탄화규소 휘스커의 합성(I) : 반응기구의 율속반응 (Synthesis of Silicon Carbide Whiskers (I) : Reaction Mechanism and Rate-Controlling Reaction)

  • 최헌진;이준근
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1329-1336
    • /
    • 1998
  • A twt -step carbothermal reduction scheme has been employed for the synthesis of SiC whiskers in an Ar or a H2 atmosphere via vapor-solid two-stage and vapor-liquid-solid growth mechanism respectively. It has been shown that the whisker growth proceed through the following reaction mechanism in an Ar at-mosphere : SiO2(S)+C(s)-SiO(v)+CO(v) SiO(v)3CO(v)=SiC(s)whisker+2CO2(v) 2C(s)+2CO2(v)=4CO(v) the third reaction appears to be the rate-controlling reaction since the overall reaction rates are dominated by the carbon which is participated in this reaction. The whisker growth proceeded through the following reaction mechaism in a H2 atmosphere : SiO2(s)+C(s)=SiO(v)+CO(v) 2C(s)+4H2(v)=2CH4(v) SiO(v)+2CH4(v)=SiC(s)whisker+CO(v)+4H2(v) The first reaction appears to be the rate-controlling reaction since the overall reaction rates are enhanced byincreasing the SiO vapor generation rate.

  • PDF

탄화규소 휘스커의 합성(I) : 반응기구의 율속반응 (Synthesis of Silicon Carbide Whiskers (I) : Reaction Mechanism and Rate-Controlling Reaction)

  • 최헌진;이준근
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1336-1336
    • /
    • 1998
  • 2단계 열탄소환원법으로 탄화규소 휘스커를 Ar과 H2분위기에서 기상-고상, 2단계, 기상-액상-고상 성장기구를 통해 각각 합성하였다. Ar분위기에서 탄화규소 휘스커는 다음과 같은 반응기구로 성장하였다. SiO2(S)+C(s)-SiO(v)+CO(v) SiO(v)3CO(v)=SiC(s)whisker+2CO2(v) 2C(s)+2CO2(v)=4CO(v) 이때 전체 반응속도는 세번째 반응에 참여하는 탄소에 의해 지배되었다. 따라서 이 반응이 휘스커 합성의 율속반응으로 판단되었다. 한편 H2 분위기에서 탄화규소 휘스커는 다음과 같은 반응기구로 성장하였다.SiO2(s)+C(s)=SiO(v)+CO(v) 2C(s)+4H2(v)=2CH4(v) SiO(v)+2CH4(v)=SiC(s)whisker+CO(v)+4H2(v) 이때 전체 반응속도는 SiO(v) 기체의발생 속도에 의해 지배되었다. 따라서 첫번째 반응이 휘스커 합성의 율속 반응인 것으로 판단되었다.

Preliminary Study on Chlorination Reaction of Lithium Carbonate for Carbon-Anode-Based Oxide Reduction Applications

  • Jeon, Min Ku;Kim, Sung-Wook;Choi, Eun-Young
    • 방사성폐기물학회지
    • /
    • 제19권2호
    • /
    • pp.225-231
    • /
    • 2021
  • The reaction between Li2CO3 and Cl2 was investigated to verify its occurrence during a carbon-anode-based oxide reduction (OR) process. The reaction temperature was identified as a key factor that determines the reaction rate and maximum conversion ratio. It was found that the reaction should be conducted at or above 500℃ to convert more than 90% of the Li2CO3 to LiCl. Experiments conducted at various total flow rate (Q) / initial sample weight (Wi) ratios revealed that the reaction rate was controlled by the Cl2 mass transfer under the experimental conditions adopted in this work. A linear increase in the progress of reaction with an increase in Cl2 partial pressure (pCl2) was observed in the pCl2 region of 2.03-10.1 kPa for a constant Q of 100 mL·min-1 and Wi of 1.00 g. The results of this study indicate that the reaction between Li2CO3 and Cl2 is fast at 650℃ and the reaction is feasible during the OR process.

