The growth of amorphous and first crystalline phase, and phase sequence by solid state reaction were examined in Co/Si multilayer thin films by DSC and XRD. The experimental results were compared with the results expected by effective driving force models, PDF and effective heat of formation models.Amorphous phase growth was not observed in Co/Si system and it was consistent with the predicted result by effective driving force. It was observed that the first crystalline phase is CoSi. According to the PDF and effective heat of formation models, the first crystalline phases were CoSi and $CO_2Si$, respectively. The experiemental results were coincident with the PDF model considering structure factors. In case of the atomic concentration ratios of 2Co : 1Si and 1Co : 2Si, the phases sequences were $CoSi\to Co_2Si$ and $CoSi \to Co_2Si \to CoSi \to CoSi_2$, respectively and it was analysized through the effective heat of formation model. The formations of CoSi, $CO_2Si$ and $COSi_2$ in initial stage were controlled by nucleation and the activation energies for the nucleation of three phases were 1.71, 2.34 and 2.79eV.
The D2EHPA/TBP co-extractants immobilized PolyHIPE membrane can be used for the selective separation of Mn (II) from Co (II). By solvent-nonsolvent method, D2EHPA/TBP co-extractants can be effectively immobilized into PolyHIPE membrane. The pore structure of PolyHIPE membrane and the presence of TBP enhance the stability of immobilized co-extractants. The optimal operating conditions for the separation of Mn (II) and Co (II) are feeding phase at pH 5.5, sulfuric acid concentration in the stripping phase of about 50 g/L and stirring speed at 400 rpm. The D2EHPA/TBP co-extractants ratio of 5:1 shows synergetic effect on Mn/Co separation factor about 22.74. The removal rate and recovery rate of Mn (II) is about 98.4 and 97.1%, respectively, while for Co (II) the transport efficiency is insignificant. The kinetic study of Mn (II) transport shows that high initial flux, $J_f^o=80.1({\mu}mol/m^2s)$, and maxima stripping flux, $J_s^{max}=20.8({\mu}mol/m^2s)$, can be achieved with D2EHPA/TBP co-extractants immobilized PolyHIPE membrane. The stability and reusability study shows that the membrane can maintain a long term performance with high efficiency. High purity of Co (II) and Mn (II) can be recovered from the feeding phase and stripping phase, respectively.
$LiMO_{2}(M=Co,Ni)$ samples were synthesized with $Li_{2}CO_{3},\;Co_{3}O_{4}$, and NiO by the solid-state reaction method. In the case of $LiCoO_{2}$, at low temperature$(T=400^{\circ}C)$ spinel structure was synthesized and the obtained spinel phase was transformed to layered phase at high temperature$(T\ge600^{\circ}C)$. The phase transition behaviors of $LiCoO_{2}$ were investigated with various heating temperature and time. The rate of transition was directly proportional to the concentrations of reactant, and activation energy of reaction was around 6.76 kcal/mol. When CoO(rock salt structure) was used as a starting material instead of $Co_{3}O_{4}$(spinel structure), layered structure of $LiCoO_{2}$ was obtained at low temperature. In the case of $LiNiO_{2}$ the transition from layered structure to rock salt structure occurred easily by disordering/ordering reaction, but did not occur in $LiCoO_{2}$. The difference in metal ion radii in $LiCoO_{2}$ and $LiNiO_{2}$ results in different behaviors of phase transitions.
Kim, Eng-Chan;Lee, S.R.;Kim, T.H.;Ryu, Y.S.;Cho, J.H.;Joh, Y.G.;Kim, D.H.
Journal of the Korean Magnetics Society
/
v.16
no.1
/
pp.11-13
/
2006
[ $M\"{o}ssbauer$ ] spectra of $Ti_{1-x-y}Co_xFe_yO_2(0.01{\leq}x,\;y{\leq}0.05)$ prepared with $^{57}Fe$ enriched iron have been taken at various temperatures ranging from 80 to 300K. The Mossbauer spectrum of $Ti0.94Co_{0.03}Fe_{0.03}O_2$ consists of a ferromagnetic (six-Lorentzian), a paramagnetic phase (doublet) and armorphous phase over all temperature ranges. Isomer shifts indicate $Fe^{3+}$ for the ferromagnetic phase and the paramagneic phase of $Ti_{1-x-y}Co_xFe_yO_2$ samples. It is noted that the magnetic hyperfine field of ferromagnetic phase had the value about 1.5 times as large as that of u-fe. The XRB data for $Ti_{1-x-y}Co_xFe_yO_2$ showed mainly rutile phase with tetragonal structures without any segregation of Co and Fe into particulates within the instrumental resolution limit. The magnetic moment per (Co+Fe) atom in $Ti0.94Co_{0.03}Fe_{0.03}O_2$, under the applied field of 1T was estimated to be about $0.332{\mu}_B$ which is ten times as large as that of $Ti0.97Co_{0.03}Fe_{0.03}O_2,\;0.024{\mu}_B$ per Co atom, suggesting a high spin configuration of Co and fe ions.
