Dielectric Properties Analysis in Paraelectric $ZrTiO_4$Thin Films (상유전 $ZrTiO_4$박막의 유전특성 분석에 관한 연구)

  • 허진희;김경해;이준신
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.547-549
    • /
    • 2001
  • The dielectric constants and dielectric losses of ZrTiO$_4$thin films deposited by DC magnetron reactive sputtering were investigated. The paraelectric properties were measured in the 100kHz range. As the deposition temperature increased (up to 67$0^{\circ}C$), the dielectric losses (tan$\delta$) decreased (down to 0.017$\pm$0.007), while the dielectric constants ($\varepsilon$) were in the range of 35$\pm$7. Post annealing at 80$0^{\circ}C$ in oxygen for 2h reduced tan$\delta$ down to 0.005$\pm$0.001, higher than those of well-sintered bulk ZrTiO$_4$.

  • PDF

Microstructure and Microwave Dielectric Properties of ZrTiO4 Thin Films Prepared by Metal-organic Decomposition (금속유기분해 법으로 제조한 ZrTiO4 박막의 미세구조 및 고주파 유전특성)

  • Park, Chang-Sun;Sun, Ho-Jung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.1
    • /
    • pp.53-60
    • /
    • 2009
  • $ZrTiO_4$ dielectric thin films were coated by metal-organic decomposition, and annealed by rapid thermal processing up to $900^{\circ}C$ for their crytallization. Crystallized single-phase $ZrTiO_4$ thin films were fabricated above the annealing temperature of $800^{\circ}C$, but their grains were randomly oriented without specific textured orientation. Best dielectric properties were presented by the sample annealed at $800^{\circ}C$ which had crystalline structure and flat surface. Dielectric constant of the film was maintained at 32 throughout full frequency range up to 6 GHz, and dielectric loss was varied between 0.01 and 0.04.

Sintering and Microstructure of PZT Ceramics Prepared from Nanoparticles by Sol-Gel Process (나노 입자를 이용한 PZT 압전 세라믹스의 소결 및 미세구조)

  • Park Yong-Kap
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.6 no.6
    • /
    • pp.457-460
    • /
    • 2005
  • Nano-sized titanium oxide and zirconium oxide powders were synthesized by hydrolysis of titanium isopropoxide $[Ti(OC_3H7)_4]$ and zirconium tetrachloride ($ZrC1_4$) via a sol-gel technique. Lead titanate powders were prepared by mixing $TiO_2$ precursors with PbO slurry made with dilute $NH_4OH$. Lead zirconate titanate powders were, then, synthesized by mixing $PbTiO_3$ with $ZrO_2$ powders. The goal of this research was to obtain the $PbZrTiO_3(PZT)$ powders and sintering these powders at low temperature. The $PbTiO_3$ and PZT powders after firing were analyzed by X-ray diffraction(XRD) and transmission electron microscopy(TEM) was utilized to observe the shape and size of the synthesized nano-particles. In the XRD pattern, the well-crystallized PZT phase could be obtained in consequence of firing at $900^{\circ}C$. SEM micrographs also showed that grains of PZT were relatively well grown with the size of the range of $2{\~}4{\mu}m$. The densified perovskite structure of $PbZrTiO_3$ could be obtained by sintering at temperature as low as $900^{\circ}C$. Characterization of the samples showed improved piezoelectric properties.

  • PDF

Oxidation of TiZrAlN nanocomposite thin films in air at temperatures between 500 and $700^{\circ}C$ (TiZrAlN의 500-$700^{\circ}C$ 사이에서 공기 중 산화)

  • Kim, Min-Jeong;Bong, Seong-Jun;Lee, Dong-Bok
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2011.05a
    • /
    • pp.167-170
    • /
    • 2011
  • Quaternary TiZrAlN nanocomposite thin films with a composition of 20.7Ti-22.2Zr-2.7Al-54.4N (at.%) were deposited by the closed-field unbalanced magnetron sputtering (CFUBMS) method and oxidized in air at temperatures between 500 and $700^{\circ}C$. The oxides formed were $TiO_2$, $ZrO_2$, and $Al_2O_3$. The films had inferior oxidation resistance because the amounts of $ZrO_2$ and $TiO_2$ were large while the amount of $Al_2O_3$ was small. The oxidation progressed primarily by the inward diffusion of oxygen and the outward diffusion of nitrogen.

  • PDF

The preparation of Pb(Zr0.53Ti0.47)O3 powders for low temperature densification (저온 소결성이 우수한 Pb(Zr0.53Ti0.47)O3 계 압전 분말 제조)

  • Lee, Yonghui;Baek, In Chan;Seok, Sang Il
    • Particle and aerosol research
    • /
    • v.4 no.1
    • /
    • pp.21-25
    • /
    • 2008
  • $Pb(Zr_{0.53}Ti_{0.47})O_3$ (PZT) was synthesized by a multiple wet dry process. Precipitates prepared from reaction between $ZrOCl_2{\cdot}8H_2O$ and $TiOCl_2$ and $NH_4OH$ in an aqueous solution was dried at $100^{\circ}C$, and calcined at $500^{\circ}C$ and $700^{\circ}C$. The mixture mixed with PbO and as-dried or calcined $Zr_{0.53}Ti_{0.47}O_4$ (ZT) powders was calcined again at 700 and $800^{\circ}C$. Well crystallized ZT and PZT were formed at even $700^{\circ}C$. PZT piezoelectric ceramics of more than 98.5% in a relative density was obtained by sintering at as low as $900^{\circ}C$.

