• Title/Summary/Keyword: (Ba,Sr)(Nb,Ti)$O_3$ thin films

Search Result 8, Processing Time 0.03 seconds

The structural properties of the (Ba,Sr)(Nb,Ti)$O_3$[BSNT] thin films with $Ar/O_2$ rates ($Ar/O_2$비에 따른 (Ba, Sr)(Nb, Ti)$O_3$[BSNT] 박막의 구조적 특성)

  • Nam, Sung-Pill;Lee, Sang-Chul;Kim, Ji-Heon;Park, In-Gil;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07b
    • /
    • pp.609-612
    • /
    • 2002
  • In this study, the electrical properties were investigated for the deposited Ba,Sr)(Nb,Ti)$O_3$[BSNT] thin films grown on $Pt/TiO_2/SiO_2/Si$ substrate by RF sputtering method. The structural properties of the BSNT thin films affected by the $Ar/O_2$ rates were investigated. In the case of the BSNT thin films deposited with condition of 60/40$(Ar/O_2)$ ratio, the $BaTiO_3$, $SrTiO_3$ and $BaNbO_3$ phases were showed. The composition ratio of Nb and Ti in the BSNT thin films were nearly equivalent. Also, in the BSNT thin films deposited with condition of 60/40 and 80/20$(Ar/O_2)$ ratios, the composition of Ba, Sr, Nb and Ti were relatively uniform. The Ba, Sr, Nb and Ti in the BSTN thin films were not diffused into the Pt layer.

  • PDF

The Structural Properties Of the (Ba1Sr)(Nb1Ti)O3[BSNT] Thin Films with Ar/O2Ratios (Ar/O2비에 따른 (Ba1Sr)(Nb1Ti)O3[BSNT] 박막의 구조적 특성)

  • 남성필;이상철;이영희;이성갑
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.4
    • /
    • pp.317-321
    • /
    • 2003
  • In this study, the structural properties were Investigated for the deposited (Ba,Sr)(Nb,Ti)O$_3$[BSNT] thin films grown on Pt/TiO$_2$/SiO$_2$/Si substrate by RF sputtering method. The structural properties of the BSNT thin films affected by the Ar/02 ratios were Investigated. In the case of the BSNT thin films deposited with condition of 60/40(Ar/O$_2$) ratio, the BaTiO$_3$, SrTiO$_3$ and BaNbO$_3$ phases were showed. The composition ratio of Nb and Ti in the BSNT thin films were nearly equivalent. Also, in the BSNT thin films deposited with condition of 60/40 and 80/20(Ar/O$_2$) ratios, the composition of Ba, Sr, Nb and Ti were relatively uniform. The Ba, Sr, Nb and Ti in the BSTN thin films were not diffused into the Pt layer.

Structural and electrical properties of Ba(Sr,Ti)O3/K(Ta,Nb)O3 multilayer thin film for the application of electro-caloric devices

  • Kwon, Min-Su;Lee, Sung-Gap;Kim, Kyeong-Min;Choi, Seungkeun
    • Journal of Ceramic Processing Research
    • /
    • v.20 no.6
    • /
    • pp.603-608
    • /
    • 2019
  • In this study, the multilayered thin films of (Ba,Sr)TiO3/K(Ta,Nb)O3 were fabricated by the sol-gel and spin coating methods, and their structural and electrical properties were investigated. The specimen showed polycrystalline X-ray diffraction (XRD) characteristics with a tetragonal structure. The average grain size and film thickness for one coating were about 30~40nm and 60nm, respectively. The phase transition temperature of specimen was lower than 10 ℃. The dielectric constant and loss at 20 ℃ of the specimen coated six times were 1,231 and 0.69, respectively. The rate of change in dielectric constant at an applied direct current (DC) voltage of the six times coated thin films was 17.3%/V. The electrocaloric effect was the highest around the temperature at which the remanent polarization rapidly changed. When an electric field of 660kV/cm was applied to the triply coated thin films, the highest electrocaloric property of 4.41 ℃ was observed.

Leakage Current of Capacitive BST Thin Films (BST 축전박막의 누설전류 평가)

  • 인태경;안건호;백성기
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.8
    • /
    • pp.803-810
    • /
    • 1997
  • Ba0.5Sr0.5TiO3 thin films were deposited by RF magnetron sputliring method in order to clarify the anneal condition and doping effect on loakage current Nb and Al were selected as electron donor and acceptor dopants respectively, in the BST films because they have been known to have nearly same ionic radii as Ti and thought to substitute Ti sites to influence the charge carrier and the acceptor state adjacent to the gram boundary. BST thin films prepared in-situ at elevated temperature showed selatively high leakage current density and low breakdown voltage. In order to achieve smooth surface and to improve electrical properties, BST thin films were deposited at room temperature and annealed at elevated temperature. Post-annealed BST thin films showed smoother surface morphology and lower leakage current density than in-situ prepared thin films. The leakage current density of Al doped thin films was measured to be around 10-8A/cm2, which is much lower than those of undoped and Nb doped BST films. The result clearly demonstrates that higher Schottky barrier and lower mobile charge carrier concentration achieved by annealing in the oxygen atmosphere and by Al doping are desirable for reducing leakage current density in BST thin films.

