• Title/Summary/Keyword: nano-powders

Search Result 604, Processing Time 0.082 seconds

Crystallization and Magnetic Properties of Non-Equilibrium Al(Fe-Cu) Alloy Powders Produced by Rod Milling and Chemical Leaching (Rod Milling과 Chemical Leaching에 의해 제작된 비평형 Al(Fe-Cu) 합금 분말의 결정화 및 자기적 특성)

  • Kim Hyun-Goo
    • Journal of Powder Materials
    • /
    • v.11 no.6 s.47
    • /
    • pp.486-492
    • /
    • 2004
  • We report the crystallization and magnetic properties of non-equilibrium $Al_{0.6}(Fe_{x}Cu_{1-x})_{0.4}(x=0.25, 0.50, 0.75)$ alloy powders produced by rod-milling as well as by new chemical leaching. X-ray diffractometry, transmission electron microscopy, differential scanning calorimetry and vibrating sample magnetometry were used to characterize the as-milled and leached specimens. After 400 h or 500 h milling, only the broad peaks of nano bcc crystalline phases were detected in the XRD patterns. The crystallite size, the peak and the crystallization temperatures increased with increasing Fe. After being annealed at $600{^\circ}C$ for 1 h for as-milled alloy powders, the peaks of bcc $AlCu_{4}\;and\;Al_{13}Cu_{4}Fe_{3}\;for\;x=0.25,\;bcc\;AlCu_{4}\;and\;Al_{5}Fe_{2}\;for\;x=0.50,\;and\;Al_{5}Fe_{2},\;and\;Al_{0.5}Fe_{0.5}\;for\;x=0.75$ are observed. After being annealed at $500{^\circ}\;and\;600{^\circ}C$for 1 h for leached specimens, these non-equi-librium phases transformed into fcc Cu and $CuFe_{2}O_{4}$phases for the x=0.25 specimen, and into bcc ${\alpha}-Fe,\;fcc\;Cu,\;and\;CuFe_{2}O_{4}$ phases for both the x=0.50 and the x=0.75 specimens. The saturation magnetization decreased with increasing milling time for $Al_{0.6}(Fe_{x}Cu_{1-x})_{0.4}$ alloy powders. On cooling the leached specimens from $800{\~}850^{\circ}C$,\;the magnetization first sharply increase at about $491.4{\circ}C,\;745{\circ}C,\;and\;750.0{\circ}C$ for x=0.25, x=0.50, and x=0.75 specimens, repectively.

Low Temperature Synthesis of BaCeO3 Nano Powders by the Citrate Process (Citrate Process를 이용한 BaCeO3 나노 분말의 저온 합성)

  • Lee, Dong-Wook;Won, Jong-Han;Joo, Kyoung;Kim, Chang-Yeoul;Shim, Kwang-Bo
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.6
    • /
    • pp.604-609
    • /
    • 2002
  • Nanosized $BaCeO_3$ powders with the stoichiometric composition of a molecular level were synthesized by the citrate process based on the Pechini method. Polymeric precursor was formed by use of citric acid and ethylen glycol, as chelating agent of metal ions and reaction medium, respectively. Single phase orthorhombic structured $BaCeO_3$powders, about 100 nm sized and uniform shaped were obtained through the calcination of the polymeric precursor at $900^{\circ}C$ for 4 h. Extremely small quantities of carbonate ions($CO_^{2-}$) were completely decomposed at over $1100^{\circ}C$. The mean size of the powders was increased twice, however, it has very uniform distribution in its size and shape.

Dielectric Properties of Al2O3 Thick Films Grown by Aerosol Deposition Method (에어로졸 데포지션법으로 성막된 Al2O3 후막의 유전특성)

  • Park, Jae-Chang;Yoon, Young-Joon;Kim, Hyo-Tae;Koo, Eun-Hae;Nam, Song-Min;Kim, Jong-Hee;Shim, Kwang-Bo
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.7
    • /
    • pp.411-417
    • /
    • 2008
  • Aerosol Deposition Method (ADM) is a novel technique to grow ceramic thick films with high density and nano-crystal structure at room temperature. $^{1,2)}$ For these unique advantages of ADM, it would be applied to the fabrication process of 3-D integration ceramic modules effectively. However, it is critical to control the properties of starting powders, because a film formation through ADM is achieved by impaction and consolidation of starting powders on the substrates. We fabricated alumina thick films by ADM for the application to integral substrates for RF modules. When the as-received alumina powders were used as a starting material without any treatments, it was observed that the dielectric properties of as-deposited alumina films, such as relative permittivity and loss tangent, showed high dependency on the frequency. In this study, some techniques of powder pre-treatments to improve the dielectric properties of alumina thick films will be shown and the effects of starting powders on the properties of AD films will be discussed.

