황토와 플라이 애시를 혼입한 시멘트 모르타르 벽돌의 물리 · 역학적 특성 (Physical and Mechanical Properties of Cement Mortar Brick with Loess and Fly Ash)

  • 임성수;성찬용
    • 한국농공학회논문집
    • /
    • 제46권3호
    • /
    • pp.57-63
    • /
    • 2004
  • This study was performed to evaluate the engineering properties of cement mortar brick with loess and fly ash. The unit weight was in the range of $2,068{\sim}2,137\;kgf/m^{3}$ and $1,899{\sim}2,045\;kgf/m^{3}$ in water and dry curing, respectively It was decreased with increasing the loess content. The absorption ratio was in the range of $5.2{\sim}13.1%$ and $8.5{\sim}13.2%$ in water and dry curing, respectively. The compressive strength was decreased with increasing the loess content. The compressive strength of the 193 $kgf/m^{2}$ in water and 188 $kgf/m^{2}$ in dry curing at the curing age 28 days of the binder volume ratio 35% was exceeded in 163 $kgf/m^{2}$ of standard compressive strength about cement bricks. The carbonation depth was in the range of $0.9{\sim}1.4$ mm, $1.2{\sim}3.6$ mm, $1.4{\sim}6.7$ mm and $2.4{\sim}12.5$ mm in dry curing of curing age 14days, 28days, 90days and 360days, respectively.

기포콘크리트를 이용한 친환경 내화충전제개발에 관한 기초적 연구 (A Fundamental Study on the Development of Fire Resistance Filling of Friendly Environment Using Aerated Concrete)

  • 이종일;임남기
    • KIEAE Journal
    • /
    • 제7권4호
    • /
    • pp.119-126
    • /
    • 2007
  • In this study, we processed two procedures of application test of filler for fire-resistance utility that are new application methods of aerated concrete and properties test of aerated concrete according to mixing ratio because we investigated the better use of aerated concrete as filler for fireproof safety and we proposed basic data about standardization of mixing of aerated concrete. We measured flow and volume change of aerated concrete. And if its volume doesn't change, we added measuring unit weight and compressive strength. To test application of aerated concrete as filler for fireproof safety, we filled up aerated concrete to fireproof safety according to suitable mixing ratio. Then we measured maximum temperature of inner part of fireproof safety in accordance with the standard test of fireproof. According to the results, aerated concrete as filler for fireproof safety could be possibly used. So when we make aerated concrete, we should consider using an adding agent as well as a foaming agent.

웜기어의 강도평가 및 설계시스템 개발에 관한 연구 (Development of Durability Estimation and Design Systems of Worm Gears)

  • 정태형;백재협
    • 한국자동차공학회논문집
    • /
    • 제5권1호
    • /
    • pp.207-216
    • /
    • 1997
  • We developed the durability estimation and design systems to minimize the volume, considering the durability, efficiency, and design requirements of worm gears. That is, we consider each kind of factors affecting on durability on the basis of AGMA Standard for the cylindrical and double-enveloping worm gears. We also estimate input power on the basis of wear and durability, bending strength and deflection of worm shaft, and we developed the durability estimation and design systems of power transmission worm gears introducing the optimal design method on the personal computer to be easily used in field. Also, we developed a method which converts the design variables obtained from the optimal design method to integer values(number of worm threads, number of worm threads, number of worm wheel teeth, etc.,) to be used in real design and production. The developed durability estimation and design method can be easily applied to the design of worm gears used as power transmission devices in machineries and is expected to be used for weight minimization of worm gear unit.

  • PDF

Properties of recycled steel fibre reinforced expanded perlite based geopolymer mortars

  • Celikten, Serhat
    • Advances in concrete construction
    • /
    • 제13권1호
    • /
    • pp.25-34
    • /
    • 2022
  • The production of geopolymer is considered as a cleaner process due to much lower CO2 emission than that from the production of Portland cement. This paper presents a study of the potential use of recycled steel fibre (RSF) coming from the recycling process of the old tires in geopolymer mortars. Ground expanded perlite (EP) is used as a source of alumino-silicate and sodium hydroxide (NaOH=5, 10, 15, and 20M) is used as alkaline medium for geopolymer synthesis. RSFs were added to the mortar mixtures in four different volume fractions (0, 0.5, 1.0, and 1.5% of the total volume of mortar). The unit weight, ultrasound pulse velocity, flexural and compressive strength of expanded perlite based geopolymer mortar (EPGM) mixtures were determined. The microstructures of selected EPGMs were examined by scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) analyses. The optimum molarity of sodium hydroxide solution was found to be 15M for geopolymer synthesis by EP. The test results revealed that RSFs can be successfully used for fibre-reinforced geopolymer production.

섬유 종류에 따른 섬유 보강 시멘트 복합체의 전기적 특성에 대한 실험적 연구 (Correlation between Electrical Conductivity and Shielding Effectiveness of Cementitous Composites according to Length and Volume Fraction of Steel Fiber)

  • 이예찬;김규용;한승현;최윤성;김문규;남정수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 봄 학술논문 발표대회
    • /
    • pp.183-184
    • /
    • 2023
  • The purpose of this study is to compare and analyze the effect of type and volume fraction of fiber on the electrical conductivity and shielding effectiveness of cementitious composites. The large specific surface area of amorphous metallic fiber, as well as the high number of fibers per unit weight, provided an advantage in the formation of conductive path. As the result, the electrical conductivity of amorphous metallic fiber was evaluated to be higher, and the shielding effectiveness was also higher. However, the shielding effectiveness according to electrical conductivity was confirmed to have a threshold point, and further research is needed to improve it.

