• Title/Summary/Keyword: piezoelectric constant

Search Result 477, Processing Time 0.029 seconds

Dielectric and Piezoelectric Characteristics of PMN-PNN-PZT Ceramics with the methods of $MnO_2$ additon ($MnO_2$ 첨가방법에 따른 PMN-PNN-PZT 세라믹스의 유전 및 압전특성)

  • Kim, Do-Hyung;Kim, Kook-Jin;Yoo, Ju-Hyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.255-256
    • /
    • 2007
  • In the study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics were fabricated using $Na_2CO_3,\;Li_2CO_3$ as sintering aids and their dielectric and piezoelectric properties were investigated according to the variations of $MnO_2$ as additives and sintering aids. At the sintering temperature of $900^{\circ}C$ and 0.1wt% $MnO_2$ as sintering aids, density, electromechanical coupling factor$(k_p)$, mechanical quality factor$(Q_m)$, piezoelectric constant$(d_{33})$, and dielectric constant $({\varepsilon}_r)$ showed the optimum value of $7.87[g/cm^3]$, 0.61, 1131, 1127 and 376, respectively, for multilayer piezoelectric actuator application.

  • PDF

Dielectric and Piezoelectric Properties of (Na0.5K0.5)0.97NbO3 Ceramics Substituted with CeMnO3 (CeMnO3 치환된 (Na0.5K0.5)0.97NbO3 세라믹스의 유전 및 압전 특성)

  • Oh, Young-Kwang;Yoo, Ju-Hyun;Mah, Suk-Burm;Jeong, Yeong-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.3
    • /
    • pp.194-199
    • /
    • 2011
  • In this study, non-stoichiometric 1-x$[(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3]$ + x $CeMnO_3$ + 0.8 mol%CuO + 0.2 wt% $Ag_2O$ (x=0, 0.005) ceramics were prepared by a conventional mixed oxide and carbonate method, their dielectric and piezoelectric properties were investigated with the variations of sintering temperature. As $CeMnO_3$ substitution incereased, the density, piezoelectric constant($d_{33}$) and dielectric constant($\varepsilon_r$) were increased and the mechanical quality factor(Qm) was decreased. At the sintering temperature of $1100^{\circ}C$, the density, electromechanical coupling factor($k_p$), dielectric constant($\varepsilon_r$) and piezoelectric constant($d_{33}$) of 0.5mol% $CeMnO_3$ specimen showed the optimun values of 4.475 $g/cm^2$, 0.437, 552 and 166 pC/N, respectively. However, the mechanical quality factor($Q_m$) showed the minimum value of 380.

Characteristics of PAN-PZI Ceramics with $BaCO_3$Addition ($BaCO_3$ 첨가량에 따른 PAN-PZT계 세라믹스의 특성)

  • 박타리;이동균;최지원;김현재;윤석진;조봉희;고태국
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.981-984
    • /
    • 2001
  • The piezoelectric properties of 0.05pb(A $l_{0.5}$N $b_{0.5}$) $O_3$-0.95Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$+0.7wt%N $b_2$ $O_{5}$ +0.5wt%Mn $O_2$ceramics with the additives of BaC $O_3$were investigated. For the additions of BaC $O_3$, the dielectric constant ($\varepsilon$$^{T}$ $_{33}$ ), the piezoelectric constant ( $d_{33}$ ), the electromechanical coupling factor ( $k_{p}$ ), and . the mechanical quality factor ( $Q_{m}$ ) were increased, but dielectric loss (tan$\delta$) was decreased. The highest piezoelectric properties and dielectric properties were observed at the sintered temperature of 120$0^{\circ}C$ and 0.4 wt% of BaC $O_3$, and the properties of $d_{33}$ , $k_{p}$ , and $Q_{m}$ were 339(x10$^{-12}$ C/N), 59% and 1754, respectively.vely.y.y.

  • PDF

FEM Analysis on the Characteristics of Piezoelectric Ceramics Using $L_{1}-B_{4}$ Vibration mode ($L_{1}-B_{4}$ 진동모드를 이용하는 압전 세라믹스의 유한요소 해석)

  • 김범진;정동석;김태열;박태곤;김명호
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.393-397
    • /
    • 2001
  • A linear ultrasonic motor was designed by a combination of the first longitudinal and fourth bending mode, the motor consisted of a straight aluminum alloys bar bonded with a piezoelectric ceramics element as a driving element. That is, L$_1$-B$_4$ linear ultrasonic motor can be constructed using a multi-mode vibrator of longitudinal and bending modes. The simulation with variation of material characteristics of piezoceramic were performed as use of finite element analysis ANSYS 5.5, such as elastic compliance, piezoelectric constant, electro-mechanical coupling coefficient, poisson's ratio and density. The results of simulation, elastic compliance constant s$_{11}$ and piezoelectric constant d$_{31}$ had the most of influence on the elliptic-motion. This results consist with using transverse effect of material. The used motor were piezoceramics of 4 layers, and the dimensions were 65$\times$5$\times$3.5mm(LxWxt).).