Effect of KHCO3 Concentration Using CuO Nanowire for Electrochemical CO2 Reduction Reaction

  • Kanase, Rohini Subhash;Kang, Soon Hyung
    • 마이크로전자및패키징학회지
    • /
    • 제27권4호
    • /
    • pp.11-17
    • /
    • 2020
  • Copper has been proved to be the best catalyst for electrochemical CO2 reduction reaction, however, for optimal efficiency and selectivity, its performance requires improvements. Electrochemical CO2 reduction reaction (RR) using CuO nanowire electrode was performed with different concentrations of KHCO3 electrolyte (0.1 M, 0.5 M, and 1 M). Cu(OH)2 was formed on Cu foil, followed by thermal-treatment at 200℃ under the air atmosphere for 2 hrs to transform it to the crystalline phase of CuO. We evaluated the effects of different KHCO3 electrolyte concentrations on electrochemical CO2 reduction reaction (RR) using the CuO nanowire electrode. At a constant current (5mA), low concentrated bicarbonate exhibited a more negative potential -0.77 V vs. Reversible Hydrogen Electrode (RHE) (briefly abbreviated as VRHE), while the negative potential reduced to -0.33 VRHE in the high concentration of bicarbonate solution. Production of H2 and CH4 increased with an increased concentration of electrolyte (KHCO3). CH4 production efficiency was high at low negative potential whereas HCOOH was not influenced by bicarbonate concentration. Our study provides insights into efficient, economically viable, and sustainable methods of mitigating the harmful environmental effects of CO2 emission.

Ni0.5Co0.5Fe2O4의 수소환원에 의한 나노구조 Fe-Ni-Co 합금의 제조 및 자성특성 (Synthesis and Magnetic Property of Nanocrystalline Fe-Ni-Co Alloys during Hydrogen Reduction of Ni0.5Co0.5Fe2O4)

  • 백민규;도경효;;박종진
    • 대한금속재료학회지
    • /
    • 제49권2호
    • /
    • pp.167-173
    • /
    • 2011
  • Nickel cobalt ferrite($Ni_{0.5}Co_{0.5}Fe_2O_4$) powder was prepared through the ceramic route by the calcination of a stoichiometric mixture of NiO, CoO and $Fe_2O_3$ at $1100^{\circ}C$. The pressed pellets of $Ni_{0.5}Co_{0.5}Fe_2O_4$ were isothermally reduced in pure hydrogen at $800{\sim}1100^{\circ}C$. Based on the thermogravimetric analysis, the reduction behavior and the kinetic reaction mechanisms of the synthesized ferrite were studied. The initial ferrite powder and the various reduction products were characterized by X-ray diffraction, scanning electron microscopy, reflected light microscope and vibrating sample magnetometer to reveal the effect of hydrogen reduction on the composition, microstructure and magnetic properties of the produced Fe-Ni-Co alloy. The arrhenius equation with the approved mathematical formulations for the gas solid reaction was applied to calculate the activation energy($E_a$) and detect the controlling reaction mechanisms. In the initial stage of hydrogen reduction, the reduction rate was controlled by the gas diffusion and the interfacial chemical reaction. However, in later stages, the rate was controlled by the interfacial chemical reaction. The nature of the hydrogen reduction and the magnetic property changes for nickel cobalt ferrite were compared with the previous result for nickel ferrite. The microstructural development of the synthesized Fe-Ni-Co alloy with an increase in the reduction temperature improved its soft magnetic properties by increasing the saturation magnetization($M_s$) and by decreasing the coercivity($H_c$). The Fe-Ni-Co alloy showed higher saturation magnetization compared to Fe-Ni alloy.

$CO_2$ 첨가가 $CH_4$-공기 대향류 확산화염의 구조 및 NOx 생성에 미치는 영향 (Effect of $CO_2$ Addition on Flame Structure and NOx Formation of $CH_4-Air$ Counterflow Diffusion Flames)

  • 이승로;한지웅;이창언
    • 한국연소학회지
    • /
    • 제4권2호
    • /
    • pp.97-108
    • /
    • 1999
  • This numerical study was to investigate the effect of $CO_2$ addition on the structures and NOx formation characteristics in $CH_4$ counterflow diffusion flame. The importance of radiation effect was identified and $CO_2$ addition effect was investigated in terms of thermal and chemical reaction effect. Also the causes of NOx reduction were clarified by separation method of each formation mechanisms. The results were as follows : The radiation effect was intensified by $CO_2$ addition. Thermal effect mainly contributed to the changes in flame structure and the amount of NO formation but the chemical reaction effect also cannot be neglected. The reduction of thermal NO was dominant with respect to reduction rate, but that of prompt NO was dominant with respect to total amount.

