Journal of the Korean Crystal Growth and Crystal Technology
/
v.5
no.3
/
pp.278-283
/
1995
The potassium titanate fibres were synthesized with wet process by the addition of KOH solution to the TiOz gel produced by the reaction between element titanium particles and $H_2O_2$ solution at $50^{\circ}C$. And then they were characterized by XRD, SEM and FT - IR. It was found that potassium titanate fibres were mainly affected by KOH/TiOz mole ratio, synthesis time and aging time in this wet process employed. For $KOH/TiO_2 = 1/1$, synthesizing time 24 hrs, aging time 24 hrs and calcination temperature of TEX>$900^{\circ}C$ for 1 hr, their products were mainly found to be potassium tetratitanate which had thin and long fibres in the range of 10 ~ 20 mm. As the synthesizing time increased and the amount of KOH decreased, potassium tetratitanate was converted into potassium hexatitanate. Also, the length of their fibres became short.
Transactions on Electrical and Electronic Materials
/
v.12
no.5
/
pp.222-225
/
2011
Lead zirconate titanate (PZT) films were fabricated on Pt/Ti/$SiO_2$/Si substrate by the sol-gel method using a sol containing poly(N-vinylpyrrolidone) (PVP). PVP in alkoxide solutions can suppress the condensation reaction in gel films during heat treatment, and increase the viscosity of alkoxide solutions. Single-phase PZT films as thick as 1 ${\mu}m$ were deposited by repetitive coating with successive third-step heat treatments at 150$^{\circ}C$, 350$^{\circ}C$ and 650$^{\circ}C$. After heat treatment, the films were crack free, and optically transparent. As a result, we demonstrated a PZT film with a PVP molar ratio of 0.5, which has a permittivity of 734, a dielectric loss of 0.042, a $P_r$ of 40.5 ${\mu}C/cm^2$ and an $E_c$ of 156 kV/cm.
전압을 인가하였을 때 전계방향에 의해 가역적으로 색이 변화하는 현상을 전기변색(electrochromism)이라고 한다. 이러한 전기채색현상을 보이는 물질을 전기채색물질(electrochromism materials)이라고 하며, 전기채색 물질에 의한 소자를 전기채색소자(electrochromism device : ECD)라고 한다. 전기채색현상은 투과율(transmittance), 반사율(reflectance)의 가역적이며 가시적인 변화이고, 전기화학적인 산화환원 반응과 관련이 있다. 따라서 본 연구에서는 Titanate nanotube(TNT)를 제조하고 전기변색소자(ECD)에 응용하였다. SEM, XRD, UV-Vis등을 이용하여 재료학적 분석을 시행하였으며, 전기화학적 테스트로 cyclic voltammetry를 측정 하였다. 그 결과 TNT 분말은 직경 약 20~30 nm, 길이 약 500~600 nm 의 입자형상을 나타내었으며, X-선 회절시험결과 $H_2Ti_2O_5{\cdot}H_2O$의 층상구조를 나타내었다. 제조된 막은 FTO glass 위에 PEI/(TNT/TBAOH)$_{n-1}$/PDDA의 순으로 코팅되었다. 전기화학적 테스트를 위하여 2전극 시스템을 제작하였으며, 여러 종류의 액체 전해질을 제작하여 cycle voltammetry를 시행하였다. 그 결과, 각각의 전해질에서 "-"영역의 산화환원전위 피크가 뚜렷하게 나타났으며, 짙은 갈색으로의 채색현상을 나타냈다. 본 연구의 결과로서 TNT 박막을 이용한 ECD은 광조절 유리로서 뿐만 아니라, 여러 전기채색 디바이스에 응용될 것으로 사료된다.
Tribological properties of novolac resin composites containing particulate barite (BaSO$_4$) or potassium titanate (K$_2$Oㆍ6(TiO$_2$))whiskers (two typical space fillers for commercial automotive brake linings) were investigated. The emphasis of the current investigation was given to the effect of the two fillers on the propensity of the stick-slip phenomena and formation of stable rubbing surface. A block-on-disk type tribometer was used for friction assessment. Results showed that the BaSO$_4$-filled composite produced large friction force oscillations at slow sliding speeds and created severe damage on the gray iron counter surface. On the other hand, the composite with $K_2$Oㆍ6(TiO$_2$) whiskers formed a stable rubbing surface and showed smooth sliding behavior without large friction force fluctuation. The microscopic observation of the rubbing surface revealed that the $K_2$Oㆍ6(TiO$_2$)whiskers played a key role in the formation of stable rubbing surface and smooth sliding behavior by effectively reinforcing the resin.
Barium Titanate(BaTiO$_3$) nanoparticles were prepared at 22$0^{\circ}C$ through glycothermal process by using barium hydroxide and amorphous titanium hydrous gel as precursor and 1,4-butanediol and distilled water as solvent. It is demonstrated that the size of BaTiO$_3$ particles can be controlled by reaction conditions such as various content of 1,4-butanediol/distilled water volume ratio. This processing method can fabricate BaTiO$_3$ powders, which have a narrow distribution and exhibit good dispersion. The particle size of BaTiO$_3$ powders obtained by glycothermal process were about 50 nm to 200 nm on the condition that reaction temperature was 22$0^{\circ}C$ and holding time was 24 h.