  • PDF

Microwave Dielectric Properties of $(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$ Ceramics according to Doped NiO and Sintering Temperature ($(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$ 세라믹스의 NiO 첨가량 및 소결온도에 따른 고주파 유전특성)

  • Yun, J.R.;Heung, S.Y.;Lee, H.Y.;Kweon, J.Y.;Kim, K.Y.
    • Proceedings of the KIEE Conference
    • /
    • 1994.07b
    • /
    • pp.1487-1489
    • /
    • 1994
  • $(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$ system which has a dielectric constant, low dielectric loss and temperature coefficient was investigated. Temperature coefficient varied from positive to negative with increasing of NiO. For the NiO content 1.0wt%. i.e $(Zr_{0.65}Sn_{0.35})Ti_{1.04}O_4$, the ceramic showed very good dielectric properties such as ${\epsilon}$=37.8, $Q{\times}f_o=49.000$ and ${\tau}_r= 4{\pm}1ppm/^{\circ}C$.

  • PDF

An Efficient and Green Approach for the Esterification of Aromatic Acids with Various Alcohols over H3PO4/TiO2-ZrO2

  • Kalbasi, Roozbeh Javad;Massah, Ahmad Reza;Barkhordari, Zeynab
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.8
    • /
    • pp.2361-2367
    • /
    • 2010
  • $TiO_2-ZrO_2$ was prepared with surfactant through a sol-gel method. Catalysts containing 5 - 35% $H_3PO_4$ were prepared using these oxides. Subsequently the catalytic performance of prepared catalysts was determined for liquid phase esterification of aromatic acids. $H_3PO_4/TiO_2-ZrO_2$ has been used as catalyst to synthesize various novel esters by esterification of some aromatic acids with aliphatic alcohols (2-propanol, 1-butanol, iso butanol, 3-pentanol, 1-hexanol, heptanol, cyclo heptanol, octanol and decanol). Under optimized conditions, maximum yields and selectivity (100%) to the corresponding ester, was obtained by using 25 wt % $H_3PO_4/TiO_2-ZrO_2$ as catalyst. The Catalyst can be easily recycled after reaction and can be reused without any significant loss of activity/selectivity performance. No by-product formation, high yields, short reaction times, mild reaction conditions, operational simplicity with reusability of the catalyst are the salient features of the present synthetic protocol. The reaction was carried out under solvent-free condition.

Perovskite-Like Strontium Titanium Zirconium Oxide Solid Solutions Prepared at Atmospheric Pressure

  • Choy, Jin-Ho;Kim, Ha-Suck;Kwon, Young-Uk;Kim Chong Hee
    • Bulletin of the Korean Chemical Society
    • /
    • v.6 no.6
    • /
    • pp.344-347
    • /
    • 1985
  • Perovskite type oxides of $SrTiO_3,SrZrO_3,and\;SrTi_{1-x}Zr_xO_3$ have been systematically synthesized at $1250^{\circ}C$and $1550^{\circ}C$ with specimens containing additions of up to x=0.9 of zirconium by solid state reactions and characterized by X-ray diffraction. X-ray diffraction studies showed that the compound $SrTi_{1-x}Zr_xO_3$ has cubic structure. The lattice paramters of $SrTi_{1-x}Zr_xO_3$ solid solutions obey the Vegard's law and fairly large increase in volume can acompany the formation of this solution with increasing Zr content(X). Assuming the lattice constants of perovskite type compounds $A(B_{1-x}B'_x)O_3$where $B_{1-x}B'_x$ is $Ti_{1-x}Zr_x$, to be a linear function of the ionic radii of B and B' ions, the disordered ion pair of $Ti^{4+}$and $Zr^{4+}$ was verified from the lattice constants of a series compounds varying x=0,0.05, 0.25, 0.5, 0.75, 0.9, and 1.0 with known isovalent pairs.

Optical Properties of $TiO_2/M/Ag/M/TiO_2$ Films with Different Diffusion Barrier Layers (확산방지막에 따른 $TiO_2/M/Ag/M/TiO_2$ 투명 열절연 박막의 광학적 성질)

  • 이경준;이진구;박주동;김진현;김영환;오태성
    • Journal of the Korean Vacuum Society
    • /
    • v.5 no.2
    • /
    • pp.147-155
    • /
    • 1996
  • Optical properties of $TiO_2/M/Ag/M/TiO_2$ films have been changed with the diffusion barrier metal M. Optimum opticla properties of $TiO_2/M/Ag/M/TiO_2$ as the transparent heat mirror film, could be obtained with Ti among diffusion barrier metals of Ti, Cu, Zr and Al. $TiO_2/M/Ag/M/TiO_2$ film, which was fabricated by sputtering of 18 nm-thick $TiO_2$ and Ag, and 4nm-thick Ti, showed maximum transimittance of 89% at visible wavelength and infrared reflectance of 97% at wavelength of 3000 nm. Optical properties of this film was not degraded by Xenon-sunshine weather test for 240 hours. For specimens with barrier layers of Cu, Zr, and Al, degradation of optical properties by weather test was increased in a sequence of films with Cu, Zr, and Al barrier layers.

  • PDF