• Title/Summary/Keyword: (111) orientation

Search Result 353, Processing Time 0.039 seconds

Microstuctures and Themal Stability of Rapidly Solidified Al-Fe-V-Si-(Mn) Alloys (급랭응고한 Al-Fe-V-Si계 합금의 미세조직과 열안정성에 관한 연구)

  • Kim, Seon-Hwa;Park, Won-Wook
    • Applied Microscopy
    • /
    • v.21 no.2
    • /
    • pp.57-66
    • /
    • 1991
  • The main purpose of this paper was to investigate the change of rapidly solidified microstructures and dispersoid behavior according to heat-treatment in the Al-Fe-V-Si-(Mn) alloys. It was found that (111) preferred orientation identified by X-ray diffraction and fine subgrain/large grain were observed in the rapidly solidified Al-Fe-V-Si-(Mn) alloys. Cell boundary of the zone A was composed of the microcrystalline, whereas that of the zone B was amorphous. Decomposition of the Al-Fe-V-Si-(Mn) alloys occurred at about $300^{\circ}C$. These alloys exhibited excellent thermal stability at the elevated temperature. Microstructure of the zone B was more stable than that of the zone A. The spherical dispersoid and 5-fold symmetry phase was also more thermally stable than the amorphous structure of cell boundary.

  • PDF

Heavy Carbon Incorporation into High-Index GaAs (고농도로 탄소 도핑된 높은 밀러 지수 GaAs)

  • Son, Chang-Sik
    • Korean Journal of Materials Research
    • /
    • v.13 no.11
    • /
    • pp.717-720
    • /
    • 2003
  • Heavily $p^{ +}$-typed ($10^{20}$ $cm^{-3}$ ) GaAs epilayers have been grown on high-index GaAs substrates with various crystallographic orientations from (100) to (111)A by a low-pressure metalorganic chemical vapor deposition. Carbon (C) tetrabromide (CBr$_4$) was used as a C source. At moderate growth temperatures and high V/III ratios, the hole concentration of C-doped GaAs epilayers shows the crystallographic orientation dependence. The bonding strength of As sites on a growing surface plays an important role in the C incorporation into the high-index GaAs substrates.

Inhomogeneity of Hot Rolling Texture in Cu/Nb Added Ultra Low Carbon Steels

  • Jiang, Ying-Hua;Park, Young-Koo;Lee, Oh-Yeon
    • Korean Journal of Materials Research
    • /
    • v.17 no.12
    • /
    • pp.634-636
    • /
    • 2007
  • The texture and microstructure in Cu/Nb added ultra low carbon steels through the different thickness layer were studied after hot rolling. It was found that the two ultra low carbon steels all show the inhomogeneity of hot rolling texture and the Cu-added ultra low carbon steel was far more inhomogeneous than Nb-added one. In the center layer, the strong ${\alpha}\;fibre,\;{\gamma}\;fibre$ textures and the shear textures including 001<110>, 111<112> were founded. Near the surface, the ${\alpha}\;fibre$ texture and the orientation texture caused by a typical plane-strain deformation condition of bcc metals were observed.

Fabrication and Structural Properties of SCT Ceramic Thin Film (SCT 세라믹 박막의 제조 및 구조적 특성)

  • 김진사;조춘남;송민종;소병문;최운식
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.1084-1087
    • /
    • 2001
  • The (Sr$\sub$0.85/Ca$\sub$0.15/)TiO$_3$(SCT) thin films are deposited on Pt-coated electrode(Pt/TiN/SiO$_2$/Si) using RF sputtering method. The crystallinity of SCT thin films is increased with increase of substrate temperature in the temperature range of 100[$^{\circ}C$]∼500[$^{\circ}C$]. Also, the crystallinity of SCT thin films are obtained at the substrate temperature above 400[$^{\circ}C$]. SCT thin films had (111) preferred orientation. The dielectric constant changes almost linearly in temperature ranges of-80∼+90[$^{\circ}C$]. The temperature properties of the dielectric loss have a stable value within 0.1. SCT thin films used in this study show the phenomena of dielectric relaxation with the increase of frequency, and the relaxation frequency is observed above 200[kHz].

  • PDF

Characterization of Solid Phase Crystallization in Sputtered and LFCVD Amorphous Silicon Thin Film (스퍼터링 및 저압화학기상증착 비정질 실리곤 박막의 고상 결정화 특성)

  • 김형택
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1995.11a
    • /
    • pp.89-93
    • /
    • 1995
  • Effects of hydrogenation in amorphous silicon rile growths on Solid Phase Crystallization (SPC) was investigated using x-ray diffractometry, energy dispersive Spectroscopy, and Raman spectrum. Interdiffusion of barium(Ba) and aluminum(Al) compounds of corning substrate was observed in both of rf sputtering and LFCVD films under the low temperature(580$^{\circ}C$) annealing. Low degree of crystallinity resulted from the interdiffusion was obtained. Highly applicable degree of crystallinity was obtained through the mechanical damage induced surface activation on amorphous silicon films. X-ray diffraction intensity of (111) orientation was used to characterize the degree of crystallinity of SPC. Nucleation and growth rate in SPC could be controllable through the employed surface treatment. IIydrogenated LPCVD films showed the superior crystallinity to non-hydrogenated sputtering films. Insignificant effects of activation treatment in sputtered film was of activation treatment in sputtered film was observed on SPC.

