• Title/Summary/Keyword: 굵은골재

Search Result 337, Processing Time 0.029 seconds

Bond Behavior of Recycled Coarse Aggregate Concrete Deteriorated by Freezing and Thawing (동결융해를 받은 순환 굵은골재 콘크리트의 부착성능)

  • Choi, Ki-Sun;Lee, Min-Jung;Yun, Hyun-Do;Kang, Ki-Woong;You, Young-Chan;Kim, Keung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.1097-1100
    • /
    • 2008
  • The purpose of this study to investigate the bond strength of recycled coarse aggregate concrete deteriorated by freezing and thawing. Concrete specimens with recycled coarse aggregate representing lower limit of the quality standard (water absorption : 3.0%, specific gravity : $2.5g.cm^3$) were manufactured and tested. The replacement ratio (0, 30, 60 and 100%) of recycled coarse aggregate and freezing-thawing cycles were considered in this test. From the test results, it was found that the bond strength of normal strength concrete is not affected by the replacement ratio of recycled coarse aggregate under freezing and thawing conditions. Also, the bond strength of the natural and recycled coarse aggregate concrete using AE admixtures was not decreased by frost action.

  • PDF

A Study on the Optimum Mix and Exposing Method of the Fine-Size Exposed Aggregate PCC Pavements (소입경 골재노출콘크리트포장의 최적 배합 및 노출기법에 관한 연구)

  • Kim, Young-Kyu;Lee, Seung-Woo;Yoo, Tae-Seok;Kim, Hyung-Bae
    • International Journal of Highway Engineering
    • /
    • v.11 no.2
    • /
    • pp.1-15
    • /
    • 2009
  • Surface of exposed aggregate concrete pavements is consists of exposed coarse aggregate by removing upper 2$\sim$3mm mortar of concrete slab. Exposed aggregate concrete pavements have advantages of maintaining low-noise and adequate skid-resistance level during the performance period. In order to provide the successful exposed concrete aggregate pavement, uniform distribution of the coarse aggregate on pavement surface through adequate the mix design and exposing method. The mix design in concrete pavement is generally designed on the basis of strength, but mix design of exposed aggregate pavement employed in this study includes the consideration of noise and skid resistance, as well as strength. Smaller of maximum coarse aggregate is known to be effective for reduce noise level. Optimum mix design and exposing method of fine-size exposed aggregate portland cement concrete pavement that can reducing the noise and maintain the adequate level of skid resistance are proposed in this study. To consider the variation of optimum exposing time due to the hardening speed of mortar by climatic condition, quantitative is also suggested measurement of hardening state.

  • PDF

The Effect of Combinations of Electric Arc Furnace Slag and Lime Stone aggregates on Engineering Properties of Ultra High Strength Concrete with 80MPa (전기로 산화슬래그 잔골재와 석회암 골재의 조합사용이 80MPa급 초고강도 콘크리트의 공학적 특성에 미치는 영향)

  • Han, Min-Cheol;Moon, Byeong-Yong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.3
    • /
    • pp.253-260
    • /
    • 2017
  • The aim of research is to investigate various physical properties of ultra high strength concrete of 80MPa class using a combination of limestone aggregate and electronic arc furnace oxidizing slag aggregate. For aggregate combinations, granite and limestone are used for coarse aggregate, granite and limestone are also used for fine aggregate. And also, limestone fine aggregate is replaced by electronic arc furnace oxidizing slag aggregate of 25% and 50%. Test results indicated that flowability and compressive strength increased when limestone fine aggregate was used compared to that using granite fine aggregate due to higher modulus of elasticity by limestone. Also substitution of electronic arc furnace oxidizing slag aggregate resulted in a decrease of compressive strength slightly. It is found that the use of electronic arc furnace oxidizing slag aggregate and limestone aggregate would be favorable for reducing the autogenous shrinkage by as much as 9~25%.

Compressive Strength Experiment of Lightweight Concrete Using Coarse Aggregate Produced by 3D Printing (3D 프린팅으로 제작한 굵은 골재를 사용한 경량콘크리트의 압축강도 실험)

  • Ahn, Byung-Ju
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.5
    • /
    • pp.54-59
    • /
    • 2020
  • Coarse aggregate is produced in various ways depending on the location and production method. Currently, the construction industry is in need of a stable supply of coarse aggregate and a way to secure standard quality. The purpose of this study is to examine whether the use of coarse aggregate in 3D printing can help solve this problem. ABS filament was selected for use in 3D printing. CATIA was used for the design of the coarse aggregate, and CUBICON Single Plus was used for the production. Six specimens were produced and cured in water for 28 days. Three of them were made with AE agent, and three were made without it. A compressive strength test confirmed that when the AE agent was used, the compressive strength was greater than the lightweight concrete design criterion specified in the concrete standard specification. This suggests that coarse aggregate produced by a 3D printer may be used for lightweight concrete. A mass production system using this method could help to solve the problems facing the construction industry, such as stable supply and demand for coarse aggregate and securing standard quality.

