• 제목/요약/키워드: wear, material transfer

검색결과 47건 처리시간 0.035초

자동차용 마찰재의 연마제(ZrSiO$_4$) 크기에 따른 마찰특성에 관한 연구 (Tribological Behavior of Automotive Brake Pads with Different Sizes of an Abrasive Material(ZrSiO$_4$))

  • 홍영석;고길주;장호
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2000년도 제31회 춘계학술대회
    • /
    • pp.180-186
    • /
    • 2000
  • Friction materials with four different sizes of zircon - l${\mu}{\textrm}{m}$, 6${\mu}{\textrm}{m}$, 75${\mu}{\textrm}{m}$, 140${\mu}{\textrm}{m}$- were investigated to evaluate the size effects of abrasive particles used in the automotive brake pads on brake performance. Although the brake pads with the largest size of zircon showed a good frictional stability and low wear, rotors were severely abraded due to the aggressiveness of coarse Bircon. As the siBe of zircon decreased. friction force and the amplitude of friction coefficient increased. Considering the above results, abrasive materials were thought to destroy transfer film and the extent of the destruction depends on the size of zircon. The small size zircon was not effective in developing a transfer layer on the rotor surface while minimizing the damage on the counter surface.

  • PDF

마찰재에 함유된 금속섬유의 종류에 따른 마찰 특성 (Tribology of friction materials containing different metal fibers)

  • 고길주;장호
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제33회 춘계학술대회 개최
    • /
    • pp.55-63
    • /
    • 2001
  • Friction and wear properties of brake friction materials containing different metal fibers (Al, Cu or Steel fibers) were investigated using a pad-on-disk type friction tester. Two different materials(gray iron and Al-MMC)) were used for disks rubbing against the friction materials. Results from ambient temperature tests revealed that the friction material containing Cu fibers sliding against cast iron disk showed a distinct negative ${\mu}$-ν (friction coefficient vs. sliding velocity) relation implying possible stick-slip generation at low speed. The negative ${\mu}$-ν relation was not observed when the Cu-containing friction materials were rubbed against the. Al-MMC counter surface. As applied loads increased, friction materials showed higher friction coefficients comparatively. Friction materials slid against cast iron disks exhibited higher friction coefficients than Al-MMC disks during high temperature tests. On the other hand, high temperature test results suggested that copper fibers in the friction material improved fade resistance and the steel fibers were not compatible with Al-MMC disks showing severe material transfer and erratic friction behavior during sliding at elevated temperatures.

  • PDF

Stellite bearings for liquid Zn-/Al-Systems with advanced chemical and physical properties by Mechanical Alloying and Standard-PM-Route

  • Zoz, H.;Benz, H.U.;Huettebraeucker, K.;Furken, L.;Ren, H.;Reichardt, R.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2000년도 춘계학술강연 및 발표대회 강연 및 발표논문 초록집
    • /
    • pp.9-10
    • /
    • 2000
  • An important business-field of world-wide steel-industry is the coating of thin metal-sheets with zinc, zinc-aluminum and aluminum based materials. These products mostly go into automotive industry. in particular for the car-body. into building and construction industry as well as household appliances. Due to mass-production, the processing is done in large continuously operating plants where the mostly cold-rolled metal-strip as the substrate is handled in coils up to 40 tons unwind before and rolled up again after passing the processing plant which includes cleaning, annealing, hot-dip galvanizing / aluminizing and chemical treatment. In the liquid Zn, Zn-AI, AI-Zn and AI-Si bathes a combined action of corrosion and wear under high temperature and high stress onto the transfer components (rolls) accounts for major economic losses. Most critical here are the bearing systems of these rolls operating in the liquid system. Rolls in liquid system can not be avoided as they are needed to transfer the steel-strip into and out of the crucible. Since several years, ceramic roller bearings are tested here [1.2], however, in particular due to uncontrollable Slag-impurities within the hot bath [3], slide bearings are still expected to be of a higher potential [4]. The today's state of the art is the application of slide bearings based on Stellite\ulcorneragainst Stellite which is in general a 50-60 wt% Co-matrix with incorporated Cr- and W-carbides and other composites. Indeed Stellite is used as the bearing-material as of it's chemical properties (does not go into solution), the physical properties in particular with poor lubricating properties are not satisfying at all. To increase the Sliding behavior in the bearing system, about 0.15-0.2 wt% of lead has been added into the hot-bath in the past. Due to environmental regulations. this had to be reduced dramatically_ This together with the heavily increasing production rates expressed by increased velocity of the substrate-steel-band up to 200 m/min and increased tractate power up to 10 tons in modern plants. leads to life times of the bearings of a few up to several days only. To improve this situation. the Mechanical Alloying (MA) TeChnique [5.6.7.8] is used to prOduce advanced Stellite-based bearing materials. A lubricating phase is introduced into Stellite-powder-material by MA, the composite-powder-particles are coated by High Energy Milling (HEM) in order to produce bearing-bushes of approximately 12 kg by Sintering, Liquid Phase Sintering (LPS) and Hot Isostatic Pressing (HIP). The chemical and physical behavior of samples as well as the bearing systems in the hot galvanizing / aluminizing plant are discussed. DependenCies like lubricant material and composite, LPS-binder and composite, particle shape and PM-route with respect to achievable density. (temperature--) shock-reSistibility and corrosive-wear behavior will be described. The materials are characterized by particle size analysis (laser diffraction), scanning electron microscopy and X-ray diffraction. corrosive-wear behavior is determined using a special cylinder-in-bush apparatus (CIBA) as well as field-test in real production condition. Part I of this work describes the initial testing phase where different sample materials are produced, characterized, consolidated and tested in the CIBA under a common AI-Zn-system. The results are discussed and the material-system for the large components to be produced for the field test in real production condition is decided. Outlook: Part II of this work will describe the field test in a hot-dip-galvanizing/aluminizing plant of the mechanically alloyed bearing bushes under aluminum-rich liquid metal. Alter testing, the bushes will be characterized and obtained results with respect to wear. expected lifetime, surface roughness and infiltration will be discussed. Part III of this project will describe a second initial testing phase where the won results of part 1+11 will be transferred to the AI-Si system. Part IV of this project will describe the field test in a hot-dip-aluminizing plant of the mechanically alloyed bearing bushes under aluminum liquid metal. After testing. the bushes will be characterized and obtained results with respect to wear. expected lifetime, surface roughness and infiltration will be discussed.

