• Title/Summary/Keyword: soft magnetic cores

Search Result 27, Processing Time 0.036 seconds

Iron Loss Comparison between Soft Magnetic Composite Core and Laminated Steel Core in Axial Flux Machine (축방향 자속형 전동기에서 연자성복합체 코어와 적층 전기강판 코어의 철손 비교)

  • Lee, Minhyeok;Nam, Kwanghee
    • Proceedings of the KIPE Conference
    • /
    • 2015.11a
    • /
    • pp.217-218
    • /
    • 2015
  • Two axial flux permanent magnet (AFPM) machines using soft magnetic composite (SMC) and lamination steel are studied. Generally stator cores of AFPM machines are manufactured using SMC because AFPM machines need 3 dimensional core structures. However, SMC cores have very disadvantages in magnetic properties. Especially permeability value is much lower than that of lamination steel, so magnetic field density is also lower. In terms of core losses, SMC cores have much larger loss values than lamination steel cores because SMC core can't be laminated. In this study, AFPM machine was designed using laminated steel, and iron losses in two machines using SMC and laminated steel were studied. Simulations were carried out by a commercial 3-D FEM tool.

  • PDF

Effect of rolling parameters on soft-magnetic properties during hot rolling of Fe-based soft magnetic alloy powders (Fe계 연자성 합금 분말의 고온 압연시 자성특성에 미치는 압연인자들의 영향)

  • Kim, H.J.;H.Lee, J.;Lee, S.H.;Park, E.S.;Huh, M.Y.;Bae, J.C.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2009.05a
    • /
    • pp.266-269
    • /
    • 2009
  • Iron-based soft magnetic materials are widely used as cores, such as transformer transformers, motors, and generators. Reducing losses generated from soft magnetic materials of these applications results in improving energy conversion efficiency. Recently, the new P/M soft magnetic material realized an energy loss of 68 W/kg with a drive magnetic flux of 1 T, at a frequency of 1 kHz, rivaling general-purpose electromagnetic steel sheet in the low frequency range of 200 Hz to 1 kHz. In this research, the effect of rolling parameters on soft magnetic properties of Fe-based powder cores was investigated. The Fe-based soft magnetic plates were produced by the hot powder rolling process after both pure Fe and Fe-4%Si powders were canned, evacuated, and sealed in Cu can. The soft magnetic properties such as energy loss and coercive power were measured by B-H curve analyzer. The soft magnetic properties of rolled sheets were measured under conditions of a magnetic flux density of 1 T at a frequency of 200 kHz. It was found that rolling reduction ratio is the most effective parameter on reducing both energy loss and coercivity because of increasing aspect ratio with reduction ratio. By increasing aspect ratio from 1 to 9 through hot rolling of pure Fe powder, a significant loss reduction of one-third that of SPS sample was achieved.

  • PDF

Magnetic Properties of FeCuNbSiB Nanocrystalline Alloy Powder Cores Using Ball-milled Powder

  • Kim, G. H.;T. H. Noh;Park, G. B.;Kim, K. Y.
    • Proceedings of the Korean Magnestics Society Conference
    • /
    • 2002.12a
    • /
    • pp.202-203
    • /
    • 2002
  • Ribbon type nanocrystalline alloy cores have shown excellent soft magnetic properties in the high frequency range because of small crystalline anisotropy and nearly zero magnetostriction[1]. In present, however ribbon alloys gives some limit in applications such as a large inductor and reactors of PFC circuit, which are required good DC bias property and low loss in the high frequency. Powder alloys with ultra fine grain structure can be an important way to overcome this kind of disadvantage, and to improve the high frequency soft magnetic properties in conventional metallic powder cores[2]. (omitted)

  • PDF

Design of Axial Flux Permanent Magnetic Motor Using Soft Magnetic Composite Core (연자성 분말코어를 적용한 축방향 영구 자속형 전동기 설계)

  • Choi, Myung-Wook;Yang, Seung-Jin;Moon, Chae-Joo
    • The Journal of the Korea institute of electronic communication sciences
    • /
    • v.17 no.4
    • /
    • pp.607-616
    • /
    • 2022
  • A new axial flux permanent magnet machine with soft magnetic composited cores is proposed for electric vehicle application in this paper. The windings and soft magnetic composited cores can be designed to form a very compact structure, and; thus, the torque density can be improved greatly. To obtain the a good flux concentrating ability, two toroidally wound internal stator machines are designed and analyzed, and the designed motor is with NdFeB magnet for high-performance electric vehicle application. The 3-D finite-element method is used to analyze the electromagnetic parameter and performance, for performance comparison, a commercial axial flux permanent magnet machine is used. The proposed motor reduced weight about 5.8%, produced torque higher than about 8Nm for existing motor.

Magnetic Properties of Powdered Fe Cores Containing Stainless Steel-making Dusts (스테인레스 제강분진을 함유한 순철 압분코아의 자기특성)

  • Kim S. W.
    • Korean Journal of Materials Research
    • /
    • v.15 no.2
    • /
    • pp.106-111
    • /
    • 2005
  • Effects of stainless steel-making dusts and binder content on compacting $density(\rho)$ and magnetic properties were evaluated. Cores compacted with the mixture of pure Fe powders, $5wt.\%$ dusts and $0.25wt.\%$ binder showed good AC magnetic properties. For example, permeability$({\mu}a)$ and core loss(P) of the cores containing $5wt.\%$ dusts at 500 kHz were 62 and $4008\;{\mu}W/cm^3$, respectively. These properties are almost equivalent to those of competitor's products (i.e, Ancorsteel TC 80 produced by $H\ddot{o}gan\ddot{a}s$ Corp.). The powdered cores obtained from the present work are expected to apply for high-performance soft magnetic components such as normal mode choke filter and pulse transformer.

