SF6/Ar 유도결합플라즈마를 이용한 ZnO 박막의 식각 특성에 관한 연구 (A Study of Etching Characteristics of the ZnO Thin Film Using a SF6/Ar Inductively Coupled Plasma)

  • 강성칠;이윤찬;이진수;권광호
    • 한국전기전자재료학회논문지
    • /
    • 제24권12호
    • /
    • pp.935-938
    • /
    • 2011
  • The etching characteristics of ZnO and etch selectivities of ZnO to $SiO_2$ in $SF_6$/Ar plasma were investigated using Inductively-coupled-plasma (ICP). The maximum etch rates of ZnO were 6.5 nm/min at $SF_6$(50%)/Ar(50%), Source power (700 W), Bias power (250 W), Working pressure(8 mTorr). The etch rate of ZnO showed a non-monotonic behavior with increasing from 0% to 50% Ar fraction in $SF_6$/ Ar plasma. The plasma diagnostic were characterized using Optical Emission Spectroscopy (OES) analysis measurements.

고밀도 $CF_{4}/Ar$ 플라즈마에서 $YMnO_3$ 박막의 식각 매카니즘 (Etching Mechanism of $YMnO_3$ Thin Films in High Density $CF_{4}/Ar$ Plasma)

  • 이철인;김동표;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 반도체재료
    • /
    • pp.12-16
    • /
    • 2001
  • We investigated the etching characteristics of $YMnO_3$ thin films in high-density plasma etching system. In this study. $YMnO_3$ thin films were etched with $CF_{4}/Ar$ gas chemistries in inductively coupled plasma (ICP). Etch rates of $YMnO_3$ were measured according to gas mixing ratios. The maximum etch rate of $YMnO_3$ is 18 nm/min at $CF_{4}/(CF_{4}+Ar)$ of 20%. In optical emission spectroscopy (OES) analysis, F radical and Ar* ions in plasma at various gas chemistries decreased with increasing $CF_4$ content. Chemical states of $YMnO_3$ films exposed in plasma were investigated with x-ray photoelectron spectroscopy (XPS) and secondary ion mass spectrometry (SIMS). There is a chemical reaction between metal (Y, Mn) and F and metal-fluorides were removed effectively by Ar ion sputtering. $YF_x$, $MnF_x$ such as YF, $YF_2$, $YF_3$ and $MnF_3$ Were detected using SIMS analysis. The etch slope is about $65^{\circ}C$ and free of residues.

  • PDF

태양전지응용을 위하여 MOCVD 방법으로 성장된 ZnO 박막의 기판온도에 따른 표면특성 (The Surface Morphology of ZnO Grown by Metal Organic Chemical Vapor Deposition for an Application of Solar Cell)

  • 김도영;강혜민;김형준
    • 한국진공학회지
    • /
    • 제19권3호
    • /
    • pp.177-183
    • /
    • 2010
  • 우리는 MOCVD (metal organic chemical vapor deposition)법을 이용하여 DEZ (Diethylzinc)을 운송하는 Ar 유속과 reactant (반응물질)의 종류에 따른 ZnO 박막 증착을 연구하였다. Bubbler 시스템을 통하여 주입되는 Ar 유속에 의해 Zn 소스인 DEZ의 양이 조절된다. 산소 기체와 수증기는 산화를 위해 반응물질로 사용된다. 본 연구로부터 표면의 거칠기(surface roughness)는 반응물질의 종류와 DEZ Ar 유속에 관계되며 박막의 두께에 의존한다는 것을 알 수 있었다. 그러나 기판 온도는 산소를 반응물로 하는 상태에서는 표면 거칠기에 영향을 주지 못함을 알 수 있었다. 우리는 ZnO 박막이 90 sccm (Standard Cubic Centimeter per Minute)의 DEZ Ar 유속, 8 Pa의 수증기압, 그리고 $140^{\circ}C$의 기판 온도에서 39.16 mm의 가장 높은 거칠기를 가진다는 것을 확인할 수 있었다. 본 논문은 태양전지의 광 흡수층으로 사용가능한 ZnO 박막을 연구하였다.