Park, Dae-Seo;O, Beom-Hoan;Park, Se-Geun;Lee, El-Hang;Park, Jae-Hyun;Lee, Seung-Gol
Journal of the Optical Society of Korea
/
v.14
no.2
/
pp.131-136
/
2010
Modification of the phase gradient formulation is proposed in order to make phase retrieval less susceptible to noise. The modified formulation is derived from separation of the phase terms and the intensity modulation terms of interferograms, and subsequent differentiation to reduce the noise-induced error of the phase gradient vector. Its performance is evaluated and compared to that of the conventional formulation, and noise-robust nature is confirmed.
CO2 storage technology in an aquifer is one of the most effective way to decrease global warming due to a high storage capacity and economics. A demonstration-scale offshore CO2 storage project was performed in a geological deep aquifer in the Pohang Basin, Korea for a technological development of large-scale CO2 storage. A challenging issue in the early design stage of the project was to establish the proper injectivity during CO2 injection. To solve this issue, injection conditions were calculated by calculating injection rate, pressure, temperature, CO2 phase change, and thermodynamic properties. For this study, we simulated and numerically analyzed CO2 phase change from gas to supercritical phase and flow behavior in transport piping and injection tubing using OLGA program. Our results provide the injectivity conditions of CO2 injection system combined with a bottomhole pressure of an aquifer.
Proceedings of the Korean Powder Metallurgy Institute Conference
/
2006.09a
/
pp.635-636
/
2006
In this study, the diffusion behaviors of C and Co in liquid phase sintering of WC-Co system were investigated whether these two components diffused in the same direction in case of having opposite gradient each other with not being $\eta$ phase. The green compacts with controlled compositions in not being of $\eta$ phase and gradient composition which one is WC-5Co-1.2%C, the other is WC-XCo-0.2%C (where X = 5, 10, 15, 20, 25) were sintered at $1350^{\circ}C$ and $1400^{\circ}C$ and then the diffusion behaviors of C and Co were investigated by analyses of compositional change, also determined for microstructure and microhardness. Also, same testing was carried out on the specimens with dual layers sintered in upright and reverse positions to evaluate the effect of gravity on the diffusion in liquid Co. From the results of this study, we can find the fact that the direction of diffusion for C and Co in WC-Co system during liquid phase sintering was different and the effect of gravity for the liquid was insignificant. Also other physical properties were changed on the diffusion of elements.
Journal of Advanced Marine Engineering and Technology
/
v.29
no.8
/
pp.946-952
/
2005
The $CO_{2}$ refrigeration cycle is expected to reduce the compressor work and increase the COP by applying two-phase ejector as a device for the recovery of dissipated expansion energy. In this study, the performance of the cycle was simulated and effects of the ejector shapes on the performance of the $CO_{2}$ refrigeration cycle were investigated. The following results were obtained through the cycle simulation. The COP of the $CO_{2}$ refrigeration cycle with two-phase ejector flow which expansion is occured in the isentropic manner is increased by a maximum of 24 $\%$ than the basic cycle with expansion valve If the velocity nonequilibrium in the mixing process is assumed the COP of the cycle is increased with the increase of the length and the decrease of the section area of the mixing tube. The best cycle performance is obtained when the divergent angle of diffuser is 7.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
1998.06a
/
pp.375-377
/
1998
The magneto-optical properties of Co/Co$_2$TiSn two-phase magnet films were studied. These films show that relatively large Kerr rotations which are -0.4 deg. at the wavelength of 400 nm, compared to that of pure Co. It is conceivable that the magneto-optical effects may be due to both contributions of ferromagnetic Co matrix and ferromagnetic Co$_2$TiSn Heusler alloy precipitate. The perpendicular magnetization curve domonstrates a typical bubble domain hysteresis loop. the saturation magnetization change of the annealed film is less sensitive to temperature in the low temperature region and the Curie temperature of Co$_2$TiSn Heusler alloy precipitate is a little higher in the annealed film. These can be explained by the increase of the number of Co-Co exchange interaction in Heusler alloy structure resulting from the change of chemical ordering by annealing.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.