  • PDF

A Study on the Properties of the Low Temperature Sintered Piezoelectrics for Actuator Application (압전 액츄에이터에 활용할 저온소결 압전 세라믹스에 관한 연구)

  • Ryu, Sung-Lim;Lee, Sang-Ho;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.3
    • /
    • pp.232-235
    • /
    • 2008
  • In this study, in order to develop the composition ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$, $Na_2CO_3$, ZnO as sintering aids and their piezoelectric and dielectric properties were investigated according to the Bi substitution, Bi substitution induced grain growth and increase of sinterablity, And also, Bi substitution suppress secondary phase due to the liquid phase sintering effect. Bi substitution enhanced electromechanical coupling factor ($k_p$) and dielectric constant ($\varepsilon_r$), However, mechanical quality factor($Q_m$) was deteriorated, At the sintering temperature of 870 $^{\circ}C$ and Bi substitution of 1 mol%, density, electromechanical coupling factor ($k_p$), mechanical quality factor ($Q_m$), Dielectric constant ($\varepsilon_r$) and piezoelectric constant ($d_{33}$) of specimen showed the optimum values of 7,878 $g/cm^3$, 0,608, 835, 1603 and 397 pC/N, respectively for multilayer piezoelectric actuator application.

A Study on the Low Temperature Sintering Piezoelectric Ceramics for Piezoelectric Actuator Application (압전 액츄에이터에 활용할 저온소결 압전 세라믹스에 관한 연구)

  • Ryu, Sung-Lim;Lee, Yu-Hyung;Lee, Sang-Ho;Yoo, Ju-Hyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.277-278
    • /
    • 2007
  • In this study, in order to develop multilayer piezo-actuator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3,\;Na_2CO_3$, ZnO as sintering aids and their piezoelectric and dielectric properties were investigated according to the Bi substitution. Bi substitution enhanced electromechanical coupling factor$(k_p)$ and dielectric constant$({\varepsilon}_r)$. However, mechanical quality factor was deteriorated. At the sintering temperature of $870^{\circ}C$ and Bi substitution of 1mol%, density, electromechanical coupling factor$(k_p)$, mechanical quality factor$(Q_m)$, Dielectric constant$({\varepsilon}_r)$ and piezoelectric constant$(d_{33})$ of specimen showed the optimum value of $7.878g/cm^3$, 0.608, 835, 1603 and 397pC/N, respectively.

  • PDF

A Study on the Dielectric and Piezoelectric Properties of xPb($Y_{1/2}Ta_{1/2})O_3-(1-x)Pb(Zr_{0.52}Ti_{0.48})O_3$Ceramics (xPb($Y_{1/2}Ta_{1/2})O_3-(1-x)Pb(Zr_{0.52}Ti_{0.48})O_3$ 세라믹스의 유전 및 압전 특성에 관한 연구)

  • 강도원;김태열;김범진;김명호;박태곤
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.294-296
    • /
    • 1999
  • Solid solution ceramics having various ratios between xPb( $Y_{1}$2/T $a_{1}$2/) $O_3$ and Pb(Z $r_{0.52}$ $Ti_{0.48}$) $O_3$were synthesized by a conventional solid state reaction for well sintered specimens, dielectric and piezoelectric prperties were studied as a function of composition. The dielectric constant of PYT-PZT ceramics of 4 mol% PYT was 1,424 at room temperature. The maximum value of electromechanical couping facotr $k_{p}$ of 51% $k_{t}$ of 30% were obtained at the composition of 4 mol% PYT, howerver mechanical quality factor( $Q_{m}$) had a minimum value of 69 at 4 mol% PYT. Also the maximum value of piezoelectric constant of $D_{33}$(310[pC/N]) and $d_{31}$(-131[pC/N]) were obtained at the composition of 4 mol% PYT content.ntent.t.t.t.