Cl-based 플라즈마에 의한 YMnO3 박막의 식각 damage에 관한 연구 (Study on Etching Damages of YMnO3 Thin Films by Cl-based Plasma)

  • 박재화;기경태;김동표;김창일;장의구
    • 한국전기전자재료학회논문지
    • /
    • 제16권6호
    • /
    • pp.449-453
    • /
    • 2003
  • Ferroelectric YMnO$_3$ thin films were etched with Ar/Cl$_2$ and CF$_4$/Cl$_2$ inductively coupled plasma (ICP). The maximum etch rate of YMnO$_3$ thin film was 300 $\AA$/min at a Ar/Cl$_2$ gas mixing ratio of 2/8, a RF power of 800 W, a DE bias of 200 V, a chamber pressure of 15 mTorr, and a substrate temperature of 30 $^{\circ}C$. From the X-ray photoelectron spectroscopy (XPS) analysis, yttrium etched by chemical reactions with Cl radicals assisted by Ar ion bombardments in Ar/Cl$_2$ plasma. In CF$_4$/Cl$_2$ plasma, yttrium are remained on the etched surface of YMnO$_3$ and formed of nonvolatile YF$_{x}$ compounds manganese etched effectively by chemical reactions with Cl and F radicals. From the X-ray diffraction (XRD) analysis, the (0004) diffraction peak intensity of the YMnO$_3$ thin film etched in Ar/Cl$_2$ plasma shows lower value than that in CF$_4$/Cl$_2$ plasma. It indicates that the crystallinty of YMnO$_3$ thin film is more easily damaged by the Ar ion bombardment than the changes of stoichiometry due to nonvolatile etch by-products.s.

비정질 텔루륨 산화물 박막 특성에 미치는 O2/Ar 가스비율의 영향 (Effect of O2/Ar Gas Ratios on the Characteristics of Amorphous Tellurium Oxide Thin Films)

  • 공헌;정건홍;여종빈;이현용
    • 한국전기전자재료학회논문지
    • /
    • 제30권5호
    • /
    • pp.294-300
    • /
    • 2017
  • $TeO_x$ thin films were deposited at various $O_2$/Ar gas-flow ratios by a reactive RFmagneton sputtering technique from $TeO_2$ and Te targets. X-ray diffraction (XRD) results revealed that the $TeO_x$ thin films were amorphous. The structure and chemical composition of the $TeO_x$ thin films were investigated by fourier transform infrared spectroscopy (FT-IR) and X-ray photoelectron spectroscopy (XPS). The optical characteristics of the $TeO_x$ thin films were investigated by an Ellipsometer and a UV-VIS-NIR spectrophotometer. According to the $O_2$/Ar gas-flow ratios, the atomic composition ratio of $TeO_x$ thin films was divided into two regions(x=1-2, 2-3). Different optical characteristics were shown in each region. With an increasing $O_2$/Ar gas-flow ratio, the refractive index of the $TeO_x$ thin films decreased and the optical bandgap of the films increased.

고주파 마그네트론 스퍼터링으로 제조한 SiO$_2$ 절연박막의 구조분석 및 절연저항에 관한 연구 (Insulation Properties and Microstructure of SiO$_2$ Film Prepared by rf Magnetron Sputtering)

  • 박태순;이성래
    • 한국표면공학회지
    • /
    • 제35권2호
    • /
    • pp.113-121
    • /
    • 2002
  • We have investigated insulating properties of $SiO_2$ interlayer for the thin film strain gauge, which were prepared by RF magnetron sputtering method in various deposition conditions, such as Ar pressure, gas flow rates and sputtering gases. SEM, AFM and FT-IR techniques were used to analyze its structures and composition. As the Ar pressure and the flow rate increased, the insulating interlayer showed low insulating resistance due to its porous structure and defects. Oxygen deficiency in $SiO_2$ was decreased as fabricated by hydrogen reactive sputtering. We could enhance the surface mobility of sputtered adatoms by using Ar/$H_2$ sputtering gas and obtain a good surface roughness and insulating property. The optimum insulating resistance of 9.22 G$\Omega$ was obtained in Ar/30% $H_2$ mixed gas, flow rate 10sccm, and 1mTorr.

$O_{2}$ re-annealing에 의한 식각된 PZT 박막의 식각 damage 개선 (Recovery of Etching Damage of the etched PZT Thin Films With $O_{2}$ Re-Annealing.)

  • 강명구;김경태;김창일;장의구;이병기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 반도체재료
    • /
    • pp.8-11
    • /
    • 2001
  • In this study. the recovery of plasma induced damage in the etched PZT thin film with $O_2$ re-annealing have been investigated. The PZT thin films were etched as a function of $Cl_2/Ar$ and additive $CF_4$ into $Cl_{2}(80%)/Ar(20)%$. The etch rates of PZT thin films were $1600\dot{A}/min$ at $Cl_{2}(80%)/Ar(20)%$ gas mixing ratio and $1970\dot{A}/min$ at 30 % additive $CF_4$ into $Cl_{2}(80%)/Ar(20)%$. The etched profile of PZT films was obtained above 70 by SEM. In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT phase revealed by x-ray diffraction (XRD). From XPS analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of TixOy is recovered by $O_2$ recombination during rapid thermal annealing process. From AFM images, it shows that the surface roughness of re-annealed sample after etching is improved.

