은비가 다른 Bi-2223 고온초전도 팬케이크 코일의 히트펄스에 대하 안정성 (Stability Against Heat Pulse for Bi-2223 HTS Pancake Coils with Different Ag/SC Ratio)

  • 장현만;오상수;하홍수;하동우;류강식;김상현
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제1권2호
    • /
    • pp.43-48
    • /
    • 1999
  • The normal zone propagation (NZP) velocity and V-I characteristics of two Bi-2223 pancake coils with different Ag/SC ratio were investigated based on the experimental results and broad resistive transition were obesved in two coils. The measured NZP velocity of coil was found to be faster due to increase of Ag/SC ratio, and agree well with calculated data from two dimensional heat balance equation.

  • PDF

펄스폭 변조 직렬공진 컨버터의 제어연구 (Control Methods of the Pulse-Width Modualted Series Resonant Converter(PWN-SRC))

  • 최현철
    • 전력전자학회논문지
    • /
    • 제4권5호
    • /
    • pp.397-404
    • /
    • 1999
  • 본 연구에서는 선형화 소신호 모델을 이용하여 불연속 모드 펄스폭 공진회로의 다양한 제어방법에 대하여 조사 하였다. 각 제어방식에 따른 시스템의 안정도와 동적 특성을 분석하기 위하여 정규화 출력 전류와 전압을 사용한 근궤적을 나타내었다. 또한, 최적의 궤적 특성을 가지는 제어기를 새로이 제안하였으며, 이러한 제어의 우수한 특성을 다른 형태의 제어방식과 비교함으로써 입증하였다.

  • PDF

DC 스퍼터법과 비대칭 바이폴라 펄스 DC 스퍼터법으로 증착된 TiN 코팅막의 물성 비교연구 (A Comparative Study of TiN Coatings Deposited by DC and Pulsed DC Asymmetric Bipolar Sputtering)

  • 전성용
    • 한국표면공학회지
    • /
    • 제44권5호
    • /
    • pp.179-184
    • /
    • 2011
  • This work investigated the effect of duty cycle and pulse frequency on the microstructures and properties of titanium nitride thin films deposited by asymmetric bipolar pulsed DC sputtering system. Oscilloscope traces of the I-V waveforms indicate high power and high current density outputs during the asymmetric bipolar pulsed mode. The grain size decreases with decreasing duty cycle. The duty cycle has a strong influence not only on the microstructural properties but also on the mechanical properties of titanium nitride films. Comparing with the continuous DC sputtering, the titanium nitride films prepared by pulsed DC asymmetric bipolar process exhibit better properties.

고전압 펄스형 전원을 사용한 질소레이저의 자체 선전리 효과 (Self-Preionization Effects of the Nitrogen Laser Using High Voltage Pulse Power Suply)

  • 이치원;안근옥;추한태;양준묵
    • 한국광학회지
    • /
    • 제1권2호
    • /
    • pp.169-177
    • /
    • 1990
  • 레이저관내에 별도의 전극을 설치하지 않고 레이저전극 자체만으로 선전리 효과를 얻을 수 있는 질소레이저를 연구하였다. 이를 위하여 펄스형 전원과 고속고전압 방전간극을 사용하는 레이저를 제작하였으며, 레이저관 양단에는 저항 또는 인덕터를 연결하여 이들이 레이저 동작특성에 미치는 영향과 자체 선전리 효과를 함께 연구하였다.

  • PDF

다중회귀모형을 이용한 벤츄리가 없는 충격기류식 여과집진장치 압력손실 예측 (Pressure Drop Predictions Using Multiple Regression Model in Pulse Jet Type Bag Filter Without Venturi)