We developed a novel synthesis strategy of titania nanowire arrays by employing simple hydrothermal reaction and ion-exchange reaction techniques. Hydrothermal reactions of metallic titanium powder with $H_2O_2$ in a 10 M NaOH solution produced a new sodium titanate compound, $Na_2Ti_6O_{13}{\cdot}xH_2O$ (x~4.2), as arrays of nanowires of lengths up to 1 mm. Acid-treatment followed by calcination of this material produced arrays of highly crystalline anatase nanowires as evidenced by x-ray diffraction, Raman spectroscopy, and transmission electron microscopy studies. In both cases of sodium titanate and anatase, the nanowires have exceptionally large aspect ratios of 10,000 or higher, and they form arrays over a large area of $1.5 {\times} 3 cm^2$. Observations on the reaction products with varied conditions indicate that the array formation requires simultaneously controlled formation and crystal growth rates of the $Na_2Ti_6O_{13}{\cdot}xH_2O$ phase.
Transactions on Electrical and Electronic Materials
/
v.18
no.3
/
pp.163-168
/
2017
The aim of the current research was to develop and present an effective methodology for simulating and analyzing the electrical and structural properties of piezoelectric material. The finite element method has been used to make precise numerical models when dielectric, piezoelectric and mechanical properties are known. The static and dynamic responses of circular ring-shaped barium titanate piezoelectric material have been investigated using the commercially available finite element software ABAQUS/CAE. To gain insight into the crystal morphology and to evaluate the purity of the material, a microscopic study was conducted using a scanning electron microscope and energy dispersive x-ray analysis. It is found that the maximum electrical potential of 6.43 V is obtained at a resonance frequency of 35 Hz by increasing the vibrating load. The results were then compared with the experimentally predicted data and the results agreed with each other.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2007.06a
/
pp.171-171
/
2007
Dysprosium-doped bismuth titanate (BDT) thin films were successfully deposited on Pt(111)/Ti/$SiO_2$/Si(100) substrates by liquid delivery MOCVD process and their structural and ferroelectric properties were characterized. Fabricated BDT thin films were found to be random orientations, which were confirmed by X-ray diffraction experiment and scanning electron microscope analysis. The crystallinity of the BDT films was improved and the average grain size increased as the crystallization temperature increased from 600 to $720^{\circ}C$ at an interval of $40^{\circ}C$. The BDT thin film annealed at $720^{\circ}C$ showed a large remanent polarization (2Pr) of $52.27\;{\mu}C/cm^2$ at an applied voltage of 5V. The BDT thin film exhibits a good fatigue resistance up to $1.0{\times}10^{11}$ switching cycles at a frequency of 1 MHz with applied pulse of ${\pm}5\;V$. These results indicate that the randomly oriented BDT thin film is a promising candidate among ferroelectric materials useti비 in lead-free nonvolatile ferroelectric random access memory applications.
Proceedings of the Korean Society of Precision Engineering Conference
/
2005.10a
/
pp.641-644
/
2005
The aim of this research is to evaluate the relationship between the total effective moment $(M^E)$ and Bemoulli-Euler bending moment (M) when the ply orientations of UD CFRP in Piezoelectric Zirconate Titanate Composite Actuator (PZTCA) are changed. The obtained results as follows. Firstly, as the performance test results by the CFRP ply orientation, the performance of [0] and [90] were stable. However, while the performance of [+45] was suddenly decreased after 5 hours. Secondly, the change of $M^E$ by the CFRP ply orientation was evaluated. As the CFRP ply orientation was increased from [0] to [+60], the $M^E$ were gradually decreased. However, they became a little bit increased from [+60] to [90]. Finally, after the change of M by the CFRP ply orientation was evaluated, it was found that $M^E=2.2M$ was valid for just [0] and that there was a relationship between $M^E$ and M according to the ply orientation.
This paper presents a novel structural composition for artificial bone scaffolds with an appropriate biocompatibility and biodegradability capability. To achieve this aim, carbon nanotubes, due to their prominent mechanical properties, high biocompatibility with the body and its structural similarities with the natural bone structure are selected in component of the artificial bone structure. Also, according to the piezoelectric properties of natural bone tissue, the barium titanate, which is one of the biocompatible material with body and has piezoelectric property, is used to create self-healing ability. Furthermore, due to the fact that, most of the bone tissue is consists of hydroxyapatite, this material is also added to the artificial bone structure. Finally, polycaprolactone is used in synthetic bone composition as a proper substrate for bone growth and repair. To demonstrate, performance of the presented composition, the mechanical behaviour of the bone scaffold is simulated using ANSYS Workbench software and three dimensional finite element modelling. The obtained results are compared with mechanical behaviour of the natural bone and the previous bone scaffold compositions. The results indicated that, the modulus of elasticity, strength and toughness of the proposed composition of bone scaffold is very close to the natural bone behaviour with respect to the previous bone scaffold compositions and this composition can be employed as an appropriate replacement for bone implants.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.