  • PDF

Epitaxial Growth of $BiFeO_3-Ba(Cu_{1/3}Nb_{2/3})O_3$ Thin Films Deposited by Pulsed Laser Deposition

  • Baek, Chang-U;Lee, Jong-Pil;Seong, Gil-Dong;Jeong, Jong-Hun;Ryu, Jeong-Ho;Yun, Un-Ha;Park, Dong-Su;Jeong, Dae-Yong
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.30.1-30.1
    • /
    • 2011
  • Multiferroic thin films with composition $0.9BiFeO_3-0.1Ba(Cu_{1/3}Nb_{2/3})O_3$ were epitaxially grown by pulsed laser deposition on $SrRuO_3(001)/SrTiO_3$ (000) substrate $0.9BiFeO_3-0.1Ba(Cu_{1/3}Nb_{2/3})O_3$, which is assumed to be morphotropic phase boundary (MPB), that showed superior dielectric, ferroelectric and magnetic properties in our study on polycrystalline films. The structures of epitaxially grown films were characterized by means of XRD. From P-E measurements, samples exhibited typical ferroelectric hysteresis loops and large remnant polarization, whose value is much larger than those of pure BFO film. The enhancement of dielectric, ferroelectric, magnetic properties was attributed to the structural distortion induced by the BCN addition and the high physical stress effect.

  • PDF

Poling-dependent Ferroelectric Properties of SBN30 Thin Films (분극에 의한 SBN30 박막의 강유전특성 변화)

  • Jang, Jae-Hoon;Lee, Dong-Gun;Lee, He-Young
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.309-312
    • /
    • 2002
  • Ferroelectric $Sr_{0.3}Ba_{0.7}Nb_{2}O_{6}$ (SBN30) thin films were deposited on Pt/Ti/$SiO_{2}$/Si(100) substrates by ion beam sputtering. During annealing treatment at $750^{\circ}C$, poling was attempted by applying dc voltage bias across polished surfaces. Phase relation, microstructure and crystallization behavior were examined using XRD and FE-SEM. Ferroelectric hysteresis characteristics were also determined where both remanent polarization and coercive values decreased with the increase of bias voltage. The measured remanent polarization and coercive field values at 5 V and 10 V bias were $36{\mu}C/cm^2$, $10{\mu}C/cm^2$ and 100kV /cm, 80kV /cm, respectively.

  • PDF

Crystallization and Electrical Properties of SBN60 Thin Films Prepared by Ion Beam Sputter Deposition

  • Jang, Jae-Hoon;Jeong, Seong-Won;Lee, Hee-Young
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.1
    • /
    • pp.10-13
    • /
    • 2005
  • $Sr_{0.6}Ba_{0.4}Nb_{2}O_{6}$, hereafter SBN60, thin films of 300 nm thickness were deposited using ion beam sputtering technique, in which sintered ceramic target of the same composition was utilized and the $Ar:O_{2}$ gas ratio was controlled during deposition onto $Pt(100)/TiO_{2}/SiO_{2}/Si$ substrate. Crystallization and orientation behavior as well as electrical properties of the films were examined after annealing treatment at $650{\sim}800{\cric}C$. It was found that the film orientation was dependent upon $Ar:O_{2}$ratio, in which strong (00l) orientation was developed when the gas ratio was about 1:4 at $4.3{\times}10^{-4}$ torr. Typical remanent polarization (2Pr), the coercive field (Ec) and the dielectric constant of Pt/SBN60/Pt thin film capacitor were approximately $10{\mu}C/cm^{2}$, 60 kV/cm, and 615, respectively.

Crystallization and Electrical Properties of SBM Thin Films by IBSD Process (IBSD법에 의한 SBN60 강유전체 박막의 배향 및 전기적 특성)

  • Jeong, Seong-Won;Jang, Jae-Hoon;Lee, Hee-Young
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.869-873
    • /
    • 2004
  • [ $Sr_xBa_{1-x}Nb_2O_6$ ] (SBN, $0.25{\leq}x{\leq}0.75$) ceramic is a ferroelectric material with tetragonal tungsten bronze (TTB) type structure, which has a high pyroelectric coefficient, piezoelectric, and a photo refractive properties. In this study, SBN60(x=0.6) thin film was manufactured by ion beam sputtering technique. Using the prepared SBN60 target in $Ar/O_2$ atmosphere as-deposited SBN60 thin film on Pt(100)/$TiO_2/SiO_2/Si$ substrate crystallization and orientation behavior as well as electric properties of SBN60 thin film were examined. SBN60 deposition up to $3000{\AA}$ in thickness, SBN60 thin film was heat-treated at $650^{\circ}C{\sim}800^{\circ}C$. The orientation was shown primarily along (001) plane from XRD pattern where working pressure was $4.3{\times}10^{-4}$ torr. The deposited layer was uniform, preferred orientatin and crystallization behavior resulted in the change of $O_2$ ratio was observed. In electric propertie of Pt/SBN60/Pt thin film capacitor remnant polarization (2Pr) value was $10{\mu}C/cm^2$, the coercive filed (Ec) 50 kV/cm, and the dielectric constant 615, respectively.

  • PDF