A study on Magnetic Properties of BaFe12O19 Fabricated by Ultrasonic Spray-pyrolysis Process Using Self-Assembly Method (자기 조립 전구체를 이용한 초음파 분무 열분해 공정으로 제조한 BaFe12O19의 자기적 특성에 대한 연구)

  • Choi, Moon-Hee;Yu, Ji-Hun;Kim, Dong-Hwan;Chung, Kook-Chae;Kim, Yang-Do
    • Journal of Powder Materials
    • /
    • v.17 no.4
    • /
    • pp.263-269
    • /
    • 2010
  • Hexagonal barium ferrite ($BaFe_{12}O_{19}$) nano-particles have been successfully fabricated by spraypylorysis process. $BaFe_{12}O_{19}$ precursor solutions were synthesized by self-assembly method. Diethyleneamine (DEA) surfactant was used to fabricate the micelle structure of Ba-DEA complex under various DEA concentrations. $BaFe_{12}O_{19}$ powders were synthesized with addition of Fe ions to Ba-DEA complex and then fabricated $BaFe_{12}O_{19}$ powders by spray-pyrolysis process at the temperature range of $800{\sim}1000^{\circ}C$. The molar ratio of Ba/DEA and heat-treatment temperatures significantly affected the magnetic properties and morphology of $BaFe_{12}O_{19}$ powders. $BaFe_{12}O_{19}$ powders synthesized with Ba/DEA molar ratio of 1 and heat-treated at $900^{\circ}C$ showed the coercive forces (iHc) of 4.2 kOe with average crystal size of about 100 nm.

Milling Behaviors of Al-B4C Composite Powders Fabricated by Mechanical Milling Process (기계적 밀링 공정에 의해 제조된 Al-B4C 복합분말의 밀링 거동 연구)

  • Hong, Sung-Mo;Park, Jin-Ju;Park, Eun-Kwang;Lee, Min-Ku;Rhee, Chang-Kyu;Kim, Ju-Myoung;Lee, Jin-Kyu
    • Journal of Powder Materials
    • /
    • v.19 no.4
    • /
    • pp.291-296
    • /
    • 2012
  • In the present work, Al-$B_4C$ composite powders were fabricated using a mechanical milling process and its milling behaviors and mechanical properties as functions of $B_4C$ sizes ( $100{\mu}m$, 500 nm and 50 nm) and concentrations (1, 3 and 10 wt.%) were investigated. For achieving it, composite powders and their compacts were fabricated using a planetary ball mill machine and magnetic pulse compaction technology. Al-$B_4C$ composite powders represent the most uniform dispersion at a milling speed of 200 rpm and a milling time of 240 minutes. Also, the smaller $B_4C$ particles were presented, the more excellent compositing characteristics are exhibited. In particular, in the case of the 50 nm $B_4C$ added compact, it showed the highest values of compaction density and hardness compared with the conditions of $100{\mu}m$ and 500 nm additions, leading to the enhancement its mechanical properties.

