해안인접지역 기초 구조물콘크리트의 내염해 성능 평가 -건축구조기준과의 성능비교- (An Evaluation on the Chloride Resistance of Concrete Footing at Coastal Area -Comparision of Performance in Korea Building Code(KBC)-)

  • 박용규;윤기원;김현우;김용로;송영찬
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 추계 학술논문 발표대회
    • /
    • pp.148-149
    • /
    • 2016
  • In this paper, the increase in chloride resistance of footing concrete at coastal area was evaluated by replacement of Mineral Admixture. In KBC 2009, the footing concrete's minimum specific concrete strength at coastal area is determined to 35MPa. However, this is criteria only based on the strength aspect. Thus, it is not considered to increase the chloride resistance by replacement of Mineral Admixture. According to the test results of chloride ions penetration resistance, 35MPa class concrete with OPC 100% shown inaccessible state. Low-strength (24~30MPa class) concretes with Mineral Admixture, however, presented better performances. In addition, chloride diffusion coefficient tests showed identical appearance. Therefore, the current KBC's chloride resistance criteria based on only concrete strength has to review for the reason it can cause many problems (ex. cost increases by growing concrete strength and the environmental issues by a lot of cement use).

  • PDF

식품 가공기술과 포장기술을 활용한 가정대용식 제품 개발 (Development of home meal replacement products by food processing and packaging technology)

  • 유아름;최윤상;홍정선;최희돈
    • 식품과학과 산업
    • /
    • 제50권3호
    • /
    • pp.39-50
    • /
    • 2017
  • In order to secure competitiveness of the home meal replacement (HMR) industry from a long-term perspective, development of packaging and processing technologies must be achieved. The development of technology that can secure freshness, nutrition, and taste but secures the shelf life is the key to the future growth of HMR. The future of HMR can be considered in terms of nutrition, environment and safety. From the nutritional point of view, it is expected that development of healthy HMR such as low-salt, low-sugar, low-fat, and high fiber and premium HMR with functional ingredient enhanced, and personalized HMR for silver, infant and patients will be done. And it is expected that development of HMR utilizing environmentally friendly food or local food, development of energy reduction and environmentally friendly disinfection technology, development of environmentally friendly packaging material, and providing information on HMR preparation using QR code and RFID from the environmental and safe point of view.

측구 콘크리트의 동결융해 저항성능 개선을 위한 실험적 연구 (An Experimental Study on the Improvement of Freezing-Thawing Resistance of Gutter Concrete)

  • 이회근;손유신;김한준;이승훈
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.577-580
    • /
    • 2006
  • This paper presents the experimental results of frost durability characteristics including freezing-thawing and de-icing salt scaling of the concrete used for gutter of the road. Mixtures were proportioned with the three level of water-binder ratio (W/B), 0.58, 0.53, and 0.48, and two binder compositions corresponding to Type I cement without any supplementary cementitious materials (OPC) and Type I cement with 30% blast-furnace slag replacement (Slag30). Also, two different solutions of calcium chloride and water that contains 0 and 8g of anhydrous calcium chloride in each 100 mL of solution, respectively, were used to evaluate their effect on the frost durability resistance. Test results showed that the Slag30 mixture exhibited higher durability factor and lower mass loss values than those made with OPC. Among the mixture tested in this work, the mixtures (OPC and Slag30) made with a relatively higher W/B of 0.58 exhibited large amount of the de-icing salt scaling regardless of calcium chloride concentration. Finally, the use of slag can be used effectively in terms of economy and frost durability of the concrete designated for gutter.

  • PDF

알코올 첨가에 의한 저식염 고추장의 양조 (Trial Manufacture of Low-Salted Kochuzang(Red Pepper Soybean Paste) by the Addition of Alcohol)

  • 이갑상;김동한
    • 한국식품과학회지
    • /
    • 제17권3호
    • /
    • pp.146-154
    • /
    • 1985
  • 사입시에 고추장 중량에 대해 4%(V/W)의 알코올을 첨가하여 무염 및 저식염의 고추장을 만들고, 그의 품질적 특징을 해석했다. 효소(${\alpha}$, ${\beta}$-amylase 및 protease)의 역가는 알코올 첨가시 식염농도가 낮은구에서 활성이 높았다. 수분은 각 시험구간에 큰차이가 없으며, 식염은 알코올 첨가구에서 숙성후기에 약간 높았다. 총당과 pH의 변화는 알코올 무첨가와 식염농도가 낮을수록 심하였으며, 적정산도는 알코올 무첨가시 현저히 증가하였으며, 식염농포가 낮은구는 담금초기에 급격히 증가하였다. 환원당은 알코올 첨가구에서 현저히 증가하였고 식염농도가 낮을수록 적게 증가하였다. 알코올 함량은 알코올 첨가시 큰변화는 없으나 알코올 무첨가구는 증가하여 2% 내외에 달하며, 식염농도가 낮은구에서 알코올 생성이 많았다. 총질소량은 큰 변화가 없으나, $NH_2$-N와 $NH_3$-N는 알코올 첨가구에 비하여 무첨가구에서 높고 식염량이 낮을수록 많았다. 고추장 숙성후 맛, 향기, 색 모두 알코올 첨가구가 우수하였고, 이때 식염농도는 대조구의 60%(고추장중에 5.1%)이었다. 따라서 감염고추장 제조시 알코올 첨가가 바람직하다고 본다.