The Strength and Length Change Properties of Recycled Aggregate Concrete(RAC) by Compressive Strength Levels (압축강도 수준별 순환골재 콘크리트의 강도와 길이변화 특성)

  • Lee, Bong-Chun;Lee, Jun;Cho, Young-Keun;Jung, Sang-Hwa
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.4
    • /
    • pp.307-312
    • /
    • 2015
  • This paper addresses mechanical properties and length change performance of the recycled aggregate concretes(RAC) in which natural coarse was replaced by recycled coarse aggregate(RCA) by compressive strength levels(20, 35, 50 MPa). A total of 9 RAC were produced and classified into three series, each of which included three mixes designed with three compressive strength levels of 20 MPa, 35 MPa and 50 MPa and three RCA replacement ratios of 0, 50 and 100%. Physical/Mechanical properties of RAC were tested for slump test, compressive strength, and length change. The test results indicated that the workability of RC could be improved or same by RCA replacement ratios, when compared with that containing no RCA. This is probably because of the RCA shape improving the workability of RAC. Also, the test results showed that the compressive strength was decreased by 9~10% as the RCA replacement ratios increase. However, the length change ratio by the RCA replacement ratios increased regardless of compressive strength levels. At 20 MPa level, the length change ratio was 8~40% which was much higher than that of 4~17% at both 35 and 50 MPa levels. Therefore, it was considered that such admixture addition preventing dry shrinkage is required in order to improve the properties of the RAC at 20 MPa level.

An Experimental Study on the Properties of Concrete according to G/S ratio classified by Maximum Size of Coarse Aggregate (굵은골재 최대치수별 굵은골재/잔골재 용적비에 따른 콘크리트의 특성에 관한 실험적 연구)

  • Kim, Duk-Hyun;Lee, Sang-Soo;Song, Ha-Young;Kim, Eul-Yong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.4 no.2
    • /
    • pp.97-103
    • /
    • 2004
  • In this study, the experiment was carried out to investigate and analyze the influence of coarse aggregate's mix ratio and maximum size on the properties of concrete. The main experimental variables were water/cement ratio 45% and 65%, coarse aggregate/fine aggregate ratio 90%, 130% and 170%, maximum size of coarse aggregate 15mm, 25mm and 40mm. According to the test results, the principal conclusions are summarized as follows. 1) The slump and flow of fresh concrete were found to be higher in the order of G/S ratio 170%, 130%, 90%, also in the order of maximum size 40mm, 25mm, 15mm. 2) The compressive strength of hardened concrete were found to be higher in the order of G/S ratio 170%, 130%, 90%, also in the order of maximum size 15mm, 25mm, 40mm.

Initial Performance Evaluation of Fine-size Exposed Aggregate PCC Pavement by Experimental Construction (시험시공을 통한 소입경 골재노출 콘크리트포장의 초기 공용성 평가)

  • Kim, Young-Kyu;Choi, Don-Hwa;Lee, Seung-Woo;Kim, Hyung-Bae
    • International Journal of Highway Engineering
    • /
    • v.12 no.1
    • /
    • pp.87-98
    • /
    • 2010
  • Surface of fine-size exposed aggregate Portland cement concrete pavements is consists of exposed coarse aggregate by removing upper 2~3mm mortar of concrete slab. Fine-size exposed aggregate PCC pavements have advantages of maintaining low-noise and adequate skid-resistance level during the performance period. In order to provide the successful exposed concrete aggregate pavement, uniform distribution of the coarse aggregate on pavement surface through adequate the mix design and exposing method. In this study, evaluated initial performance of fine-size exposed aggregate PCC pavement by experimental construction. And it was known that fine-size exposed aggregate concrete pavement which can reduce the noise and maintain the adequate level of skid resistance and strength.

Influence of the Fine and Coarse Aggregate on the Fluidity of High Flowing Concrete (고유동콘크리트의 유동특성에 미치는 잔골재 및 굵은골재의 영향)

  • 김규용;이정율;박선규;정하선;이석홍;손영현;김무한
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10a
    • /
    • pp.301-306
    • /
    • 1998
  • Aggregate as the component of High Flowing Concrete has much influence on the properties of High Flowing Concrete according to the quality and condition because the aggregate occupy a lot of concrete volume. The shape and size of aggregate affect a lot spatial passibility and fillingability. The segregation is easy to occur when the rate of Fine aggregate is high so that Fluidity is much affected by aggregate factor. In this study, therefore, we try to understand the various fluidity according to the fine aggregate of standard grade rang, the size of Coarse aggregate and the rate of fine aggregate to confirm the manufacturing possibility of High Flowing Concrete by examination on the influence of fresh state of high flowing concrete such as flowability, reinforcement passibility, fillingability, segregation resistance.

  • PDF

Engineering Characteristics of Resource-Cycling Mortar according to the Variation of Illite Replacement Ratio and Fine Aggregate Type (굵은골재 및 잔골재 조합변화가 초고강도 콘크리트의 기초적 특성에 미치는 영향)

  • Lee, Sun-Jae;Song, Yuan-Lou;Yun, Jeong-Wan;Han, Dong-Yeop;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2015.05a
    • /
    • pp.61-62
    • /
    • 2015
  • This study has analyzed the engineering characteristics of resource-cycling mortar according to the variation of fine aggregate type using illite with high development potentials by setting the goal as developing eco-friendly construction materials. As a result, while flow has increased if recycled fine aggregate and waste refractory are used separately or mixing them adequately in case of flow and compressive strength, the flow had somewhat declined followed by illite replacement. However, the possibility of such usage is determined to be adequate if used by mixing illite, recycled fine aggregate and waste refractory properly due to the dry shrinkage effect.

  • PDF