The Properties of Mn, Ni, and Al Doped Cobalt Ferrites Grown by Sol-Gel Method

  • Choi, Seung Han
    • Korean Journal of Materials Research
    • /
    • v.28 no.7
    • /
    • pp.371-375
    • /
    • 2018
  • The manganese-, nickel-, and aluminum-doped cobalt ferrite powders, $Mn_{0.2}Co_{0.8}Fe_2O_4$, $Ni_{0.2}Co_{0.8}Fe_2O_4$, and $Al_{0.2}CoFe_{1.8}O_4$, are fabricated by the sol-gel method, and the crystallographic and magnetic properties of the powders are studied in comparison with those of $CoFe_2O_4$. All the ferrite powders are nano-sized and have a single spinel structure with the lattice constant increasing in $Mn_{0.2}Co_{0.8}Fe_2O_4$ but decreasing in $Ni_{0.2}Co_{0.8}Fe_2O_4$ and $Al_{0.2}CoFe_{1.8}O_4$. All the $M{\ddot{o}}ssbauer$ spectra are fitted as a superposition of two Zeeman sextets due to the tetrahedral and octahedral sites of the $Fe^{3+}$ ions. The values of the magnetic hyperfine fields of $Ni_{0.2}Co_{0.8}Fe_2O_4$ are somewhat increased in the A and B sites, while those of $Mn_{0.2}Co_{0.8}Fe_2O_4$ and $Al_{0.2}CoFe_{1.8}O_4$ are decreased. The variation of $M{\ddot{o}}ssbauer$ parameters is explained using the cation distribution equation, superexchange interaction and particle size. The hysteresis curves of the ferrite powders reveal a typical soft ferrite pattern. The variation in the values of saturation magnetization and coercivity are explained in terms of the site distributions, particle sizes and the spin magnetic moments of the doped ions.

Synthesis of Ga2O3 powders by precipitation method (침전법을 이용한 Ga2O3 분말의 합성)

  • Jung, Jong-Yeol;Kim, Sang-Hun;Kang, Eun-Tae;Kim, Jin-Ho;Han, Kyu-Sung;Hwang, Kwang-Teak;Cho, Woo-Seok
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.1
    • /
    • pp.8-14
    • /
    • 2014
  • In this study, we investigated synthesis and characteristics of gallium oxide ($Ga_2O_3$) powders prepared by precipitation method. $Ga_2O_3$ powders were synthesized using $Ga(NO_3)_3$ as a starting material and $NH_4OH$ as a precipitant. The oxidation temperature of $Ga(OH)_3$ and phase transition temperature of $Ga_2O_3$ was revealed using TG-DSC analysis. The crystal structural change of $Ga_2O_3$ powders was investigated by XRD analysis. The morphologies and size distributions of $Ga_2O_3$ particles were analyzed using SEM.

Mechanical Properties and Fabrication of Nanostructured Ti3Al-Al2O3 Composite from Mechanically Synthesized Powders by Pulsed Current Activated Sintering (기계적 합성된 분말로부터 펄스전류활성 소결에 의한 나노구조 Ti3Al-Al2O3 복합재료 제조 및 기계적 특성)

  • Shon, In-Jin;Wang, Hee-Ji;Suh, Chang-Yul;Cho, Sung-Wook;Kim, Wonbaek
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.5
    • /
    • pp.374-379
    • /
    • 2011
  • Nano-powders of $Ti_3Al$ and $2Al_2O_3$ were synthesized from $3TiO_2$ and 5Al powders by high energy ball milling. A nanocrystalline $Al_2O_3$ reinforced composite was consolidated by pulsed current activated sintering within 2 minutes from mechanochemically synthesized powders of $Al_2O_3$ and $Ti_3Al$. Nanocrystalline materials, have received much attention as advanced engineering materials due to their improved physical and mechanical properties. The relative density of the composite was 99.5%. The average obtained hardness and fracture toughness values were 1510 kg/$mm^2$ and $9\;MPa{\cdot}m^{1/2}$, respectively.

Consolidation of Segment Powder for Diamond Tool by Magnetic Pulsed Compaction (자기펄스 압축성형법에 의한 다이아몬드 공구용 세그먼트 분말 성형)

  • Yun, J.S.;Lee, J.G.;Lee, M.K.;Rhee, C.K.;Park, M.S.;Hong, S.J.
    • Journal of Powder Materials
    • /
    • v.15 no.5
    • /
    • pp.378-385
    • /
    • 2008
  • This article presents the successful consolidation of the mixed Co and Diamond powders for a drilling segment by the combined application of magnetic pulsed compaction (MPC) and subsequent sintering, and their properties were analyzed. Homogeneous hardness (Hv 220) and density (97%) of sintered bulks fabricated by MPC were obtained by the new technique, where higher pressure has been employed for short period of time than that of general process. A fine microstructure and homogeneous hardness in the consolidated bulk were observed without cracks. Relatively higher drilling speed of 9.61 cm/min and life time of 6.55 m were found to the MPCed specimens, whereas the value of the specimens fabricated by general process was 11.71 cm/min and 7.96 m, respectively. A substantial improvement of mechanical properties of segment was achieved through this study.