  • PDF

초고층 건축물 매트 기초용 고성능 콘크리트 내구성 평가 (Durability Evaluation of High-Performance, Low-Heat Self-Compacting Concrete for Foundation of Tall Buildings)

  • 김영봉;박동천
    • 한국건축시공학회지
    • /
    • 제22권5호
    • /
    • pp.425-430
    • /
    • 2022
  • 초고층 건축물용 매트기초에 사용되는 콘크리트는 시공성 및 품질확보를 위하여 일체타설로 진행되는 경우가 많다. 하지만 일체타설의 경우 수화반응 과정에서 온도균열이 발행할 우려가 높으며 혼화재 치환을 통해 고성능 고내구성 콘크리트 최적배합을 도출할 필요가 있다. 본 연구에서는 저자의 기존연구에서 도출한 최적 고성능 저발열 콘크리트 배합으로 제작된 시험체를 대상으로 염해 및 탄산화, 내황산염에 대한 실험을 실시하고 염소이온 확산계수와 탄산화계수, 황산염에 대한 시멘트 매트릭스의 저항을 정량적으로 평가하였다. 혼화재의 혼입에 의한 잠재수경성 및 포졸란 반응에 의한 높은 저항성을 확인할 수 있었다.

광물질혼화재 혼합 모르타르의 해수침식 저항성 (Seawater Attack Resistance of Mortars Containing Mineral Admixtures)

  • 문한영;이승태;최강식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.527-530
    • /
    • 2002
  • In the present study, immersion test using artificial seawater was performed to evaluate the resistance of mortar specimens with or without ground granulated blast-furnace slag (SG) and fly ash (FA). Another variable was the fineness levels of SG (4,450, 6,000 and 8,000 ㎠/g). From the results of the immersion test for 270 days of exposure, the excellent resistance to seawater attack for SG mortar mixtures, especially in a high fineness levels, was confirmed. However, the reductions in compressive strength of FA mortar specimens was similar to those of OPC mortar specimens irrespective of replacement of FA.. In order to understand the deterioration mechanism due to seawater attack, X-ray diffraction (XRD) analysis were also carried out. Some reactants such as ettringite, gypsum, brucite and Friedel's salt were possibly detected through XRD technique.

  • PDF

해양환경에 노출시킨 콘크리트의 내염성능 평가 (An Experimental Study on the Salt Resistance Properties with Concrete Materials under Marine Environment)

  • 고정재;김영웅;김동철;신도철;김상용;변대봉
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.790-793
    • /
    • 2004
  • The factors influencing concrete deterioration in marine environment can be generally divided into the physical and chemical action. The physical attack due to drying and wetting would increase the internal stress of concrete. The chemical attack resulting from the diffusion of ions$(i,e,\;Cl^-,SO_4^{2-},Mg^+)$ from seawater through the pores in concrete. The objective of this study is to evaluate corrosion characteristics of steel when using the various concrete materials under marine exposure environment. After 3 years of exposure, concrete specimen incorporating $40\%$ blast-furnace slag as replacement for type I cement with low w/c ratio of 0.42 and using the inhibitor shows excellent performance.

  • PDF

Development of Lighting Compressed by Injection Yellow Ocher Soil

  • Kwak, Woo-Seob
    • 한국가구학회지
    • /
    • 제19권6호
    • /
    • pp.452-459
    • /
    • 2008
  • The compressed injection yellow ocher soil is the process-technology by drying the product through sunshine, not by firing like pottery and ceramic ware. It is the technology of development being able to achieve the far infrared ray and humidity adjustment by adding recycling paper, Korean paper and bamboo salt, and it corresponds with the construction enforcement ordinance 2007 as an interior-finishing product which is fire-resistant. In case that the yellow ocher soil would be used as lighting device and interior-finishing material and decoration, it could contribute to an improvement of National Health by avoiding the sick house syndrome and adding humidity adjustment, and it has more efficient economic effect due to using recycle-available additives. Through such developments of the yellow ocher soil products the domestic market of lighting device and construction material can be advanced and the replacement effect of imported goods & also export effect can be expected accordingly.

  • PDF

해양환경에 폭로한 콘크리트의 내염특성에 대한 실험적 연구 (폭로기간 : 5년) (An Experimental Study on the Salt Resistance Properties with Concrete Materials under Marine Environment (Exposure period : 5 years))

  • 김용철;석준열;신도철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계 학술발표회 논문집(II)
    • /
    • pp.169-172
    • /
    • 2006
  • The IIA structures exposed to marine environment is subject to many different types of potential attack. The physical attack due to drying and wetting would increase the internal stress of concrete. The chemical attack resulting from the diffusion of ions$(Cl^-,SO_4^{2-},Mg^+)$ from seawater through the pores in concrete. Therefore the sea water resistance of concrete must be considered when it is used for structure in the ocean. The objective of this study is to evaluate chloride diffusion and corrosion characteristics of concrete when using the various concrete materials under marine environment. After 5 years of exposure, concrete incorporating 40% blast-furnace slag as replacement for type I cement with low w/c ratio of 0.42 and using the inhibitor shows excellent performance.

  • PDF

장기폭로실험에 의한 철근콘크리트구조물 보수재료$\cdot$공법의 철근부식특성 평가 (A Study on the Reinforcement Corrosion Evaluation of Repair Material and Method for Reinforced Concrete Structure by Long Term Exposure Experiment)

  • 김영선;이의배;김영덕;조봉석;김재환;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.197-200
    • /
    • 2005
  • In this study, for the establishment of the performance evaluation methods and the quality control standards of durability recovery method, the quantitative exposure data by long term exposure test under the coast is accumulated and analyzed Investigating and evaluating the result of exposure test at 30 month of exposure age under the coastal environment, carbonation and salt damage are not happened at all but the difference in electric potential are found. Therefore, it is considered that the reinforcement corrosion at replacement with repair material are caused by active-passive corrosion macrocells.

  • PDF