatic spreading resistance probe analysis method. The thermal conductivity of DLC films is superior to that of PSG oxide and improved by increasing the hydrogen gas flow rate. The patterning techniques of the DLC films is developed using the lift-off and RIE methods to form 5${\mu}$m line. Finally, power transistor with the DLC film as passivation layer is fabricated and analyzed. The test result shows the improsved long-term stability and higher breakdown voltage.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.19
no.8
/
pp.701-706
/
2006
In addition to its similarity to genuine diamond film, diamond-like carbon (DLC) film has many advantages, including its wide band gap and variable refractive index. In this study, DLC films were prepared by the RF PECVD (Plasma Enhanced Chemical Vapor Deposition) method on silicon substrates using methane $(CH_4)$ and hydrogen $(H_2)$ gas. We examined the effects of the post annealing temperature on the structural variation of the DLC films. The films were annealed at temperatures ranging from 300 to $900^{\circ}C$ in steps of $200^{\circ}C$ using RTA equipment in nitrogen ambient. The thickness of the film and interface between film and substrate were observed by surface profiler, field emission scanning electron microscopy (FESEM), high resolution transmission electron microscopy (HRTEM), respectively. Raman and X-ray photoelectron spectroscopy (XPS) analysis showed that DLC films were graphitized ($I_D/I_G$, G-peak position and $sp^2/sp^3$ increased) ratio at higher annealing temperature. The variation of surface as a function of annealing treatment was verified by a AFM and contact angle method.
Kim, Woo-young;Lee, Hyun-woo;Yang, Dae-ho;Hong, Sung-tae
Transactions of the Korean Society of Automotive Engineers
/
v.23
no.6
/
pp.656-662
/
2015
In the present study, multi-layered Si DLC (Silicon Diamond-Like Carbon) coatings with HMDSO (Hexamethyldisiloxane) buffer layers are applied on SKD 11 substrates by PECVD (Plasma Enhanced Chemical Vapor Deposition) with different HMDSO gas flow rates, while the gas flow rate of $C_2H_2$ is fixed to enhance the electric resistivity of forming dies for electrically assisted forming. The HMDSO buffer layer is introduced to increase adhesion between the base metal and Si-DLC layers. The result of evaluation of electric resistivity and adhesion strength shows that the properties are affected by the flow rate of HMDSO, while the flow rate of 80 sccm results in the coating with the highest electric resistivity and adhesion strength among the selected flow rates.
Choi, W.S.;Cho, Y.;Park, Y.S.;Jeon, Y.;Heo, J.;Chung, I.;Hong, B.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2005.07a
/
pp.166-167
/
2005
본 연구에서는 RF 플라즈마 화학기상증착 장비를 사용하여 동일조건에서 합성된 100 nm 두께의 DLC박막을 RTA 장비를 사용하여 $N_2$ 분위기로 여러 가지 온도에서 ($300\sim900^{\circ}C$) 후열처리된 DLC 박막들의 마찰특성 변화를 AFM (Atomic Force Microscopy)의 FFM (Friction Force Microscopy) 모드를 사용하여 관찰하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.