  • PDF

Pyroelectric and dielectric properties of the modified PZT thin films and bulk ceramics (Modified PZT계 박막과 bulk의 초전 및 유전특성 비교)

  • Kim, K.W.;Kang, D.H.;Shin, S.H.;Cho, S.C.;Kim, Y.H.;Gil, S.K.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07b
    • /
    • pp.743-745
    • /
    • 2002
  • Pyroelectric and dielectric properties of modified PZT thin film and bulk ceramics were studied. In case of bulk specimens were prepared by conventional ceramic process and thin films with same composition and (111) preferred orientation were prepared by the sol-gel process. Their crystal structure, pyroelectric and dielectric properties were investigated after poling at $150^{\circ}C$ for 30 min for bulk ceramics and no poling treatment, respectively. Dielectric constants and losses of bulk and thin film were 600, 875 and 0.028, 0.025, respectively. Pyroelectric coefficients obtained were $50nC/cm^2K$ and $30nC/cm^2K$, respectively.

  • PDF

Mechanical Properties and Fatigue Characteristics of CrN Coated Ti-6Al-4V alloy (CrN 박막처리된 Ti-6Al-4V 합금의 기계적 성질과 피로특성)

  • Park, Yong-Gwon;Baeg, Chang-Hyung;Wey, Myeong-Yong
    • Korean Journal of Materials Research
    • /
    • v.12 no.8
    • /
    • pp.669-675
    • /
    • 2002
  • CrN film coated by AIP method, improved the mechanical properties (Hardness, Roughness, wear and fatigue) of Ti-6Al-4V alloy. The properties were studied using GXRD, XPS, Hardness, Roughness, wear and fatigue testers. CrN thin film thickness was about 7.5$\mu\textrm{m}$ and grew with (111) orientation. Hardness of CrN thin film was very high (Hv 1390) and roughness of the surface layer was greatly improved (Ra=0.063$\mu\textrm{m}$) compared with matrix alloy (Ra=0.321$\mu\textrm{m}$). Such changes of hardness and roughness could be contributed to improving the wear resistance and fatigue life. Striation like pattern with dimples and voids, a typical fatigue fracture mode, was observed throughout the specimen.

Nanoscale Islands of the Self Assembled Monolayer of Alkanethiol

  • Saha, Joyanta K.;Yang, Mino;Jang, Joonkyung
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.12
    • /
    • pp.3790-3794
    • /
    • 2013
  • Molecular dynamics simulations were performed to study the structure and stability of a nanoscale self-assembled monolayer (SAM) of alkanethiol on a gold (111) surface. The tilt angle and orientational order of the alkyl chains in the SAM island were examined by systematically varying the size of the island. The chain length dependence of the SAM island was examined by considering alkanethiols containing 12, 16, 20, and 24 carbon atoms. The minimum diameter of SAM islands made from 1-tetracosanethiol, 1-ecosanethiol, 1-hexadecanethiol and 1-dodecanethiol were 2.29, 1.9, 4.7 and 4.76 nm, respectively. These set the ultimate resolution that can be patterned by soft nanolithography. As the length of alkanethiol increases, the SAM islands became more ordered in both orientation and conformation of the alkyl chains.

Structural Phase Transformations in Semiconductor Material Induced by Nanoindentation (나노압입에 의한 반도체 소재의 구조상전이 해석)

  • Kim, D.E.;Oh, S.I.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.77-80
    • /
    • 2006
  • Structural phase transformations of silicon during nanoindentation were investigated in detail at the atomic level. The molecular dynamics simulations of nanoindentation on the (100), (110) and (111) surface of single crystalline silicon were simulated, and this supported the theoretical prediction of the anisotropic behavior of structural phase transformations. Simulations showed that microscopic aspects of phase transformation varied according to the crystallographic orientation of the contact surface and were directly linked to the slip system.

  • PDF

An Electrical Characteristics on the Pentacene-Based Organic Thin-Film Transistors using PVA Alignment Layer (PVA 배열층을 이용한 펜타신 유기 박막 트랜지스터의 전기적 특성)

  • Jun, Hyeon-Sung;Oh, Hwan-Sool
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.3
    • /
    • pp.177-182
    • /
    • 2010
  • The pentacene-based organic thin film transistors(OTFTs) using polyvinylalcohol(PVA) alignment layer were fabricated on the $SiO_2$ evaporated to n-type (111) Si substrates. The pentacene film was deposited by thermally evaporated at $10^{-7}$ torr. X-ray diffraction (XRD) and atomic force microscope(AFM) measurement showed pentacene film which deposited on rubbed PVA layers were partially crystallized at (001) plane. The pentacene OTFTs with PVA layers rubbed perpendicular to the direction of current flow was shown to align better orientation than parallel rubbed case and thus to enhance the mobility and saturation current by a factor of 2.3 respectively. We obtained mobility by 0.026 $cm^2$/Vs and on-off current ratio by ${\sim}10^8$.