Non-PR direct bumping for 3D wafer stacking (3차원 실장을 위한 Non-PR 직접범핑법)

  • Jeon, Ji-Heon;Hong, Seong-Jun;Lee, Gi-Ju;Lee, Hui-Yeol;Jeong, Jae-Pil
    • Proceedings of the KWS Conference
    • /
    • 2007.11a
    • /
    • pp.229-231
    • /
    • 2007
  • Recently, 3D-electronic packaging by TSV is in interest. TSV(Through Silicon Via) is a interconnection hole on Si-wafer filled with conducting metal such as Copper. In this research, chips with TSV are connected by electroplated Sn bump without PR. Then chips with TSV are put together and stacked by the methode of Reflow soldering. The stacking was successfully done and had no noticeable defects. By eliminating PR process, entire process can be reduced and makes it easier to apply on commercial production.

  • PDF

High-Speed Cu Filling into TSV and Non-PR Bumping for 3D Chip Packaging (3차원 실장용 TSV 고속 Cu 충전 및 Non-PR 범핑)

  • Hong, Sung-Chul;Kim, Won-Joong;Jung, Jae-Pil
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.18 no.4
    • /
    • pp.49-53
    • /
    • 2011
  • High-speed Cu filling into a through-silicon-via (TSV) and simplification of bumping process by electroplating for three dimensional stacking of Si dice were investigated. The TSV was prepared on a Si wafer by deep reactive ion etching, and $SiO_2$, Ti and Au layers were coated as functional layers on the via wall. In order to increase the filling rate of Cu into the via, a periodic-pulse-reverse wave current was applied to the Si chip during electroplating. In the bumping process, Sn-3.5Ag bumping was performed on the Cu plugs without lithography process. After electroplating, the cross sections of the vias and appearance of the bumps were observed by using a field emission scanning electron microscope. As a result, voids in the Cu-plugs were produced by via blocking around via opening and at the middle of the via when the vias were plated for 60 min at -9.66 $mA/cm^2$ and -7.71 $mA/cm^2$, respectively. The Cu plug with a void or a defect led to the production of imperfect Sn-Ag bump which was formed on the Cu-plug.