Magnetic Properties of Sintered Fe Cores Containing Stainless Steel-making Dusts (스테인레스 제강 분진을 함유한 순철 소결코아의 자기특성)

  • 김상원
    • Journal of the Korean Magnetics Society
    • /
    • v.11 no.3
    • /
    • pp.114-121
    • /
    • 2001
  • Effect of sintering temperature and dusts content on sintered density ($\rho$) and magnetic properties were evaluated. Cores sintered at 1350 $^{\circ}C$ for 1 hour with the Fe powders containing up to 10 wt.% dusts showed a good AC/DC properties. For example, the DC magnetic properties of magnetic induction (B$_{15}$), coercive force (H$_{c}$) and permeability ($\mu$$_{max}$) of cores containing 10 wt.% dusts were ranging over 9.8~ 10.9 kG, 2.2-2.3 Oe and 1950~2050, respectively. These magnetic properties are equivalent to those of competitor's (i.e, Ancorsteel produced by Hoganas). The cores obtained from the present work are expected to apply for high-performance soft magnetic components such as automotive and DC motor.

  • PDF

Test Results of SMC Cores as Some Types of Motor Cores

  • Asaka, Kazuo;Ishihara, Chio;Enomoto, Yuuji;Ito, Motoya
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.796-797
    • /
    • 2006
  • SMC(Soft Magnetic Composite) materials which we have newly developed were studied for their applying effects. It shows almost the same motor output power as the laminated Si-steels of 0.35mm in thickness, although core loss of SMC is about 1.5 times that of the laminations. As shown in the results, the SMC motor core is sufficient for real use as a motor core. Furthermore, a 3-D shaped motor core made of SMC can improve approximately 20% of the output compared with the same size motor made of laminations.

  • PDF

Development of Hybrid Insulating Coating for Fe-based Soft Magnetic Powder (철계 연자성 분말용 하이브리드 절연 코팅막 개발)

  • Kim, Jungjoon;Kim, Sungyeom;Kim, Youngkyun;Jang, Taesuk;Kim, Hwi-jun;Kim, Youngjin;Choi, Hyunjoo
    • Journal of Powder Materials
    • /
    • v.28 no.3
    • /
    • pp.233-238
    • /
    • 2021
  • Iron-based amorphous powder attracts increasing attention because of its excellent soft magnetic properties and low iron loss at high frequencies. The development of an insulating layer on the surface of the amorphous soft magnetic powder is important for minimizing the eddy current loss and enhancing the energy efficiency of high-frequency devices by further increasing the electrical resistivity of the cores. In this study, a hybrid insulating coating layer is investigated to compensate for the limitations of monolithic organic or inorganic coating layers. Fe2O3 nanoparticles are added to the flexible silicon-based epoxy layer to prevent magnetic dilution; in addition TiO2 nanoparticles are added to enhance the mechanical durability of the coating layer. In the hybrid coating layer with optimal composition, the decrease in magnetic permeability and saturation magnetization is suppressed.

Effect of Ca and Al Additions on the Magnetic Properties of Nanocrytalline Fe-Si-B-Nb-Cu Alloy Powder Cores

  • Moon, Sun Gyu;Kim, Ji Seung;Sohn, Keun Yong;Park, Won-Wook
    • Journal of Magnetics
    • /
    • v.21 no.2
    • /
    • pp.192-196
    • /
    • 2016
  • The Fe-Si-B-Nb-Cu alloys containing Ca and Al were rapidly solidified to thin ribbons by melt-spinning. The ribbons were ball-milled to make powders, and then mixed with 1 wt.% water glass and 1.5 wt.% lubricant. The mixed powders were burn-off, and then compacted to form toroidal-shaped cores, which were heat treated to crystallize the nano-grain structure and to remove residual stress of material. The characteristics of the powder cores were analyzed using a differential scanning calorimetry (DSC) and a B-H meter. The microstructures were observed using transmission electron microscope (TEM). The optimized soft magnetic properties (${\mu}_i$ and $P_{cv}$) of the powder cores were obtained from the Ca and Al containing alloys after annealing at $530^{\circ}C$ for 1 h. The core loss of Fe-Si-B-Nb-Cu-based powder cores was reduced by the addition of Ca element, and the initial permeability increased due to the addition of Al element.

Effects of Crystal Grain Size and Particle Size on Core Loss For Fe-Si Compressed Cores

  • Takemoto, Satoshi;Saito, Takanobu
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1183-1184
    • /
    • 2006
  • Core loss of soft magnetic powder cores have been focused on to achieve high efficiency of power supplies. In this study the effects of crystal grain size on core loss were investigated by changing heat treatment conditions. It was found that core loss is influenced by crystal grain size because eddy current loss decreased and hysteresis loss increased by making crystal grain size smaller, and it is also influenced by particle size.

  • PDF