  • PDF

세라믹 ${ZrO}_{2}, {Si}_{3}{N}_{4}$ 및 SiC를 SiC, AISI 4340 및 청동으로 윤활 및 건조조건에서 미끄름시험하였을 때의 마찰 및 마멸 거동 (Friction and wear characteristics during sliding of ${ZrO}_{2}, {Si}_{3}{N}_{4}$ and SiC with SiC, AISI 4340 and bronze under dry and lubricated condition)

  • 강석춘
    • 대한기계학회논문집
    • /
    • 제13권3호
    • /
    • pp.404-410
    • /
    • 1989
  • 본 연구에서는 공업용 세라믹(요업재료등)으로 개발된 것 중에서 가장 마찰특성이 우수할 것으로 간주되고 있는 SiC, Si$_{3}$N$_{4}$와 ZrO$_{2}$ 의 건조 및 윤활마찰특성과 금속과의 마찰특성을 실험적으로 밝히려 한다.

화학적으로 기능화된 탄소나노튜브를 사용한 고분자 복합재료의 제조 및 물성 평가에 대한 연구 (Manufacturing/Material Property Characterization of Polymer Nano-composites with Chemically Functionalized Carbon Nanotubes)

  • 김태구;곽정춘;이내성;이종휘;박주혁
    • 대한기계학회논문집A
    • /
    • 제28권10호
    • /
    • pp.1534-1540
    • /
    • 2004
  • This study aims to obtain fundamental understandings involving the manufacturing processes of nano-composites with chemically surface-modified multi-walled carbon nanotubes(MWCNTs), and explore the role of functionalized MWCNTs in the epoxy/MWCNT composites. For this purpose, MWCNTs were purified by the thermo-chemical oxidation process, and incorporated into an epoxy matrix by in situ polymerization process, the surface of MWCNTs were functionalized with carboxyl functions which were demonstrated by an infrared spectroscopy. The mechanical properties of epoxy/MWCNT nano-composites were measured to investigate the role of a chemically functionalized carbon nanotubes. To improve the dispersion quality of MWCNTs in the epoxy matrix, methanol and acetone were exploited as dispersion media with sonification. The epoxy/MWCNT nano-composites with 1 or 2 wt.% addition of functionalized carbon nanotubes show an improved tensile strength and wear resistance in comparison with pure epoxy, which shows the mechanical load transfer improves through chemical bonds between epoxy and functionalized MWCNTs. The tensile strength with 7 wt.% functionalized MWCNTs increases by 28% and the wear resistance is dramatically improved by 100 times.

플라즈마 용사된 Al2O3-TiO2 코팅의 전기적 특성 (The Electrical Behavior of Plasma Sprayed Al2O3-TiO2 Coatings)

  • 박상준;이성민
    • 한국전기전자재료학회논문지
    • /
    • 제30권12호
    • /
    • pp.788-793
    • /
    • 2017
  • Electrical behaviors of plasma-sprayed $Al_2O_3-TiO_2$ coatings have been investigated in terms of their $TiO_2$ content. On increasing the $TiO_2$ content from 6 to 30 wt%, the DC electrical conductivity increased by several orders of magnitude. From impedance spectroscopy analysis, the total conductivity of the grains and grain boundaries and their respective activation energies were determined without the electrode effects that could impede ionic transfer. An electron transference number was also estimated, ranging between 6.5% and 7.3% for 13 wt% $TiO_2$ and between 0.4% and 0.7% for 30 wt% $TiO_2$ in the coating. Because of the high electronic contribution to the total conductivity, the $Al_2O_3-TiO_2$ coating could be a new candidate material to obtain superior electrical conductivity as well as corrosion and wear resistances.