  • 서정민;박정호;조재환;진경호;정문섭;이병인;홍성철;시바쿠마르;최금찬
    • 한국환경과학회지
    • /
    • 제23권12호
    • /
    • pp.2045-2056
    • /
    • 2014
  • In this study, pressure drop was measured in the pulse jet bag filter without venturi on which 16 numbers of filter bags (Ø$140{\times}850{\ell}$) are installed according to operation condition(filtration velocity, inlet dust concentration, pulse pressure, and pulse interval) using coke dust from steel mill. The obtained 180 pressure drop test data were used to predict pressure drop with multiple regression model so that pressure drop data can be used for effective operation condition and as basic data for economical design. The prediction results showed that when filtration velocity was increased by 1%, pressure drop was increased by 2.2% which indicated that filtration velocity among operation condition was attributed on the pressure drop the most. Pressure was dropped by 1.53% when pulse pressure was increased by 1% which also confirmed that pulse pressure was the major factor affecting on the pressure drop next to filtration velocity. Meanwhile, pressure drops were found increased by 0.3% and 0.37%, respectively when inlet dust concentration and pulse interval were increased by 1% implying that the effects of inlet dust concentration and pulse interval were less as compared with those changes of filtration velocity and pulse pressure. Therefore, the larger effect on the pressure drop the pulse jet bag filter was found in the order of filtration velocity($V_f$), pulse pressure($P_p$), inlet dust concentration($C_i$), pulse interval($P_i$). Also, the prediction result of filtration velocity, inlet dust concentration, pulse pressure, and pulse interval which showed the largest effect on the pressure drop indicated that stable operation can be executed with filtration velocity less than 1.5 m/min and inlet dust concentration less than $4g/m^3$. However, it was regarded that pulse pressure and pulse interval need to be adjusted when inlet dust concentration is higher than $4g/m^3$. When filtration velocity and pulse pressure were examined, operation was possible regardless of changes in pulse pressure if filtration velocity was at 1.5 m/min. If filtration velocity was increased to 2 m/min. operation would be possible only when pulse pressure was set at higher than $5.8kgf/cm^2$. Also, the prediction result of pressure drop with filtration velocity and pulse interval showed that operation with pulse interval less than 50 sec. should be carried out under filtration velocity at 1.5 m/min. While, pulse interval should be set at lower than 11 sec. if filtration velocity was set at 2 m/min. Under the conditions of filtration velocity lower than 1 m/min and high pulse pressure higher than $7kgf/cm^2$, though pressure drop would be less, in this case, economic feasibility would be low due to increased in installation and operation cost since scale of dust collection equipment becomes larger and life of filtration bag becomes shortened due to high pulse pressure.

Characterization of a Micro-Laser-Plasma Electrostatic-Acceleration Hybrid-Thruster

  • Akira Igari;Masatoshi Kawakami;Hideyuki Horisawa;Kim, Itsuro ura
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2004년도 제22회 춘계학술대회논문집
    • /
    • pp.271-277
    • /
    • 2004
  • As one of the concepts of the laser/electric hybrid propulsion system, a feasibility study on possibilities of electrostatic acceleration of a laser ablation plasma induced from a solid target was conducted. Energy distributions of accelerated ions were measured by a Faraday cup. A time-of-flight measurement was also conducted for ion velocity measurement. It was found that an average speed of ions from a pure laser ablation in this case was about 20 km/sec for pulse energy of 40 $\mu$J/pulse with pulse width of 250 psec. On the other hand, through an electrostatic field with a + I ,000 V electrode, the speed could be accelerated up to 40 km/sec. It was shown that the electrode with positive potential was more effective than that with negative potential for positive-ion acceleration in laser induced plasma, or pulsed plasma, in which ions were induced with the Coulomb explosion following electrons. In addition, the ion-acceleration or deceleration strongly depended on conditions of pairs of inner diameter and electrodes gap.

  • PDF

Experimental Investigation of Output Current Variation in Biased Silicon-based Quadrant Photodetector

  • Liu, Hongxu;Wang, Di;Li, Chenang;Jin, Guangyong
    • Current Optics and Photonics
    • /
    • 제4권4호
    • /
    • pp.273-276
    • /
    • 2020
  • We report on the relationship between output current for quadrant photodetector (QPD) and bias voltage in silicon-based p-i-n (positive-intrinsic-negative) QPD examined using millisecond pulse laser (ms pulse laser) irradiation. The mechanism governing the relationship was further studied experimentally. The output current curves were obtained by carrying out QPD under different bias voltages (0-40 V) irradiated by ms pulse laser. Compared to other photodetectors, the relaxation was created in the output current for QPD which is never present in other photodetectors, such as PIN and avalanche photodetector (APD), and the maximum value of relaxation was from 6.8 to 38.0 ㎂, the amplitude of relaxation increases with bias value. The mechanism behind this relaxation phenomenon can be ascribed to the bias voltage induced Joule heating effect. With bias voltage increasing, the temperature in a QPD device will increase accordingly, which makes carriers in a QPD move more dramatically, and thus leads to the formation of such relaxation.

[$Na^+-Ca^{2+}$ Exchange Curtails $Ca^{2+}$before Its Diffusion to Global $Ca^{2+}{_i}$ in the Rat Ventricular Myocyte