  • PDF

콘크리트용 골재로서 실리콘 망간슬래그의 물리적 적합성 평가 (Physical Suitability Evaluation of Silicon manganese slag as Aggregate for Concrete)

  • 정의인;김봉주;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.41-42
    • /
    • 2015
  • The concrete aggregate generates carbon dioxide in production but its demanding is gradually increased in accordance with the depletion of natural resources. Therefore we evaluated compatibility and basic physical properties of Silicon manganese slag generated in iron production as an applicable concrete aggregate. In our test, the silicon maganese slag shows 2.8g/㎥ of density in 10mm of maximum particle size similar to a natural aggregate, and its absorption rate was 0.3% similar to the electric furnace slag. Unit volume weight and ratio of absolute volume was respectively 2,001㎏/㎥ and 51%. Strength properties of Silicon manganese slag will be evaluated with further studies and experiments.

  • PDF

제강 슬래그를 이용한 콘크리트의 동결융해에 대한 실험적 연구 (An Experimental Study on the Freezing and Thawing of Concrete Mixed with Steel Slag)

  • 정원섭;조성현;권기주;박성우;김진만
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.48-53
    • /
    • 2003
  • The steel slag, a by-product which is produced on the process of manufacturing steel by refining pig iron is mainly used as road materials after aging it. It is necessary to age steel slag for long time in air because the reaction with water and free-CaO in steel slag could make the volume expanded. Due to this reason it prevents steel slag from being used as aggregate of concrete. But steel slag used in this study is controled by a air-jet method which rapidly cools substance melted at a high temperature. Rapid cooling prevents from generating of free-CaO in steel slag. In this study, it was investigated that steel slag manufactured by air-jet method affects on concrete in the freezing and thawing. As results of this study, concrete mixed with steel slag was worse in the freezing and thawing than concrete mixed with sand in spite of using air entraining agent. To obtain durability of concrete in the freezing and thawing, it is desirable to mix 50% of steel slag in concrete per unit weight of volume.

  • PDF

급냉 전기로 산화슬래그 대체율에 따른 무수축 그라우터의 공학적 특성 (Engineering Properties of Non Shrinkage Grouter According to Replacement Ratio of Rapidly Cooled Electric Arc Furnace Oxidizing Slag)

  • 성종현;선정수;홍성록;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.318-320
    • /
    • 2013
  • The spherical bead manufactured by rapidly cooling process shows high density of 3.64g/㎤, high unit volume weight of 2.6kg/l, and high solid volume of 71%. When it applies to the grouter, it is possible to obtain even high fluidity with only a small amount. This study, focusing the grouter using a rapidly-cooled electric arc furnace oxidizing slag(RC-EAFS), deals with the properties of flow and setting time in fresh state, compressive strength and length variation at 1, 3, 7 and 28 curing day in hardened state. As the results, even though the grouter with RC-EAFS shows comparative low strength, it will be possible to development the competitive product due to the properties of increasing flow and low cost.

  • PDF

경량잔골재 치환율에 따른 고로슬래그 대량사용 모르타르의 유동성 및 압축강도 평가 (Evaluation of the Fluidity and Compressive Strength of Mortar Containing High Volume Blast Furnace Slag by Replacement Ratio of Lightweight Fine Aggregate)

  • 김도빈;김영욱;김성진;김정현;반준모;최세진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2017년도 춘계 학술논문 발표대회
    • /
    • pp.208-209
    • /
    • 2017
  • This study analyzed the fluidity and strength properties of mortar containing high volume blast furnace slag by replacement ratio of lightweight fine aggregate for reducing the unit weight of concrete structures.

  • PDF

도석을 점결제로 상용한 하수슬러지 인공경량골재의 개발에 관한 실험적 연구 (An Experimental Study on the Development of Sewage Sludge Artificial Light-weight Aggregate Using Pottery Stone)

  • 정의승;사순헌;지석원;서치호
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2010년도 춘계 학술논문 발표대회 1부
    • /
    • pp.91-94
    • /
    • 2010
  • The purpose of this study is to produce artificial lightweight aggregate. The properties of aggregate are deducted by analysing the plasticity of aggregate according to the addictive contents of $CaCO_3$ and $Al_2O_3$ on constant plastic temperature($1150^{\circ}C{\sim}1160^{\circ}C$) and the specific gravity, the percentage of water absorbtion. The density on the temperature of $1150^{\circ}C{\sim}1160^{\circ}C$ which results from that the plastic temperature of pottery stone is decreased by increasing the addictive contents of $CaCO_3$ and $Al_2O_3$ manufacturing artificial light weight aggregate using pottery stone is included in the arrange of light weight aggregate density. And the percentage of water absorbtion is 4.2~14% which is similar to or lower than existing artificial light weight aggregate. The unit volume weight is in inverse proportion to density and to increase addictive contents of flux.