  • PDF

Sensitivity Properties of Acoustic Emission Sensor Using NKN System Ceramics (NKN계 세라믹을 이용한 음향방출 센서의 감도 특성)

  • Hong, Jae-Il;Shin, Sang-Hoon;Yoo, Ju-Hyun;Jeong, Yeong-Ho;Lee, Sang-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.11
    • /
    • pp.696-701
    • /
    • 2014
  • In this study, in order to develop coupled vibration mode piezoelectric devices for Acoustic Emission (abbreviated as AE) sensor application with outstanding displacement and piezoelectric properties have been simulated by ATILA FEM program. And, From the results of ATILA simulation, the AE sensor specimen, obtained superior electromechanical coupling factor and displacement, when the size of specimen is $3.45mm{\Phi}{\times}3.45mm$ with ratio of diameter/thickness(${\Phi}/T$)= 1.0. Therefore, AE sensor was fabricated by (Na,K,Li)(Nb,Ta) $O_3$(abbreviated as NKL-NT) system piezoelectric ceramics using coupled vibration mode. The piezoelectric properties of NKL-NT ceramics was exhibited that piezoelectric constant($d_{33}$), piezoelectric voltage constant($g_{33}$) and electro mechanical coupling factor($k_p$) have the excellent values of 261[pC/N], 40.10[$10^{-3}Vm/N$], and 0.44, respectively. The manufactured piezoelectric device with ratio of ${\Phi}/T$= 1.0 indicated the optimum values of resonant frequency(fr)= 556.5[kHz], antiresonant frequency(fa)=631.1[kHz], and effective electromechanical coupling factor(keff)= 0.473. The maximum sensitivity of the coupled vibration mode AE sensor was 55[dB] at the resonant frequency of 75[kHz]. The results show that the coupled vibration mode piezoelectric device is a promising candidate for the application AE sensor piezoelectric device.

Piezoelectric and Dielectric Properties of NKN-(1-x)BNT-xBT Ceramics (NKN-(1-x)BNT-xBT 세라믹스의 압전 및 유전특성)

  • Lee, Seung-Hwan;Nam, Sung-Pill;Lee, Sung-Gap;Lee, Young-Hie
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.10
    • /
    • pp.771-775
    • /
    • 2010
  • In this study, piezoelectric and dielectric properties of the $(Na_{0.5}K_{0.5})NbO_3-(1-x)(Bi_{0.5}Na_{0.5})TiO_3-xBaTiO_3$ [NKN-(1-x)BNT-xBT] ceramics were investigated. The lead-free NKN-(1-x)BNT-xBT ceramics were fabricated by a conventional mixed oxide method. The results indicate that the addition of $BaTiO_3$ significantly influences the sintering, microstructure, phase transition and electrical properties of NKN-BNT ceramics. A gradual change in the piezoelectric and dielectric properties was observed with the increase of BT contents. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased at the morphotropic phase boundary (MPB). The $d_{33}$=184 pC/N, $k_p$=0.38, dielectric constant=1455 with dielectric loss value of less than 1% were obtained for the NKN-0.95BNT-0.05BT ceramics sintered at $1150^{\circ}C$ for 2h. These results demonstrate that the NKN-(1-x)BNT-xBT ceramics is an attractive candidate for lead-free piezoelectric materials.

Piezoelectric Properties of Pb-free Bi(Na,K)TiO3-SrTiO3 Ceramics with the Amount of La2O3 Addition (La2O3첨가에 따른 무연 Bi(Na,K)TiO3-SrTiO3 세라믹스의 압전 특성)

  • 류주현;이현석;박창엽;정광현;이덕출;정영호;홍재일
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.8
    • /
    • pp.830-834
    • /
    • 2004
  • In this study, lead-free pirzoelectric ceramics were investigated for pressure sensor applications as a function of the amount of ${La}_2{O}_3$ addition at $Bi(Na, K)Ti{O}_3-SrTi{O}_3$system. With increasing the amount of addition, the density and dielectric constant increased up to 0.9 wt% ${La}_2{O}_3$ addition and decreased above 0.9 wt% ${La}_2{O}_3$addition. Electromechanical coupling factor( $K_{P}$) showed the maximum value at 0.2 wt% ${La}_2{O}_3$addition and decreased above 0.2 wt% ${La}_2{O}_3$ addition. Electromechanical coupling $factor{(K)}_P$, density, dielectric constant$(\varepsilon_\Gamma)$, piezoelectric constant$(d_33)$ and curie temperature$(T_C)$ showed optimum value of 0.40, 5.75 g/㎤, 768, 215 pC/N and 320 $^{\circ}C$ at 0.2 wt%${La}_2{O}_3$addition, respectively.