  • PDF

Applications of Ar Gas Cluster Ion Beam Sputtering to Ta2O5 thin films on SiO2/Si (100)

  • Park, Chanae;Chae, HongChol;Kang, Hee Jae
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2015년도 제49회 하계 정기학술대회 초록집
    • /
    • pp.119-119
    • /
    • 2015
  • Ion beam sputtering has been widely used in Secondary Ion Mass Spectrometry (SIMS), X-ray Photoelectron Spectroscopy (XPS), and Auger Electron Spectroscopy (AES) for depth profile or surface cleaning. However, mainly due to severe matrix effects such as surface composition change from its original composition and damage of the surface generated by ion beam bombardment, conventional sputtering skills using mono-atomic primary ions with energy ranging from a few hundred to a thousand volts are not sufficient for the practical surface analysis of next-generation organic/inorganic device materials characterization. Therefore, minimization of the surface matrix effects caused by the ion beam sputtering is one of the key factors in surface analysis. In this work, the electronic structure of a $Ta_2O_5$ thin film on $SiO_2/Si$ (100) after Ar Gas Cluster Ion Beam (GCIB) sputtering was investigated using X-ray photoemission spectroscopy and compared with those obtained via mono-atomic Ar ion beam sputtering. The Ar ion sputtering had a great deal of influence on the electronic structure of the oxide thin film. Ar GCIB sputtering without sample rotation also affected the electronic structure of the oxide thin film. However, Ar GCIB sputtering during sample rotation did not exhibit any significant transition of the electronic structure of the $Ta_2O_5$ thin films. Our results showed that Ar GCIB can be useful for potential applications of oxide materials with sample rotation.

  • PDF

R.F. 마그네트론 스퍼터링을 이용한 LiCoO2 양극활물질의 Ar 증착분압에 따른 박막전지 전극 특성 (Electrode Properties of Thin Film Battery with LiCoO2 Cathode Deposited by R.F. Magnetron Sputtering at Various Ar Partial Pressures)

  • 박호영;임영창;최규길;이기창;박기백;권미연;조성백;남상철
    • 전기화학회지
    • /
    • 제8권1호
    • /
    • pp.37-41
    • /
    • 2005
  • Ar공정 분압에 따라 스퍼터링된 $LiCoO_2$박막 양극의 $400^{\circ}C$저온 열처리를 통한 전기화학적 및 미세구조적 특성을 연구하였다. Ar분압이 변화함에 따라 양극 박막의 미세구조 및 조성이 변화하였으며, Ar분압이 증가할수록 $LiCoO_2$ 박막의 안정성 및 전기화학적 특성이 개선되었다. 순환전류전위법 및 정전류 충방전 시험에 의해 전극반응의 가역성 및 안정성 등을 고찰하였으며, 박막의 조성, 결정성, 표면 특성 등 물리적 특성은 ICP-AES, XRD, SEM 및 AFM을 통해 분석하였다.

$BCl_3/Ar$ 유도 결합 플라즈마를 이용한 ZnO 박막의 식각 특성 (The Etching Characteristics of ZnO thin Films using $BCl_3/Ar$ Inductively Coupled Plasma)

  • 우종창;김관하;김경태;김종규;강찬민;김창일
    • 전기학회논문지
    • /
    • 제56권3호
    • /
    • pp.566-570
    • /
    • 2007
  • The specific electrical, optical and acoustic properties of Zinc Oxide (ZnO) are important for semiconductor process which has many various applications. Piezoelectric ZnO films has been widely used for such as transducers, bulk and surface acoustic-wave resonators, and acousto-optic devices. In this study, we investigated etch characteristics of ZnO thin films in inductively coupled plasma etch system with $BCl_3/Ar$ gas mixture. The etching characteristics of ZnO thin films were investigated in terms of etch rates and selectivities to $SiO_2$ as a function of $BCl_3/Ar$ gas mixing ratio, RF power, DC bias voltage and process pressure. The maximum ZnO etch rate of 172 nm/min was obtained for $BCl_3$ (80%)/Ar(20%) gas mixture. The chemical states on the etched surface were investigated with X-ray photoelectron spectroscopy (XPS).