RF 스퍼터링법에 의한 Al-Sn계 코팅베어링의 제작과 특성 평가 (Preparation of Al-Sn Coating Bearings by RF Sputtering Method and Evaluation of Their Properties)

  • 이찬식;이명훈
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제24권6호
    • /
    • pp.139-146
    • /
    • 2000
  • The development of high performance materials is very important subject in order to enhance the properties of bearings whose role is to transfer energy harmoniously by reducing the problem of friction and wear down, etc. between the interacting solid surfaces in relative motion under high loads in comply with mechanical operating mechanism of engines. In this study, several (100-x)Al-xSn coating films (where x=85, 75, 65 atomic % at Al) on substrates which are abt. 2mm thickenss of Kelmet layer sintered back steel were prepared by using RF sputtering system. These coating films were observed the morphology by SEM(Scanning Electron Microscope) and investigated the crystal structure by XRD(X-ray Diffractor) for their properties. And friction coefficient of these films was measured by ball-on-disc tester for their tribological properties. From the experimental results, it was shown that high performance properties of bearing can be improved greatly by controlling the composition and morphology of material surface with effective use of the plasma-assisted sputtering process.

  • PDF

선삭에서 절삭 속도 제어를 통한 표면 거칠기 향상 (Improvement of Surface Roughness by the Cutting Speed Control for Turning Operation)

  • 최종환
    • 한국기계가공학회지
    • /
    • 제7권2호
    • /
    • pp.23-30
    • /
    • 2008
  • As a basic machining process, turning is a widely used machining process in which a single-point cutting tool removes material from the surface of a rotating material. A common method of evaluating machining performance is to measure the surface roughness. In a turning operation, it is important to select cutting conditions for achieving high cutting performance. As a rule, cutting conditions can be classified into feed rate, depth of cut and insert radius. While cutting process even though cutting conditions are optimized, the average roughness can be deterioration due to wear of the cutting tool edge. In this study, the aim is to maintain the average roughness even though the cutting condition is irregularly changing within the predictable range due to the working environment. First, the surface roughness model influenced by cutting conditions is constructed based on the experimental results in a turning operation, Second, applying the sliding mode control theory to the turning operation model which is composed of the surface roughness model and the motor transfer function, the surface roughness is closed to the desired value. Finally, the effectiveness of this approach is demonstrated through the computer simulation.

  • PDF

마찰재에 함유된 금속섬유와 마찰 특성의 연관관계 (The Effect of Metal Fibers on the Tribology of Automotive Friction Materials)

  • 고길주;조민형;장호
    • Tribology and Lubricants
    • /
    • 제17권4호
    • /
    • pp.267-275
    • /
    • 2001
  • Friction and wear properties of brake friction materials containing different metal fibers (Al, Cu or Steel fibers) were investigated. Based on a simple experimental formulation, friction materials with the same amount of metal fibers were tested using a pad-on-disk type friction tester. Two different materials (gray cast iron and aluminum metal matrix composite (MMC)) were used for disks rubbing against the friction materials. Results front ambient temperature tests revealed that the friction material containing Cu fibers sliding against gray cast iron disk showed a distinct negative $\mu$-v (friction coefficient vs. sliding velocity) relation implying possible stick-slip generation at low speeds. The negative $\mu$- v relation was not observed when the Cu-containing friction materials were rubbed against the Al-MMC counter surface. Elevated temperature tests showed that the friction level and the intensity of friction force oscillation were strongly affected by the thermal conductivity and melting temperature of metallic ingredients of the friction couple. Friction materials slid against cast iron disks exhibited higher friction coefficients than Al-MMC (metal matrix composite) disks during high temperature tests. On the other hand, high temperature test results suggested that copper fibers in the friction material improved fade resistance and that steel fibers were not compatible with Al-MMC disks showing severe material transfer and erratic friction behavior during sliding at elevated temperatures.

소성 가공 해석을 통한 티타늄 합금 볼트 열간 단조 공정 분석 (Titanium alloy bolt hot forging process analysis through plastic working analysis)

  • 최두선;김태민;항봉석;한유진;고강호;박정래;박규백;이정우;김도언
    • Design & Manufacturing
    • /
    • 제14권1호
    • /
    • pp.42-48
    • /
    • 2020
  • Titanium alloy has been in the spotlight as a core material in high-tech industries that require high strength and light weight because it has excellent strength and corrosion resistance and strength is higher than that of steel. Therefore, in various industries, existing steel products are intended to be replaced with titanium alloys. Titanium alloys can cause cutting tool breakage during cutting, and heat generated during cutting does not dissipate, accumulates in tools and workpieces, resulting in large wear and tear on thin workpieces. In addition, since titanium alloy is a metal with high chemical activity, the wear of the tool becomes more severe when the cutting speed is high, so machining of titanium bolt through cutting is very disadvantageous in terms of productivity. Therefore, the production of bolts using titanium alloys is being produced through a forging process to improve productivity and product quality. In this paper, hot forging molding analysis was performed on bolts used for fastening automobile parts using Ti-6Al-4V alloy, which is the most commonly used titanium alloy.