• Title/Summary/Keyword: superconducting wire

Search Result 254, Processing Time 0.031 seconds

A study on the superconducting properties of Bi-Pb-Sr-Ca-Cu-O superconducting wire with cooling conditions. (냉각 조건에 의한 Bi-Pb-Sr-Ca-Cu-O 초전도 선재의 특성 연구)

  • Kim, Min-Ki;Choi, Hyo-Sang;Choi, Sung-Hyan;Park, Sung-Jin;Han, Byoung-Sung
    • Proceedings of the KIEE Conference
    • /
    • 1993.11a
    • /
    • pp.213-215
    • /
    • 1993
  • Silver-sheathed Bi-Pb-Sr-Ca-Cu-O wires by the powder-in-tube method were preparated to study on the superconducting properties with cooling conditions. Superconducting wires were cooled down in the furnace, air and liquid $N_2$ after sintering at $840^{\circ}C$. Critical current density of sample cooled in the furnace is $5.1{\times}10^3\;A/cm^2$ at 77K, zero magnetic field and Jc of sample cooled in the air is very low. 2223 high-Tc superconducting phase of sample cooled in the air was distroyed. Therefore, we knew that superconducting wire need to cool slowly to get the high critical current density.

  • PDF

The Effect of Different Heat Treatment Processes on Critical Properties of Bi2212/Ag ROSAT Wire (열처리 공정 변화에 따른 Bi2212/Ag ROSAT 선재의 임계 특성)

  • Oh, W.S.;Jang, G.E.;Kim, S.C.;Ha, D.W.;Oh, S.S.
    • Progress in Superconductivity
    • /
    • v.9 no.1
    • /
    • pp.111-114
    • /
    • 2007
  • We have investigated the effect of different heat treatment processes on electrical and magnetic properties of Bi2212/Ag ROSAT wire. The ROSAT wire was fabricated by stacking and arranging 12 filaments Bi2212/Ag tapes in triple rotation symmetry in a Ag tube. ROSAT wires have been prepared using a partial melting method with changing $T_{max}$ and $T_a$ in oxygen atmosphere. The highest critical current density($J_c$) at 65 K under 0 T was $21,158\;A/cm^2$ for wire prepared $890\;^{\circ}C(T_{max})$ and $840\;^{\circ}C(T_a)$, respectively. SEM results indicated that the wire prepared at $890\;^{\circ}C(T_{max})$ and $840\;^{\circ}C(T_a)$ showed better directional phases than the other samples. However the result of magnetic susceptibility measurement indicates that the wire prepared $890\;^{\circ}C(T_{max})$ and $835\;^{\circ}C(T_a)$ had better superconducting phases than the other samples. It was revealed that heat treatment temperature was important factor for superconducting properties of the ROSAT wire.

  • PDF

Analysis of Self-Field Losses in AC Superconducting Wire (교류용 초전도선에서의 자기자계 손실에 관한 연구)

  • Lee, Ji-Kwang;Cha, Guee-Soo;Hahn, Song-Yop
    • Proceedings of the KIEE Conference
    • /
    • 1997.07a
    • /
    • pp.250-252
    • /
    • 1997
  • Phase difference of external magnetic field and self field is known to do an important role in the generation of the AC loss. This paper analize the AC loss of AC superconducting wire in combined action of an AC transport current and AC magnetic field for various phase differences.

  • PDF

Time Delay of Quench Phenomenon in Superconducting wire (초전도선재의 퀜치현상의 시간지연)

  • Oh, B.H.;Hong, I.S.;Jin, H.B.;Ryu, K.S.;Lee, S.H.
    • Proceedings of the KIEE Conference
    • /
    • 1997.07a
    • /
    • pp.270-272
    • /
    • 1997
  • Superconducting wire is quenching as soon as transport current exceeded the critical current value. However transport current exceeded the critical current value, quench is not generated immediately. In this paper, the results of the theoretical study for time delay of quench phenomenon are described.

  • PDF

Numerical Calculation of AC transport current loss of stacked BSCCO wires (수치해석을 이용한 BSCCO 적층 선재들에 교류 통전시 발생하는 손실 계산)

  • Lim, Hyoung-Woo;Han, Byung-Wook;Cha, Guee-Soo;Lee, Hee-Joon
    • Proceedings of the KIEE Conference
    • /
    • 2007.10c
    • /
    • pp.56-58
    • /
    • 2007
  • AC transport current losses is an important factor in the development of superconducting tapes and superconducting power applications. In this paper we compared measurement, calculation and Norris equation of AC transport current loss in BSCCO single and multi stacked wire. And present a distribution flux density and current density in the HTS single wire and multi stacked wire. The result of Measurement and calculation of Ac transport current loss show that the same. And show that HTS characteristic of inside HTS wire.

  • PDF

STUDY ABOUT A CONNECTIVE METHOD OF HIGH Tc SUPERCONDUCTING WIRE FOR LONG WIRE (고온 초전도 선재의 장선화를 위한 접속에 관한 연구)

  • 임성훈;강형곤;이재윤;임성우;한병성
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1997.04a
    • /
    • pp.222-224
    • /
    • 1997
  • This study is about a connective method of High Tc wire for long wire. We prepared silver-sheathed BiPbSrCaCuO wires by the powder-in-tube method. Since the superconducting wires are ceramic, it is very hard to connect each other. In this study, we used a silver sleeve to contract wires and pressed them by various preasures. Then optimum preasure was 9,000 Kgf/$\textrm{cm}^2$ to get the high critical current. The higest critical current was 10A.

  • PDF

Analysis of mechanical characteristics of superconducting field coil for 17 MW class high temperature superconducting synchronous motor

  • Kim, J.H.;Park, S.I.;Im, S.H.;Kim, H.M.
    • Progress in Superconductivity and Cryogenics
    • /
    • v.15 no.3
    • /
    • pp.13-19
    • /
    • 2013
  • Superconducting field coils using a high-temperature superconducting (HTS) wires with high current density generate high magnetic field of 2 to 5 [T] and electromagnetic force (Lorentz force) acting on the superconducting field coils also become a very strong from the point of view of a mechanical characteristics. Because mechanical stress caused by these powerful electromagnetic force is one of the factors which worsens the critical current performance and structural characteristics of HTS wire, the mechanical stress analysis should be performed when designing the superconducting field coils. In this paper, as part of structural design of superconducting field coils for 17 MW class superconducting ship propulsion motor, mechanical stress acting on the superconducting field coils was analyzed and structural safety was also determined by the coupling analysis system that is consists of commercial electromagnetic field analysis program and structural analysis program.

Superconducting properties of internal tin processed $Nb_3Sn$ superconducting wires (내부확산법으로 제조한 $Nb_3Sn$ 초전도 선재의 초전도 특성)

  • Ha, Dong-Woo;Oh, Sang-Soo;Ha, Hong-Soo;Lee, Nam-Jin;Ryu, Kang-Sik
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1556-1558
    • /
    • 1999
  • $Nb_3Sn$ superconducting wires were fabricated in order to investigate the effect of pre-heat treatment for internal tin process. 2 types of Sn reservoir were fabricated. One was arranged one large Sn reservoir in the center of wire, the other arranged several Sn reservoirs inthe wire. Diffusion of Sn is better in the strand divided Sn equally than in the strand had one large Sn reservoir during pre heat-treatment. Critical current was better in the wires divided Sn reservoirs uniformly after whole heat treatment.

  • PDF