  • Ahn, Sung-Wan;Ko, Chang-Mann
    • The Korean Journal of Physiology and Pharmacology
    • /
    • 제9권2호
    • /
    • pp.95-101
    • /
    • 2005
  • In the heart, $Na^{+}-Ca^{2+}$ exchange (NCX) is the major $Ca^{2+}$ extrusion mechanism. NCX has been considered as a relaxation mechanism, as it reduces global $[Ca^{2+}]_i$ raised during activation. However, if NCX locates in the close proximity to the ryanodine receptor, then NCX would curtail $Ca^{2+}$ before its diffusion to global $Ca^{2+}_i$ This will result in a global $[Ca^{2+}]_i$ decrease especially during its ascending phase rather than descending phase. Therefore, NCX would decrease the myocardial contractility rather than inducing relaxation in the heart. This possibility was examined in this study by comparing NCX-induced extrusion of $Ca^{2+}$ after its release from SR in the presence and absence of global $Ca^{2+}_i$ transient in the isolated single rat ventricular myocytes by using patch-clamp technique in a whole-cell configuration. Global $Ca^{2+}_i$ transient was controlled by an internal dialysis with different concentrations of BAPTA added in the pipette. During stimulation with a ramp pulse from +100 mV to -100 mV for 200 ms, global $Ca^{2+}_i$ transient was suppressed only mildly, and completely at 1 mmol/L, and 10 mmol/L BAPTA, respectively. In these situations, ryanodine-sensitive inward NCX current was compared using $100{\mu}mol/L$ ryanodine, $Na^+$ depletion, 5 mmol/L $NaCl_2$ and $1{\mu}mol/L$ nifedipine. Surprisingly, the result showed that the ryanodine-sensitive inward NCX current was well preserved after 10 mmol/L BAPTA to 91 % of that obtained after 1 mmol/L BAPTA. From this result, it is concluded that most of the NCX-induced $Ca^{2+}$ extrusion occurs before the $Ca^{2+}$ diffuses to global $Ca^{2+})i$ in the rat ventricular myocyte.

$Bi_2O_3$치환에 따른 $(Pb_{1-2x/3}Bi_x)[(Ni_{1/3}Nb_{2/3})_{0.4}(Ti_{0.6}Zr_{0.4})_{0.6}]O_3$ 세라믹스의 압전 및 전계유기 왜형 특성 (Piezoelectric and Electro-induced Strain Properties of $(Pb_{1-2x/3}Bi_x)[(Ni_{1/3}Nb_{2/3})_{0.4}(Ti_{0.6}Zr_{0.4})_{0.6}]O_3$Ceramics with the Substitution of $Bi_2O_3$)

  • 윤현상;정회승;임인호;윤광희;김준한;박창엽
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권5호
    • /
    • pp.434-439
    • /
    • 1997
  • It this paper, the piezoelectric and electro-induced strain properties of (P $b_{1-}$2x/3/B $i_{x}$ )[N $i_{1}$3/N $b_{2}$3/)$_{0.4}$( $Ti_{0.6}$Z $r_{0.4}$)$_{0.6}$] $O_3$ceramics (x=0, 0.005, 0.02) were investigated with the substitution of B $i^{3+}$, and the feasibility of the application for bimorph actuator was evaluated by measuring the dynamic properties of the piezoelectric bimorph fabricated with above ceramics. Dielectric constant was enhanced with the increase of B $i^{3+}$ substitution, and appeared the maximum value of 5032 at x=0.01 composition. Increasing the substitution of B $i^{3+}$, the electromechanical coefficient( $k_{p}$ , $k_{31}$ ) was increased up to the substitution of 0.5 mol% B $i^{3+}$, showed the value of 0.656, 0.439, respectively. The piezoelectric constant( $d_{33}$ $d_{31}$ ) had the highest value of 344, 825 with the substitution of 0.5 mol% B $i^{3+}$. The strain, generated by 60 Hz AC electric field, had the largest value of 1200($\times$10$^{-6}$ $\Delta$1/1) in the composition with the substitution of 0.5 mol% B $i^{3+}$. The dynamic properties of the bimorph actuator, fabricated with the composition substitution of 0.5 mol% B $i^{3+}$, showed the largest value of 325 $\mu$m at $\pm$150 V square pulse. square pulse.are pulse..

  • PDF

Trade-off Characteristic between Gate Length Margin and Hot Carrier Lifetime by Considering ESD on NMOSFETs of Submicron Technology

  • Joung, Bong-Kyu;Kang, Jeong-Won;Hwang, Ho-Jung;Kim, Sang-Yong;Kwon, Oh-Keun
    • Transactions on Electrical and Electronic Materials
    • /
    • 제7권1호
    • /
    • pp.1-6
    • /
    • 2006
  • Hot carrier degradation and roll off characteristics of threshold voltage ($V_{t1}$) on NMOSFETs as I/O transistor are studied as a function of Lightly Doped Drain (LDD) structures. Pocket dose and the combination of Phosphorus (P) and Arsenic (As) dose are applied to control $V_{t1}$ roll off down to the $10\%$ gate length margin. It was seen that the relationship between $V_{t1}$ roll off characteristic and substrate current depends on P dopant dose. For the first time, we found that the n-p-n transistor triggering voltage ($V_{t1}$) depends on drain current, and both $I_{t2}$ and snapback holding voltage ($V_{sp}$) depend on the substrate current by characterization with a transmission line pulse generator. Also it was found that the improved lifetime for hot carrier stress could be obtained by controlling the P dose as loosing the $V_{t1}$ roll off margin. This study suggests that the trade-off characteristic between gate length margin and channel hot carrier (CHC) lifetime in NMOSFETs should be determined by considering Electrostatic Discharge (ESD) characteristic.