  • PDF

습식 화학적 환원법에 의한 AgNO3로부터 Ag 분말의 제조 1. 균일한 구형 Ag 분말의 제조를 위한 최적 반응계 확립 (Preparation of Ag Powder from AgNO3 by Wet Chemical Reduction Method1. The Establishment of Optimum Reaction System for the Preparation of Spherical Ag Powder)

  • 윤기석;박영철;양범석;민현홍;원창환
    • 한국분말재료학회지
    • /
    • 제12권1호
    • /
    • pp.56-63
    • /
    • 2005
  • Ag powder was prepared from $AgNO_3$ by wet chemical reduction method using various reduction agent system involving $AgNO_3$, $AgNO_2$(AgCl) and Ag complex ion aqueous solution. The pure Ag powder could be prepared regardless of reaction system but the particle shape and distribution were affected very much according to the kind of reduction agents and reaction systems. The optimum reaction system for the preparation of the silver powder having the uniform particle shape and size distribution was Ag complex ion aqueous solution-reduction agent system and in particular, $H_2O_2$ and $C_6H_8O_6$as a reduction agent leaded the more uniform particle shape and size distribution.

산화-환원 싸이클 조업에 의한 고순도 수소생성 (High Purity Hydrogen Production by Redox Cycle Operation)

  • 전법주;박지훈
    • 한국수소및신에너지학회논문집
    • /
    • 제21권5호
    • /
    • pp.355-363
    • /
    • 2010
  • High purity hydrogen, 97-99 vol.%, with CO at just ppm levels was obtained in a fixed bed of iron oxide employing the steam-iron cycle operation with reduction at 823K and oxidation in a steam-$N_2$ mixture at 773K TGA experiments indicated that temperature of the reduction step as well as its duration are important for preventing carbon build-up in iron and the intrusion of $CO_2$ into the hydrogen product. At a reduction temperature of 823K, oxide reduction by $H_2$ was considerably faster than reduction by CO. If the length of the reduction step exceeds optimal value, low levels of methane gas appeared in the off-gas. Furthermore, with longer durations of the reduction step and CO levels in the reducing gas greater than 10 vol.%, carbidization of the iron and/or carbon deposition in the bed exhibited the increasing pressure drop over the bed, eventually rendering the reactor inoperable. Reduction using a reducing gas containing 10 vol.% CO and a optimal reduction duration gave constant $H_2$ flow rates and off-gas composition over 10 redox reaction cycles.

Stoichiometry, Thermal Stability and Reducibility of Perovskite-Type Mixed Oxide LaBO$_3$ (B = Fe, Co, Ni)

  • Park, Il-Hyun;Lee, Hyung-Pyo
    • Bulletin of the Korean Chemical Society
    • /
    • 제9권5호
    • /
    • pp.283-288
    • /
    • 1988
  • The titled properties on reduction of the perovskite $LaBO_3$ (B = Fe, Co, Ni) have been investigated by means of temperature-programmed reduction, isothermal reduction and X-ray diffraction methods. Nominal composition of $LaFeO_{3.18},\;LaCoO_{3.00}\;and\;LaNiO_{2.92}$ are determined. Reduction reaction of these mixed oxides differed according to B-site transition metal and thermal stability on reduction decreased as following order: $LaFeO_{3.18}$ > $LaCoO_{3.00}$ > $LaNiO_{2.92}$. From the results of isothermal reaction, kinetics on reduction of the perovskite has been discussed in detail.

Reduction Behavior of Self-Reducing Pellets of Chromite and Si Sludge with and without Carbon

  • Jung, Woo-Gwang;Hossain, Sakib Tanvir;Kim, Jong-Ho;Chang, Young-Chul
    • 한국재료학회지
    • /
    • 제29권10호
    • /
    • pp.592-602
    • /
    • 2019
  • Feasibility is investigated for reduction of chromium ore by Si sludge with mixed silicothermic and carbothermic reaction. The reduction behavior of chromium ore using Si sludge is investigated precisely to determine the effects of carbon addition, reaction time, and reaction temperature. The pellets are dropped into the furnace after temperature stabilized. As the amount of C addition increases, the amounts of CO and $CO_2$ gas generation increase. After the dropping of the pellets, the pellets are heated and the reaction starts at about 1,573 K or higher. The pellets maintain their shape until 10 min after the drop, and then melted. As the holding time increased, the size of the reduced metal particles increased. The chromium ore is rapidly reduced by the Si sludge, and the slag penetrated into the chromium ore and reduction progressed inside. As the reduction temperature increased, the reaction initiation time is shortened and the reaction fraction of the reduction reaction increased. As the reaction temperature increased, agglomeration of reduced ferrochrome metal is promoted.